Reducing Extractives Stain in Western Red Cedar Sidewall Shingles
2014 - IRG/WP 14-30654
One of the aesthetic challenges that western red cedar shingles face is extractives redistribution stain, particularly in unpainted sidewall applications. Dip and pressure treatments with a mixture of quaternary ammonium compounds and alkyl amine oxides were investigated for their ability to prevent this stain. After nine months of exposure in Vancouver, extractives stain was present on nearly all...
R Stirling


The role of hydrophobins in surface growth by the Blue Stain fungi Aureobasidium pullulans
2015 - IRG/WP 15-10837
Hydrophobins are small proteins found exclusively in filamentous fungi. These proteins are able to assemble spontaneously into amphiphilic monolayers at hydrophobic–hydrophilic interfaces. Hydrophobins have a diverse role, e.g. allowing the fungi to break through interfaces during aerial hyphae formation, sporulation, fruit body production and cell penetration. In this ongoing study, we are look...
J Stenbæk, L Riber, J Blæsbjerg Nielsen, C Møller Hansen, B Jensen


The whitening cause of Korean wooden heritage by flame retardant treatment
2015 - IRG/WP 15-20560
Korean wooden heritage used to treat by flame retardants in order to protect fire. There are 2 types flame retardant using for wooden heritage. These flame retardants treatment are basic measure that apply to wooden heritage along with other fire protection. The flame retardants cause white stains by reacting with Korean traditional wood painting (Dancheong) and increase wood humidity. The Korean ...
Jin Qyu Kim, Gyu-Seong Han, Yong Jae Chung, Hwa Soo Lee, Dong Won Son


Mould growth on spruce claddings and the effect of selected influencing factors after 4 years of outdoor testing
2015 - IRG/WP 15-30671
Norway spruce (Picea abies) is the most frequently chosen wood species as claddings in façades in Norway, and is used both coated and uncoated. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more often growth of mould and blue stain fungi is the main challenge. A field test with synchronous monitoring of relative humidity, air temperature, material temperature and wood moisture content in Norway spruce claddings has been performed in southern Norway as part of the ClimateLife project. Visual evaluation of blue stain and mould growth according to EN 927-3 was performed, and evaluation data after 46 months exposure is presented. The objectives were to study the effect of 1) environment, 2) cardinal direction and 3) colour of the coated surface on growth of blue stain and mould fungi and to study the variation in relative humidity, air temperature, wood moisture content and material temperature. After 46 months exposure, the red coating system had generally the lowest mould ratings and the uncoated claddings had the highest. Of the white coloured claddings the ones facing south had lower mould ratings than those facing north, but the opposite were found for red coloured claddings. The relative humidity was higher in front of claddings exposed northwards and in a shaded environment compared to an open environment against south. In an open environment red coloured claddings had the lowest wood moisture content and highest material temperature, and red coloured claddings against south had the highest maximum material temperature.
L Ross Gobakken, G I Vestøl


Susceptibility of wood substrates to Aurebasidium pullulans at different temperatures
2016 - IRG/WP 16-10863
There is an increasing awareness of how the aesthetical performance of wood exposed outdoors changes over time and especially in the first few years after installation. Mould and blue stain fungi are biological agents that contribute to the weather grey colour on a wooden façade, and the blue stain fungi Aureobasidium pullulans is commonly identified as colonizer on coated and uncoated wood expos...
L Ross Gobakken, G Alfredsen


Identification of the key factors influencing development of the blue stain fungi
2016 - IRG/WP 16-10872
Service life of wood is more and more frequently affected by aesthetic requirements than functional ones. In order to elucidate various aspects of service life, model house with façade elements made of 22 materials was built on the field test site at Department of Wood Science and Technology in Ljubljana. Colour and fungal disfigurement is among other parameters monitored on this house. In parall...
D Kržišnik, B Lesar, N Thaler, M Humar


Effect of the Storage Time of Logs in Anti-Stain Treatment Effectiveness
2016 - IRG/WP 16-30683
Storage of green lumber, for 7 months, operationally treated with anti-stain products, depending on the storage time of the logs (10, 20 and 30 days) post harvesting allows to affirm that with increasing storage time of the logs, occurs a progressive increase in intensity, severity and types of fungi present in the logs. It is further noted, a significant increase in the percentage of sawn lumber ...
M A Peredo, C Barria


Assessment of the biological durability of wood treated with organosilicon compounds
2016 - IRG/WP 16-30685
The European wood construction market is in need of environmentally friendly wood-based products whose service life meets the expectations of end users. Non-biocidal silicon-based water repellents, which can be applied to different materials, help minimize their vulnerability/susceptibility to liquid water. Consequently, they have the potential of increasing wood’s resistance against decay fungi...
M Kutnik, M Montibus, S Derocker, S Salivati, J-P Lecomte


Colorant Treatments to Enhance the Weathering Resistance of Western Red cedar
2016 - IRG/WP 16-40737
Western redcedar is renowned for its decay resistance, but, like most wood products, it requires frequent maintenance in many exterior applications to maintain its appearance. To provide adequate long-term performance in exterior applications, it must be protected against light, water, and disfiguring fungal growth. Colorant treatments, with and without preservatives, were investigated for their a...
R Stirling, V Landry


Development of methodologies to evaluate tanning blocking coatings
2016 - IRG/WP 16-40760
In Europe an increased interest in using home-grown hardwoods as sustainable and renewable construction materials started a few years ago. Amongst these species oak and chestnut are two interesting candidates as their heartwood contain a significant amount of tannins which contribute to their natural durability. To avoid wood greying and dimensional variations, oak and chestnut must be protected b...
C Reynaud, L Podgorski


Effects of climatic factors and material properties on mould growth on untreated wooden claddings
2017 - IRG/WP 17-10884
Mould growth is an important contributor to colour change of untreated wood exposed outdoors. Predicting the development of mould growth is therefore important to ensure successful use of untreated wood as a façade material. More knowledge about the factors affecting mould growth on outdoor exposed wood is required to give better predictions. In this study, climatic factors and material propertie...
S Karlsen Lie, G I Vestøl, O Høibø, L Ross Gobakken


Fungal growth on coated wood exposed outdoors: influence of coating pigmentation, cardinal direction and inclination of wood surfaces
2017 - IRG/WP 17-10896
The objective of the SERVOWOOD project was to develop and establish European Standards that will facilitate the prediction of service life for exterior wood coatings. One of the objective of this project was to study fungal growth of the field exposed panels. Two coatings applied in 2 and 3 coats were exposed for one year outdoors at 45° south: one solventborne (alkyd based) and one waterborne (a...
L Podgorski, C Reynaud, M Montibus


Bio-friendly wood protection systems - resistance to mould and blue-stain fungi
2017 - IRG/WP 17-30713
With stricter restrictions on the use of biocides and increasing environmental awareness there is a pronounced need for effective bio-friendly protection systems in the wood preservative and wood coating industry. One of the possible pathways is to exploit and utilize natural substances with active biological effects. Silanes, caffeine, natural oils and potassium carbonate were chosen as compounds...
L Ross Gobakken, W Perdoch, B Mazela, P Kwaśniewska-Sip, G Cofta


Black-stain Resistant Acrylic Latexes for Wood Coatings Applications
2017 - IRG/WP 17-40786
Translucent coatings on wood in exterior applications often fail due to photodegradation and colonization by black-stain fungi and require frequent refinishing. This limits competitiveness with alternative materials. In this project, it was hypothesized that an effective dispersion of inorganic nanoparticles will provide a translucent coating with long-term resistance to black-stain fungi. Functio...
G Boivin, A M Ritcey, P I Morris, V Landry


Bacterial adhesion to selected wood finishes
2017 - IRG/WP 17-40793
A new generation of furniture, including antibacterial surfaces, should adjust to the changing needs of an ageing population. Respectively, determination of bacterial adhesion on wooden surfaces, finished with various wood finishes or coating is an important topic. The main aims of our work were of a preliminary character. We wanted to state if the existing methods for testing of bacterial adhesio...
M Petrič, D Kekec, J Žigon, K Godič Torkar, K Bohinc


Plasma-assisted bleaching of blue-stain from lodgepole pine wood
2017 - IRG/WP 17-40799
We hypothesize that plasma will etch wood and fungal hyphae in blue-stained lodgepole pine, and increase the ability of hypochlorite bleach to remove discolouration from blue-stained wood. Blue-stained lodgepole pine wood was exposed to a glow-discharge plasma derived from water, and the surface wettability, permeability and colour of the treated wood was measured. Plasma-treated wood was dipped i...
A Jamali, P D Evans


Visual appearance of unpainted wooden claddings during the first year of outdoor exposure: Evaluation of surface mould growth, lightness (L*) and wasp attack
2018 - IRG/WP 18-40841
This study addresses changes in visual appearance of unpainted wood materials exposed outdoors. Specimens of Norway spruce (Picea abies) Scots pine (Pinus sylvestris), aspen (Populus tremula), acetylated Radiata pine (Pinus radiata) and DMDHEU-modified Scots pine sapwood were exposed facing south in Ås, Norway for 60 weeks. During this period, surface mould growth development and wasp attack were...
S Karlsen Lie, L Ross Gobakken, G I Vestøl, O Høibø


Performance of a water-borne stain on beech, spruce, MDF and OSB improved by plasma pre-treatment
2020 - IRG/WP 20-40897
Coatings are an important part of wood protection, especially for outdoor applications. In order to provide a good protection, protective coatings need to exhibit good adhesion, mechanical resistance, and weathering resistance. Plasma pre-treatments are an established method to increase the performance of existing coatings including those on wood and wood-based substrates. Moreover, plasma deposit...
S Dahle, J Žigon, I Uranjek, M Petrič


Effect of MVOC exposure on mycelial growth of wood rotting fungi
2021 - IRG/WP 21-10977
It is well known that wood rotting fungi produce microbial volatile organic compounds (MVOCs) as metabolites. In our previous studies, we have found that some MVOCs produced by wood rotting fungi are common to fungal species tested in the studies, while others are specific to each species. Furthermore, it has been also shown that each wood rotting fungi do not always produce the same type of MVOCs...
S Horikawa, R Konuma, M Yoshida


Effect of volatile organic compounds produced by wood rotting fungi on mycelial growth
2023 - IRG/WP 23-11023
Microorganisms such as fungi or bacteria produce volatile organic compounds (so-called MVOCs: Microbial Volatile Organic Compounds) as metabolites. Some MVOCs have been found to be biologically active, for example inhibition of spore germination, and when fungi of different species encounter each other, the MVOCs pattern change, suggesting that MVOCs play a role as a mediator for biological intera...
S Horikawa, R Konuma, M Yoshida


Influence of weathering of wood surfaces before and after treatment with iron(II) sulphate
2023 - IRG/WP 23-30786
Outdoor wood is exposed to various factors that cause the wood to grey or age. The ageing processes can vary greatly depending on the exposure. Parts of the wood that are not exposed to external factors, e.g. under the eaves, are less exposed and the ageing process is therefore slower. This can be accelerated by solutions based on iron ions. In this way, the wood greys quickly and evenly. However,...
B Lesar, M Humar, F Osvald