Improved preservative penetration of spruce after pre-treatment with selected fungi. II. Creosote treatment, analysis and strength testing
1998 - IRG/WP 98-40106
This paper describes the creosote treatment and analysis of logs pre-treated with selected fungal agents as a method of increasing the porosity of the wood prior to preservative treatment. The paper also reports the subsequent strength testing of the timber to evaluate the effects of the fungal pre-treatment on the structural integrity of the wood. European spruce logs were pre-treated with eithe...
E J Tucker, A Bruce, H J Staines, B Rosner, K Messner


A field test with anti-stain chemicals on sawn pine timber in Brazil
1989 - IRG/WP 3513
Field tests were carried out in São Paulo State - Brazil, to evaluate pre-treatment formulations of O-Phenyl-Phenol (OPP) based products. The Sodium Pentachlorophenate solution was used as a reference formulation. The treated test blocks were stacked in a covered shed, and in an uncovered place for air drying. The evaluation was done by measuring the percentage of stained surface on each test blo...
M B B Monteiro, S Brazolin


Wood decay of Pinus sylvestris L. and Fagus sylvatica L. by marine fungi. Part 2
1991 - IRG/WP 1471
The water-logged wood conservation requires a good knowledge of the wood decay organims which produce the degradation. Previous conducted studies (ESCORIAL, TROYA, GARCIA DE LOS RIOS, 1990) have shown that the incubation times normally used for in vitro laboratory tests are not sufficients for a significant wood degradation. This has been the reason why the aim of this work was the study of such d...
M T De Troya, A M Navarrete, M C Escorial


Accelerated termicidal performance data for new water-based copper linoleate formulations
1996 - IRG/WP 96-30104
An organic solvent based copper linoleate (Culin) has proved itself as an effective wood preservative in long term field trials in South Africa over a period of 30 years. Whilst the organic solvent based product offers good wood preservative performance, primary industrial interest has been in an emulsified version of the product. The objective of this study was to evaluate the influence of two di...
D Conradie, P Turner


Improved preservative penetration of spruce after pre-treatment with selected fungi. I. Fungal pre-treatment of pole sections
1998 - IRG/WP 98-40117
European spruce logs were pre-treated with either Phanaerochete chrysosporium, Dichomitus squalens, Trichoderma viride and Trichoderma aureoviride for incubation periods of between 1-4 weeks prior to pressure treatment with creosote in a commercial treatment plant and analysed for strength and creosote uptake (see part II Tucker et al.). A method to pre-treat logs was optimised. The pole sections ...
B Rosner, K Messner, E J B Tucker, A Bruce


Artificial weathering as an aid to assessing the effectiveness of chemicals for preventing blue stain in service - a co-operative study
1984 - IRG/WP 2215
The paper reports co-operative studies carried out within Working Group II of the International Research Group on Wood Preservation to assess the effects of different artificial weathering systems on the performance of fungicides to control blue-stain in service. It has been shown that Atlas, Xenotest and Marr equipments operated according to particular standard schedules can give essentially the ...
A F Bravery, D J Dickinson


Silicon tetrachloride: A potential wood preservative
1980 - IRG/WP 3133
In its present form, this paper is a preliminary draft of a paper that will eventually be submitted for publication in the Forest Products Journal. We are continuing the work on the effects of silicon tetrachloride on wood and expect to have additional data for the meeting in May 1980. Specifically we are measuring the penetration rate and depth of SiCl4, and we are chemically analyzing the treate...
C W Owens, W T Shortle, A L Shigo


Leaching from CCA-treated wood submerged in seawater: Effect of high loadings, and a comparison between laboratory and marine conditions
1996 - IRG/WP 96-50080
This study of leaching examined the following variables: CCA loading; marine versus laboratory exposure and length of submergence. Blocks of Pinus sylvestris were treated to a range of nominal retentions from 15 to 50 kg/m³. Each block was then divided into three cubes and all transverse faces were sealed. All cubes were allowed to fix at ambient temperature for a minimum of one week. One set of ...
R M Albuquerque, S M Cragg, J D Icely


Collaborative soft rot tests: Tests conducted at Princes Risborough and Delft on soil samples from collaborating laboratories
1972 - IRG/WP 210
The laboratories which took part in the original collaborative soft rot test (Savory and Bravery, Holz u Org 5 (1) 58-90, 1970) sent samples of the soil used in the original test to Princes Risborough. Portions of this material were sent to Dr Hof for soil analyses at TNO and the remainder was employed at Princes Risborough for the conduct of comparative tests of soil virulence when used as a comb...
J G Savory


Preservative treatment of rubber wood (Hevea brasiliensis) to increase its service life
2005 - IRG/WP 05-40320
Rubber wood (Hevea brasiliensis) possess excellent properties for interior designing, wood working and furniture making. But it is very much susceptible to sap stain and mould fungi which decreases the service life. For profitable uses , it is necessary to increase the service life of rubber wood. To protect the rubber wood from wood degrading agents, the sawn timber were treated with Borax – b...
K Akhter


Microemulsion formulations for wood protection chemicals
1993 - IRG/WP 93-30030
A microemulsion is a thermodynamically stable oil-water dispersion system. As a formulation it provides many unique features such as water compatibility for water-insoluble chemicals, formulation stability, good bioavailability and environmental acceptance. This paper discusses the major criteria for the formulations of water-insoluble wood biocides and the comparison in properties between convent...
Bing Yu, L E Leightley


Which substrate to use in a laboratory test with soft rot micro-fungi: vermiculite or unsterile soil?
1991 - IRG/WP 2372
A draft European Standard is being proposed by CEN TC 38 in which a vermiculite-burial and a soil-burial test to be carried out in succession are required. Various experiments with both procedures were set up with CCA, CC and propiconazole-formulations. The results show that vermiculite and unsterile soil yield comparable threshold values against soft rot. This poses the question of whether a two-...
A R Valcke


The treatability of five Indonesian wood species with BFCA preservative
1987 - IRG/WP 3428
This paper deals with a preliminary study on the treatability of five Indonesian wood species, i.e. Altingia excelsa (AE), Rhodoleria teysmanii (CA), Litsea odorivera (LO), Schima wallichii (SW) and Cratoxylon arborescens (CA). Wood samples measuring 4 x 4 x 100 cm³ were dipped into BFCA preservative solution for about 30 seconds. Preservative penetration and the surface area of treated zone were...
Nana Supriana, T K Waluyo


Collaborative soft rot tests: Statistical treatment of results of soil analyses
1971 - IRG/WP 29
Institutes taking part in the collaborative experiments already reported forwarded samples of the soils employed in the tests to the Forest Products Research Laboratory, England. The soils were then autoclaved sterilised under uniform conditions and sent to the Department of Forest Soils, the Royal College of Forestry, Stockholm, Sweden. The results of the soil analyses are given in Table 1, toget...
A F Bravery


Simulation test of subchronic inhalation toxicity of TBTO vapours in the air
1987 - IRG/WP 3454
The test was carried out in a wainscotted room of a normal size. Wooden panelling had been treated with one coat of basic preserving agent and, after the installation, with 2 coats of stain. Laboratory animals (rats) were kept in this room for 90 days. For the same period a control group of test animals was kept in a room of equal size where there was no panelling. During the test, concentration o...
V Skubic, S Kobal, J Stupar, R Ajlec, J Korošin, G R Pecenko


The efficacy of polymer/preservative treatments in soil-bed exposure
1992 - IRG/WP 92-3729
Southern pine was treated with CCA, CCB, sodium borax/boric acid, or disodiumoctaborate, alone or in combination with an acrylic polymer system containing a water repellent. Treated samples were subjected to an unsterile soil burial test. The addition of polymer reduced the weight loss in borontreated samples at the lower retentions but not at the higher retention. Results with borates indicate th...
R J Murphy, H M Barnes, S M Gray


Practical experiments with Boracol 10 Rh used as a fungicide in the repair process after attack by the dry rot fungus (Serpula lacrymans)
1987 - IRG/WP 3458
The test is carried out in an old house in Nyhavn, Copenhagen. The roof and the walls close to were heavily attacked by dry rot fungus (Serpula lacrymans) because damage to the zinc covering the frontspice were letting in water to the wood and wall construction. An attack by the dry rot fungus is more complicated to repair compared with other wood destroying fungi because beside the damage on wood...
J Bech-Andersen


Dura-Treet II, a water dispersible pentachlorophenol
1980 - IRG/WP 3165
During the past several decades, penta petroleum wood treating has become increasingly popular. Penta is an effective chemical compound against wood organisms causing decay and rot, is safe to handle, also clean and easy to use. In terms of preservative cost, it has been and remains by far the least expensive of the three major preservatives. However, when the cost of petroleum carrier is added, t...
D B Hatcher


Natural durability of larch heartwood against decay
1997 - IRG/WP 97-10201
Larch heartwood has been promoted in Sweden and in other European countries as an alternative to preservative treated timber. It has even beeen stated that larch heartwood is more durable than preservative treated timber. This paper presents a compilation of facts from scientific reports on the durability of larch heartwood. Some recent data from this department are also reported. All data suggest...
T Nilsson


Penetration as Key Factor for Determining the Performance of Wood Preservatives
2004 - IRG/WP 04-20293
Stakes of Scots pine sapwood with a dimension of 4 x 4 x 75 cm³ were impregnated with preservatives containing 2 % of propiconazole which had passed the EN 113 test criteria without any problems. The penetration of the colourless preservative was determined successfully by a fungal screening test described by Sutter (1978). The test revealed the insufficient penetration behaviour within the gi...
H Leithoff, I Stephan, R-D Peek


Silafluofen: Novel chemistry and versatility for termite control
1995 - IRG/WP 95-30069
A novel silicon - containing insectizide, HOE 084498 ('Silafluofen'), with a favourable toxicological profile, has shown activity against a broad spectrum of agricultural and environmental health pests. Results from laboratory and field studies around the world have demonstrated that silafluofen is effective at protecting timber from attack by various species of termite and wood-...
A J Adams, A Jermannaud, M-M Serment


In-house accelerated method for testing decay resistance of treated wood
2004 - IRG/WP 04-20286
Fungicidal compounds often change their effectiveness when they are incorporated into candidate formulations. For this reason fungistatic effectiveness needs to be re-evaluated as many times as the formula has been modified for better performance. To avoid multiple expenses, in-house fungistatic tests are essential. Our goal was to develop in-house usable, simple but reliable and reproductive proc...
N Vidovic


Evaluation of the effectiveness of defence anti-stain in the control of sapstain in laboratory and field tests
1990 - IRG/WP 3593
The anti-sapstain product Defence Anti-stain (DAS) has been evaluated internationally in laboratory and field tests during the years 1988 and 1989. Results of tests carried out by institutes and by own companies in countries like Indonesia, Ivory Coast, Japan, Portugal, Belgium, The Netherlands and Spain will be presented. In the several tests Defence Anti-stain showed a high fungicidal activity t...
G Rustenburg, C J Klaver


Preliminary tests on the effect of naturally occurring chemicals on termites
1983 - IRG/WP 1181
Twenty-eight naturally occurring chemicals consisting of monoterpenes, quinones and wood·extractives were tested against seven species of termite. Small pieces of filter pad and agathis wood chips measuring 5 mm by 10 mm were treated with the chemicals and exposed to the termites in polystyrene weighing bottles. Results of the tests revealed that the chemicals inhibited the feeding behaviour of t...
Nana Supriana


Standard principles of testing termiticides: A discussion paper
1991 - IRG/WP 1502
Recent restrictions and banning of termiticides such as organochlorines in some countries has focussed attention on the need for new and novel compounds as termiticides. However, this poses problems for both wood preservative manufacturers and termitologists. Test procedures have to be devised to evaluate the new termiticides so that the tests are practical, encourage vigorous termite activity, an...
J R J French