Ibuprofen inhibits in vitro growth of brown-rot fungi
1996 - IRG/WP 96-10160
Ibuprofen, a phenyl propionic acid derivative (2-(4-isobutylphenyl)propionic acid) inhibited growth in vitro of 17 brown-rot fungi at a concentration of 100 µg/mL, while exhibiting no growth inhibition for 8 white-rot fungi at the same concentration. Propionic acid did not inhibit fungal growth in vitro. Morphological changes were noted in fungi that were able to grow in the presence of ibuprofen...
C A Clausen


Analysis of volatile emissions as an aid in the diagnosis of dry rot
1992 - IRG/WP 92-2393
The dry rot fungus, Serpula lacrymans was grown in pure culture on malt extract and on sapwood of pine. The volatile compounds emitted from the cultures were determined by diffusion sampling on tubes filled with Tenax TA, thermal desorption and gas-chromatography-mass-spectrometry in order to find markers for attack of the fungus....
J Bjurman, J Kristensson


Monographic information on Serpula incrassata (Berk. and Curt.) Donk
1980 - IRG/WP 1128
J G Palmer, W E Eslyn


Biological resistance of phenol-resin treated wood
1990 - IRG/WP 3602
Biological resistance of PF (phenol formaldehyde resin) - treated wood has been tested in relation to the resin properties, wood species and biological factors. When tested using water-soluble PF (mol. wt. 170), ca. 10% RI (resin impregnation) was enough to suppress the decay of Japanese cedar (Cryptomeria japonica) and western hemlock (Tsuga heterophylla) blocks exposed to Tyromyces palustris (br...
M Takahashi, Y Imamura


Suppression of aerial hypha formation by spent culture filtrate of a non-degradative strain of Postia placenta
1991 - IRG/WP 1498
ME20, a wild-type monokaryotic strain of the brown-rot fungus Postia placenta, does not cause significant weight losses in standard soil-wood block decay tests and fails to form aerial hyphae in liquid and agar culture. This abnormal morphological feature may be caused by the same aberrant physiology that prevents the strain from degrading wood efficiently. ME20 releases elevated levels of the aut...
J A Micales


The Relationship of Fiber Cell Wall Ultrastructure to Soft Rot Decay in Kempas (Koompassia malaccensis) Heartwoo
2004 - IRG/WP 04-10541
The ultrastructure of fiber walls in kempas (koompassia malaccensis) heartwood was examined in relation to soft rot cavity formation. The fibers consisted of middle lamella and thick secondary wall. The secondary wall was differentiated in to a S1 layer, and a unique multi-lamellar S2 layer. Two distinct forms of lamellae were recognisable, one type being considerably thicker than the other. They ...
A P Singh, A H H Wong, Yoon Soo Kim, Seung-Gon Wi


Influence of variable lignin content on brown rot decay of wood
1987 - IRG/WP 1320
Compilation of published data and new experiments with brown-rotting fungi on different timber species suggest that their decay activity, in contrast to soft rot and white rot fungi, is not greatly influenced by the type or amount of lignin present....
T Nilsson, G F Daniel


First draft of a monographic card for Gloeophyllum abietinum (Bull. ex Fr.) Karst
1973 - IRG/WP 116
T Hof


Defining fungal decay types - Final proposal
1988 - IRG/WP 1355
The term soft rot is proposed for all forms of decay caused by Ascomycetes and non-basidiomyceteous Fungi imperfecti. The terms brown rot and white rot should be used only for decay caused by Basidiomycetes. Brown rot is characterized by extensive depolymerization of the cellulose and limited lignin degradation. White rot is characterised by significant degradation of the lignin component in wood....
T Nilsson


Collaborative soft rot experiments 1974. Preliminary analysis of results
1975 - IRG/WP 251
J K Carey, J G Savory


On the Influence of Wood Destroying Fungi on the Feeding Intensity of Termites
2017 - IRG/WP 17-10893
The baiting and feeding stimulating effect of wood attacked by fungal isolates of the species Coniophora, Lentinus, Poria and Gloeophyllum on termites Reticulitermes santonensis is examined. There are significant relationships between the activity of fungal isolates and the feeding behaviour of termites. The most active isolates can be used for increase the attractiveness of wood to wood-destroyin...
W Unger, T L Woods


The use of TCMTB in applications other than sapstain prevention: A review
1990 - IRG/WP 3606
The efficacy of TCMTB against staining fungi and surface moulds has been thoroughly investigated during the last decade. As a result, the chemical is used as an alternative to the chlorinated phenols in various parts of the world for the preservation of freshly sawn timber. Less known are the data obtained against brown rot, white rot and soft rot fungi. The termite repellent and bactericidal prop...
R Van der Eynde


Effect of mineral wools on growth and decay capacities of Serpula lacrymans and some other brown-rot fungi
1991 - IRG/WP 1481
The influence of stone wool and glass wool on growth and decay capacities of Serpula lacrymans and some other brown-rot fungi was studied. Mass losses of pine wood caused by Serpula lacrymans and Gloeophyllum trabeum were increased when stone wool was present. Glass wool had no influence on mass losses. Coniophora puteana, Serpula lacrymans and Gloeophyllum trabeum grew into stone wool and destroy...
L Paajanen, A-C Ritschkoff


Wood degradation mechanisms by the brown rot fungus Gloeophyllum trabeum
1997 - IRG/WP 97-10229
A mechanism for the degradation of wood by the brown rot fungus Gloeophyllum trabeum is outlined. The mechanism includes the function of redox-cycling, low molecular weight phenolic derivatives which sequester and reduce iron in acidic environments. The role of oxalate for the sequestration of iron (hydr)oxides and the pH dependent transfer of iron to the G. trabeum phenolic chelators, as well as ...
B Goodell, J Jellison


Preliminary screening of diffusion formulations for the control of soft rot
1978 - IRG/WP 2104
We have an urgent need in Australia to develop in situ remedial treatments for the present population of in-service transmission poles. For various reasons we have opted for formulations which can be applied as bandage treatments and thus we are primarily concerned with assaying diffusable toxicants. Two basic approaches have been made: an assay of the formulation's toxicity; and a combin...
H Greaves


Positive dosage response of CCA in hardwood power poles to soft rot indicated from New South Wales soft rot survey dat
1983 - IRG/WP 3233
Experience and observation have shown that retentions of less than 16 kg/m³ in the sapwood of individual hardwood poles are unlikely to delay its deterioration sufficiently to ensure an economic performance in some instances. The higher retentions of current practice should do so subject to adequate inspection and maintenance. Increases in retentions requirements up to 35 kg/m³ more or less, dep...
A J Witheridge


Analysis of degradation observed on ancient wooden objects buried underground
2001 - IRG/WP 01-10403
Ancient wooden objects were sometimes excavated from the moat of mounded tombs in Japan. Such wooden objects were in the shape of a sunshade, bird, shield, pole, yugi(a bag that holds arrows) among others. Archaeologists discussed the usage of such shaped objects, but no one could clearly explain their use. Some objects were observed using an ordinary microscope. Deterioration by bacteria was foun...
H Sakai


Mapping soft rot decay distribution using image analysis
1993 - IRG/WP 93-20011
Image analysis has been shown to be a useful technique for the assessment of soft rot decay caused by Chaetomium globosum in birch and bamboo (Wickens and Murphy, 1992). The technique can permit assessment of decay in individual or small groups of cells and this has been used to undertake soft rot decay mapping in thin sections of bamboo. Assessments were made of the extent of soft rot decay with ...
P J Wickens, R J Murphy, G F M Watts


The use of plastic meshes in soft rot monoculture testing
1990 - IRG/WP 2353
Plastic meshes were introduced between the wood blocks and agar medium in a miniaturised soft rot monoculture test in order to minimise transfer of the preservative from the wood and mineral salts from the agar. Although several different sizes and types of mesh were used and the blocks were wetted up to an appropriate moisture content for soft rot attack the amount of decay was substantially redu...
S M Gray


Effects of artificial UV weathering and soft rot decay on heat treated wood
2005 - IRG/WP 05-40302
Oil and inert gas oven heat treated pine wood strips 100 µm thick were mildly heat treated (200°C, 30 mins linseed oil, 120 mins oven). Following treatment, specimens were exposed to UV weathering (300 hours) and decay by the soft rot fungus, Chaetomium globosum. The effects of each treatment were assessed by zero span tensile testing, microscopy and by FTIR. Tensile testing of heat treated s...
M D C Hale, S C Ghosh, M J Spear


Relative performances of DNBP and CCA wood preservatives in accelerated decay tests
1988 - IRG/WP 3496
The effectiveness of 2-sec-butyl-4,6-dinitrophenol (DNBP) was compared with that of CCA. Test blocks of Pinus patula and Eucalyptus grandis were impregnated to precisely known retentions of approximately 3, 6, and 10 kg/m³ CCA and solvent-borne DNBP respectively. They were then challenged in decay tests comprising soil burial and exposure to monocultures of Chaetomium globosum, Coriolus versicolo...
W H Schnippenkoetter, L D Abraham, A A W Baecker


Iron in stone wool - one reason for the increased growth and decay capacity of Serpula lacrymans
1992 - IRG/WP 92-1537
The chemical compositions of stone wool and glass wool were analysed. There was more iron in the stone wool than in the glass wool. It was found that iron present in stone wool was easily dissolved by oxalic acid that Serpula lacrymans is able to produce. The stone wool promoted the decay of pine wood by Serpula lacrymans. The glass wool had no effect on the decay capacity of Serpula Iacrymans. Th...
L Paajanen, A-C Ritschkoff


Physiologic response of Phanerochaete chrysosporium to exposure to triazole fungicides
1994 - IRG/WP 94-10066
Triazoles are increasingly important fungicides which are employed for a variety of applications included wood protection. Several recent studies suggest that white rot fungi are more tolerant of triazole compounds than other wood degrading fungi. Cultural studies using a white rot fungus, Phanerochaete chrysosporium, and 0.2 or 0.8 ppm of tebuconazole or propiconazole suggested that mycelial dry ...
J J Morrell, R K Velicheti


Polyflavonoid tannins - From a cause of CCA soft-rot failure to the "missing link" between lignin and microdistribution theories
1986 - IRG/WP 3359
Polyflavonoid tannins are proven to be fast-reacting with CCA solutions and hence, to be strong competitors of the structural wood constituents for fixation of CCA preservatives. The consequence of this effect is that even relatively small amounts of tannin cause severe undertreatment of the structural wood constituents which in turn badly affects the long term durability of CCA-treated timber. Th...
A Pizzi, W E Conradie, M Bariska


Decay types observed in small stakes of pine and Alstonia scholaris inserted in different types of unsterile soil
1990 - IRG/WP 1443
The attack of various wood-degrading microorganisms occurring in mini-stakes of pine and Alstonia scholaris buried in various types of unsterile soil was studied. Attacks by white rot, brown rot, soft rot, erosion bacteria, tunnelling bacteria and actinomycetes were found. Soft rot occurred in all soils, whereas attack by white rot and especially brown rot and erosion bacteria was rare. The type o...
T Nilsson, G F Daniel