Movement of chloropicrin, Vapam, and methylisothiocyanate in southern pine and Douglas fir timbers
1987 - IRG/WP 3410
Douglas fir and southern pine timbers, 15.2 x 15.2 x 426 cm³ (6-in x 6-in x 14-ft), were "inoculated" with brown-rot and white-rot fungi as vapor-sensing agents to evaluate the movement and distribution of fungitoxic concentrations of chloropicrin, Vapam, and methylisothiocyanate (MIT) over a 20-week period. Residual fumigant in timbers was determined by a bioassay with Gloeophyllum trabeum. The ...
T L Highley


Why don't more people work with Serpula lacrymans nowadays? A discussion of some of the different approaches to experimenting with this unique fungus
1989 - IRG/WP 1383
Remarkably few laboratories are currently investigating this well-known fungus. Not only has it failed to gain acceptance as a standard test organism (for wood preservative evaluation) in many countries, but is also sometimes excluded from pure research studies when it ought to be an obvious first choice as a representative basidiomycete. This paper discusses some different approaches that have be...
J D Thornton


Suitability of different termite species for laboratory testing
1982 - IRG/WP 1159
Different termite species were tested in the laboratory to evaluate the effectiveness of insecticides and wood preservatives in wood against termite attack. Determined were the optimum group size and composition, the matrix (vermiculite) volume and its moisture content. Choice feeding tests with fully impregnated wood blocks which are carried out according to a modified EN 117 procedure for Reticu...
U Kny, H Kühne


A new process for in situ polymerization of vinyl monomers in wood to delay boron leaching
1998 - IRG/WP 98-40110
Efforts were accelerated on effective use of boron compounds in wood preservation owing to their environmentally safe characteristics and relatively low costs in addition to their well-known high bioactivity and fire resistant properties. Although having these unique favorable properties, they are readily leachable from treated wood at humid conditions. Therefore, they had limited market for exter...
M K Yalinkilic, W Dwianto, Y Imamura, M Takahashi


Penetration of oil-borne preservatives in American elm
1975 - IRG/WP 355
Pressure treatment of elm posts and cants by Rueping schedules resulted in erratic penetration. Instead of the expected gradual decrease in retention from surface inward in posts, inner zones frequently contained more preservative than the surface quarter inch. Heartwood was found penetrated when sapwood was not. There were numerous skips in treated zones. The prevalence and possible causes were i...
E A Behr


Protection of pine sawtimber and sawn timber against blue stain in Poland
1983 - IRG/WP 3193
The purpose of this paper is the synthesis of more important results of basic and applied research that have been grouped in the following problems: 1.: Fungi causing blue stain in the pine wood, occurring in Poland. 2.: Moisture content changes of pine sawtimber and sawn timber as the factor of blue stain producing fungi development. 3.: Effect of sapwood moisture content on the degree of wood st...
E Tarocinski, M H Zielinski


Factors affecting the resistance of fibre building boards to fungal attack
1975 - IRG/WP 252
Fungal decay is initiated at lower moisture contents in standard and tempered hardboards (18%) than in pine sapwood (26%). In contrast, in a saturated atmosphere, the equilibrium moisture contents of standard hardboard (14%) and of tempered hardboard (12.5%) are much lower than the moisture content permitting decay initiation whilst the equilibrium moisture content of pine sapwood (25.1%) approach...
C Grant, J G Savory


Effects of the delay in the beginning of treatment on absorption and distribution of water-soluble salts in posts treated by sap-replacement method
1992 - IRG/WP 92-3719
One of the most important matters in green wood treatments, such as sap-replacement method, is knowing the longest time available for beginning treatment without losing efficacy. In this paper, the influence of this factor on absorptions and distribution of the preservative into the wood is analized. Tree start-up times were first chosen: 3-6 hours, 48 h and 120 h after being cut down. The treatme...
M V Baonza Merino


Moisture correction for ultrasonic MOE measurements above fibre saturation point in Scots pine sapwood
2006 - IRG/WP 06-20333
There is a high correlation between methods for dynamic modulus of elasticity (MOEdyn) and static modulus of elasticity (MOEstat). MOEdyn methods have been found sensitive to detect early stages of decay and may be seen as an option for non-destructive wood durability testing. As the MOEstat measurements do not change after reaching the fibre saturation point, the uncorrected MOEdyn data from ultr...
E Larnøy, G Alfredsen, H Militz


Laboratory methods for assessing the resistance of wood plastic composites to fungal attack.
2006 - IRG/WP 06-20340
Wood plastic composites (WPC’s) have many attractive material features including dimensional stability and resistance to moisture, but the wood in these materials remains susceptible to fungal attack. Assessing WPC decay resistance in laboratory trials has proven difficult because the slow moisture sorption characteristics of this material do not allow for sufficient fungal attack over the trad...
J J Morrell


L-joint based testing for service life prediction of exterior plywood in out of ground contact conditions
2006 - IRG/WP 06-20342
Good biological performance of several plywood types in exterior conditions is most probably related to altered wood moisture behaviour compared to solid wood. Therefore a test set up was developed, using EN 330 L-joint testing methodology, to facilitate differentiation of plywood for exterior applications. The proposed test set up is an adaptation of an accelerated L-joint method introduced by V...
J De Smet, I De Windt, J Van Acker


CCB Preservative treatment of split muli (Melocanna baccifera ) bamboo by soaking process
2006 - IRG/WP 06-40336
This study was carried out in order to investigate the retention of chemicals inside the split muli ( Melocanna baccifera ) bamboo after preservative treatment by soaking process. Treatment with 10% aqueous solution of CCB (copper-chrome-boron) was applied in split bamboo of two sizes (1/4 part and 1/8 part) at three different moisture contents and five time periods (24, 48, 72, 96, 120 hours). It...
K Akhter, M H Chowdhury


Wood plastic composites from modified wood; Part 1 - Conceptual idea, mechanical and physical properties
2006 - IRG/WP 06-40338
Wood plastic composites, WPCs, are rapidly taking shares from preservative treated wood on the decking market. However, the long term performance of the WPC products in this application is uncertain. Therefore, in an attempt to increase the long term performance and durability, the substitution of the unmodified wood component with modified wood has been studied in the work presented in this paper...
P Larsson Brelid, B K Segerholm, M Westin, M E P Wålinder


The Effect of Wick Action upon Moisture Distribution in Ellagate Treated Pinus radiata Wood
2006 - IRG/WP 06-40328
Sapwood stakes of Pinus radiata D. Don were treated with water-soluble tetraguanidinium, tetracholine and tetrakis-benzyltrimethylammonium ellagates. The effect of these treatments upon moisture distribution was investigated by wick action. Given that chemical reactions within the wood substrate between nutrients and treatment solutions may alter the properties of the wood with regard to moistur...
S R Przewloka, B J Shearer, J A Hann


The Influence of Extractives on Western Redcedar’s Equilibrium Moisture Content
2006 - IRG/WP 06-40331
The high natural durability of western redcedar (Thuja plicata Donn) heartwood is often attributed to the presence of the thujaplicins, which are toxic to fungi. However, sound, twenty-five year old western redcedar shakes and shingles were found to contain only traces of the thujaplicins, but significant quantities of plicatic acid (which is only weakly toxic to fungi). This suggests that factors...
R Stirling, P I Morris


Service life prediction of plywood
2007 - IRG/WP 07-20367
Plywood is the wood based panel showing the best physical and mechanical properties for application under moist construction conditions. Appropriate physico-mechanical durability for exterior applications in transportation or construction systems can be guaranteed by assessment of the glue bond quality and mechanical characteristics. However, due to the fact that mainly non-durable wood species ar...
J Van Acker, J De Smet


Use of Moisture Meters with Treated Wood
2007 - IRG/WP 07-40382
Drying wood treated with waterborne preservatives after treatment to near outdoor EMC conditions improves its physical performance characteristics. This is primarily due to the reduced checking, splitting and warping which can occur when wet wood, particularly if restrained from shrinking by being nailed or otherwise fastened, shrinks in use. Monitoring of the drying process, rate, and end point...
W B Smith, Hwan Myeong Yeo, C Stark, B Morey, C Tascioglu, P Schneider, D Herdman, M Freeman


Effect of barriers on moisture content of treated and non-treated utility poles
2007 - IRG/WP 07-40369
The potential for non-biocidal barriers to slow moisture sorption was investigated using butt treated western redcedar poles immersed in either water or moist soil over a 2 year period. Moisture sorption was initially slowed by the barriers, but openings at the bottoms of the barriers eventually allowed moisture to migrate upward. Moisture levels in wrapped poles eventually reached those found in...
C S Love, J J Morrell


The Role of Moisture Content in Above-ground Leaching
2007 - IRG/WP 07-50245
This paper reviews previous reports on the moisture content of wood exposed above ground and compares those values to moisture contents obtained using simulated rainfall and immersion methods. Laboratory leaching trials with CCA-treated specimens were also conducted and the results compared to published values for leaching of CCA-treated specimens exposed above ground outdoors. Previous researcher...
S Lebow, P Lebow


Control of Moisture Content in Wood Materials for Mold Growth
2007 - IRG/WP 07-10630
Mold growth on wood materials is a major concern for house owners, as it can cause health and aesthetic problems. Mold fungi, present everywhere, usually appear as black or gray patches on wood surfaces in humid environments, and are common in houses. Like any living organism, molds need food, water, oxygen, and a specific temperature range in order to grow. To avoid mold growth on wood materia...
Dian-Qing Yang


Water Absorption of Various Building Materials and Mold Growth
2008 - IRG/WP 08-10657
Mold growth is a major problem for house owners, as it often occurs on the surface of building materials in damp houses. The principal method to control mold growth on building materials is to prevent water penetration into the materials. A study was recently conducted to determine water absorption rates of different wood species and panel materials used as building materials, when water intrusi...
Dian-Qing Yang


In-service performance of wood depends upon the critical in-situ conditions. Case studies.
2008 - IRG/WP 08-20382
Wood is a unique building material, but is by nature designed to deteriorate. A detailed understanding of the factors and interactions involved are important when working with service life prediction of wooden components in buildings. Wood may experience exponential fungal degradation caused by variation in the climatic factors within a small limited area and by minor imperfection in the wooden ...
L Ross Gobakken, J Mattsson, G Alfredsen


A preliminary note on the role of moisture absorption rate in durability assessment
2008 - IRG/WP 08-20383
The rate of moisture uptake was studied in 15 wood species using vermiculite at varying moisture levels as the exposure medium. As might be expected, moisture uptake varied widely among the species studied. While some of the more durable wood species were also resistant to moisture uptake, this was not always true. The results are discussed in relation to performance in under varying environmenta...
J J Morrell, L P Francis


Service life prediction of wood: scale-dependent tools within a bio-engineering framework
2008 - IRG/WP 08-20387
Service life prediction (SLP) is a complex yet essential method for the building industry. Accurate and precise assessment of the components is crucial for a strong position of wood on the market. As it is a biological material, wood has an inherent variability and is susceptible to fungal attack. Therefore a profound knowledge of these characteristics is the corner stone of SLP for wood products....
J Van den Bulcke, J Van Acker, M Stevens


Preservative treatment of strips of Bambusa balcooa by soaking process using Borax-Boric acid
2008 - IRG/WP 08-30478
Bamboo strips made from Borak bamboo (Bambusa balcooa) were treated with 10% borax-boric acid aqueous solution by soaking process. The moisture contents of the bamboo strips were 12%, 20% and 30%. The strips were soaked for one, two, three, four and five days. The penetration of the solution was investigated by colour test after soaking and drying. Full penetration was observed after three days ...
K Akhter, M W Sheikh, M M Rahman, T A Chowdhury, M H Chowdhury