Three-year field test of preservative-treated Canadian species in Korea
2014 - IRG/WP 14-30646
The purpose of this study was to generate field performance data in Korea on Canadian softwood species preservative-treated to Canadian standards. Two field tests of preservative-treated Canadian softwood species, one in ground contact and one above ground, were installed in Jinju, Korea in November 2010. Western hemlock and white spruce were incised and pressure-treated with alkaline copper quate...
Jieying Wang, Jong Bum Ra, P I Morris


Resistance to Decay Fungi of Scots Pine Impregnated with Natural and Chemical Preservatives
2014 - IRG/WP 14-30650
In this study, heart-wood and sap-wood specimens of the Scots pine which is naturally grown in Turkey were treated with natural (valex) and some chemical preservatives such as CCA - C (Copper / Chrome / Arsenic), CBA - A (Copper / Boron / Azole). The wood protective efficacies of these preservatives were investigated by means of fungi decay test (EN 113). As a result of the study it was found t...
S Yildiz, U B Şimşek


Borate Redistribution in Glulam in an Above Ground Field Test
2014 - IRG/WP 14-30652
Researchers have refocused on the use of boratesin the wood protection industry in the last two decades due to their broad spectrum effectiveness against fungi and insects, and favourable environmental characteristics. This study was designed to determine borate distribution in a limited number of samples from a large field test of composites protected by a combination of coating and borate treatm...
P I Morris, A Temiz, J Ingram


Dynamic mechanical analysis (DMA) of nano cupric oxide (CuO) modified aqueous phenol formaldehyde (PF) resin
2014 - IRG/WP 14-40654
Phenol formaldehyde (PF) resins, modified by nano CuO incorporating alkane surfactant and polyvinyl alcohol (PVA) 17-99, were analyzed by dynamic mechanical analysis (DMA). The mechanical properties of its bonded plywood including tensile strength, modulus of rupture (MOR), modulus of elasticity (MOE) and shear strength under five test conditions were evaluated. Results indicated that the incorpor...
Wei Gao, Guanben Du


Decay resistance of wood-plastic composites reinforced with extracted or delignified wood flour
2014 - IRG/WP 14-40655
The moisture and decay resistance of wood-plastic composites (WPCs) reinforced with extracted or delignified wood flour (WF) was investigated. Three different extractions were preformed: toluene/ethanol (TE), acetone/water (AW), and hot water (HW). Delignification (DL) was performed using a sodium chlorite/acetic acid solution. All WPCs specimens were made with 50% by weight HDPE and WF, first com...
R E Ibach, Yao Chen, N M Stark, M A Tshabalala, Yongming Fan, Jianmin Gao


Termite resistance of wood modified with short- and long-chain siloxanes
2014 - IRG/WP 14-40660
Scots pine (Pinus sylvestris L.) sapwood specimens modified with short- and long-chain amino-functional siloxane emulsions were exposed to subterranean termites (Reticulitermes flavipes Kollar). Laboratory choice and no-choice tests following the standard EN 117 (2013) were conducted for 8 weeks in order to evaluate the influence of these silicon-based compounds on the termite resistance of treate...
P Gascón-Garrido, M-F Thévenon, H Militz, C Mai


Modern Instrumental Methods to Investigate the Mechanism of Biological Decay in Wood Plastic Composites
2014 - IRG/WP 14-40674
Various instrumental techniques were used to study the fungal decay process in wood plastic composite (WPC) boards. Commercial boards exposed near Hilo, Hawaii (HI) for eight years in both sun and shadow locations were inspected and tested periodically. After eight years of exposure, both boards were evaluated using magnetic resonance imaging (MRI), while a selected area of the board exposed in sh...
G Sun, R Ibach, M Gnatowski, J Glaeser, M Leung, J Haight


Possible targets of wood modification in brown rot degradation
2014 - IRG/WP 14-40676
Wood modification protects wood from fungal degradation in a non-toxic manner. However, the mechanisms behind the decay resistance in modified wood are currently unknown. The aim of this study was to discuss the i) colonisation, ii) nutrient recognition, iii) transcription, iv) depolymerisation and v) hydrolysis steps in the brown rot degradation progress and explore whether they are inhibited by ...
R Ringman, A Pilgård, G Alfredsen, B Goodell, K Richter


The Physical Properties of Heat Treated Fir Wood and Outdoor Durability
2014 - IRG/WP 14-40677
Wood might be easily susceptible to degrade by biotic and abiotic factors. Therefore, wood should be protected from fungi, insects and other degradation factors by applying treatment methods. Especially, for the wood have used in the external environment. Chemical treatment methods have some disadvantages such as use of toxic chemicals (Arsenic and chromium) and treatability of refractory wood spe...
O E Özkan, H Vurdu, A Temiz, G Köse


Laboratory Study of Relative Leachability of Chromated Copper Arsenate Preservative from Treated Woods among Soil Types of Sarawak
2014 - IRG/WP 14-50307
Wood and soils are important natural resources from the environment and serves mankind well respectively as structural materials and natural platform erecting such materials. With shortfalls of naturally durable timber species for protected in-ground uses under Malaysian environments, Chromated Copper Arsenate (CCA) treated woods are widely used instead, incurring serious potential threats of pres...
A H H Wong, P K F Chong


Interpretation of moisture monitoring data - Relevance of moisture content thresholds for fungal decay
2015 - IRG/WP 15-10839
It is widely accepted that besides temperature wood moisture content (MC) is the key factor when it comes to durability of wooden structures exposed to weathering. Many approaches to predict the service life of wooden structures have therefore been based on using wood MC as one major input-variable to develop dose-response relationships between material climate and decay response. However, to impr...
L Meyer, C Brischke


An update on durability of New Zealand grown timber
2015 - IRG/WP 15-10851
Classification and predication of in-service performances of naturally durable timber is much more difficult than preservative treated timber due to the variability of wood properties within and between trees of the same species and the variable nature of the hazard to which the timber will be exposed. A combination of field test and in-service testing has been used to classify the suitability of ...
D Page, T Singh


Durability of treated wood Corymbia torelliana and Eucalyptus grandis x Eucalyptus urophylla against subterranean termite
2015 - IRG/WP 15-20563
This work aimed to analyze the durability of woods against termite Nasutitermes corniger Motsch. Fence posts from this study were collected in Pinheiros, north of Espírito Santo state, Brazil. Used the Corymbia torelliana and Eucalyptus grandis x Eucalyptus urophylla species with 11 and 9 years, respectively and plant spacing of 3.00 x 2.00 m. Were used 72 samples from discs removed the 0.50 m of...
D Junior Verly Lopes, J Benigno Paes, P N de Medeiros Neto, G dos Santos Bobadilha


Building solid foundations to support market growth of preserved wood in the UK – treatment quality, product approval and the largest national field trial of preservative treated wood in 50 years
2015 - IRG/WP 15-30662
The Wood Protection Association (WPA) has just commissioned Britain’s largest ever durability trial of home grown timber, having contracted Building Research Establishment (BRE) to conduct a long term controlled field trial of sawn and pressure treated British Softwood posts at two sites with differing soil conditions. This large scale Field Trial is the last of an innovative and substantial thr...
E Suttie, G Ewbank


Potential of teak heartwood extractives as a natural preservative against Nasutitermes corniger termite
2015 - IRG/WP 15-30666
Most low durability timber are treated with waterborne preservatives consisting of metallic salts, however, these substances make the process expensive and are harmful to man and the environment, requiring cares with handling, dosing and leaks. Due to these facts, several researches have shown the use of natural substances, extracted from the wood of various naturally durable species, as potential...
V Fassina Brocco, J Benigno Paes, L Gonçalves da Costa, S Brazolin


The effect of preservative treatment on mechanical strength and structural integrity of wood
2015 - IRG/WP 15-30667
The use of wood for demanding construction applications is increasing in Europe. Wooden constructions are frequently designed of susceptible conifer wood, which is endangered by wood decay fungi in wet applications. Therefore in many cases treating wood with preservatives is unavoidable to ensure the desired service life. However, chemical treatment of wood can result in changes of its mechanical ...
M Humar, D Kržišnik, C Brischke


Durability of Fence Posts of Four Wood Species After 20 Years in Field Test
2015 - IRG/WP 15-30670
In the past years, wood consumption from native forests has drastically reduced the availability of wood. Fast-growing species such as Pinus and Eucalyptus suitably impregnated with chemicals may show a service life equal or higher than hardwood with high natural durability. The field tests have been an alternative widely used to evaluate the durability of wood and the efficiency of preservatives....
A Florian da Costa, A C Salgado de Freitas, E Meneses Oliveira


Mould growth on spruce claddings and the effect of selected influencing factors after 4 years of outdoor testing
2015 - IRG/WP 15-30671
Norway spruce (Picea abies) is the most frequently chosen wood species as claddings in façades in Norway, and is used both coated and uncoated. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more often growth of mould and blue stain fungi is the main challenge. A field test with synchronous monitoring of relative humidity, air temperature, material temperature and wood moisture content in Norway spruce claddings has been performed in southern Norway as part of the ClimateLife project. Visual evaluation of blue stain and mould growth according to EN 927-3 was performed, and evaluation data after 46 months exposure is presented. The objectives were to study the effect of 1) environment, 2) cardinal direction and 3) colour of the coated surface on growth of blue stain and mould fungi and to study the variation in relative humidity, air temperature, wood moisture content and material temperature. After 46 months exposure, the red coating system had generally the lowest mould ratings and the uncoated claddings had the highest. Of the white coloured claddings the ones facing south had lower mould ratings than those facing north, but the opposite were found for red coloured claddings. The relative humidity was higher in front of claddings exposed northwards and in a shaded environment compared to an open environment against south. In an open environment red coloured claddings had the lowest wood moisture content and highest material temperature, and red coloured claddings against south had the highest maximum material temperature.
L Ross Gobakken, G I Vestøl


Some comments on durability testing of WPC according to EN 15534-1
2015 - IRG/WP 15-40695
The standard EN 15534-1 (2014) gives advice for broad characterization of WPC materials and products. It contains instructions for test procedures concerning different properties e.g. mechanical properties, thermal properties, as well as durability. In this paper some WPC materials from the market were tested for their resistance against brown rot. Furthermore, the water uptake and bending prope...
S Bollmus, A Gellerich, H Militz


Termite and insect resistance of acetylated wood
2015 - IRG/WP 15-40703
The benefits from acetylation of wood to enhance resistance against fungal decay and dimensional stability have been known for many years. Since 2007 Accsys Technologies has been commercially producing Accoya® wood that is based on acetylation of radiata pine. A number of studies on the resistance of acetylated wood to attack by wood destroying termites have been conducted, but there is no common...
F Bongers, M Kutnik, I Paulmier, J Alexander, H Militz


Experimental Measurements of Fire Retardants on Plywood at Fire Test
2015 - IRG/WP 15-40709
The use and development of wood composite materials increased in the past few years. However, in Brazil there are some restrictions on these products regarding their use, since it could be considered a potential risk at a fire situation. Thus, becomes evident the need for researches aiming to fit these in safety standards. This study aims to evaluate the efficiency of two new fire retardant produc...
G C A Martins, L A Marcolin, J M Vidal, C Calil Jr


Shells of Coconut and their Durability against Termite Attack
2015 - IRG 15-10853
All tropical and subtropical areas of the Earth are inhabited by termites. In climates with moderate temperatures, they occur less frequently. Especially wood and non-wood materials that grows in tropical areas and used there in timber constructions and woodworking, wood durability and protection against termites should be researched. This paper reports findings from an experimental “AW011” la...
M Dass, A H H Wong, W Unger


High-frequency monitoring of mass loss due to brown rot degradation of modified wood
2016 - IRG/WP 16-10862
Fungi growing in liquid culture undergoes three separate phases in which they i) adapt to the new environment, ii) grow unrestrictedly and exponentially, and iii) are inhibited to increase in number/mass due to lack of nutrients etc. Filamentous fungi have been shown to exhibit similar growth phases in a solid food substrate and have been modelled to grow in this way also in solid wood. In modifie...
R Ringman, A Pilgård, K Richter


Susceptibility of wood substrates to Aurebasidium pullulans at different temperatures
2016 - IRG/WP 16-10863
There is an increasing awareness of how the aesthetical performance of wood exposed outdoors changes over time and especially in the first few years after installation. Mould and blue stain fungi are biological agents that contribute to the weather grey colour on a wooden façade, and the blue stain fungi Aureobasidium pullulans is commonly identified as colonizer on coated and uncoated wood expos...
L Ross Gobakken, G Alfredsen


Moisture induced risk and fungal development in various field test set-ups in and above ground
2016 - IRG/WP 16-20577
A high number of studies on the decay performance of wood in outdoor exposure have been conducted in the past. However, no testing methodology for wooden components exposed above ground reflecting the variety of different loads has been established so far. Many test protocols were modified in different ways throughout the years and results were often published in an encoded or incomplete way. This...
L Meyer-Veltrup, C Brischke