Developments in wood preservation
1978 - IRG/WP 3121
The purpose of this paper is to comment very briefly upon recent developments and trends in wood preservation so that members of this Working Group have a basic knowledge of activities in other countries. The last paper was prepared in September 1977 and the present paper refers to developments since that time....
B A Richardson


The proposal for optimalization of the agar-block method for wood preservatives fungitoxic evaluation
1995 - IRG/WP 95-20065
On the base of own research and other scientists results the proposal for optimalization of agar-block method was presented by: - selection of test fungal species and strains and central distribution of their pure cultures, - change of the treatment and control samples exposure procedure, - application of mathematical estimation of toxic value results, - shortening the duration of fungitoxic t...
J Wazny


Criteria for basidiomycetes testing and ways of defining natural durability classes
1998 - IRG/WP 98-20144
Within the framework of a European research project several laboratories have tested a series of 17 wood species covering the total range of natural durability. Basidiomycete tests are part of the total set up. Although generally based upon standard methods some minor differences in execution of the tests were evaluated for their impact on the results. This variation was superimposed with the fac...
J Van Acker, M Stevens, J K Carey, R Sierra-Alvarez, H Militz, I Le Bayon, G Kleist, R-D Peek


Transmission poles with sub-standard retentions protected by Field Liners outperform standard poles in service
1997 - IRG/WP 97-40095
Eucalyptus cloeziana 12m transmission poles were treated with sub-standard creosote retentions of 80kg/m3 and Field Liners were fitted to the poles before they were placed in service at Umbumbulu, Kwazulu Natal. Poles treated with standard creosote retentions of 130kg/m3 but without Field Liners were also placed in service in the same area. Core samples were taken from both groups of poles after 1...
M R Behr, G D Shelver, A A W Baecker


SEM of wood dust particles
1997 - IRG/WP 97-50084
Dust particles from beech and oak trees have been classified in Germany as being "working materials which are definitely carcinogenic to humans". All other wood dusts, including those from softwoods, are classified as being materials "with reasonable suspicion of carcinogenic potential". The carcinogenic principle of action continues to remain unclear. The mechanical irritation is one of a number ...
U Schmitt, R-D Peek, A O Rapp


Effect of wood moisture on ability of Sphaeropsis sapinea to colonise Pinus radiata
1999 - IRG/WP 99-10311
The factors influencing colonisation of unseasoned radiata pine logs by sapstaining fungi which can result in detrimental wood discolouration, are being explored. The objective of the current study was to determine the effect of wood moisture content on fungal growth and wood colouration (melanisation). Five replicate trials were set up using increment cores (10mm diameter) which were taken from ...
B Kreber, D R Eden, R N Wakeling, C M Chittenden, J G Van der Waals, B Carpenter


Rapport sur l'activité du CEN/TC 38 "Méthodes d'essais des produits de préservation du bois"
1982 - IRG/WP 2188
M Pottevin


Questionnaire: The use of computers in wood preservation research
1985 - IRG/WP 2240
E F Baines


The effect of steam conditioning on Southern yellow pine treated with copper naphthenate
1997 - IRG/WP 97-40086
The current study was undertaken to investigate the influence of steam conditioning on Southern yellow pine treated with copper naphthenate (Cu-N). Pre-steamed and /or kiln-dried Southern yellow pine were pressure treated with Cu-N. After treatment, one group of samples were post-steamed. It was found that samples changed color from green to dark-brown after post-steaming. To elucidate the effect ...
Jun Zhang, D P Kamdem, M H Freeman, R D Arsenault


The use of the Pilodyn for detecting soft-rot decay in CCA treated eucalypt poles
1986 - IRG/WP 2251
A 6 Joule Pilodyn unit with 2.5 mm diameter pin was used to inspect CCA treated eucalypt poles, suspected of suffering groundline soft-rot decay. Pole plugs were removed at the inspection region and the amount of soft-rot decay present determined microscopically. High correlation (R² = 0.73) was obtained between the amount of soft-rot and Pilodyn pin penetration. The Pilodyn is recommended as a u...
L E Leightley, G A Willoughby


Patterns of bacterial attack in preservative treated eucalypt power transmission poles
1984 - IRG/WP 1223
Patterns of bacterial decay have been examined using light and scanning electron microscopy. Two morphologically distinct patterns have been recognised in preservative treated eucalypt power transmission poles. Bacterial Decay I (BDI) involves the removal of the secondary wall layers initiating with erosion of the S3 layer from the cell lumen. As decay progresses the S2 layer and S1 layer are degr...
G A Willoughby, L E Leightley


Leaching of CCA from Pinus patula during marine trials in the southern hemisphere
1991 - IRG/WP 4167
Pinus patula stakes were treated with CCA to retentions of 31 kg/m³ salts, and were sited in the sea of Port Alfred, South Africa, for two years. Samples were then removed to the laboratory and analysed as before for copper and arsenic. Prelimiary data showing CAA losses from these stakes in the marine environment showed that CCA was longitudinally leached from them, and was also transversly redi...
G D Shelver, C D McQuaid, A W W Baecker


Towards a colour assay of wood degradation
1982 - IRG/WP 2180
A colour assay for the enzyme catalase is described. Since the activity of this enzyme has previously been shown to be correlated with degree of wood degradation as determined by other methods, this assay may provide a rapid quantitative indicator of superficial and internal wood decay....
M A Line


Influence of variable lignin content on brown rot decay of wood
1987 - IRG/WP 1320
Compilation of published data and new experiments with brown-rotting fungi on different timber species suggest that their decay activity, in contrast to soft rot and white rot fungi, is not greatly influenced by the type or amount of lignin present....
T Nilsson, G F Daniel


Penetration of deltamethrin in micro-emulsion formulation after injection in wood
1996 - IRG/WP 96-40068
In the Netherlands (and some other European Countries) the remedial treatment of death watch beetle is still a problem. This is because the larvae of this insect penetrate the central heartwood of mainly large oak beams. The heartwood is difficult to treat. The preventive treatment of wood boring insects has only recently been permitted in the Netherlands. Since 1989 injection of insecticides is r...
P Esser, W L D Suitela


Less environmental impact of wood preservatives by considering the risk of attack in addition to the hazard class system
1995 - IRG/WP 95-50040-10
Hazard classes, which are standardized in Europe in EN 335, are most useful to direct chemical wood preservation towards the organisms which may attack wood in the various fields of utilisation. However, hazard only signifies the fact that an attack may occur without considering the actual risk to attack. To minimize the application of chemicals with respect of less environmental impact it is nece...
H Willeitner


Soil contamination at the wood preservation industry: Treatment technologies
2001 - IRG/WP 01-50166-16
The soil is a specific compartment of the biosphere, because it is not only a geochemical sink for contaminants, but it also acts as a natural buffer, controlling the transport of chemical elements and substances to the atmosphere, hydrosphere, and biota. Soil contamination problems are expected at wood preservation sites, particularly at those which use(d) inorganic wood preservatives or creosote...
A B Ribeiro, L M Ottosen


Reference numbers of papers of the International Research Group on Wood Preservation issued to date
1970 - IRG/WP A 4
IRG Secretariat


A bibliography of organic solvent-based wood preservatives
1973 - IRG/WP 313 E
H Alliot


Heat treatment of wood strands for OSB production: Effect on the mechanical properties, water absorption and dimensional stability
2002 - IRG/WP 02-40238
The effect of heat treatment on the mechanical and physical properties of commercial OSB strands was evaluated. Heat treatment was applied under inert atmospheric conditions to wood strands. The aim of this study was to examine the heat treatment parameters to achieve significant reduction of thickness swelling (upon exposure to moisture in service) without causing excessive reductions in stren...
G J Goroyias, M D C Hale


A Vision for the Future
2002 - IRG/WP 02-20257
This paper focuses on the future of the pressure preservative treatment industry in North America, but also considers the potential role of aspects now considered peripheral. It puts forward the premise that the wood preservation industry risks extinction if it does not evolve. The driving forces for evolution are reviewed and the internal constraints are discussed. A number of alternative stra...
P I Morris


The efficacy of polyurethane coatings on wood samples exposed in the marine environment. Final Report -10 Year Assessment
1996 - IRG/WP 96-10170
The results of an IRG collaborative marine trial to investigate the long-term permanence and efficacy of polyurethane coatings against marine borers are reported. PU-coated wood samples were exposed at a range of sites from tropical to cold temperate locations. The marine borer species present at the sites included teredinids, pholads, limnoriids and sphaeromatids so that each site offered its own...
R A Eaton


Tebuconazole - a new triazole fungicide for wood preservation
1991 - IRG/WP 3680
The great potential of Tebuconazole for wood preservation is demonstrated. Test carried out by official institutes shown that Tebuconazole is particularly effective against wood-rotting basidiomycetes strains. The efficacy of Tebuconazole against the brown rot Gloeophyllum trabeum is outstanding: the toxic value measured in accordane with EN 113, without·ageing, after leaching (EN 84) and after e...
O Exner


Agenda Special Seminar: Screening techniques for potential wood preservative chemicals
1978 - IRG/WP 2115
IRG Secretariat


Biocide Treatments for Wood Composites - A Review
2006 - IRG/WP 06-40323
This paper reviews the biocidal treatment of wood composites. Included are in-process and post-process treatments. Various biocides are covered as are methods of application. Novel treatments and technologies are also presented....
J W Kirkpatrick, H M Barnes