Development of marine borers research in Sao Paulo State, Brazil
1985 - IRG/WP 4117
This paper describes some field tests which have been carried on marine sites in Sao Paulo State mainly to investigate the natural resistance of Brazilian woods and the occurrence of marine borers. Some laboratory breeding tests which are being developed are also describe...
G A C Lopez


Above ground performance of CCA-treated fingerjointed lumbe
1993 - IRG/WP 93-40003
Studs made from short lengths by finger jointing are becoming more commonly used in North America. Recently Forintek has received enquiries about the performance of such material in a treated form. Treated and untreated nominal 2x4 inch² spruce-pine-fir (SPF) studs exposed above ground for 12 years in southwestern British Columbia were evaluated for evidence of decay. Despite shallow preservative...
P I Morris, G E Troughton


Information from the COIPM Wood Group. Summary received via Mme Dr Anna Gambetta (Italy)
1987 - IRG/WP 4139
Two co-operative programmes were discussed: 1) The IRG/COIPM co-operative programme on the CCA/CCB wood treatments and 2) The IRG/COIPM co-operative programme for testing the resistance of plastic wrapping for wooden pilings. The following was reported: In the wood treatment programme, beech, pine and alstonia wood samples have been pressure treated with 3 retentions (3%, 6% and 10%) of CCA and CC...
J R DePalma


Collaborative experiments in testing the toxicity of wood preservatives to soft rot fungi
1970 - IRG/WP 25
Eight Institutes from seven countries, Austria, England, France, Germany, Holland, Sweden and Switzerland have collaborated in an attempt to assess the suitability of various laboratory test procedures for acceptance as standard methods of determining the toxicity of wood preservatives to the cellulose-attacking micro-fungi which cause 'soft rot' of wood. Pure culture methods wit...
J G Savory, A F Bravery


Forest products laboratory methodology for monitoring decay in wood exposed above ground
1995 - IRG/WP 95-20074
Research at the Forest Products Laboratory on the durability of wood in service has included a full complement of laboratory and field tests. In this report, we present a review of past and current methods used to evaluate the condition of preservative-treated wood exposed above ground. Current protocols are described for tests on wood packaging, roofing, and dimension lumber....
R C De Groot, T L Highley


Fungus cellar and stake tests with tall oil derivatives. Progress Report after 5 years' testing
1987 - IRG/WP 3442
Two derivatives of tall oils have been tested for five years in fungus cellar and stake tests. The samples were relatively quickly attacked on the surface by decay fungi, mainly soft rot, but the decay has progressed very slowly. The performance of the stakes in the tests has so far been equivalent or even better than some CCA preservatives and creosote....
J Jermer, Ö Bergman, T Nilsson


A critical review of the AWPA standard method (M12-72) for laboratory evaluation to determine resistance to subterranean termites
1986 - IRG/WP 1298
The American Wood Preservers' Association standard (M12-72) for evaluation of candidate wood preservatives against subterranean termites is reviewed and suggestions for revision are made. The most serious flaws in the current test procedure involve a failure to recognize inter- and intraspecific variation and a lack of quantification of test results....
J P La Fage, M Jones


Co-operative research project on L-joint testing. Progress report to March 1988
1988 - IRG/WP 2315
Further sets of data received from CTFT (France), BAM (Germany) and PRL (UK) after 46-48 months exposure and STU (Sweden) after 22 months exposure are presented and discussed in conjunction with data reported previously. Colonisation and attack of the L-joints has progressed with increasing exposure period. The new data are generally in agreement with those presented previously and the major diffe...
J K Carey, A F Bravery


Environmental impact of CCA poles in service
1997 - IRG/WP 97-50087
Soil samples from different depths and distances from CCA treated utility poles in Canada were analyzed for copper, chromium and arsenic content for a number of soil types, two wood species red pine (Pinus resinosa) and jack pine (P. banksiana) and different pole ages in service. A limited number of poles were equipped with water traps to collect rain water that dripped down the poles and where su...
P A Cooper, Y T Ung, J-P Aucoin


What can DNA fingerprinting, aggression tests and morphometry contribute to the identification of colonies of the Formosan subterranean termite
2000 - IRG/WP 00-10371
Multilocus DNA fingerprinting, aggression tests and morphometry were compared to evaluate their potential for the identification of colonies of the Formosan subterranean termite, Coptotermes formosanus (Isoptera: Rhinotermitidae) in Hawaii. DNA fingerprinting separates the termites from all studied collection sites. Since the genetic similarity between termites from different collection sites lies...
C Husseneder, J K Grace


How best to specify retentions of preservative treatments: kg/m3 or % (m/m)
1998 - IRG/WP 98-20151
When specifying treatments according to the European Standard EN 351-1, retentions in the analytical zone are based on the amount of product found to be effective in biological tests; this is expressed in terms of the retention of the product per unit volume (kg/m3) for penetrating treatments and per unit area (g/m2) for superficial treatments. However, to check whether the retentions have been ac...
J K Carey


A collaborative test to determine the efficacy of polyurethane coatings on wood samples exposed in the marine environment
1984 - IRG/WP 4113
Aims are: a) to determine the effectiveness of elastomeric polyurethane as a protective coating against marine wood boring animals in a range of tropical and tempreate sites; b) to compare the adhesion of polyurthane coatings on different wood species exposed in seawater; c) to record the severity of attack in failed samples and to identify the causal marine organisms....
R A Eaton


Diffusion of fused borate rods in top ends of poles
1989 - IRG/WP 3518
Diffusion tests of fused borate rods were carried out on extremities of sapwood poles in service. Rods were set in drills under the cone with or without addition of liquid Boracol 40. After one year of weathering, a good diffusion in the slice under the cone and even below the slice and in the cone itself was observed in Scots pine and spruce poles. The rods were still intacts and constitute, in f...
D Dirol, J P Guder


Efficacy of some extractives from Pinus heartwood for protection of Pinus radiata sapwood against biodeterioration. Part 1: Fungal decay
1995 - IRG/WP 95-30072
Chemical compounds thought to contribute to the natural durability of heartwood of Pinus spp. were either chemically synthesised in the laboratory or extracted from the heartwood of Pinus elliottii or Pinus caribaea. These compounds included the stilbenes, pinosylvin and its mono- and di-methyl ethers, and the flavonoids, pinobanksin and pinocembrin. Small blocks of Pinus radiata sapwood were impr...
M J Kennedy, J A Drysdale, J Brown


A note on testing the efficacy of wood preservatives above ground
1995 - IRG/WP 95-20078
A number of test methods have been used to evaluate the performance of wood preservatives in above ground situations. These have included EN 113 tests following natural exposure weathering (NEWT), L-joint or T-joint tests, lap-joint tests, and decking tests. A new test referred to as the A-frame test has been developed and is under evaluation. This is based on a sandwich-type test in which a thin ...
G R Williams, J A Drysdale, R F Fox


Accelerated wood decay in a soil bed test under greenhouse conditions compared with a stake test under field condition
1991 - IRG/WP 2384
The rate of decay of oak, beech, Douglas fir, pine and spruce stakes in an outside test field were compared with the decay rate of the same species in a greenhouse soil-bed test. Strength loss after four and six months respectively was measured by determining the compression strength parallel to the grain. The results show that all species, strength loss in the greenhouse was 2 to 4 times higher t...
J E Polman, S G Michon, H Militz


Durability of different heat treated materials from industrial processes in ground contact
2005 - IRG/WP 05-40312
In this study the durability of heat treated wood originating from four different European industrial heat treatment processes in ground contact was examined. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood/Finland, New Option Wood/France and Menz Holz/Germany where Oil-Heat treated Wood (OHT) is produced. All heat treated materials showed significantly i...
C R Welzbacher, A O Rapp


Evaluation of polystyrene as a protective of wood in sea-water
1986 - IRG/WP 4129
A test is described on the biological protection of wood by treatment with polystyrene. The results, obtained in marine trials, after 18 months, show that the treatment with polystyrene is not all that effective in preventing the attack of marine borers....
A Gambetta


Collaborative soft rot tests: Summary of comments on 'Proposals for a standardized soil burial test'
1971 - IRG/WP 202
J G Savory


Collaborative soft rot tests: 2nd interim report
1975 - IRG/WP 258
J G Savory, J K Carey


CEN Draft Standard (38 N 460F): Méthode d'essai pour determiner l'efficacité d'un produit de préservation du bois en milieu marin
1986 - IRG/WP 4132 F
G Castan


Preventive action against fungal decay: A comparative experiment on the effects of natural and artificial infection of wood by Basidiomycetes
1981 - IRG/WP 2160
M Fougerousse


Report of field test results for dichloro-n-octyl-isothiazolone: A potential new wood preservative
1988 - IRG/WP 3495
In a previous report (IRG/WP/3306) we presented preliminary laboratory test results on 4,5-dichloro-2-n-octyl-4-isothiazolone (RH 287). Laboratory data indicated toxic threshold values for RH 287 ranging from 0.37 to 0.50 kg/m³. In this report we present field test results on an IRG L-joint test and an in-ground stake test for RH 287, pentachlorophenol and biocide free test units. (a) L-joint tes...
D E Greenley, B M Hegarty


Potentialities of protein borates as low-toxic, long-term wood preservatives - Preliminary trials
1999 - IRG/WP 99-30212
Boron compounds are efficient wood preservatives, as well as safe for the mammals and environmentally acceptable. Their natural solubility allows them to treat almost any wood species, but is also the cause of their high depletion from treated timber in outside exposure. In order to reduce this leachability, potentialities of proteinic polymer networks retaining boron within the wood have been inv...
M-F Thévenon, A Pizzi, J P Haluk


The rate of redistribution and loss of leachable preservatives under service conditions
1993 - IRG/WP 93-30026
This paper describes experiments carried out to determine patterns of preservative redistribution and any associated losses which occur when wood containing unfixed water-soluble wood preservatives is exposed to service conditions where leaching is possible. Scots pine sapwood treated with disodium octaborate was used as a model system. Results are recorded and discussed for trials representing pa...
R J Orsler, G E Holland