Mould growth on spruce claddings and the effect of selected influencing factors after 4 years of outdoor testing
2015 - IRG/WP 15-30671
Norway spruce (Picea abies) is the most frequently chosen wood species as claddings in façades in Norway, and is used both coated and uncoated. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more often growth of mould and blue stain fungi is the main challenge. A field test with synchronous monitoring of relative humidity, air temperature, material temperature and wood moisture content in Norway spruce claddings has been performed in southern Norway as part of the ClimateLife project. Visual evaluation of blue stain and mould growth according to EN 927-3 was performed, and evaluation data after 46 months exposure is presented. The objectives were to study the effect of 1) environment, 2) cardinal direction and 3) colour of the coated surface on growth of blue stain and mould fungi and to study the variation in relative humidity, air temperature, wood moisture content and material temperature. After 46 months exposure, the red coating system had generally the lowest mould ratings and the uncoated claddings had the highest. Of the white coloured claddings the ones facing south had lower mould ratings than those facing north, but the opposite were found for red coloured claddings. The relative humidity was higher in front of claddings exposed northwards and in a shaded environment compared to an open environment against south. In an open environment red coloured claddings had the lowest wood moisture content and highest material temperature, and red coloured claddings against south had the highest maximum material temperature.
L Ross Gobakken, G I Vestøl


Some comments on durability testing of WPC according to EN 15534-1
2015 - IRG/WP 15-40695
The standard EN 15534-1 (2014) gives advice for broad characterization of WPC materials and products. It contains instructions for test procedures concerning different properties e.g. mechanical properties, thermal properties, as well as durability. In this paper some WPC materials from the market were tested for their resistance against brown rot. Furthermore, the water uptake and bending prope...
S Bollmus, A Gellerich, H Militz


How does the test methodology influence the outcome of durability testing of thermally modified wood
2015 - IRG/WP 15-40699
Thermally modified wood is commercially available on the European market since many years. Today, many production units with various production capacities and different modification processes exist. Industrial scale wood heat treatment processes, under the trade name of ThermoWood were developed in Finland. ThermoWood has two standard treatment classes with different target properties, namely Ther...
A Gellerich, S Bollmus, H Militz


Global survey on durability variation – on the effect of the reference species
2016 - IRG/WP 16-20573
Climate change due to anthropogenic emissions is the largest environmental challenge of our time. Forest-based value chains play an important role in reducing the accumulation of CO2 in the atmosphere. Maximizing the use of wood to tackle climate change requires improved understanding of the service life of timber products. This information can best be obtained from field testing and while there i...
R Stirling, G Alfredsen, C Brischke, I De Windt, L P Francis, E Frühwald Hansson, M Humar, J Jermer, M Klamer, M Kutnik, P Laks, I Le Bayon, S Metsä-Kortelainen, L Meyer-Veltrup, P I Morris, J Norton, T Singh, J Van Acker, J Van den Bulcke, T M Venås, H Viitanen, A H H Wong


Moisture induced risk and fungal development in various field test set-ups in and above ground
2016 - IRG/WP 16-20577
A high number of studies on the decay performance of wood in outdoor exposure have been conducted in the past. However, no testing methodology for wooden components exposed above ground reflecting the variety of different loads has been established so far. Many test protocols were modified in different ways throughout the years and results were often published in an encoded or incomplete way. This...
L Meyer-Veltrup, C Brischke


Bundle tests - Simple alternatives to standard above ground field test methods
2016 - IRG/WP 16-20581
Within this study we applied different new above ground test set ups to untreated Norway spruce (Picea abies Karst.) and Scots pine sapwood (Pinus sylvestris L.) which are frequently used as reference or control species in wood durability field tests. The overall aim of this study was to find a simple alternative method to the few standardized above ground field test methods, such as the L-joint a...
C Brischke, L Meyer-Veltrup


Modelling the performance of bio-based building materials
2016 - IRG/WP 16-20582
The ‘bio-based economy’ represents a growing area of development globally and covers a wide range of building materials including wood and wood-based products. A ‘bio-based’ material is intentionally made from substances derived from living (or once-living) organisms. In this context it means that the materials and products are made from renewable resources, with the criteria that a renewa...
C Brischke


Evaluation of field test data
2016 - IRG/WP 16-20594
The resistance against fungal decay and insect attack of wood can be highly variable, between boards and even within boards. The variability in durability is not always an issue, but for high demanding applications information about its reliability is required. This comprises the variability of outdoor performance. Durability testing in laboratory and outdoor exposures can provide a good basis to ...
F Bongers, C Brischke, J Van den Bulcke, W Gard, I De Windt, H Militz


Estimation of wood degradation determined by visual inspection, mechanical testing and DNA characterisation – report after 3 years of exposure
2016 - IRG/WP 16-30700
The influence of two separate treatments, thermal modification and alkaline copper quaternary (ACQ, Silvanolin©) treatment, on fungal decay, visual disfigurement, deterioration in mechanical properties and fungal community structure was assessed on Norway spruce (Picea abies) and compared with the performance of two naturally more resistant tree species native to North America: Douglas fir (Pseud...
N Thaler, T Martinović, M Bajc, D Finžgar, H Kraigher, A Sinha, J J Morrell, M Humar


Durability Testing of a Cattail (Typha spp.) based Insulation Material against Termite Attack
2017 - IRG/WP 17-10879
The use of insulating materials is particularly important in the construction industries, especially with regard to the use of wood and naturally occurring substances. The use and durability of natural materials as insulating materials is of keen interest to many construction experts, and continues to be a topic of intense investigation. It is generally agreed that the use of natural substances ...
M Dass, W Unger, T L Woods


Comparative studies on the durability of English oak (Quercus robur L.) under in-service, field and laboratory conditions
2017 - IRG/WP 17-10881
The durability of many wood species varies due to differences in extractive content, anatomical features, growth conditions, and not at least in dependence of the respective exposure conditions either under test or in real life applications. And so does the durability of English oak (Quercus robur L.), which has recently been considered in the revised European standard EN 350 (2016) and is now cla...
C Brischke, L Meyer-Veltrup, A Soetbeer, M Höpken, E Melcher, J Trautner


Laboratory test to determine the effect on durability of combining biobased building materials with timber in construction
2017 - IRG/WP 17-20604
The use of Structural Insulated panels is a construction approach that is seeing more abundant use and is becoming a widely available method. Preformed units are usually a composite structure which often include a range of bio-based materials such as timber, wool or straw. Traditional laboratory based wood decay tests do not take into account this combination of biobased materials and it may be po...
S F Curling, G A Ormondroyd


Bio-deterioration of Southern Pine Stakes at Geographically Different Testing Sites
2017 - IRG/WP 17-20609
Southern pine (SP) sapwood is commonly used in preparing the standardized stakes for performance testing as referenced in the American Wood Protection Association (AWPA) Book of Standards. For example, the standardized above ground test methods E16/E18 and the standardized ground contact test method E7 all use sapwood of SP as the preferred wood species for preservative performance test. In this...
Jun Zhang, J Horton


Testing of the resistance of acetylated wood against marine borers at three Italian sites
2017 - IRG/WP 17-30719
The aim of this research is the determination of resistance of acetylated wood against marine biodeterioration in use class 5 (EN 335) in temperate sea waters. The resistance of acetylated Pinus radiata (radiate pine) in solid and MDF form is compared with that of the untreated radiata pine and other untreated wood of European species such as Fagus sylvatica (European beech) Castanea sativa (chest...
S Palanti, M Faimali, D Tagliapietra, M Andrenacci, M Anichini, M Sigovini


Testing the durability of timber products above ground using the block-test method – A critical review
2018 - IRG/WP 18-20637
The block-test method for testing the durability of wood and wood products above ground is reviewed critically with respect to practical aspects, moisture loads, corresponding decay development, and the possibilities of assessing test specimens by determining the dynamic modulus of elasticity (MOEdyn) of wood. In total, 36 blocks representing different modifications of the original set-up and a wi...
C Brischke, A Gellerich, H Militz


Above-ground testing methods – review of Rotorua, New Zealand test site results after ten years
2018 - RG/WP 18-20642
A series of seven different types of above ground durability tests were initially conducted over four years to determine which type of tests would give the fastest, most consistent results. Five types of test; ground proximity, two types of decking, flat panels and double layer, were reassessed after ten years. Exposure conditions varied between tests with ground proximity producing close to groun...
D Page, T Singh


Resistance of modified wood to termite attack assessed in laboratory and field testing: A review of internal research
2018 - IRG/WP 18-40824
Within the past decades, new wood modification technologies have been investigated in order to improve certain wood characteristics and enable the use of timber products for outdoor applications. Some of these non-biocidal technologies have been developed and commercialized recently. Thus, various material properties were studied intensively and shown to be improved. To a great extent, previous re...
L Emmerich, P Gascón-Garrido, H Militz


Selection of heat flux value for wood fire retardants testing using MLC
2018 - IRG/WP 18-40846
One of more crucial elements of investigating treated wood combustion properties with the use of a cone calorimeter is a proper selection of heat flux (HF). The HF level is directly reflected in time to ignition and a thermal degradation degree. The ignition of raw wood or of wood ineffectively protected against fire occurs at a low HF level, i.e. 10-20 kW/m2. By contrast, the ignition of wood whi...
B Mazela, W Perdoch, W Grześkowiak, A Batista


Exploring the use of X-ray micro CT as a tool for the monitoring of moisture production and mass loss during lab-based fungal degradation testing
2019 - IRG/WP 19-20654
Bio-based building materials, such as wood and wood-engineered products, are susceptible to degradation by decay fungi. In-depth knowledge on the intricate material-fungus relationship as well as performance data for many bio-based building materials are still lacking, and especially knowledge on how a material’s structure and moisture properties affect the degradation process is missing. Althou...
L De Ligne, J Van den Bulcke, A De Muynck, J M Baetens, B De Baets, L Van Hoorebeke, J Van Acker


Improvement of analytical methods of wood preservatives and its validation with collaborative testing
2019 - IRG/WP 19-20655
This discussion paper presents on-going collaborative test of analytical methods of wood preservatives according to the standardization process of Japan Agricultural Standard (JAS) by the Ministry of Agriculture, Forestry and Fisheries (MAFF). Food and Agricultural Materials Inspection Center (FAMIC) in close cooperated organization with the MAFF, has wide range of tasks about inspections and anal...
T Miyauchi, K Yamamoto, N Shota, Y Akabori, M Ikeda, J Eisawa, K Kambara, T Osawa, C Igarashi, Y Baba, W Ohmura, M Shimizu, M Samejima


Performance of field cut preservatives above-ground and in ground contact exposures
2019 - IRG/WP 19-30742
Field cut preservatives are needed to protect cut ends and drill holes that expose the untreated interior of preserved wood. A series of field cut preservatives were assessed in ground contact and above-ground exposures. After 10 years in ground contact exposure, all of the untreated controls had failed or exhibited very advanced decay. In contrast, the copper naphthenate (2% Cu in mineral spirits...
R Stirling, D Wong


Durability testing of mass timber building elements: a call for a collaborative trial
2019 - IRG/WP 19-40875
Mass timber buildings have captured the imagination of architects and engineers seeking more environmentally friendly building materials. The mass timber movement has tremendous potential to markedly increase timber use in mid-rise to high rise buildings. With great promise, however, comes great risk. Most mass timber structures that have been built or are being planned use no protective treatm...
J J Morrell


Performance of naturally durable decks after 15 years of field exposure
2020 - IRG/WP 20-10963
A decking test of Canadian species considered to be naturally durable was inspected after 15 years of exposure at test sites in Ontario and British Columbia. Based on the materials used in this experiment, Douglas-fir and yellow cypress had the greatest decay resistance, followed by eastern white cedar and western redcedar, and then by western larch and tamarack. All materials tested were more dur...
R Stirling, D Wong


The role of specimen format in wood durability testing
2020 - IRG/WP 20-20672
The experimental basis for testing the biological durability of wood are often incubation experiments with wood-destroying basidiomycetes. Numerous parameters can affect the mass loss by fungal decay (MLF) in laboratory durability tests and therefore being decisive for the resulting durability classification. Among others, the dimension of the wood specimen and the time of incubation impact on fun...
C Brischke, L K Grünwald, S Bollmus


Development of procedures for sampling, testing, and classification to determine the biological durability of wood and wood products
2020 - IRG/WP 20-20676
This paper informs about a research project, which deals with several shortcomings and a lack of clarity within EN 350:2016. The project started in January 2020, will run for 3 years, and is operated by the Institute of Wood Technology Dresden (IHD) and the University of Goettingen (UGOE). Determination and classification of durability of wood and wood products against wood-destroying organisms ...