The effects of pH on leaching of copper-chrome-arsenate (CCA) from pressure-treated Kenyan-grown Eucalyptus saligna and Acacia mearnsii: Initial findings.
2002 - IRG/WP 02-30298
The effects of pH on leaching of CCA from pressure-treated Kenyan-grown Eucalyptus saligna and Acacia mearnsii were tested under laboratory conditions. Small samples of the two species (100mm x 30mm x 40mm) were smooth sawn from 8-year old trees to represent equal amounts of both sapwood and heartwood, air-dried to 12% moisture content, end-sealed, and pressure-treated at a commercial treatment p...
R Venkatasamy


Co-operative tests concerning the influence of solvent and drying method on the toxic limit of wood preservatives against Coniophora cerebella
1972 - IRG/WP 216
In the working group II of the IRG it was agreed that more knowledge was necessary concerning the influence of the solvent on the toxic limit of organic solvent types of wood preservatives against Basidiomycetes. A test program was drawn up and after discussion in the mentioned working group the final program was accepted by the co-operating institutes in 1969. In the test program two fungicides, ...
T Hof


Borate diffusion from fused borate rods in douglas-fir transmission poles
1994 - IRG/WP 94-30042
Pressure-treated utility poles have given many years of excellent service, but their lifetime is often shortened by internal decay of the untreated heartwood center, particularly in refractory species, such as Douglas-fir. This paper reports the distribution of boron from fused borate rods installed in CCA-treated Douglas-fir transmission poles. The boric acid equivalent was roughly monitored by t...
T L Highley, W Finney, F Green III


Redistribution of boric acid in radiata pine during drying after preservative treatment
1993 - IRG/WP 93-40010
Samples of 100 x 50 mm² radiata pine were processed with a variety of options to produce dry, boron-treated wood. Concentrations of boric acid in the central one-ninth and in the whole of the wood cross-sections were determined by chemical analysis and compared. Diffusion treated material was dried by air, conventional kiln (70/60°C), or high temperature kiln (120/70°C). Four different predryin...
A J Bergervoet, D R Page, J A Drysdale


A novel method for evaluating the performance of water repellents
1987 - IRG/WP 2279
Application of water repellent formulations to timber surfaces offers protection from the weather, reducing degrade and movement. A novel test method has been developed to evaluate the comparative efficacy of such formulations when samples are exposed to weather. The method uses sapstain free sapwood of defect free, untreated, seasoned Radiata pine, (Pinus radiata D. Don.) Water Repellency was det...
A R Moffat


Penetration of oil-borne preservatives in American elm
1975 - IRG/WP 355
Pressure treatment of elm posts and cants by Rueping schedules resulted in erratic penetration. Instead of the expected gradual decrease in retention from surface inward in posts, inner zones frequently contained more preservative than the surface quarter inch. Heartwood was found penetrated when sapwood was not. There were numerous skips in treated zones. The prevalence and possible causes were i...
E A Behr


Experimental variations in the distribution of CCA preservative in lignin and holocellulose as a function of treating conditions (temperature, concentration, pH, species, and time)
1984 - IRG/WP 3277
The exact distributions between lignin and holocellulose and retentions on wood of copper, chromium and arsenic as a function of various sets of conditions in a 3x3x4x2 factorial experiment in which combinations of three temperatures of treatment, three CCA solution concentrations, four pH's of the initial CCA solution and two timber species, namely Pinus radiata and Eucalyptus grandis, a...
A Pizzi, E Orovan, M Singmin, A Jansen, M C Vogel


Resistance of board materials against fungal decay: A comparative experiment on Kolle flask tests method and direct test method
1985 - IRG/WP 2243
Two sets of plywood (Aucoumea klaineana Pierre) 7 and 11 ply, treated by two preservatives, and untreated, were tested by two methods: 1. Kolle flask test method on malt-agar substrate according to the French standard NF B 51.295; 2. A direct test method in non sterile conditions according to DocNo: IRG/WP/2214. The exposure time far both methods was 12 weeks. After exposure, the degree of attack ...
G R Y Déon, L N Trong


The potential of high pressure pulsation processes to treat white spruce lumber with water-borne preservatives
1988 - IRG/WP 3471
Laboratory work using end sealed 4x8x46 cm³ white spruce samples has been done to explore the suitability of three variants of a 2.1 MPa pulsation process for the impregnation of white spruce with CCA. The results showed that the process improved significantly the penetration of the preservatives and reduced significantly cell collapse, when compared with the results of treatment using a 2.1 MPa ...
J P Hösli, J N R Ruddick


A combined method for drying and preserving wood in a single step process
2000 - IRG/WP 00-40183
Based on a convective dryer, this process allows to dry and treat wood blocks with diffusible preservatives in the same time. A boric acid solution (heated to fix the wet temperature of the system) is pumped and introduced in the flow system through a venturi, where the air coming back from the drying cell also arrives. The role of the venturi is to create a dispersion of boric acid solution micro...
O Colin, C Dupuis, E Mougel, A Zoulalian, M-F Thévenon


Leaching from field test stakes. Results from two different methods of analysis
1993 - IRG/WP 93-50013
Field test stakes treated with Boliden K33 containing copper, chromium and arsenic exposed at three different fields in Sweden and rejected due to decay, have in two studies been analysed regarding leaching and remaining preservatives. The stakes have been exposed during 20 to 43 years. The density of the stakes and content of copper, chromium and arsenic have been determined in the top part of th...
F G Evans, M-L Edlund


Preservative treatment of round bamboos by a new technique - Some further studies. Part 1
1990 - IRG/WP 3607
In general, the easy susceptibility of bamboos to wood destroying agencies is a major constraint in its rational utilisation. This is more so in tropical countries like India where wood destroying agencies are quite active. In an earlier publication, it was reported that round bamboo specimens of Bambusa balcooa, having three nodes, could be satisfactorily treated by CCA by a new technique develop...
V R Sonti, B Chatterjee


Multiple-Phase Pressure (MPP) Process: One-stage CCA treatment and accelerated fixation process. 3. Effect of process variables on sapwood treatment and CCA fixation.
1998 - IRG/WP 98-40114
The Multiple-Phase Pressure (MPP) Process achieves treatment and fixation as combined process using hot CCA, within a 2-3 hour time-frame. Timber is treated to saturation with hot CCA using an empty cell process. During the pneumatic pressure phase, hot solution is held in the wood in an otherwise liquid-free treatment vessel until fixation is >95% complete. This report details a factorial des...
H Pearson, K Nasheri, J A Drysdale, G Durbin, M E Hedley


Acoustic technique for assessing decay in preservative treated wood
1998 - IRG/WP 98-20138
This study investigated the suitability of vibration techniques to assess the performance of wood preservatives in ground contact. Small stakes (10 x 5 x 100 mm3) of treated and untreated Scots pine sapwood were exposed to decay in lab-scale terrestrial ecosystems. Tests were conducted using three different soils including a garden compost soil, and soils obtained from a test field and a conifer f...
L Machek, M-L Edlund, R Sierra-Alvarez, H Millitz


Influence of the nature of the substrate and the method of inoculation on the degradative activity of soft rot fungi
1998 - IRG/WP 98-20133
The European Standard (ENV-807) determines the threshold of effectiveness of wood preservatives against the action of soft rot Ascomycetes fungi. Its application in the treatment of wood used in the hazard class 4 does not always offer repeatable results, which could be expected in an experimental norm. For this reason, in this paper, we have evaluated the diverse variables that might influence t...
M T De Troya, A M Navarrete, F Rubio, J Jiménez, D Muñoz-Mingarro, C Rodríguez-Borrajo, F Llinares, M Yuste


Effects of the delay in the beginning of treatment on absorption and distribution of water-soluble salts in posts treated by sap-replacement method
1992 - IRG/WP 92-3719
One of the most important matters in green wood treatments, such as sap-replacement method, is knowing the longest time available for beginning treatment without losing efficacy. In this paper, the influence of this factor on absorptions and distribution of the preservative into the wood is analized. Tree start-up times were first chosen: 3-6 hours, 48 h and 120 h after being cut down. The treatme...
M V Baonza Merino


New method to find out the volatile organic compounds (VOC) of wooden material
2000 - IRG/WP 00-20189
Volatile organic compounds (VOC) of pine, spruce and larch wood were studied using a new technique developed at VTT Chemical Technology. 50 mg of crushed wood material was placed into glass tubes. The tubes were closed with a glass wool, which is pressed with a tube cap. Wood samples were analysed with a gas chromatograph after thermal desorption using four different temperatures (50°C, 100°C, 1...
H Viitanen, K Villberg, K Saarela


Estimating the size of subterranean termite colonies by a release-recapture technique
1980 - IRG/WP 1112
The technique is described and the results of an exploratory field trial are presented. The colony size estimate from weekly termite collections varied considerably, but nevertheless permitted assigning termites at three locations to three categories of greatly different colony size. The sizes of the three estimates were much greater than anticipated and included a multimillion termite complex of ...
G R Esenther


The results of detection on CCA components of the soils contacted with CCA-treated woods - A trial study for the availability of the burial Method as a disposal CCA treated wood waste
1993 - IRG/WP 93-50005
The objecteve of this experiment is to get a knowledge that, when CCA treated wood wastes were buried in a soil as a disposal, the soil would be or not be contaminated by the components of CCA preservatives in wood wastes. The specimens used were cutting logs and chips made of the CCA treated electric pole waste. The soil was buried to the 15 cm depth and the log specimens were set in the soil for...
K Suzuki, H Sonobe


The “wire-loop slicing technique” for the rapid field collection of large numbers of Coptotermes acinaciformis termites from above-ground mound colonies
2006 - IRG/WP 06-10583
This technique of rapidly slicing through an above-ground C. acinaciformis mound colony with a steel wire-loop attached to a vehicle allows the collection of large numbers of termites. The sliced mound topples onto a tarpaulin arranged on the ground, the outer wall layers break away in large segments, and the carton materials incorporating the termites are readily collected and transferred to larg...
B M Ahmed, J R J French


High-energy multiple impact (HEMI)-test – Part 2: A mechanical test for the detection of fungal decay
2006 - IRG/WP 06-20339
The suitability of the high-energy multiple impact (HEMI)-test for detection of early fungal decay was examined. The HEMI – test characterizes the treatment quality of thermally modified wood by stressing the treated material by thousands of impacts of pounding steel balls. This method differentiates between heat treatment intensities, which are expressed by structural changes of the wood. Simil...
C R Welzbacher, C Brischke, A O Rapp


High-energy multiple impact (HEMI)-test – Part 1: A new tool for quality control of thermally modified timber
2006 - IRG/WP 06-20346
Thermal modification processes improve durability and dimensional stability of wood, but the strength properties, especially the dynamic ones, are compromised and need to be considered with respect to industrial quality control. Results from standard dynamic strength testing, such as impact bending tests, suffer from high variability, and therefore require a high number of replicates. To overcome ...
C Brischke, A O Rapp, C R Welzbacher


Water analysis in chemicals, wood or chemically treated wood using a new analytical method for selective water detection
2006 - IRG/WP 03-30391
Water or moisture content analysis can be a challenging task in many applications. However, knowing accurately the type of water which can be found in a given sample or product can provide important information about a chemical compound used for wood treatment and especially about the treated wood sample. Moisture content in wood plays an important role in fungal growth and it needs to be extensi...
R Craciun, D Taylor


The Development of a novel method to preserve reeds using an environmentally friendly timber preservative and a unique engineering design.
2006 - IRG/WP 06-40335
Reeds are used in the construction of bush lodges in Northern Kwa- Zulu Natal, South Africa. Fungal, insect and ultra-violet damage to these reeds is posing a severe problem. Within a space of two years, the reeds are attacked and have to be subsequently replaced; a time consuming and costly exercise. A novel method has been used to successfully preserve these reeds with an environmentally friendl...
K Govender, K G Moodley


Non-pressure preservation technique of five less durable timber species – Kadam (Anthocephalus cadamba), Shimul (Bombax ceiba), Pithalu (Trewia nudiflora), Am (Mangifera indica) and Boroi (Ziziphus jujube) of Bangladesh
2006 - IRG/WP 06-40322
Wood is a versatile renewable resource, which has been extensively used as a reliable construction material as well in furniture ever since the beginning of civilization. The Major disadvantage of wood is its susceptibility to biodeterioration by fungi, insects and bacteria. In tropical countries like Bangladesh, fungi is the most significant of these biodeterioration agents. Kadam (Anthocephalus...