Immuno-electron microscopic localization of extracellular metabolites in spruce wood decayed by brown-rot fungus Postia placenta
1990 - IRG/WP 1441
Degradation by Postia placenta in spruce and birch wood was shown to occur not only in the wood cell wall but also in the middle lamellae region. Middle lamellae was often found to be degraded along the centerline so that cells could separate along this line. Extracellular membrane structures were found surrounding the hyphae and this matrix labelled positively with antisera produced to Postia pla...
Y S Kim, B Goodell, J Jellison


Field and greenhouse testing of window joinery of pine and spruce treated with LOSP
1991 - IRG/WP 3658
Norwegian window frame components of full size were double vacuum-treated with TBTN and TBTO, and connected as 'L-joints' and subsequently coated with stains. The corner sections were exposed (out of ground contact) both in field (temperated coastal climate, Taastrup, Denmark) and in a greenhouse (Uppsala, Sweden). The window frame L-joints of spruce (Picea abies Karst.) - treate...
F G Evans, B Henningsson, E Borsholt


Models of the critical time of humidity and temperature conditions for the development of mould fungi in pine and spruce sapwood
1995 - IRG/WP 95-20066
Regression models of the time factor for the growth of mould fungi in pine and spruce sapwood are studied. The first group of models are based on the results of exposures of mould fungi in static humidity and temperature conditions indicating the time for the start of mould growth in wood. The second group of models are based on the exposures of mould fungi in fluctuating or alternating humidity a...
H Viitanen


The effect of pretreatments on the impregnation of air-dried sawn Belgian spruce
1988 - IRG/WP 3490
In general the impregnation of airdried spruce results in a variable treatment and limited penetration. This is the result of pit aspiration that occurs during drying of the spruce sapwood and heartwood. Spruce timber is becoming of greater importance in Belgium and hence research for better treatment of this vulnerable wood species is needed. Squared airdried timber of different dimensions were e...
J Van Acker, M Stevens


The effect of water storage on the cell-structure of Sitka spruce (Picea sitchensis) with reference to its permeability and preservation
1970 - IRG/WP III 3A
Commercial treatment trials with full sized transmission poles have shown that water storage considerably improves the permeability of Sitka and Norway spruce. These results were confirmed by laboratory measurements which showed that in the sapwood of ponded Sitka spruce there is a vast improvement in permeability in all three grain directions. Heartwood permeability does not seem to be affected t...
J A Dunleavy, A J McQuire


Integrated protection of freshly sawn lumber using Bacillus subtilis and selected fungicide
1997 - IRG/WP 97-10235
Bioprotection against stain fungi has tremendous potential for reducing discoloration of freshly sawn wood while decreasing chemical consumption. Unfortunately, most bioprotectants appear to be unable to consistently perform under the array of conditions to which freshly sawn wood is exposed. While research is underway to understand the nature of the inconsistent performance, a more pragmatic appr...
M E Mankowski, M Anderson, J J Morrell


Supercritical fluid treatment: Effects on bending strength of white spruce heartwood
1993 - IRG/WP 93-20008
The effects of supercritical carbon dioxide on wood strength were evaluated using white spruce heartwood, a species known to be especially susceptible to collapse during exposure to higher pressures. The effects of pressures of 2000 or 3600 psig and temperatures of 40 or 80°C were evaluated using 30 or 60 minute exposure periods. No significant differences were noted in modulus of rupture or modu...
S M Smith, J J Morrell, E Sahle-Demessie, K L Levien


Laboratory and field trials of novel antisapstain formulations
1997 - IRG/WP 97-30146
This document covers the results of laboratory and field trials of combinations of fungicides formulated using a patented technology (PCT NZ 96/00143). A 3 week laboratory trial that uses radiata pine (Pinus radiata D. Don) branch discs as a substrate was used to determine which combinations possessed a suitable spectrum of fungitoxicity against key sapstain, mould and decay fungi. In particular f...
R N Wakeling, P N Maynard, D R Eden, C M Chittenden, B Carpenter


Effect of climate, species, preservative concentration and water repellent on leaching from CCA-treated lumber exposed above ground
2001 - IRG/WP 01-50178
Few studies have examined leaching of chromated copper arsenate (CCA) from treated wood in above ground exposures due to the assumption that leaching is less severe compared to wood in continuous contact with soil or water. However, a significant portion of CCA treated wood is used for above ground applications, exposing considerable volumes of the preservative to precipitation and potential leach...
J L Taylor, P A Cooper


Kerfing reduces checking in ACA-treated western white spruce poles
1988 - IRG/WP 3477
Western white spruce poles, pressure treated with pentachlorophenol and ammoniacal copper arsenate (ACA) were installed in the Westham Island test site. The pentachlorophenol treated poles were unkerfed, while both unkerfed and kerfed ACA poles were placed in test. The checking and kerf width and depth were recorded at the time of installation. After ten years of weathering the checking characteri...
J N R Ruddick


Field evaluation of CCA movement in sap-displaced copper chrome arsenic treated softwood poles
1989 - IRG/WP 3539
Commercial sap-displaced UK grown Scots and Corsican pine, and Sitka and Norway spruce poles were exposed in a field site at Dundee, Scotland and radial distribution profiles of CCA monitored prior to implantation and after subsequent field exposure. Results show that groundline levels of all preservative elements were higher after 1 and 2 years field exposure compared with those recorded prior to...
S D Hainey, G M Smith, A Bruce, P D Evans, B King, H J Staines


Characterisations of the mode of action(s) of Methylene bisthiocyanate (MBT) in Ophiostoma floccosum
2005 - IRG/WP 05-10554
Potassium (K+) leakage, oxygen consumption, glucose depletion and level of ATP formation were determined to elucidate the potential target site(s) of MBT on the sapstain fungus O. floccosum. Treatment of O. floccosum with MBT caused an efflux of intracellular K+ ions from the cells, and the rate of leakage increased with increasing MBT concentrations up to a certain value. This observation sugge...
T Singh, B Kreber, A Stewart, M Jaspers


Soil treatment tests with the three products of boric acid for the prevention of the hyphal growth of Serpula lacrymans
1992 - IRG/WP 92-3693
Laboratory soil treatment tests were conducted for the evaluation of fungicidal or fungistatic effect of boric acid products against Serpula lacrymans. Boric acid products tested were the following three: a thickened boric acid solution in triethanolamine, boric acid-silica gel complex granules, and a nonwoven fabric laminated with a polypropylene film and coated with boric acid granules on one si...
S Doi, A Yamada, Y Mineki, M Mori


The improvement of wood durability by retification process
1993 - IRG/WP 93-40015
A material with new properties is obtained by retification process. It consists of a light pyrolysis of wood which becomes more stable and especially more resistant to fungal attack with few decrease of mechanical properties. Tests were carried out on three susceptible wood species (Poplar, Spruce, Fir) that are used in construction and are difficult to treat with wood preservatives. Retified wood...
D Dirol, R Guyonnet


Preservative treatment of wood by diffusion processes - Simulation of commercial treatment processes
1988 - IRG/WP 3498
Spruce (Picea abies), Scots pine (Pinus sylvestris) and birch (Betula pendula) were preservative treated by diffusion with mixtures of copper sulphate and arsenic pentoxide. The preservative was fixed after a suitable diffusion storage period by soaking in ammonia solution. A high standard of treatment could be achieved in spruce sapwood. This was attributed to its low wood density, and high wood ...
P Vinden


Cell wall microdistribution of chloropicrin and methylisothiocyanate in treated spruce
1989 - IRG/WP 3548
Chloropicrin and methylisothiocyanate (MIT) residues were observed using SEM/EDXA and TEM/EDXA in treated spruce wafers that had been exposed to the vapors of the two fumigant preservatives. Chlorinated residues from chloropicrin were found throughout the wood cell wall, even in acetone extracted material. The residues were most heavily concentrated in extractive materials in the rays, but unlike ...
G F Daniel, B Goodell


Growth of sapstain fungi in scots pine and the effect of timber ageing
1998 - IRG/WP 98-10269
A trial was initiated to study the growth of known isolates of sapstain fungi in scots pine (Pinus sylvestris) which had been naturally aged or sterilised by autoclaving or irradiation. Sawlogs cut from commercial thinnings were reduced to billet size and the exposed ends were painted with a bituminous sealant to reduce moisture loss. Some billets were inoculated after autoclaving or gamma-irradia...
N J Strong, J F Webber, R A Eaton


Persistance of active ingredients in treated wood
1993 - IRG/WP 93-50001-20
Disposing of chemically protected waste wood implies the distinction between surface and pressure treatment. Considering that barked round-wood merely contains, after 7 months open storage, less than 30 g per ton of bark or 25 mg per ton of sapwood, depending on the type of insecticide, the bark or sapwood shavings may be incinerated normally, according to less severe legal prescriptions than for ...
E Graf, P Manser, S Rezzonico, B Zgraggen


Investigations of the treatability of various commercially significant Turkish timbers
1976 - IRG/WP 370 E
Timbers which naturally deteriorate quickly can only be used commercially when their life is increased by the use of chemical treatments. The treatment of the timber can only be planned on a regular basis when the treatability of the wood is known. The purpose of the experiments was therefore to determine to what extent the various types of wood could be sufficiently impregnated. The question of t...
R Ilhan


Färbeverfahren zur Unterscheidung von Holzzonen mit unterschiedlichem Absorptionsvermögen, insbesondere bei Fichtenholz (Picea abies Karst.). [Staining method for distinguishing zones of wood with different absorption behaviour, particularly in spruce (Picea abies Karst.)]
1980 - IRG/WP 3163
A simple regressive staining method for crosscut wood surfaces is described. Phloroglucinol-hydrochloric acid serves as stain; flowing water and a solution of sodium carbonate are used for development and fixation of a picture showing the differences of absorption. Hydrophobic zones and, contrary to this, zones with a high water content can also be shown. Comparing green spruce wood before and dur...
S Cymorek


Accelerated diffusion treatment of sawn Sitka spruce grown in the UK
1986 - IRG/WP 3395
The treatment of 'green' sapwood and heartwood of Sitka spruce by diffusion methods was investigated. Steam/dip treatment processes gave increased solution uptakes and depths of penetration of copper in comparison with a simple dip treatment. Further investigation is required to reduce diffusion gradients with copper based formulations and to improve the penetration of '...
R J Murphy, D J Dickinson


Sawn timber of fir (Abies alba Mill.) - Treatability and usability for the Hazard Classes 3 and 4
1999 - IRG/WP 99-40147
Within a national research project, tests on the treatability on sawn timber of fir (Abies alba Mill.) in oscillation pressure, vacuum pressure and double-vacuum processes have been worked out with 95 trunks taken from 3 different altitude levels (up to a height of 590 metres, 600 to 990 metres and over 1000 metres) and from 4 different regions of Switzerland. As the treatability of round wood can...
E Graf, T Bör


Window test. Direct testing of wood resistance to decay: A study of its fitness, its reliability and its accelerating factor
1984 - IRG/WP 2219
This is the results of an experiment using the window-test specimens, exposing the specimens to three different types of testing procedure: 1. Natural infestation in the open air; 2. Artificial infestation and exposure in the open air; 3. Artificial infestation in a green-house. The results show good similiraties of the three parallel tests in term of decay, and assess the reliability of the windo...
G R Y Déon, L N Trong


Colonisation and detection of New Zealand sapstain fungi
2000 - IRG/WP 00-10329
Sapstain is the bluish black discolouration in logs and timber caused in New Zealand by Sphaeropsis sapinea (Diploida pinea) and more than twenty different species of the Ophiostomataceae Family. Laboratory and field trials were conducted by inoculating radiata pine to establish staining colour and extent of colonisation with various New Zealand sapstaining fungal species. Colonisation patterns, c...
J M Thwaites, R L Farrell


Organic nitrogen in wood: Growth substrates for a sapstain fungus
1993 - IRG/WP 93-10019
The nitrogen content of mature wood from lodgepole pine was 0.046% as determined by micro-Kjeldahl. Low molecular weight proteins between 14 and 21 kDa were identified in mature wood, branch wood and sap pressed from wood chips. Amino acids were quantified in acid-hydrolyzed wood samples and accounted for between 19 and 35% of the nitrogen in wood. The sapstaining ascomycete Ophiostoma piceae stra...
L D Abraham, C Breuil


Previous Page | Next Page