Field and laboratory studies on anti-sapstain preservatives
1982 - IRG/WP 3205
The field tests included 11 different anti-sapstain preservatives and were carried out at different sawmills in southern Sweden. Drying conditions, climate and the local fungus flora were not identical for the different preservatives and comparisons between the preservatives should therefore be made with caution. Results obtained in the field tests are, however, in relatively good agreement with t...
M-L Edlund, B Henningsson


Decay resistance of high performance biocomposites based on chemically modified fibres
1998 - IRG/WP 98-40120
Different partners within the framework of a European research project produced high performance biocomposites aiming at the utilisation of board materials as durable products both in dimensional and biological degrading circumstances. This paper summarises test data, which indicate the potential of board materials produced with modified fibre material. The chemical modifications applied cover a r...
V Rijckaert, J Van Acker, M Stevens


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. 3rd Interim Report
1983 - IRG/WP 4101
This paper updates the results of microbiological examination and marine borer assessment of untreated wood samples (15 x 2 x 2 cm³) and samples treated with 3, 6 and 10% CCA and CCB preservatives. Three reference species - Alstonia scholaris, Fagus sylvatica, Pinus sylvestris were used at all the test sites in addition to local species chosen by participants in the test....
R A Eaton


Incorporating insect behaviour in standard tests of wood preservatives - A possible way to reduce pesticide loadings
2000 - IRG/WP 00-20190
The application of wood preservatives to protect timber against insect infestation is common practice world wide. The effectiveness of wood protecting insecticides is usually determined in various standard tests. Depending on the target pest species and the test method, larvae of different developmental stages and sizes or adult insects are exposed artificially to the insecticide-treated commodity...
H Hertel, R Plarre


A collaborative test to determine the efficacy of poyurethane coatings on wood samples exposed in the marine environment. 1st Interim Report
1988 - IRG/WP 4145
Wood samples coated with elastomeric polyurethane (ca. 50 mils thick) were exposed for up to 2 years in 12 tropical and temperate marine test sites with known teredinid, pholad and/or crustacean infestations. All uncoated control samples were destroyed or partially destroyed. Polyurethane-coated samples were not attacked, the surfaces of the coating were sound and the polyurethane adhered well to ...
R A Eaton


Natural durability of some common Indian timbers and marine plywood against biodeterioration in Kochi waters (India)
1992 - IRG/WP 92-4177
Panels of thirty-eight timber species and marine plywood were tested in Kochi harbour (South-west India) for periods ranging from 3 to 21 months, so as to evaluate their natural resistance against marine borers. Results indicate that all the timber species studied are non-durable, 6 of them having undergone more than 50% internal destruction within 3 months; 14 species in 6 months, 13 species and ...
L N Santhakumaran, M V Rao


An experimental method to simulate incipient decay of wood by basidiomycete fungi
2000 - IRG/WP 00-20200
At very early stages of decay of wood by basidiomycete fungi, strength loss can be measured from wood before any measurable weight loss. Therefore, strength loss is a more efficient measure of incipient decay than weight loss. However, common standard decay tests (e.g. EN 113 or ASTM D2017) use weight loss as the measure of decay. A method was developed that allowed progressive removal of samples ...
S F Curling, J E Winandy, C A Clausen


Decay patterns observed in butylene oxide modified ponderosa pine after exposure in unsterile soil
1982 - IRG/WP 3211
Small blocks of ponderosa pine (Pinus ponderosa Laws) chemically modified with butylene oxide to three different weight gains were exposed for 6 weeks in unsterile soil. Severe surface decay caused by soft rot fungi and tunnelling bacteria was observed in blocks with 8 weight percent gain. The soft rot attack was restricted to the outer parts of the radial walls in the latewood tracheids. Bacteria...
T Nilsson, R M Rowell


Criteria for basidiomycetes testing and ways of defining natural durability classes
1998 - IRG/WP 98-20144
Within the framework of a European research project several laboratories have tested a series of 17 wood species covering the total range of natural durability. Basidiomycete tests are part of the total set up. Although generally based upon standard methods some minor differences in execution of the tests were evaluated for their impact on the results. This variation was superimposed with the fac...
J Van Acker, M Stevens, J K Carey, R Sierra-Alvarez, H Militz, I Le Bayon, G Kleist, R-D Peek


Methods for testing fumigant efficacies against termites
1986 - IRG/WP 1297
Methodologies for testing fumigants against termites are reviewed and factors needed to be taken under consideration for standardization listed. Toxicity should be defined by both direct exposure to the gas and under more practical "barrier" conditions which include test enclosures simulating abiotic surroundings of the termites, i.e. wood, nest material, etc. To observe latent effects, mortality ...
N-Y Su, R H Scheffrahn


The variability of preservative distribution in test blocks
1973 - IRG/WP 220
The techniques for the assessment of likely effectiveness of preservative systems have long been the subject of much discussion. The whole field has recently been reviewed by Hilditch and Hamblyn (1971) who described in detail many of the laboratory test procedures used, but who also indicated the deficiencies in many of these techniques. It has long been the view of many associated with the wood ...
F W Brooks, M R Gayles, R W Watson


Occurrence of manganese deposits in test stakes exposed in groung contact situations
1996 - IRG/WP 96-10182
Dark spots and flecks were frequently recognized on the surface and within non-preservative treated hard- and softwood test stakes placed in soil contact. Energy dispersive X-ray microanalysis in conjunction with electron microscopy showed the flecks to be composed primarily of manganese dioxide. Detailed transmission electron microscopy observations indicated intrusion of manganese into the wood ...
G F Daniel, T Nilsson, J Volc


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 9: Report of third inspection (2 years) in Italy
1980 - IRG/WP 461
The wood samples were submerged in the sea at Follonica, Italy, in April 1977. Follonica, latitudine 42°55' North and longitude 10°45' East, is situated on the Tyrrhenian sea. The recorded temperature varies between 13°C to 25°C, salinity 37-38% and pH about 8. The inspections were carried out after 6 months (10/1977), 1 year (4/1978) and 2 years (4/1979)....
A Gambetta, E Orlandi


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 7: Second report on the samples in Papua New Guinea
1980 - IRG/WP 459
This report presents the findings to date regarding specimens installed in Papua New Guinea, as part of a world-wide marine trial of certain timbers treated with CCA or CCB preservatives. The details of the trial are set out in document number IRG/WP/414. The report discusses the findings in the context of the conditions prevailing at the trial site and of the properties of the trial timbers. The ...
S M Cragg, C R Levy


Ekki heartwood - is “Durable”
2002 - IRG/WP 02-10444
Severe decay damages of bridges made of ekki (Lophira alata Banks) wood which is classified as a durable species in the EN 350:2 as already reported at the 31 IRG annual meeting. This paper deals with results of long-term decay tests of ekki heartwood specimens using 3 isolates (Loweporus tephroporus 2 strains and a fungus of other sp. from damaged ekki bridges) and Trametes versicolor as a refere...
S Doi, R Itoh, S Horisawa


Test Methods – Performance Based Requirements
2004 - IRG/WP 04-20297
In this paper is briefly described the present approach to service life prediction as an essential part of the architectural engineering process. The system of testing the durability of wood is described more in detail including laboratory tests as well as field trials. It is concluded that the system has a lot of weaknesses which makes it less well suited for practical building applications. A le...
M-L Edlund, F Englund, J Jermer, T Nilsson, M Westin, K Ödeen


Evaluating the natural durability of a number of lesser known species of Ghanaian hardwoods using a short term laboratory assay
2004 - IRG/WP 04-10540
Resistance of a number of Ghanaian hardwoods to attack by the crustacean Limnoria quadripunctata was assessed by measuring the production of faecal pellets under forced feeding conditions over a two week period. Small sticks of commercially available, lesser known timber species, were leached in seawater for one week then placed in a cell culture chamber with one animal and 4 ml of seawater. At in...
J R Williams, S M Cragg, L M S Borges, B Shayler


Leachability of borate-modified oriented strandboard: A comparison of zinc and calcium borate
2002 - IRG/WP 02-40232
The leachability of boron in zinc and calcium borate-modified oriented strandboard (OSB) was investigated in this study. The leaching experiments were conducted by exposing edge-sealed OSB samples under running water for 8, 24, 72, and 216 hours. The results were compared with those from the unleached controls. Boron leaching of the modified OSB occurred upon the initial water exposure, and the le...
S Lee, Q Wu


Test methods used for approval of wood preservatives in Indonesia
1994 - IRG/WP 94-20045
Indonesian regulation stipulates that all pesticides, including wood preservatives, must be registered and obtain legal permit from the Minister of Agriculture, c.q. the Pesticide Committee before they are eligible for public use. For that purpose they have to meet safety and efficacy requirements approved by the Pesticide Committee. To meet the efficacy requirements, wood preservatives must be te...
A Martawijaya


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 20: Report on the inspection of specimens at Sekondi, Ghana after 48 months
1985 - IRG/WP 4116
The results of the second inspection of CCA- and CCB-treated test panels exposed at Sekondi, Ghana, in June 1980, are presented. The panels of Pinus sylvestris treated with 3% CCA are stil unattacked after 48 months. Panels treated with 10% CCA and still in test (Fagus sylvatica, Pinus sylvestris and Alstonia scholaris) are still free of attack. Locol species treated with 3% CCB have all been dest...
F F K Ampong, N Asare-Nyadu


Natural durability of wood in ground contact - A correlation between field and laboratory tests
1985 - IRG/WP 2182
A field test is being carried out to evaluate the natural durability of 20 hardwoods. The resistance to decay and termite attack was evaluated in accelerated laboratory tests. The results of the field test after 6 years and 8 months indicate that there is not necessarily agreement between results from laboratory and field tests. It is pointed out that apart from the artificiality of the laboratory...
M S Cavalcante, G A C Lopez, R G Montagna, M E S Fosco Mucci


Leaching of copper, chromium and arsenic from CCA-treated slash pine heartwood
1994 - IRG/WP 94-50020
Drying green slash pine with any of three high temperature drying schedules produced a product in which both the sapwood and the heartwood could be penetrated with CCA using a modified Bethell treatment schedule. Required H3 retentions were achieved in both sapwood and heartwood, from 200 litres per m³ charge uptake. Post-treatment fixation/drying was accomplished by three different regimes, incl...
M J Kennedy, G Palmer


Co-operative field trial. Background notes and questionnaire for field sites
1992 - IRG/WP 92-3733
The first co-operative field trial was designed to study the occurrence of soft-rot in CCA treated hardwoods. Generally speaking very similar results were obtained from the different field sites. In the early part of the trial considerable variability was evident with regard to the rate and type of attack which occurred in the untreated material. With the CCA treated timber the type of decay was p...
D J Dickinson


In-ground evaluation of a copper azole wood preservative (Tanalithâ E) at a tropical Australian test site
1996 - IRG/WP 96-30100
A field trial to determine the in-ground termite and decay resistance of Pinus radiata D. Don impregnated with a copper azole formulation, TANALITHâ E, has been established at a tropical site in the Northern Territory of Australia. Four retentions of TANALITHâ E, containing 1.54, 2.08, 2.92 and 4.30 kg/m³ of Cu, are being evaluated. For comparison, Pinus radiata specimens treated to two retenti...
J W Creffield, J A Drysdale, N Chew


Natural resistance of different species of timber to marine borer attack in the Trondheimsfjord (Western Norway)
1978 - IRG/WP 435
Natural resistance of 34 timber species to marine wood-borers has been discussed, based on data collected from panels immersed in selected localities in the Trondheimsfjord during 1977-78. The wood-borers encountered on the panels were Psiloteredo megotara, Xylophaga dorsalis, Xylophaga praestans and Limnoria lignorum. The number of borers present and their growth were taken as the criterion for a...
L N Santhakumaran, J A Sneli


Previous Page | Next Page