IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 923 documents. Displaying 25 entries per page.


Effectiveness of sol-gel treatments coupled with copper and boron against subterranean termites
2009 - IRG/WP 09-30493
Wood modification by sol-gel treatments shows many positive features, like antimicrobial properties. Wood was also successfully modified with alkoxysilanes enhancing its resistance against soil micro-organisms. Silver, copper, zinc compounds, boric acid or organic biocides such as alkylammonium compounds may be added to the sol-gel to enhance its biocidal properties. Nevertheless, if some of these...
E Feci, L Nunes, S Palanti, S Duarte, G Predieri, F Vignali


Resistance to decay fungi of ammonium borate oleate treated wood
2009 - IRG/WP 09-30505
Ammonium borate oleate molecule (ABO) produced from reaction between boric acid, ammonia and oleic acid was tested as wood preservative treatment against brown and white rot fungi according to European standards. This compound was prepared according to a previous study which has proved existence of synthesis reaction and effectiveness against termites (Lyon et al. 2007b). Four solutions of ABO in ...
F Lyon, M-F Thevenon, A Pizzi, J Gril


Laboratory test of some formulations against stain and mould fungi isolated from bamboo wood
2009 - IRG/WP 09-30508
To screen the effective anti-mould formulations, fungicides such as carbendazim, tebuconazole, fludioxonil, difenoconazole, prochloraz, benomyl and 8-hydroxy-quinoline copper (copper oxine) were selected to conduct the laboratory test of fungicidal activity by method of inhibition zone against Botryodiplodia theobromae Pat., Fusarium sp., Alternaria tenuis Nees., Penicillium purpurogenum Stoll, Tr...
Xingxia Ma, Airui Sun, Mingliang Jiang, Daochun Qin


Environmental Emission of Wood Preservatives: Interpretation of Data Relevant to BPD Risk Assessments
2009 - IRG/WP 09-50259
The risk assessments for the use of wood preservatives proposed by the OECD and used under the Biocidal Products Directive (BPD) (98/8/EC) require the derivation of leaching rates for active substances. These rates are to be used as input data in to agreed exposure scenarios. The leaching rates can be derived from laboratory testing and from field testing. The relationship between laboratory and f...
D G Cantrell


Estimating the heat treatment intensity through various properties of thermally modified timber (TMT)
2009 - IRG/WP 09-40459
The suitability of different measures for prediction of the heat treatment intensity was investigated. Therefore, the resistance to impact milling (RIM), the lightness L*, the equilibrium moisture content (EMC), the anti swelling efficiency (ASE) and the total amount of soluble carbohydrates (TSC) of heat treated specimens were correlated with corresponding fungal resistance achieved by heat treat...
C R Welzbacher, C Brischke, A O Rapp


Biological Performance of Boron-based Chemicals Treated Wood Composites
2009 - IRG/WP 09-40464
In this study, the biological performance of wood-based composites panels treated with boron containing chemicals against to a fungus was determined. Boric acid, borax, zinc borate and agricultural borate (Tarım-borâ„¢), developed and patented by National Boron Research Institute, were mixed with wood chips or fibers and then particleboard, medium strand board and middle density fiberboar...
Ãœ C Yıldız, H Kalaycıoğlu, S Yıldız, A Temiz, E Tomak Dizman, A Çavdar Dönmez


Termite Resistant Properties of Wood and Natural Fiber Plastic Composites - AWPA E1 Test Data
2009 - IRG/WP 09-40466
This paper deals with resistance properties of wood plastic composites against Formosan Subterranean Termites (FSTs) based on the AWPA E1 test standard. Sixteen laboratory WPC formulations, four WPC commercial materials, and southern pine (Pinus sp.) wood control were tested for termite mortality, sample weight loss, and sample damage rating. The results show that FSTs did attack WPC products in ...
Q Wu, T Shupe, J Curole, K Ragon, M Voitier, M Freeman, D Ring


A fast and economic method to produce grey wooden surfaces for decking and cladding: preliminary results
2009 - IRG/WP 09-40474
Uncoated wood is commonly used in France for cladding and decking to minimise maintenance. However wood surfaces progressively turn grey due to exposure to sunlight and water. This grey colour develops after several months depending on the wood species and the exposure: in the northern hemisphere surfaces facing south and west are most exposed and turn grey more rapidly than those facing north and...
L Podgorski, V Georges, I Garmendia, B Sánchez Sarachu


Utilidad práctica de mini estacas en ensayos de campo
2008 - IRG/WP 08-20395
For testing chemicals for the wood against degradation agents of biotic, known as preservatives, both testing in the laboratory and in the fields are used. Field trials (Cemetery stakes) are often accepted as more "real" whose frequency of observation is set to more or less a year in temperate climates and six months or less in tropical situations, taking into accounts the aggressiveness of the so...
O Encinas, J V Puentes, N K Sarmiento, N Mora


Seasonal shifts of fungal community structure at the interface of treated or untreated wood and soil
2010 - IRG/WP 10-10721
Many wood species are degraded rapidly in soil by the fungal community. In order to preserve wood and structures in which it is used, chemical preservatives are used. Little is known about the interaction of treated wood and the surrounding soil fungal community. For this work, presented at IRG 41, wooden specimens (Pinus sylvestris sapwood, sizes 25 mm x 50 mm x 500 mm (longitudinal)) were treate...
M Noll, I Stephan


Natural Durability of Fence Poles from Fourteen Semi-Arid Land Species after Six-Month Exposition
2010 - IRG/WP 10-10724
A sample of thirty fence poles from each of fourteen tree native species from Northeast Mexico were tested in ground contact in a wood-cemetery area located in Linares, Nuevo Leon, Mexico. The samples were submitted to six treatments (control, debarked, chemical treated, used cooking oil, thermal and creosote) and randomly distributed in five blocks. The effectiveness of using a bark gauge tool â€...
A Carrillo, F Garza, V Bustamante, S Sandoval, H Villalón


Decay Resistance of Maple (Acer Insigne) Wood Against White Rot
2010 - IRG/WP 10-10740
In this study, the decay resistance of maple (Acer insigne) in natural state and treated with ACC (Acid copper chromate) was investigated against the white rot fungus (Coriolus versicolor). ACC is a kind of water borne preservatives that was used in this study for treating specimens under vacuum and pressure (Bethell procedure) with 3 percent concentration. In conducting mentioned evaluation, koll...
V Tazakor Rezaei


Glued laminated poles - Progress report after 30 years testing
2010 - IRG/WP 10-20427
In 1979 a number of glued laminated poles treated with CCA and creosote were placed in a greenhouse at Uppsala, at the Simlångsdalen test field in southern Sweden and in a power lane in Vuollerim in northern Sweden in order to study their resistance against biological degradation. The tests have shown that the best performance will be obtained if each lamination is treated with a water-borne pre...
Ö Bergman, J Jermer


The Relative Performance of an Organic Preservative System under UC3A and UC3B Conditions using Two Test Methods
2010 - IRG/WP 10-20429
Coated L-joints have been used for decades to evaluate the performance of wood preservatives in protected environments. This study was conducted using matched coated and uncoated L-joints to simulate above ground protected and unprotect exposures. When exposed to constant moisture in a greenhouse environment, coated and uncoated L-joints give very similar performance results. In contrast, exposi...
C F Schauwecker, A Zahora, A F Preston


Determination of a fixation time of wood preservatives: A discussion paper
2010 - IRG/WP 10-20436
The intention of that paper is to initiate a discussion on the basis of a French method in combination with a German approach regarding the need of a method for the determination of a fixation time and especially to obtain input as well as ideas concerning a possible test design. Since no harmonised European approach exists up to now concerning the determination of a fixation time, CEN TC 38 (2009...
E Raphalen, E Melcher


Diagnosis of failures in wood beams from historical house in Banská Štiavnica – Relations between ultrasonic measurements and bending properties
2010 - IRG/WP 10-20437
Various degrees of rot and other damages in ceiling beams with dimensions of 6500-8800 x 160-200 x 240-310 mm (length x height x width) situated in one historical bourgeois house in the UNESCO town Banská Štiavnica, Slovakia were determined visually and by the PUNDIT-plus ultrasonic device. Subsequently, for seventeen of the most bio-damaged fir (Abies alba Mill.) beams chosen for exchange were ...
L Reinprecht, M Pánek


Service life prediction of wooden components – Part 1: Determination of dose-response functions for above ground decay
2010 - IRG/WP 10-20439
Scots pine sapwood (Pinus sylvestris L.) and Douglas fir heartwood (Pseudotsuga menziesii Franco) specimens were exposed in double layer field trials at 24 different European test sites under different exposure conditions (in total 28 test sets). The material climate in terms of wood moisture content (MC) and wood temperature was automatically recorded over a period of up to eight years and compar...
C Brischke, A O Rapp


Impact of climate change on wood deterioration - Challenges and solutions for cultural heritage
2010 - IRG/WP 10-20441
Deterioration of wood in cultural assets follows the same physiological mechanisms as in modern structures. Therefore rules and data for prediction of service life derived from old wooden structures can be used to model the service life of recent wooden structures and vice versa. The latter is done in this paper: From experimental test set ups in the field spread over Europe, climatic data, wood t...
C Brischke, A O Rapp, M Hasan, R Despot


Stress wave and visual analysis of treated and non treated fence posts after 15 years in field test
2010 - IRG/WP 10-20449
Wood preservation may play an important role in protecting tropical rain forest. Basically, it can reduce pressure on natural resources by increasing wood durability. Field tests are conducted to simulate final use of woods under different environmental conditions. Visual analysis, non destructive testing, and non destructive evaluation techniques were applied to assess wood resistance and chemica...
A Florian da Costa, R Faustino Teles, J Costa Gonçalves


Improved analysis of field test data related to service life prediction of tropical wood species
2010 - IRG/WP 10-20458
Long field trials of wood in ground contact give valuable data on the natural durability of the material. The European Standard EN 350 gives guidance on how to perform these durability classification, but is limited to the use of averages of in-service life of a set of specimens compared to a reference set. Starting from a database of visual assessment of field stake testing, it is possible to obt...
J Van den Bulcke, A Wong, Ling Wang Choon, Yoon Soo Kim, J Van Acker


Service life prediction for exterior timber cladding
2010 - IRG/WP 10-20460
This discussion paper considers service life prediction for timber and the work within the pan-European WoodExter project. The project aims to develop a model for service life prediction of exterior timber cladding, to enable better end use selection of material suitable for delivering the required service life of cladding and to provide information for professionals wanting to understand and use ...
E Suttie, F Englund


Synthesis of novelty borate compounds for wood preservatives: Laboratory test of leachability and decay resistance
2010 - IRG/WP 10-30520
A novel series of ammonium tetraphenylborate (ATB) and borate chemical compounds (BBC) were synthesized as wood preservatives. The leaching rates and decay resistance of boron formulations containing ATB and BBC were conducted. The laboratory leaching results showed that boron leaching rate of treated wood by ATB formulations was from 2.1% - 6.7%, while that of BBC formulations from 23.3% -59.0%. ...
Zhiqiang Li, Mingliang Jiang, Xingxia Ma


Comparison of Bifenthrin Formulations for Their Skin and Eye Irritation Potential Using the Pollen Tube Growth Test
2010 - IRG/WP 10-30521
The Pollen Tube Growth Test (PTGT) is an effective screening method for measuring the potential of a chemical formulation to affect living cells. The PTGT has been compared against other types of testing, and it shows a good correlation with, for example, the Draize rabbit eye test and the human skin patch assay. It measures the EC50, which is the effective concentration at which 50% growth is o...
S Millward, P Lobb


Evaluation of ACQ-D treated Chinese fir and Mongolian Scots pine with different post-treatments after 20 months of exposure
2010 - IRG/WP 10-30530
The performance of alkaline copper quat-type D (ACQ-D) treated Chinese fir (Cunninghamia lanceolata Hook.) and Mongolian Scots pine (Pinus sylvestris Linn. var. mongolica Litv.) stakes after 20 months exposure in Chengdu and Guangzhou of southern China were evaluated according to AWPA standard E07-07. The ACQ-D treatments used two concentration levels (0.5 and 1.0%) and four different post-treatme...
Lili Yu, Jinzhen Cao, Wei Gao, Haitao Su


Copper preservative systems: A rapid investigation into effects of co-biocides and used treating solutions
2010 - IRG/WP 10-30541
The efficacy of various micronized and amine copper preservative systems was evaluated using soil block testing with the copper tolerant brown rot fungi, Postia placenta. The American Wood Protection Association E22 protocol was used to compare the relative efficacy of preservatives by monitoring compressive strength losses of the systems in southern pine wood. As information, the weight losses ...
T F Shupe, K Ragon, Q Wu, M H Freeman, C R McIntyre


Previous Page | Next Page