IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 750 documents. Displaying 25 entries per page.


Leaching characteristics, decay and termite resistance of treated wood with boron compounds, N'-N-(1,8-Naphthalyl) hydroxylamine (NHA-Na), and hydroxynaphthalimide (NHA-H)
2003 - IRG/WP 03-30307
Despite many advantages of boron wood preservatives, boron itself does not adequately protect wood in ground contact and exterior applications because its natural diffusibility and susceptibility to leaching. As a result of previous studies to limit or decrease boron leaching, several fixation systems have been developed. In this study, we evaluated the effects of N'-N-(1, 8-Naphthalyl) h...
S N Kartal, Y Imamura


The natural durability of wood in different use classes
2003 - IRG/WP 03-10457
The natural durability of important European wood species has been tested on 3970 specimen in field trials. The wood was exposed at five test fields in Germany with different climates at each site in European hazard class 4 and 3 (with and without soil contact). Within EHC 3 it was distinguished between tree different expositions (end grain sheltered, unsheltered and with water trap). The test is...
U Augusta, A O Rapp


Comparison of three methods for assessing the in-ground termite resistance of treated timber, durable timber and plastics at sites in Australia, USA and Thailand - First results
1998 - IRG/WP 98-20132
The in-ground resistance of materials to attack by subterranean termites is most commonly assessed with one form or another of the conventional graveyard method, despite the significant shortcomings of this method. In Australia, an alternative method, in which all samples of test materials are placed below-ground, has been in use for more than 10 years. The method provides reliable exposure of sam...
M Lenz, A F Preston, J W Creffield, K J Archer, B M Kard, C Vongkaluang, Y Sornnuwat


Resistance of painted wood to mould fungi. Part 3. The effect of weathering, wood substrate and fungicides on mould growth
1998 - IRG/WP 98-10284
The effect of 6 month outdoor weathering on the resistance of acrylate paint systems on different types of pine and spruce sapwood to mould fungi was studied. Dipping into the preservative prior to painting, a primer with and without a fungicide (propiconazole + IPBC 0.50 + 0.2%) and a topcoat with and without a fungicide (propiconazole + IPBC 0.25 + 0.12%) were combinations of the treatments stud...
H Viitanen, P Ahola


Accelerated laboratory testing of preservatives on 13 North American wood species
1999 - IRG/WP 99-30201
The ability of selected water and solvent based biocides to protect wood against fungal attack was evaluated on 13 North American wood species using 7 decay fungi in a modified soil block test. Most preservatives were capable of providing protection at their recommended above ground and soil contact use levels. Many decay fungi caused substantial weight losses on blocks treated with chlorothalonil...
J J Morrell, C M Freitag


A comparison of the leaching resistance of diammine-copper complexes and copper carbonate precipitated in wood
1997 - IRG/WP 97-30158
Previous studies have shown that during treatment of wood with ammoniacal copper solutions, both simple copper precipitates and diammine-copper complexes are formed. The objective of the present study is to determine the relative importance of both forms of copper, on such aspects as preservative leachability and biological performance. In the current experiment, the leachability of copper carbona...
Xiao Jiang, J N R Ruddick


Curing conditions for a low formaldehyde etherificated melamine resin
1998 - IRG/WP 98-40108
Waterbased methanol etherificated melamine formaldehyde resins have the potential to increase the resistance of impregnated wood against wood destroying fungi. Previous studies indicated that the resin with the lowest formaldehyde content tested showed the best results regarding fungal resistance, dimensional stability and formaldehyde emissions after curing. In the present paper the influence of ...
D Lukowsky, R-D Peek, A O Rapp


Decay and termite durabilities of heat-treated wood
2004 - IRG/WP 04-40272
Decay and termite resistances of Plato-treated timbers were evaluated using a modified JIS decay test method, feeding test in a laboratory scale and a field exposure against Reticulitermes speratus (Kolbe) or Coptotermes formosanus Shiraki. The results showed that no significant decay durability of the treated timbers although mass loss from decay slightly decreased in case of treated timbers. ...
S Doi, K Hanataa, E Kamonji, Yuuji Miyazaki


Assessment of wood decay in small-scale unsterile soil-bed tests
1997 - IRG/WP 97-20111
This study is concerned with the investigation of wood decay in small-scale unsterile soil-bed tests. Tests were performed with untreated heartwood samples from five hardwood species of different natural durability classes ranging from highly perishable to very resistant. Our results confirmed the critical role of soil moisture content on wood decay. The highest decay rates were observed at moistu...
L Machek, A M Derksen, R Sierra-Alvarez


Preservation of robinia wood (Robinia pseudoacacia L.) stakes by vintners
1982 - IRG/WP 3194
This work discusses decay resistance of robinia wood to fungi Trametes versicolor (L.ex Fr.) Pil. and Coniophora puteana (Schum. ex Fr.) Karst., and also the possibility of influencing its resistance by means of chemical protection. The results showed that natural resistance of robinia wood to these two different agents of wood decay is not the same. It is much less resistant to the fungus Conioph...
R Benko


The natural durability story
1997 - IRG/WP 97-20119
Wood species with superior natural durability were in use since the beginning of timber utilisation. Their importance decreased with increasing industrial timber impregnation. In recent time, however, they gained worldwide new interest due to environmental problems involved with treated timber. In Europe a special Standard (EN 350) has been published and a multinational research project on testing...
H Willeitner, R-D Peek


Durability of five wood species against Coriolus versicolor
1992 - IRG/WP 92-1578
The durability of following five wood species Zelkova carpinifolia, Ulmus glabra, Carpinus betulus, Acer trauvetteri and Pterocarya fraxinifolia were studied against Coriolus versicolor under laboratory conditions according to DIN 52176 standards. Zelkova caprinifolia shows a reduction in weight of 2.19%, Ulmus glabra 41.69%, Carpinus betulus 45.64%, Acer trauvetteri 53.05%, and Pterocarya fraxini...
S M Kazemi


Laboratory bioassays with termites – The importance of termite biology
2005 - IRG/WP 05-10550
Subterranean termites are frequently used in bioassays to asses the effectiveness of insecticides or the resistance of materials. Termites which appear to be vigorous with high inherent levels of activity are often relied upon, yet at the end of the experiments survival may be very unsatisfactory, even in the favourable environment of controls. Consequently, results from such bioassays may be mean...
M Lenz


Natural durability of 4 different Larix species tested in soil contact
2002 - IRG/WP 02-10434
Importers of Siberian Larch claimed to have a material which can replace pressure treated wood in soil contact. This gave reason to investigate the durability of 4 different Larix species (L. decidua, L. sibirica, L. decidua x sibirica, L. gmelini var ologenis) coming from 7 different origins in comparison with sapwood of Pinus sylvestris untreated as well as pressure impregnated with retentions o...
A O Rapp, H Viitanen, T Nilsson


Effect of boron compounds-furfuryl alcohol treatment of wood on dimensional stability, termite resistance and boron leachability
2001 - IRG/WP 01-40195
Sapwood blocks of Japanese cedar (Cryptomeria japonica) and Caribbean pitch pine (Pinus caribaea) measuring 20 (tangential) x 20 (radial) x 10 (longitudinal) mm were impregnated with furfuryl alcohol (FFA) by a vacuum-diffusion process followed by curing under heating. Boron compounds (boric acid, ammonium borate and ammonium biborate) were mixed in the impregnation solution of FFA. Anti- swelling...
S K Ozaki, M K Yalinkilic, Y Imamura, M F Souza


Termite and fungal resistance of in situ polymerized tributyltin acrylate and acetylated Indonesian and USA wood
2000 - IRG/WP 00-30219
Wood [Indonesian pine (IP), Indonesian Jabon (IJ) and USA southern yellow pine (USP)] was either in situ polymerized with tributyltin acrylate (TBTA) or acetylated and then exposed to termite and fungal degradation both in laboratory tests and field exposure. The TBTA woods had an average weight percent gain (WPG) of 11% for IP, 12% for IJ, and 10% for USP. The acetylated woods had a WPG of 15-27%...
R E Ibach, Y S Hadi, D Nandika, S Yusuf, Y Indrayani


Natural durability, density and extractive contents of 42 wood species of Bangladesh.
2003 - IRG/WP 03-10490
Natural durability, density and major extractive contents of 42 lesser used or unused wood species of Bangladesh have been studied. Correlation analysis between these properties has been performed. It has been shown that natural durability of these species neither explained by water soluble nor by alcohol benzene extractive contents. Density has a weak but significant positive correlation with dur...
S Akhter, K Akhter, S C Das


Natural progression of decay in unrestrained, Southern pine sapwood exposed above ground
1995 - IRG/WP 95-20060
In this study, the natural progression of decay is being monitored in 2.4-m (8-ft) lengths of dimension lumber. The 2.4-m lengths are supported without restraint in a horizontal plane approximately 0.75 m above ground in a partially shaded field plot in southern Mississippi. The lumber is 100% sapwood. Prior to installation in the field, each piece was planed to exactly 38 by 89 mm² (1.5 by 3.5 i...
R C De Groot, R J Ross, W Nelson


Studies on the resistance of DMDHEU treated wood against white-rot and brown-rot fungi
2005 - IRG/WP 05-10566
Beech wood (Fagus sylvatica) modified with the textile finishing agent 1,3 dimethylol-4,5-dihydroxyethylen urea (DMDHEU) has shown to improve durability against the white-rot fungus Trametes versicolor. In a mini-block test, the weight loss over eight weeks of incubation decreased with increasing weight percent gain (WPG) of DMDHEU. At 25% WPG, no significant weight loss was observed, while untrea...
P Verma, C Mai, A Krause, H Militz


Factors affecting resistance to sapstain infection in freshly felled softwood logs
2003 - IRG/WP 03-10467
Previous studies in the UK have shown a marked difference in the susceptibility of logs of five softwood species to infection by sapstain fungi over a 4 month field trial. Recently this result has been confirmed and the rank order of greatest to least susceptibility in these commercially important species is lodgepole pine > Scots pine > Norway spruce > Japanese larch > Sitka spruce. C...
E J Young, R A Eaton, J F Webber, M A W Hill


The effect of wood preservatives on the relation between the electric resistance and moisture content in scots pine (Pinus sylvestris L.) sapwood
1998 - IRG/WP 98-20142
The effect of two types wood preservatives (TBTO and CuHDO) on moisture content measurements with an electric resistance meter in pine sapwood is assessed. High and low concentration impregnated pine sapwood is climatized at different relative humidities. Once climatized the samples are weighed and the moisture content is measured with an electric resistance meter by fixed stainless steel, isolate...
B W Holleboom, W J Homan


A field method for determining the above-ground resistance of wood and wood products to attack by subterranean termite
1994 - IRG/WP 94-20035
A method for determining the above-ground resistance of wood and wood products to subterranean termites in the field is described. Termites are aggregated in 20-litre steel drums, each containing a highly susceptible timber substrate. At the centre of each drum, specimens of the test material under evaluation are sandwiched, using circular sections of wire mesh, between two layers of the substrate...
J W Creffield


The natural durability assessments of secondary timber species - field trials
1998 - IRG/WP 98-10297
Secondary or 'alternative' hardwood timber species can replace traditional hardwoods and contribute significantly to satisfying the overall demand for hardwoods in the UK timber market. A selection of these 'alternative' hardwoods is currently being tested at BRE-WTC for natural durability both in ground contact (to EN252) at two field sites, and out of ground c...
E D Suttie, R J Orsler


Eucalyptus globulus. Impregnability in relation with plantation and crop
1992 - IRG/WP 92-2402
Eucalyptus globulus Lasill is currently classified in Pr EN 350 on the basis of the characteristics of the first log. In practice, there are usually several following crops of branches developped on each stump in plantations. Up to a diameter of 8 cm, round wood of 2nd crop and further crops present a maximum of sapwood and characteristics which differ significantly from the basic classification a...
D Dirol


Combustion properties of Alder wood treated with some new environment friendly natural extractives. Part 1. Effect of Natural Tannins on the Combustion Properties
2002 - IRG/WP 02-40234
Powders of the brutia pine bark, sumach leaves, acorn, gall-nut and boric acid and borax which are known as potential environment friendly wood preservatives were impregnated according to ASTM D 1413-88 in order to determine their combustion properties. A commercial treatment compound, Tanalith-CBC, was also used for comparison. The results indicated that the natural extractives did not have an...
Ü C Yildiz, A Temiz, E D Gezer, S Yildiz


Previous Page | Next Page