IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 638 documents. Displaying 25 entries per page.


Natural durability of 4 different Larix species tested in soil contact
2002 - IRG/WP 02-10434
Importers of Siberian Larch claimed to have a material which can replace pressure treated wood in soil contact. This gave reason to investigate the durability of 4 different Larix species (L. decidua, L. sibirica, L. decidua x sibirica, L. gmelini var ologenis) coming from 7 different origins in comparison with sapwood of Pinus sylvestris untreated as well as pressure impregnated with retentions o...
A O Rapp, H Viitanen, T Nilsson


Natural durability, density and extractive contents of 42 wood species of Bangladesh.
2003 - IRG/WP 03-10490
Natural durability, density and major extractive contents of 42 lesser used or unused wood species of Bangladesh have been studied. Correlation analysis between these properties has been performed. It has been shown that natural durability of these species neither explained by water soluble nor by alcohol benzene extractive contents. Density has a weak but significant positive correlation with dur...
S Akhter, K Akhter, S C Das


Resistance of various wood species against decay by Coniophora cerebella (Pers) Duby and Lenzites trabea (Pers) Bres
1976 - IRG/WP 142
Both fungi, Coniophora cerebella and Lenzites trabea, are important destroyers of timber. Coniophora often occurs inside buildings and Lenzites trabea has been observed on southern facades of buildings, on balconies and window frames. In most instances that we investigated coniferous timber had been decayed. But both species are known to attack also various hardwoods. For this reason tests similar...
O Wälchli


Natural progression of decay in unrestrained, Southern pine sapwood exposed above ground
1995 - IRG/WP 95-20060
In this study, the natural progression of decay is being monitored in 2.4-m (8-ft) lengths of dimension lumber. The 2.4-m lengths are supported without restraint in a horizontal plane approximately 0.75 m above ground in a partially shaded field plot in southern Mississippi. The lumber is 100% sapwood. Prior to installation in the field, each piece was planed to exactly 38 by 89 mm² (1.5 by 3.5 i...
R C De Groot, R J Ross, W Nelson


Silafluofen, a new insecticide against wood-boring insects and termites
1991 - IRG/WP 3666
Hoe 084498 (proposed common name: Silafluofen) is a new insecticidal compound from Hoechst Aktiengeesellschaft and has been extensively tested to determine its potential use as an insecticide against wood-boring insects and soil termites. Various tests in official institutes indicate a good activity against several wood-boring insects and soil termites. The active ingredient is resistant to weathe...
G Rustenburg, C J Klaver


Leaching of active components from preservative-treated timber - Ongoing research: Status after approx. 4 months’ out-door exposure
2003 - IRG/WP 03-20276
The Danish Technological Institute is together with manufacturers of active ingredients and formulators of wood preservatives running a project aiming at finding realistic leaching rates from preservative treated wood in hazard class 3 (above ground). The project is focussed on developing a field trial method for investigating leaching. According to BPD hazard assessment has to be carried out f...
N Morsing


Some recent studies on the marine wood-borers of the west coast of India
1982 - IRG/WP 486
Occurrence and distribution of marine wood-borers along the west coast of India from Mangalore to Kandla are presented together with the distribution pattern of all the molluscan and crustacean wood-borers so far reported from India coasts. The survey, conducted for the first time along this coast, revealed the presence of 14 species of Teredinidae, 2 species of Pholadidae, 3 species and one varie...
L N Santhakumaran


X-ray photoelectron spectroscopic analysis of CCA treated wood
1992 - IRG/WP 92-3700
Ponderosa pine and Douglas-fir wood sections were treated with CCA preservative. To elucidate the mechanism of fixation of the CCA, the wood surface was analyzed by X-ray photoelectron spectroscopy (XPS). CCA treatment increased C1 (carbon bonded to carbon and/or hydrogen) and decreased C2 (carbon bonded to one oxygen) in XPS C1s spectra, both in unextracted and pre-extracted sections. This sugges...
J N R Ruddick, K Yamamoto, P C Wong, K A R Mitchell


Natural resistance of timbers to marine borer attack. A laboratory test with Limnoria tripunctata
1977 - IRG/WP 430
Attack of the timber specimens was much less severe in the laboratory than in some marine localities. This is not surprising. One reason is certainly that wood-boring molluscs (Teredinidae and Pholodidae) which were missing in the laboratory are the most important wood-destroying organisms in the open sea. Another reason is that it is not possible to offer the gribbles optimal environmental condit...
H Kühne


The natural durability assessments of secondary timber species - field trials
1998 - IRG/WP 98-10297
Secondary or 'alternative' hardwood timber species can replace traditional hardwoods and contribute significantly to satisfying the overall demand for hardwoods in the UK timber market. A selection of these 'alternative' hardwoods is currently being tested at BRE-WTC for natural durability both in ground contact (to EN252) at two field sites, and out of ground c...
E D Suttie, R J Orsler


Eucalyptus globulus. Impregnability in relation with plantation and crop
1992 - IRG/WP 92-2402
Eucalyptus globulus Lasill is currently classified in Pr EN 350 on the basis of the characteristics of the first log. In practice, there are usually several following crops of branches developped on each stump in plantations. Up to a diameter of 8 cm, round wood of 2nd crop and further crops present a maximum of sapwood and characteristics which differ significantly from the basic classification a...
D Dirol


Fungitoxic effect of the quaternary ammonium compounds preservatives against Basidiomycetes by using agar-plate and agar-block methods
1996 - IRG/WP 96-30118
Results of investigations on the fungitoxic value of three versions of wood preservatives based on the quaternary ammonium compounds (lauryldimethylbenzylammonium chloride, lauryldimethyl-benzylammonium bromide and alkylbenzyldimethylammonium chloride) and borates in relation to the wood destroying fungi have been presented. The agar-plate (screening) and agar-block method were applied. A wide ran...
J Wazny, P Rudniewski


Combustion properties of Alder wood treated with some new environment friendly natural extractives. Part 1. Effect of Natural Tannins on the Combustion Properties
2002 - IRG/WP 02-40234
Powders of the brutia pine bark, sumach leaves, acorn, gall-nut and boric acid and borax which are known as potential environment friendly wood preservatives were impregnated according to ASTM D 1413-88 in order to determine their combustion properties. A commercial treatment compound, Tanalith-CBC, was also used for comparison. The results indicated that the natural extractives did not have an...
Ü C Yildiz, A Temiz, E D Gezer, S Yildiz


Treatability and natural durability of some lesser used or unused wood species of Bangladesh
2000 - IRG/WP 00-40170
A research study was conducted to determine the natural durability and treatability of heartwood of some lesser used or unused wood species. The treatability of species has been studied along with certain anatomical concepts association with preservative penetrability of the wood. It was observed that grain structure and presence of tyloses appeared to be correlated with penetrability of the wood....
K Akhter, M Younusuzzaman, M H Chowdhury


Metal Leaching from Pressure Treated Wood in Sanitary Landfill Leachate
2004 - IRG/WP 04-50220
Pressure treated wood products contain heavy metals to prevent biological decay. Scrap treated wood from construction activities and demolished structures containing treated wood are typically disposed in landfills. To examine the potential mobility of metals from pressure-treated wood disposed in landfills, wood samples were leached using leachate from lined landfills and the concentrations of ar...
B Dubey, T G Townsend, H M Solo-Gabriele


Leaching from CCA-impregnated wood to food, drinking-water and silage
1987 - IRG/WP 3433
During the last years The Norwegian Institute of Wood Technology (NIWT) has analysed different foodstuff for contamination by copper, chrome and arsenic from CCA-impregnated wood. There has been some interest for using CCA-impregnated wood in contact with food and drinking-water. Before giving their permission the Norwegian Health Authorities want results from experiments. NIWT therefore started t...
F G Evans


Biofumigation of sapstaining fungi using natural products
2002 - IRG/WP 02-10428
Control of deep-seated fungal infections in raw logs of radiata pine continues to be a challenge for achieving consistent and satisfactory protection of high value logs destined for export markets. To develop solutions for this problem, a study was undertaken to investigate inhibition of spore germination and growth of sapstaining fungi by volatiles released from a selection of natural products. ...
B Kreber, C Chittenden, R N Wakeling


Variation in natural durability of British grown Douglas fir ((Pseudotsuga menziesii (Mirb.) Franco). Part I. Effect of density and growth rate
2002 - IRG/WP 02-10445
Seed origin trials of Douglas fir (Pseudotsuga menziesii) in Britain have provided important information on growth differences between origins (Lines, 1987), but the variation in wood properties between origins has not been reported. The present paper describes a study of the variation in natural durability against two brown rot fungi (Coniophora puteana and Postia (Poria) placenta) and in a fung...
S Akhter, M D C Hale


Applications of the shower test. Part A: Results from CCA type C treated wood: influence of fixation process
1993 - IRG/WP 93-50009
This report outlines the results of shower tests conducted on CCA type C treated wood. The results indicate the inherent good fixation of CCA type C, as judged by the leaching limits within the Environmental Regulations. The shower test has proven to be a useful quality control and research test. It determines reasonably accurately the leaching under simulated conditions and, admittedly from a lim...
W J Homan, H Militz, D A Lewis


Kinetics and mechanism of fixation of Cu-Cr-As wood preservatives. Part 5: Effect of wood species and preservative composition on the leaching during storage
1975 - IRG/WP 354
Conversion reactions during storage of CCA treated wood take place even at and below the fiber saturation point as long as ion transport is possible. Increase in drying temperature increases the final pH of the treated wood and the leachability of Cu and decreases slightly the leachability of Cr, while the leachability of As is not affected. This temperature effect is considered to be of no techni...
S-E Dahlgren


Venezuelan net of test fields for the study of the effectiveness of treatments of non commercial timbers from natural tropical forests
2005 - IRG/WP 05-20318
A net of 13 tests fields were established in Venezuela for the study of the effectiveness of the CCA and CCB treatment in secondary or non commercial woods from natural forests, two woods from fast growth plantations wee included for promote them as treated timber mainly for fence posts uses. Partial results after two years are presented and discussed the preliminary results obtained both in field...
O Encinas, N Mora


Durability of exterior natural wood finishes in Brazil
1985 - IRG/WP 3343
Wood finishes systems were evaluated in natural weathering conditions during 5 (five) years, over "Parana-pine" (Araucaria angustifolia). Test samples results show that: - Semitransparent wood preservative stains, based on polimerized linseed oil, provided very good protection to the wood, compared with the one based on alkyd varnish; - Solid color wood preservative stains provided good durability...
D R Macedo


Durability of Anogeissus acuminata timber used for plank-built catamarans
2005 - IRG/WP 05-10551
Catamaran, the most versatile traditional fishing craft used along the Indian coast is made hitherto of solid timber of a few selected species of broad-leaved soft woods. Due to scarcity coupled with high cost of these timbers, the craft, of late, are fabricated from the wooden planks of an indigenous hardwood species, namely, Anogeissus acuminata (Yon) belonging to the family Combretaceae. Infor...
M V Rao, M Balaji, V Kuppusamy, K S Rao


Influence of felling time on the natural durability of norway spruce (Picea abies (L.) Karst.)
1998 - IRG/WP 98-10250
Natural durability was tested in a laboratory test according to EN 113. The test fungi were Coniophora puteana and Poria placenta. Additionally, the test method was modified by using water agar instead of malt agar, so that wood was the only nutrient source for the fungi. In a third attempt the samples were inoculated with Trichoderma harzianum before testing. The trees were felled on the 22.7.97...
M Hirmke, K Messner, J Fellner, A Teischinger, R Wimmer


Natural durability of fifty species of Indian timber in Goa waters against marine wood-borers
1989 - IRG/WP 4150
Results of the investigations on the natural durabilitv of fifty species of Indian timber, based on data collected bv exposing test panels at Betim near Panaji (Goa) continuously for a period of 11 months are presented. The study revealed that none of the timber species tested has any natural resistance at this locality and all the panels were completely destroyed within 11 months. Details on the ...