Preservative performance of copper naphthenate (SANPRESER-OGR) in brush treatment of timber
1991 - IRG/WP 3663
Preservative efficacy of copper naphthenate (SANPRESER-OGR) was evaluated in the laboartory and field trials when timber was treated by brushing. Results of field trial indicated that service life of the brush-treated timber could be approximately 10 years or longer under ground contact conditions, although life span was slightly varied with timber species and test sites. After four years&apos...
Y Sugai, K Hamada, M Kitada, K Tomoi


In-ground evaluation of a copper azole wood preservative (Tanalithâ E) at a tropical Australian test site
1996 - IRG/WP 96-30100
A field trial to determine the in-ground termite and decay resistance of Pinus radiata D. Don impregnated with a copper azole formulation, TANALITHâ E, has been established at a tropical site in the Northern Territory of Australia. Four retentions of TANALITHâ E, containing 1.54, 2.08, 2.92 and 4.30 kg/m³ of Cu, are being evaluated. For comparison, Pinus radiata specimens treated to two retenti...
J W Creffield, J A Drysdale, N Chew


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 4: Report of second inspection (12 months) in Australia
1979 - IRG/WP 448
Previous reports have presented full details of the treatment and installation of the test specimens in Sydney Harbour during December, 1977, and of the results of the first (6 months) inspection made during June, 1978. At the June inspection it was apparent that the plastic tubing used to make up the frames from which to suspend the specimens was inadequate for the job and not strong enough to su...
J Beesley


Leaching of CCA preservative from treated timber in marine environment
2001 - IRG/WP 01-30254
Knowledge on the amount of preservatives leaching out of treated wood is essential to optimise the chemical loading in various species of timber required for different end uses. In order to gain more insight into this aspect, the residual CCA content in 40 treated timber panels belonging to 14 species removed on destruction by marine organisms from a series of durability tests conducted in Kochi w...
M V Rao, V Kuppusamy, K S Rao, L N Santhakumaran


Natural resistance of different species of timber to marine borer attack in the Trondheimsfjord (Western Norway)
1978 - IRG/WP 435
Natural resistance of 34 timber species to marine wood-borers has been discussed, based on data collected from panels immersed in selected localities in the Trondheimsfjord during 1977-78. The wood-borers encountered on the panels were Psiloteredo megotara, Xylophaga dorsalis, Xylophaga praestans and Limnoria lignorum. The number of borers present and their growth were taken as the criterion for a...
L N Santhakumaran, J A Sneli


The yeast Pichia sp. As a short-term biological control agent to fungal spoilage of sawn softwood timber
2000 - IRG/WP 00-10362
Previous work has found isolates of the yeast Pichia to be a successful biological control agent toward moulding of fruits. An isolate was tested for the ability to protect sapwood of Pinus sylvestris timber against visual degrade by surface growth of moulds and staining fungi. Successful protection of autoclaved wood sprayed with a mixture of common wood moulding fungi was achieved when the yeast...
C Payne, H J Staines, A Bruce


Changes to New Zealand Timber Treatment Specifications
2004 - IRG/WP 04-20288
Changes have been made to the New Zealand timber treatment specifications in response to frequent incidences of decay in framing timber and doubts about the long-term performance of tributyltin formulations when used in exposed situations. Changes have been made to Hazard Class H1 to allow a level of treatment to provide short to medium decay resistance to framing which would protect it, should l...
M E Hedley


Incursion of Hylotrupes bajulus Linnaeus (European House Borer) into Western Australia
2005 - IRG/WP 05-10558
In January 2004, an adult Hylotrupes bajulus Linnaeus was detected emerging from a beam of Pinus pinaster in a house in Perth, Western Australia. The timber had been locally grown and milled. Surveys to define the extent of the infestation show it is restricted to dead pine trees in 28 sites around Perth. The biological and economic feasibility of eradication is being assessed. Since about 2001, k...
M Grimm


Chemical analyses of IRG/COIPM INTERNATIONAL MARINE TEST (to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water) samples
1987 - IRG/WP 4114
Chemical analysis of CCA and CCB treated timber was carried out after exposure at tropical and temperate marine sites. Results indicated that losses of all elements had occurred. In particular, losses of boron were severe. Arsenic and copper were also lost. The chromium components in both formulations was the most dominant metal remaining. The results suggest that chromium modification was importa...
L E Leightley


An engineering model for the decay of timber in ground contact
2003 - IRG/WP 03-20260
To predict the residual strength of an engineered structure, it is first necessary to predict the effect of decay. A model was developed in which the effective area of structural decay in large section timbers was defined as that area that could be picked out with a pen-knife. Some limited studies indicated that for practical purposes the remaining wood could be assumed to have its full residual s...
R H Leicester, C-H Wang, M N Nguyen, J D Thornton, G Johnson, D Gardner, G C Foliente, C MacKenzie


An evaluation on durability of untreated mining timber support
1997 - IRG/WP 97-20121
Wedge blocks in dimension of 5 x 7 to 8 x 155 cm3 were cut from indigeneous scots pine pitprops. Each of wedge block pairs were numbered and half of them were placed as the test blocks between the steel arches and the strata in a hard coal pit. Controls in laboratory and test wedge blocks in the mine were then sawn into 20 by 20 by 300 mm standard test sticks. Impact bending, static bending and MO...
A Bobat


Chromium on the surface of CCA-treated wood
1978 - IRG/WP 386
Chromium in solutions of CCA preservatives is predominantly in the hexavalent state (Cr VI). It is well known that Cr VI is associated with dermatitis and skin ulceration in workers handling chromium containing products and processes. When reduced to the trivalent state, however, chromium is considerably safer. An essential part, therefore, of safety procedures in any chromium - using industry is ...
C R Coggins, P Hiscocks


The chemical analysis and biological evaluation of wood extractives as potential timber preservatives
1995 - IRG/WP 95-30090
Work involved the biological performance of water and organic solvent soluble extractives of four naturally durable wood species, namely; Matumi, Tamboti, Sneezewood and the Turpentine tree. These timber species are known to be naturally durable against termites and fungi (±25 to 35 years). The extractives were evaluated against termites and fungi using impregnated pine pencil stakes in field tes...
P Turner, D Conradie


Cuticular hydrocarbons for species determination of tropical termites
1990 - IRG/WP 1465
Insect species have unique mixtures of cuticular hydrocarbons in the protective wax of their integument. We use hydrocarbons to evaluate similarities among termite populations. Our assumption is that colonies with similar hydrocarbon profiles are closely related. We have collected Reticulitermes in California from areas suspected to have only Reticulitermes hesperus or Reticulitermes tibialis. The...
M I Haverty, M Page, B L Thorne, P Escoubas


Sludge formation in timber treatment with CCA preservatives. Origin and elimination
1984 - IRG/WP 3276
The exact distributions between lignin and holocellulose and retentions on wood of copper, chromium and arsenic as a function of various sets of conditions in a factorial experiment in which combinations of three temperatures of treatment, three CCA solution concentrations, four pH's of the initial CCA solution and two timber species, namely Pinus radiata and Eucalyptus grandis, are repor...
A Pizzi, W E Conradie, A Jansen


The use of a physical field model to study the effects of remedially treated timber on the growth of perennial ryegrass (Lolium perenne) and rye (Secale cereale), and the accumulation of toxic preservative constituents in Lolium perenne
1995 - IRG/WP 95-50040-02
Low cost laboratory model systems can be used to give relatively rapid indications of the environmental effects of preservative treated timber in soil contact. This paper details the effects of remedially treated timber on the growth of crops of Lolium perenne and Secale cereale seeded on soilbeds of different texture in close proximity to remedially treated creosoted pole sections. Lolium perenne...
D C R Sinclair, G M Smith, A Bruce, H J Staines


The shower test method. A leaching test for assessing preservative losses from treated timber under simulated open storage conditions
1993 - IRG/WP 93-50001-04
In the late 1980's against the background of increasing environmental concern a laboratory based accelerated leaching test method for assessing preservative losses-from stored, treated timber was developed by the Dutch organisation for applied Scientific Research (TNO). This test method quantifies the amount of specific preservative components which leach from treated timber under simulat...
J B G A Havermans, W J Homan, M J Boonstra


The dip diffusion treatment of tropical building timbers in Papua New Guinea
1972 - IRG/WP 310
In Papua New Guinea a dip diffusion process using a multi salt preservative developed by C.S.I.R.0. has been in commercial use for 8 years. Over 200 million super feet (236,000 m³ ) of timber has been treated during this period and current rate of treatment is 34 million super feet (80,400 m³ ) of timber per year in 70 licenced treatment plants. The process has been found to be simple to apply, ...
C R Levy, S J Colwell, K A Garbutt


An environmental assessment of timber treatment plants in Australia
1999 - IRG/WP 99-50124
Australian Standard AS 2843 Timber Preservation Plant Safety Code, sets the specifications for the design and operation of timber treatment plants in Australia. The Timber Preservers' Association of Australia has carried out an environmental survey of timber treatment plants throughout Australia using the operational checklist provided in Appendix C of Part 2 of the Standard. Third party ...
J Norton, K Riley


Characterization of tropical wood-decaying fungi by RFLP analysis of PCR amplified rDNA
1998 - IRG/WP 98-10251
Five brown-rot fungi (Tyromyces palustris, Gloeophyllum trabeum, Antrodia sp., Poria placenta, Coniophora puteana) and three white-rot fungi (Coriolus versicolor, Pycnoporus sanguineus, Lentinus squarrosulus) registred as representative wood-decaying fungi for international standards of wood durability tests have been characterized using molecular tools (PCR/RFLP). The Internal Transcribed Spacer ...
A Zaremski, M Ducousso, Y Prin, D Fouquet


Sampling rates and the probability of detecting defective treatment in the sampling of preservative treated timber
1987 - IRG/WP 2277
When attempting to enforce standards of penetration and retention set for treated timber, the regulating authority must establish a sampling or inspection scheme which will prevent large quantities of substandard product entering the market. On the other hand, the scheme should not penalise treaters for the small quantities of such material which are inevitably produced by any industrial process. ...
M J Kennedy, L E Leightley


Preservation of two Indonesian timber species for marine environment purposes
1994 - IRG/WP 94-10079
This paper deal with the experiment of CCA full cell processed two non-durable Indonesian species for placed in the marine environment. 80 samples of 5 x 5 x 60 cm³ dried durian (Durio zibethinus) and mahogany (Swietenia mahagony) timber were CCA-full cell processed using 4 combination treatment of: without steaming; one hour steaming; 3% and 5% CCA solution concentration. 40 samples of them were...
P Permadi, I M Padlinurjaji, F Rasmita


Comparative study on physical properties of four fast growing timber species of Bangladesh
2006 - IRG/WP 06-10570
Ghoraneem (Melia azedarach), Rain tree (Albizia saman), Sissoo (Dalbergia sissoo Roxb.) and Akashmoni (Acacia auriculiformis) plantations are started as a fast growing timber specie from a few years back in Bangladesh. Initian objectives were to get fuel wood only from those trees, but a very positive response was found for Ghoraneem, Rain Tree, Sissoo and Akashmoni timber in the users market by c...
M M Islam, B K Dey, M O Hannan, G N M Ilias


Dip-diffusion of dressed timber - Effect of drying
1989 - IRG/WP 3509
The effect of drying on dip-diffused dressed freshly sawn timber was determined by the depth of penetration of boron achieved on the two test timber species, White cheesewood (Alstonia scholaris) and Light Hopea (Hopea papuana). The results obtained showed that light density White cheesewood was completely penetrated even after 3 days drying while Light hopea, treated immediately achieved 5.2 mm p...
H C Konabe


Translation of titles of papers listed in Document No: IRG/WP/311
1972 - IRG/WP 312
BAVENDAMM W and W EHLERS: Investigation under conditions similar to those obtained in practice on the impregnation of structural timber by means of brushing and spraying. Holz als Roh- und Werkstoff, 12 (1954) 183 185. BAVENDAMM W and H ANOZYKOWSKI: Investigations under conditions similar to those obtained in practice on the impregnation of structural timber by means of short period dipping and o...