A preliminary note on the role of moisture absorption rate in durability assessment
2008 - IRG/WP 08-20383
The rate of moisture uptake was studied in 15 wood species using vermiculite at varying moisture levels as the exposure medium. As might be expected, moisture uptake varied widely among the species studied. While some of the more durable wood species were also resistant to moisture uptake, this was not always true. The results are discussed in relation to performance in under varying environmenta...
J J Morrell, L P Francis


Service life prediction of wood: scale-dependent tools within a bio-engineering framework
2008 - IRG/WP 08-20387
Service life prediction (SLP) is a complex yet essential method for the building industry. Accurate and precise assessment of the components is crucial for a strong position of wood on the market. As it is a biological material, wood has an inherent variability and is susceptible to fungal attack. Therefore a profound knowledge of these characteristics is the corner stone of SLP for wood products....
J Van den Bulcke, J Van Acker, M Stevens


Preservative treatment of strips of Bambusa balcooa by soaking process using Borax-Boric acid
2008 - IRG/WP 08-30478
Bamboo strips made from Borak bamboo (Bambusa balcooa) were treated with 10% borax-boric acid aqueous solution by soaking process. The moisture contents of the bamboo strips were 12%, 20% and 30%. The strips were soaked for one, two, three, four and five days. The penetration of the solution was investigated by colour test after soaking and drying. Full penetration was observed after three days ...
K Akhter, M W Sheikh, M M Rahman, T A Chowdhury, M H Chowdhury


Effects of Moisture Content and Species on Penetration of Liquid in Laser Incised Lumber by the Passive Impregnation Method
2008 - IRG/WP 08-40408
Penetration of liquid by passive impregnation method for Douglas-fir (Pseudotsuga menziesii Franco), sugi (Cryptomeria japonica D. Don) and Japanese larch (Larix leptolepis Gordon) were studied. Effects of initial moisture content of sugi (16, 43 and 70% moisture content) on liquid penetration by the method were also studied. Dried Douglas-fir and sugi, and green Japanese larch and sugi were treat...
N Hattori, M Nazrul Islam, K Ando, H Yamauchi


Radial flow of Bornmullerian fir (Abies bornmulleriana Mattf.) as affected by wood tapering and the condition of end wall structure of uniseriate ray parenchyma cells
2008 - IRG/WP 08-40441
Amenability to radial permeability of Bornmullerian fir (Abies bornmulleriana Mattf.) was studied on the base of the effects of wood tapering and the structure of end walls of uniseriate ray parenchyma cells. The results showed that the most remarkable culprits of the greatest fluid uptake (as the percentage of void volume filled by the fluid in the radial flow direction, RVVF%) are the lesser woo...
I Usta, S Aslan


Laboratory and field exposures of FRT plywood: Part 1. Physical test data
2008 - IRG/WP 08-40426
Our understanding of the laboratory induced degradation with fire retardant systems is currently limited since we are unable to correlate laboratory steady-state experiments with actual in-service field degradation. Current model studies have generally been limited to isothermal rate studies with selected model FR chemicals. Other factors also play a major role in the degradation of FR-treated woo...
H M Barnes, J E Winandy, C R McIntyre


High Temperature Treated Wood
2008 - IRG/WP 08-40429
High temperature can modify internal structure and physic-chemical properties of wood by a controlled pyrolysis process. Such treatment, among other changes in properties, modifies the wood color in a way that resembles exotic species, increasing its market value. The main objective of this work is to determine the changes in wood properties caused by the effect of temperature and time, in order t...
C C Borges, A L Barbosa, R Faber de Campos, S T Targas


Accelerated weathering of nine tropical wood species from Cameroon
2009 - IRG/WP 09-10705
The natural durability of tropical species for building components has been a subject of recent concern and questioning, mainly the resistance to weathering. Weathering resistance of nine tropical species from Cameroon, namely Azobe, Bilinga, Bubinga, Teak, Dousie, Moabi, Musanga, Sipo and Padauk were evaluated using an accelerated weatherometer for 2016 hours. Measurement of moisture fluctuation,...
S Pankras, Jinzhen Cao, D P Kamdem


Moisture adsorption isotherms of wood studies using a dynamic vapour sorption apparatus
2009 - IRG/WP 09-20398
Five types of wood including two Malaysian hardwoods acacia mangium (Acacia mangium) and sesenduk (Endospermum malaccense), two temperate softwoods, Sitka spruce (Picea sitchensis), radiata pine (Pinus radiata) and Accoya (commercially modified wood) were studied to determine their moisture sorption behaviour using a Dynamic Vapour Sorption (DVS) apparatus. The isotherm plot for each species teste...
J Zaihan, C A S Hill, S Curling


Service Life Prediction of Wood Claddings by in-situ Measurement of Wood Moisture Content: Status after 5 years of Outdoor Exposure
2009 - IRG/WP 09-20401
The Danish Technological Institute is in co-operation with industry partners running a project aiming at predicting the service life of different wood protecting systems. The project focuses on examining the moisture reducing effect of different protecting systems for timber claddings and the ability of these to maintain the appearance of the surfaces, when the wood is used in service class 3 (EN ...
E Tang Engelund, B Lindegaard, N Morsing


Building with termites: The challenge of biomimetic design for carbon neutral buildings.
2009 - IRG/WP 09-20405
The main aim of this paper is to present humanity and termites as design partners in the creation of a new dimension of ecosystem understanding. “Beyond biomimicry: What termites can tell us about realizing the living building”, Turner and Soar (2008) opens up a new era in how we think of human habitations, not only on earth, but maybe on other planets, and using the termite model as the corne...
J R J French, B M Ahmed (Shiday)


Evaluation of exposure conditions for wooden facades and decking
2009 - IRG/WP 09-20408
During their functional life, building components are exposed to moisture and other environment stress conditions in numerous ways. This is a fact that should be taken into account during manufacture, product development, designing and work execution of building components. For wood material, moisture stress and biological factors like mould and decay fungi are often critical in cladding and decki...
H Viitanen, T Toratti, R Peuhkuri, T Ojanen, L Makkonen


Evaluation of variables that influence dynamic MOE in wood decay studies
2009 - IRG/WP 09-20409
The effect of wood moisture content (MC) and outdoor exposure of southern pine lap-joint components on dynamic MOE values was investigated. The use of dynamic MOE as a method of measuring progressive biodeterioration of above ground test samples shows promise, but the accuracy of this method for evaluating test samples subjected to fluctuating environmental conditions has not been reported. The re...
D Nicholas, J Shi, T Schultz


Continuous moisture measurement (CMM) to detect failure of moisture resistance
2009 - IRG/WP 09-20422
A wood coating system will fail to perform properly after a certain time of weathering. From that moment, the substrate is especially prone to fungal attack. Moisture plays a key role on weathering performance, wood protection efficacy and decay susceptibility of wood. Therefore, knowledge of the moisture dynamics of the applied wood protection is of significant importance in the prediction of the...
I De Windt, J Van den Bulcke, J Van Acker


Microwave Surface Modification of Radiata Pine Peeler Cores for Preservative Treatment
2009 - IRG/WP 09-40453
Radiata pine peeler cores are classified as a by-product derived from the cores of logs left over after the veneer peeling process. The core can be potentially developed for value added solid wood products as it is abundantly available and has a constant diameter. However, the core needs to be preservative treated because of low durability in ground contact. An additional problem is that the wood ...
K Sugiyanto, G Torgovnikov, P Vinden


Estimating the heat treatment intensity through various properties of thermally modified timber (TMT)
2009 - IRG/WP 09-40459
The suitability of different measures for prediction of the heat treatment intensity was investigated. Therefore, the resistance to impact milling (RIM), the lightness L*, the equilibrium moisture content (EMC), the anti swelling efficiency (ASE) and the total amount of soluble carbohydrates (TSC) of heat treated specimens were correlated with corresponding fungal resistance achieved by heat treat...
C R Welzbacher, C Brischke, A O Rapp


Weathering of Wood Modified with the N-Methylol Compound 1,3‑dimethylol-4,5-dihydroxyethyleneurea (DMDHEU)
2009 - IRG/WP 09-40467
Scots pine (Pinus sylvestris L.) sapwood boards were treated with a methylated 1,3‑dimethylol-4,5-dihydroxyethyleneurea (mDMDHEU) causing weight gains of approx. 25% and exposed to weathering for 18 months. Compared to untreated boards, treatment with mDMDHEU reduced surface discoloration mainly caused by staining fungi. Boards treated with mDMDHEU exhibited clearly lower moisture content th...
C Mai, Yanjun Xie, A Krause, K Urban, P D Evans, K Richter, H Militz


Selection of an appropriate coating system for wooden boats to be used in fresh water
2009 - IRG/WP 09-40472
Properties of several, most commonly used protective low-price coatings, which are used by the pletnja boat owners in Bled, Slovenia, were extensively studied. The aim of this professional, practically oriented study was to compare various coating systems, and to recommend the most suitable one to the boat owners. Regarding specific use conditions, the following properties, including their resista...
M Petrič, B Kričej, A Logar, M Pavlič


The effect of chemical changes on the wood-moisture relationships in thermally-modified wood
2009 - IRG/WP 09-40473
Small specimens of three wood species were thermally modified following twenty schedules in the 190-245°C temperature range for treatment times between 0.3 and 16 h. Five wood-moisture relations were subsequently determined, namely: anti-swelling efficiency (ASE), movement, hygroscopicity (adsorption and desorption), transversal swelling (radial and tangential directions), and equilibrium moistur...
M M González-Peña, M D C Hale


Modelling hyphal growth of the bio-incising fungus Physisporinus vitreus
2010 - IRG/WP 10-10710
The white-rot fungus Physisporinus vitreus preferentially degrades the pit membranes of bordered pits in tracheids and subsequently enhances wood permeability. Thus, P. vitreus can be used to improve the uptake of wood preservatives and environmentally-benign wood modification substances. This process can be used to enhance the use and sustainability of native conifer wood species by the wood indu...
M Fuhr, C Stührk, F W M R Schwarze, M Schubert, H J Herrmann


A review of Sitka spruce (Picea sitchensis (Bong.) Carr.) as its Importance and Breeding
2010 - IRG/WP 10-10717
Foresters tend to concentrate on those species which are the easiest to handle silviculturally, and which will produce the greatest volume of generally useful wood in the shortest time. Sitka spruce (Picea sitchensis (Bong.) Carr.), which is a softwood species from the western seaboard of North America with a range extending from southern Alaska to northern California, is one of the pioneer specie...
I Usta, R Despot


Measurements of rot fungal activity as a function of moisture content by isothermal calorimetry
2010 - IRG/WP 10-20428
Measurements of heat production rate have been made on wood samples with the brown rot fungus Postia placenta at different moisture contents. The results clearly indicate that the heat production rate (a measure of respiration rate and activity) is moisture dependent. When the moisture content is decreased, less heat is produced, and when the moisture content is increased, more heat is produced. I...
L Wadsö, A Pilgård, G Alfredsen


Service life prediction of wooden components – Part 1: Determination of dose-response functions for above ground decay
2010 - IRG/WP 10-20439
Scots pine sapwood (Pinus sylvestris L.) and Douglas fir heartwood (Pseudotsuga menziesii Franco) specimens were exposed in double layer field trials at 24 different European test sites under different exposure conditions (in total 28 test sets). The material climate in terms of wood moisture content (MC) and wood temperature was automatically recorded over a period of up to eight years and compar...
C Brischke, A O Rapp


Impact of climate change on wood deterioration - Challenges and solutions for cultural heritage
2010 - IRG/WP 10-20441
Deterioration of wood in cultural assets follows the same physiological mechanisms as in modern structures. Therefore rules and data for prediction of service life derived from old wooden structures can be used to model the service life of recent wooden structures and vice versa. The latter is done in this paper: From experimental test set ups in the field spread over Europe, climatic data, wood t...
C Brischke, A O Rapp, M Hasan, R Despot


Trace chemicals used for studying fluid permeability of wood
2010 - IRG/WP 10-20442
Wood is a construction material and in its natural condition vulnerable to biological decay caused by fungi, insects and bacteria. To facilitate its outdoor application, wood protection systems are applied since ages. In the course of restrictions for well established but hazardous wood protection treatments, newer systems get utilized. Its uniform allocation within the wooden matrix is essential ...
K Zimmer, E Larnøy, O Høibø