Wood preservatives treatment of black spruce
1997 - IRG/WP 97-40092
A representative sample of black spruce logs from Central Newfoundland was harvested and processed to dressed 2"x4" lumber. Over 400 pieces of lumber were then incised and treated with ACQ preservative in a semi-industrial retort. 9 charges of 20 samples were used to determine treating parameters and 11 charges of 20 pieces were treated using the optimized process. This material was inspected by a...
A R Zahora, J P Hösli


Preliminary desk research in the Netherlands on development of a Knowledge Based System for Life Cycle Assessment of wood products
1997 - IRG/WP 97-50093
TNO is currently coordinating an EC-project (LIFE-SYS WOOD) to develop a consistent approach to Life Cycle Assessment (LCA) of wood products. Existing and new LCA-inventory data of six wood products will be evaluated on reliability and consistency. After validation, LCA-results will be made available through a Knowledge Based System (by 1998-1999). The aim of the KBS is to make LCA-results availab...
P Esser, D Robson, R Vanhauten


Studies in an accelerated soil bed facility on the decay susceptibility of U.K. grown spruce and pine poles treated with copper/chrome/arsenic (CCA) by pressurised sap-displacement. Part 1: Setting up of soil beds and initial soft rot results
1990 - IRG/WP 2344
The paper describes the methodology used in the construction and early operation of an accelerated soil bed facility used to examine the decay susceptibility of U.K. grown Scots and Corsican pine and Sitka and Norway spruce treated with C.C.A. by high pressure sap-displacememt. The design and control of the facility as well as the preparation, soil exposure and soft rot decay analysis of quarter p...
A Bruce, S D Hainey, G M Smith, B King, P D Evans


An analysis of the effects of some factors on the natural durability of pine (Pinus sylvestris L.) and spruce (Picea abies Karst.)
1986 - IRG/WP 1279
The effects of some factors on the natural resistance of pine and spruce sapwood against fungal decay and against attack of house-longhorn beetle larvae have been studied in laboratory tests and the results are evaluated by analysis of variance and regression analysis. Following conclusions were reached: Wood from summer-felled trees did not have a lower inherent natural durability against fungal ...
J B Boutelje, T Nilsson, S Rasmussen


Methods to determine the efficacy of three water repellent additives in waterborne preservatives
1997 - IRG/WP 97-30142
The paper describes the methods used to determine the efficacy of three different water repellent additives in waterborne preservatives. The wooden samples used are pine (Pinus sylvestris) and spruce (Picea abies) that are treated with 9 different waterborne preservatives in retention for hazard class 3 (above ground commodities). There are two sample sizes exposed, cladding boards (19 x 148 mm) w...
F G Evans, B Nossen, K M Jenssen, L R Wilhelmsen, G Fuglum


Creosote and cancer -Cancer incidence among workers exposed to creosote
1990 - IRG/WP 3572
Creosote is a wood preservative that contains polycyclic aromatic hydrocarbons, which are known to be carcinogenic. Cancer incidence among 919 male workers in Sweden and Norway exposed to creosote in the wood preserving industry was studied. The expected numbers of cases were based on the incidence rates of cancer according to the Cancer Registries of Sweden and Norway. A total of 129 cancer cases...
S Karlehagen, A Andersen, C-G Ohlson


The effect of kerfing on check formation in treated white spruce (Picea glauca) poles
1981 - IRG/WP 3167
62 white spruce poles, 6 m in length, were cut from full size utility poles commercially pressure treated with preservative. 21 of the poles were treated with pentachlorophenol, while of the remainder, all of which were treated with ammoniacal copper arsenate, 22 were kerfed and 19 were unkerfed. The poles were installed in the Westham Island field test site, near Vancouver, and inspected annually...
J N R Ruddick


Preliminary indications of the natural durability of Spruce bark board
1999 - IRG/WP 99-10312
A board material made from pressed bark, with no added adhesive, has been developed by Forintek's composites group and tested for durability by Forintek's treated-wood group and the University of Hawaii. This material was also manufactured with veneers in a one-step process. Since one role of bark on the tree is protection against pests and diseases, barkboard was expected to hav...
P I Morris, J K Grace, G E Troughton


Influence of fungal exposure on the redistribution of copper in treated spruce wood
2002 - IRG/WP 02-10450
The redistribution of copper in treated wood after exposure to basidiomycete decay fungi is described. The micro-distribution of copper in copper(II) sulphate or copper(II) octanoate/ethanolamine treated Norway spruce wood before and after exposure to 3 different wood decay fungi was studied using transmission electron microscopy with X-ray microanalysis. The copper content of the mycelium and the...
M Humar, F Pohleven, R J Murphy, D J Dickinson, I Moris, M Zupancic, P Kalan, M Petric


The potential of high pressure pulsation processes to treat white spruce lumber with water-borne preservatives
1988 - IRG/WP 3471
Laboratory work using end sealed 4x8x46 cm³ white spruce samples has been done to explore the suitability of three variants of a 2.1 MPa pulsation process for the impregnation of white spruce with CCA. The results showed that the process improved significantly the penetration of the preservatives and reduced significantly cell collapse, when compared with the results of treatment using a 2.1 MPa ...
J P Hösli, J N R Ruddick


Amenability of radial permeability of Sitka spruce (Picea sitchensis (Bong.) Carr.) as affected by aspects of cell ends in uniseriate ray parenchyma tissue
2003 - IRG/WP 03-40252
The principal objective of this article was to recognise and understand the amenability of ray parenchyma cell ends (end platform) in uniseriate ray tissue to influence the radial permeability of Sitka spruce (Picea sitchensis (Bong.) Carr.) by examination of most (Queen Charlotte Islands in Rhondda, South Wales) and the least (South Oregon in Dalby, North-East England) seed origins that grown in ...
I Usta, M D C Hale


Leaching from field test stakes. Results from two different methods of analysis
1993 - IRG/WP 93-50013
Field test stakes treated with Boliden K33 containing copper, chromium and arsenic exposed at three different fields in Sweden and rejected due to decay, have in two studies been analysed regarding leaching and remaining preservatives. The stakes have been exposed during 20 to 43 years. The density of the stakes and content of copper, chromium and arsenic have been determined in the top part of th...
F G Evans, M-L Edlund


Evaluation of decay fungi in Norwegian buildings
2005 - IRG/WP 05-10562
During a period of 2 years and 3 months (1 January 2001 - 20 March 2003) Mycoteam had 3161 consultations in buildings in southern Norway, 1428 revealing damage from decay fungi. One consultation often revealed several occurrences of fungi, and the total number of occurrences of decay fungi was 3434. Thirty-five different species/genera/groups of decay fungi were recorded. During this period brown ...
G Alfredsen, H Solheim, K Mohn Jenssen


The influence of UV and IR radiation on leaching of copper and chromium from preservative-treated pine and spruce
1992 - IRG/WP 92-3687
The influence of artifical UV- and IR-radiation on the leaching of copper and chromium components of a CCB-preservative from freshly treated pine and spruce was evaluated. On small pinewood samples it could be shown, that the leaching of copper and chromium can considerabely be reduced by UV-radiation. A Philips HPA lamp type reduced the leaching most effective. IR-radiation lead to higher leachin...
H Militz


New method to find out the volatile organic compounds (VOC) of wooden material
2000 - IRG/WP 00-20189
Volatile organic compounds (VOC) of pine, spruce and larch wood were studied using a new technique developed at VTT Chemical Technology. 50 mg of crushed wood material was placed into glass tubes. The tubes were closed with a glass wool, which is pressed with a tube cap. Wood samples were analysed with a gas chromatograph after thermal desorption using four different temperatures (50°C, 100°C, 1...
H Viitanen, K Villberg, K Saarela


Observations on the morphology, ecology and biology of Xylophaga dorsalis (Turton) (Mollusca: Xylophagainae) in the Trondheimsfjord (Western Norway)
1981 - IRG/WP 466
The paper deals with the various aspects of the systematics, ecology and biology of the little known pholad wood-borer, Xyophaga dorsalis (Turton) of the Trondheimsfjord (Western Norway). Diagnostic characters of the species have been given, based on examination of fresh living specimens and accomodating the several morphological variations. A key to the identification of Norwegian species of Xylo...
L N Santhakumaran


Resistance of pine and spruce heartwood against decay - The effect of wood chemical composition and coating with water-borne wood oil product
2006 - IRG/WP 06-10597
Natural durability of wood has been widely studied, but the combination of the natural durability and different treatments has not been the focus of many studies. The durability of wooden products is mainly based on the water permeability and the resistance against organisms. In this study, the water absorption and decay resistance of sapwood and heartwood of Scots pine and Norway spruce were exam...
H Viitanen, S Metsä-Kortelainen, T Laakso


Effect of fungal attack on maximum load capacity of simulated wall assemblies
2007 - IRG/WP 07-20363
The effects of moisture intrusion and fungal attack on the maximum load capacity of nailed assemblies was investigated using one white and one brown rot fungus against 4 material combinations over a 20 week period. Wetting significantly reduced the maximum load capacity of all four material combinations, while wetting and autoclaving only affected the OSB sheathing/spruce stud. The white rot fung...
N Melencion, J J Morrell


Wood furfurylation process development. Part 1: Oscillating Pressure Method
2007 - IRG/WP 07-40376
Furfurylated wood (wood modified by furfuryl alcohol) has over the last years gained marked shares from both tropical wood and conventional preservative treated wood and this has, in turn, generated several research projects concerning process development. The impregnation of spruce is well known from literature to be a difficult task. Furthermore, the sapwood of Scandinavian-grown Scots pine is a...
E Larnøy, M Westin, B Källander, S Lande


Effects of sodium hypochlorite on compression strength and copper retention of spruce wood treated with copper azole and alkaline copper quat
2007 - IRG/WP 07-40362
This work investigates the effects of sodium hypochlorite on compression strength values and copper retention ratios of refractory spruce wood (Picea oriental L.) treated with the waterborne preservative Copper Azole, (CBA-A, Tanalith-E 3492) and alkaline copper quat (ACQ-2200). Before the copper azole and alkaline copper quat treatment, the samples were immersed in 500 ml of sodium hypochlorite s...
S Yildiz, E Dizman, A Temiz, Ü C Yildiz


The effects of chemical modification on the biological properties of alder and spruce particleboards
2007 - IRG/WP 07-40363
This study is evaluated by measuring the weight loss, and the ability of white and brown-rot fungi to attack unmodified and modified particleboards manufactured using spruce (Picea orientalis (L.) Link.) and alder (Alnus glutinosa) chips. The chips were reacted with acetic, succinic, maleic and phthalic anhydride at constant temperature for 3 hours then, hot pressed at 150 °C by using phenol for...
Ü C Yildiz, E Dizman, S Yildiz, A Temiz, M Aslan, E D Gezer


Quantitative and qualitative losses in wood of oriental spruce, Picea orientalis (L.) Link., induced by insects from forest to utility
2008 - IRG/WP 08-10647
In this study, some quantitative and qualitative losses in wood of oriental spruce, Picea orientalis (L.) Link., induced by insects from forest to utility were evaluated. In experimental plots, volume of trees damaged by Dendroctonus micans (Kug.) was 34% of the volume of total standing spruce trees in the oriental spruce forests of Turkey. The volume of standing trees that D. micans damaged was ...
H A Akinci, M Eroglu, G E Özcan, Ü C Yildiz


Effects of acetic acid and nitric acid pre-treatment on copper content of spruce wood treated with CBA-A and CCA
2008 - IRG/WP 08-40406
This work investigates the effects of nitric acid and acetic acid on compression strength values and copper retention contents of refractory spruce wood (Picea oriental L.) treated with the waterborne preservative Copper azole, (CBA-A, Tanalith-E 3492) and copper / chrom / arsenic (CCA). Before the CBA-A and CCA treatment, the samples were immersed in 500 ml of nitric and acetic acid solutions for...
S Yildiz, E Dizman, Ü C Yildiz


Changes in hygroscopic, mechanical and surface properties of Scottish-grown Sitka Spruce (Picea sitchensis) wood subjected to dry heat treatment
2008 - IRG/WP 08-40415
Heat-treatment is a wood modification method which has been used to some extent in improving timber quality. However, the main limitation in the use of this technique despite its numerous advantages is the adverse effects on the various properties associated with the use of wood as an engineering material. Dry heat treatment of Scottish-grown Sitka spruce (Picea sitchensis) wood was carried out at...
L Awoyemi, M C Jarvis, A Hapca


Effects of CCB on wood strength of Eastern spruce (Picea orientalis L.)
2008 - IRG/WP 08-40416
The effects of CCB (chromate copper boron) on the static bending properties of Eastern spruce (Picea orientalis L.) based on MOE (modulus of elasticity) and MOR (modulus of rupture) were evaluated after full-cell vacuum/pressure treatment using a 3.0 % concentration followed by kiln-drying at 15 and 30 % moisture contents with heating the preservative at 30 and 40 ºC. The results showed that MOE ...
I Usta, M Hale