Your search resulted in 110 documents. Displaying 25 entries per page.


Some practical implications from recent research on the fixation of CCA preservatives
1975 - IRG/WP 358
The mechanism of fixation of CCA preservatives is briefly described. If the temperature is increased during the primary fixation period, the formation of intermediate fixation compounds is less extensive. The length of the primary fixation period is of practical interest. It is determined by preservative composition and concentration, temperature and wood species. Diagrams are given for Pinus sylv...
S-E Dahlgren


The effect of storage and subculturing on in vitro fruit body formation and spore production in Gloeophyllum sepiarium and Oligoporus placentus
2001 - IRG/WP 01-20232
Spores are widely assumed to be the main mode of infection of wood in conditions conducive to decay above ground. In order to supply spores on demand as an experimental material, fruiting body and basidiospore production in vitro by Gloeophyllum sepiarium and Oligoporus placentus have been examined. The optimum medium, time to spore production, and duration of fruiting as well as fruiting body sha...
S Choi, J N R Ruddick, P I Morris


Migration of chlorothalonil and carbendazim in fruits stored in wood treated with the anti-sapstain formulation Tuff Brite C
1997 - IRG/WP 97-50097
Fruits and vegetables stored in treated wood boxes are in contact with the products used for the treatment. In order to obtain regulatory approval for incidental food contact it is necessary to determine the quantity of residues on these fruits or vegetables. When the active materials are used in agriculture it is required that residues found are below to the MRL fixed for these substances. In the...
J F Cooper, D Riboul, M De Vleeschauwer, T L Woods


Exterior wood stains
1979 - IRG/WP 3136
The use of semi-transparent exterior wood stains has grown remarkably since their development during the 1960s. This can be partly attributed to their offering a break with tradition at a time when it was being recognised that changes in the quality of timber and how it was used demanded different methods of exterior wood finishing. Information is already available on the characteristics and uses ...
E R Miller


The association of bacteria with the increased permeability of water-stored spruce wood
1973 - IRG/WP 325
A microbiological investigation was undertaken to check our earlier work on patterns of bacterial counts and pH changes in water-stored wood. A survey of industrial activity was conducted upstream from the storage site with a view to explaining the existing bacterial flora. Further experiments were carried out with spruce bolts in enclosed tanks, using lake water with its natural bacterial flora a...
J A Dunleavy, J P Moroney, S E Rossell


Wood injurers found at wood processing plants in SR Sloveni
1981 - IRG/WP 1140
This report describes the stating of damages on wood and taking stock of wood injurers found in the warehouses of wood processing plants in SR Slovenia. The results of this research show that in the process of manufacture vast quantities of spruce-wood, pine-wood, beech wood, oak-wood, and poplar-wood are exposed to numerous injurers, both fungi and insects. The reasons for such a state lie in con...
R Benko


An analysis of the effects of some factors on the natural durability of pine (Pinus sylvestris L.) and spruce (Picea abies Karst.)
1986 - IRG/WP 1279
The effects of some factors on the natural resistance of pine and spruce sapwood against fungal decay and against attack of house-longhorn beetle larvae have been studied in laboratory tests and the results are evaluated by analysis of variance and regression analysis. Following conclusions were reached: Wood from summer-felled trees did not have a lower inherent natural durability against fungal ...
J B Boutelje, T Nilsson, S Rasmussen


Permeability measurements on surface layers for detecting wood with abnormally high permeability
1988 - IRG/WP 2298
Wet storage of timber during the warm period of the year may lead to an increased permeability of the wood, an undesirable phenomenon for several wood industries and also for many end-uses. Neither before nor after drying, such wood with "wet storage damage" can be visually distinguished from wood with a normal permeability. A non-destructive method for inspecting the permeability of surface layer...
J B Boutelje, G Hägglund


Application of oscillating pressure to improve treatability of refractory species
1987 - IRG/WP 3449
Under practical conditions a minimum moisture content of 80% demande by the German quality standard RAL-RG 411 can not be guaranteed throughout the year. Storage of logs with bark prolonges the drying process; a storage without bark must be avoided. A sufficient penetration according the standard can be achieved at least with a moisture content of 60%, optimal conditions may prevail between 100% a...
R-D Peek


Impregnation of timber with tannin as a mean of improving its dimensional stability
1992 - IRG/WP 92-3695
The results of a joint project carried out at the Timber Division of LNEC under the 2nd research programme of the CEC DGXII - "Wood as a renewable raw material" entitled "Stabilization of wood by impregnation processes" is presented. Pieces Maritime pine timber was impregnated with tannin under pressure to see if the treatment with tannin improved the behavior of wood regarding its dimensional sta...
J S Machado


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 4: Conversion reactions during storage
1974 - IRG/WP 332
Precipitates simulating those produced in wood by preservative fixation reactions were prepared by the reduction of Boliden K 33 and Celcure AP solutions with hydrogen peroxide and hydrazine. The pH changes on aging at 20 and 50°C were studied and related to the chemistry of fixation previously described. Hydrolysis of copper arsenates may render arsenic acid temporarily water soluble pending pre...
S-E Dahlgren


Mould growth and permeability in relation to wet-storage
1989 - IRG/WP 1414
The positive influences of wet-storage of roundwood to avoid attack by blue stain fungi and insects and to avoid cracking of wood during storage are well documented. Comparatively little information is, however, available on the effects on microbial susceptibility of the material after the storage period. The permeability of the wet-stored and the non-wet-stored material was determined. Wood block...
J Bjurman, E L Holappa


Evaporation and redistribution of creosote in pine poles during storage
1996 - IRG/WP 96-50064
During the work with European standards for pressure treated wood, it has been questioned if the lapse of time between impregnation and chemical analysis of the retention is critical, especially for creosote. "The Norwegian Control Scheme for Preservative Treated Wood" has not discovered any retention problems analysing CCA preservatives in wood. If the lapse of time between impregnation with creo...
F G Evans, B Nossen


Surface and system treatments of wood for outdoor use
2006 - IRG/WP 06-30412
The project “Surface and system treatment of wood for outdoor use” was initiated the summer 2001. The project evaluates environmentally friendly preservatives and water borne coating systems, to find the best protection for timber indented for outdoor use. The wood species selected as test material were pine and spruce. The different treatments were exposed in several outdoor accelerated tests...
B Jacobsen, F G Evans


Laboratory Leaching Tests to Study the Effects of Post-Treatment Storage Periods on CCA Leachability and Fixation in Treated Permeable and Refractory Malaysian Hardwoods
2006 - IRG/WP 06-50240
The biological resistance and environmental safety of CCA-treated wood relies on the extent of post-treatment storage fixation of CCA in wood prior to being utilized. A study on the comparative leachability (fixation) of CCA-treated refractory and permeable heartwoods of 3 Malaysian hardwoods subjected to different post-treatment storage (fixation) periods of up to 4 weeks, at 2 laboratory leachin...
A H H Wong, H C Lai, N P T Lim


Expected service life of outdoor wooden structures such as guard fences and noise barriers indicated by questionnaire survey
2007 - IRG/WP 07-20372
Forestry Agency, Japan has intended to expand the utilization of domestic wood in many areas such as not only housing constructions also outdoor structures. In order to respond the policy, actual durability and service life of these structures should be clarified, and the guide line for archiving planned service life also should be established. Japan Wood Preservers Industries Association carried ...
K Yamamoto, A Makita, A Yamaguchi, T Shiraishi, K Maeda, D Tezuka, S Katsumata, M Higaki


Refinement of emission values for preserved wood in the ‘Storage Scenario’, for use in the environmental risk assessment of Wood Preservatives under the Biocidal Products Directive
2007 - IRG/WP 07-50244
The evaluation of an active substance or a biocidal product under the Biocidal Products Directive (BPD) requires that an environmental risk assessment is carried out. The risk assessment for wood preservatives includes a scenario for the treated wood in storage after treatment, in which the predicted environmental concentration (PEC) in soil, surface water and groundwater is calculated, using emis...
E F Baines


Comparative Laboratory Leaching Test Methods to Study Post-Treatment Storage Period Impacts on CCA Leachability and Fixation in Treated Kempas (Koompassia malaccensis) Heartwood
2007 - IRG/WP 07-20376
Three laboratory leaching test methods were compared to determine the effects of different post-treatment storage fixation periods on leachability/fixation of CCA components from treated kempas (Koompassia malaccensis) permeable heartwood. End-sealed test wood blocks of permeable were treated with CCA to target retention of 5.6 kg/m3, immediately stored to fix at ambient conditions for 0 and 48 ho...
A H H Wong, H C Lai


Run-off quality from sprinkled debarked logs and logs with bark from Picea abies and Pinus contorta
2007 - IRG/WP 07-50248
Storage of roundwood is necessary for efficient industrial production at sawmills and pulpmills. The need for wood storage becomes even more critical when large storm fellings create huge volumes of wood that is at risk for deterioration. In Scandinavia, the technique of sprinkling of water on roundwood is used to protect stored wood from fungal and insect infestation and drying during the summer....
M Jonsson


Primary Study on Compressed Preservative-treated Wood (CPW) for Outdoor Applications
2008 - IRG/WP 08-40412
In this study, the compressed wood samples pre-treated with hot water bath or water spraying were immersed in the ammoniacal copper quat –type D (ACQ-D) preservative solution to get compressed preservative-treated wood (CPW). The liquid absorption and the recovery rate of compression deformation of the compressed wood was determined, as well as the surface hardness, the distribution of density a...
Jinzhen Cao, Jia Mao


Service Life Prediction of Wood Claddings by in-situ Measurement of Wood Moisture Content: Status after 5 years of Outdoor Exposure
2009 - IRG/WP 09-20401
The Danish Technological Institute is in co-operation with industry partners running a project aiming at predicting the service life of different wood protecting systems. The project focuses on examining the moisture reducing effect of different protecting systems for timber claddings and the ability of these to maintain the appearance of the surfaces, when the wood is used in service class 3 (EN ...
E Tang Engelund, B Lindegaard, N Morsing


Study on the thickness swelling of mould-resistant chemical treated bamboo strand woven outdoor flooring
2010 - IRG/WP 10-40489
To prevent bamboo strand woven flooring from mould, several preservatives were chosen to treat bamboo strand before dipping into adhesives and pressing. The thickness swelling and mould resistant effect of the finished board were studied. Results showed that different preservatives had different influences on the thickness swelling of BSWF, and in order to reduce the thickness swelling of the fini...
Fangli Sun, Binfu Bao, Shenyuan Fu, Anliang Chen


Deterioration of wooden heritage in outdoor exposure in Romania
2010 - IRG/WP 10-40535
The paper contains a study of the deterioration of wooden heritage in Romania, in outdoor exposure. Romania belongs to the few countries having a rich heritage of this kind. A quantitative image of this heritage reveals the 1,350 objectives transferred and reconstructed in 16 open-air museums, over 1,500 wooden churches, more than 4,000 buildings and technical facilities, historical monuments ...
L Bucşa, C Bucşa


Riverbed Construction Technology using Thinned Timbers for Carbon Dioxide Sink in Korea
2010 - IRG/WP 10-50271
The Climatic Change Convention is a big burden in limiting the energy usage like the blood of economy. The certification standard about the carbon storage of timbers after harvesting them is expected to be an important role in setting the goal for future reduction of the green house gas(CO2). The extension of a timber's life span through its preservation is one of technologies for carbon sink...
Dong-heub Lee, Won-Joung Hwang


Performances of Douglas fir in real outdoor use conditions
2011 - IRG/WP 11-20472
The European standard EN 350-2 classifies Douglas fir as moderately resistant to fungal decay on the basis of standardized laboratory and field tests. However, the lifespan expectancy of outdoor structures such as cladding, decking and elements of wood construction carpentry may also vary according to environmental conditions (climate, exposure to weathering), maintenance and design. An investigat...
M Kutnik, S Lepetit, S Le Nevé


Previous Page | Next Page