IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 1065 documents. Displaying 25 entries per page.


A short note on fungal decay in K33-treated poles
1982 - IRG/WP 1169
Soft rot cavities and erosion of the lumen have been found in K33-treated Pinus sylvestris poles from the years 1956-66 by microscopic studies. Poor treatment quality has been proved for some of these poles. The microscopy showed an unusual pattern of attack, and pre-treatment decay is suspected but not yet proved. Sounding the poles and using the Pilodyn indicated decay, but poking did not. Quant...
H Friis-Hansen


Accelerated wood decay in a soil bed test under greenhouse conditions compared with a stake test under field condition
1991 - IRG/WP 2384
The rate of decay of oak, beech, Douglas fir, pine and spruce stakes in an outside test field were compared with the decay rate of the same species in a greenhouse soil-bed test. Strength loss after four and six months respectively was measured by determining the compression strength parallel to the grain. The results show that all species, strength loss in the greenhouse was 2 to 4 times higher t...
J E Polman, S G Michon, H Militz


Wood preservation in the Australian beekeeping industry
1988 - IRG/WP 3473
This paper reports the results of a survey of Australian commercial beekeepers working 200 or more hives in June/July 1985. Nine hundred and forty seven apiarists were asked to participate and to provide information on their wood preservation methods, painting procedures and maintenance of bee boxes. Three hundred and eighty-four apiarists returned completed questionnaires (41%). The main wood pre...
P J Robinson, J R J French


Effect of sterilization method on germination of spores of wood decay fungi observed by contact agar block method
1978 - IRG/WP 2117
Previous studies of germination of spores of wood decay fungi on wood have generally concluded that method of wood sterilization has little significant effect on germination response. This study expands the numbers of test fungi as well as number of sterilization methods employed to determine the influence of sterilization method on spore germination response of decay fungi. Germination was assess...
E L Schmidt, D W French


Non-enzymatic Gloeophyllum trabeum decay mechanisms: Further study
2001 - IRG/WP 01-10395
Information will be presented on the mechanisms involved in, and potential application of, non-enzymatic wood decay by brown rot decay fungi. Specifically, the hypothesized role of low molecular weight phenolate derivatives will be discussed in relation to non-enzymatic degradation of wood. The mechanism of binding of iron by cellulose, and binding and reduction of iron by fungal derivatives and m...
B Goodell, J Jellison


Combined effects of the treatment of wood with formaldehyde
1978 - IRG/WP 3117
Treatment of fibrous materials with reagents in a vapor phase is neither new nor unique. Numerous examples exist in literature of vapor phase experiments on cellulose fibers and fabrics, and on wood. For many years the textile research and industry have used vapor phase processes for the treatment of textiles. The chemical modification of cellulose is based on different types of reactions e.g. est...
M Stevens, J Schalck


Recent names for some common decay fungi
1976 - IRG/WP 143
A Käärik


An approach to testing the preventive effectiveness of preservative treatments for wooden joinery
1981 - IRG/WP 2156
The ecological sequence established in field trial samples exposed out of ground contact has shown the need for outdoor exposure in testing potential joinery preservative pretreatments. A system of exposure of L-joint units is proposed. Data obtained by examining samples destructively show promise as the basis for predicting service life after relatively short exposure periods (within 2 years)....
J K Carey, A F Bravery, J G Savory


Evaluation of the decay caused by Chaetomium globosum Kunze, in the course of time
1987 - IRG/WP 2288
The main research done on soft rot has been directed to determining, by microscopic study, the different stages of penetration into the wood of the fungi that cause it. On the basis of the information furnished by this research, in this work we have tried to quantify its effect, by evaluating the weight loss caused by Chaetomium globosum Kunce in wood of Pinus sylvestris L. and Fagus sylvatica L. ...
M T De Troya, A M Navarrete


The use of C CP/MAS NMR in the chemical identification of decayed and undecayed, tropical timber species
1984 - IRG/WP 1224
13C CP/MAS NMR was found to be an extremely powerful tool for elucidating the chemical composition of Eucalyptus maculata, Pinus elliottii and Alstonia scholaris. The differences in lignin composition were different for each timber and discussed in relation to decay caused by soft-rot and white rot fungi. In particular the presence of syringyl and guaiacyl lignin types are discussed.
L E Leightley


Étude in vitro de la colonisation et de la dégradation structural du bois de hêtre par Coriolus versicolor (L.) Quélet
1976 - IRG/WP 158
L'attaque du bois de Hêtre par Coriolus versicolor (L.) Quélet, agent de pourriture fibreuse blanche est étudiée après des périodes d'exposition à ce champignon variant de 15 jours à trois mois. L'observation des premiers stades, c'est à dire de la colonisation du bois par les filaments de champignon est faite en microscopie optique, puis au fur et à m...
D Dirol


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water: Final report
1987 - IRG/WP 4133
Three timbers chosen as reference species were treated with 3, 6 and 10% solutions of CCA and CCB preservatives and exposed for up to 93 months at 8 tropical and temperate marine sites. Eleven local species treated in the same way were exposed at 4 of the 8 sites. There was no apparent difference in performance between CCA and CCB treated specimens. The severest test site was Panama Canal but mari...
R A Eaton


Effects of the anaerobic wood decay bacterium Clostridium xylanolyticum on unbleached Pinus and Eucalyptus pulp
1991 - IRG/WP 1506
Clostridium xylanolyticum has been shown to produce extracellular enzymes capable of degrading wood. The present work was conducted to quantify growth on various lignocellulosic substrates and degradation of pulped wood fibre. In the latter tests Clostridium xylanolyticum was incubated at 35°C under anaerobic conditions in a medium containing 0.2% (w/v) peptone and 4% (w/v) unbleached Pinus and E...
G D Shelver, U Matai, W Van Wyk, A A W Baecker


Model questionnaire for preparation of monographic cards for wood-destroying fungi
1972 - IRG/WP 103
C Jacquiot


Questionnaire for Volume 2 of the basidiomycete monographs
1985 - IRG/WP 1254
12 monographs of wood destroying basidiomycetes were published in volume 1. Volume 2 includes the following 17 basidiomycetes: Antrodia serialis, Chondrostereum purpureum, Climacocystic borealis, Fomitopsis pinicola, Hyphoderma tenue, Lentinus degener, Lentinus squarrulosus, Paxillus panuoides, Phellinus contiguus, Poria xantha, Pycnoporus sanguineus, Rigidoporus vitreus, Serpula himantoides, Sistotrema brinkmannii, Stereum sanguinolentum, Trametes corrugata
T Nilsson


Decay resistance of resin treated wood
1999 - IRG/WP 99-30206
Selected natural resin systems were evaluated for their potential as wood protecting agents according to standard test procedures. As indicated by the European standard EN 599 both a Basidiomycete test according to EN 113 and a ENV 807 soil bed test were carried out. Six resin treatments were tested using 3 concentration or treatment levels. Using the biocidal activity criteria as usually applied ...
J Van Acker, A J Nurmi, S M Gray, H Militz, C Hill, H Kokko, A O Rapp


On the use of % weight loss as a measure for expressing results of laboratory decay experiments
1992 - IRG/WP 92-2394
It is suggested that careful consideration should be given for the presentation of data from laboratory decay experiments, especially when comparisons are being made from experiments involving wood blocks of varying densities. Percent weight loss can be used for comparisons of durability even if wood blocks vary in density. It is suggested that the absolute weight loss for a given volume (g/cm³) ...
T Nilsson, G F Daniel


Wood decay in Danish buildings
1985 - IRG/WP 1261
At Technological Institute identification of fungi and advisory activity concerning repair of damages has taken place since 1935. Statistical analyses based on material from 1982 and 1983 are compared to earlier investigations worked out by L. Harmsen. The material shows that building traditions influence the diversity and frequency of fungal species. Many fungal damages in the last decade have sh...
A P Koch


Estimation of service life of durable timber species by accelerated decay test and fungal cellar test
2002 - IRG/WP 02-20249
Many kinds of durable wood species for outdoor uses has been imported from all over the world to Japan. However information on the natural durability of these species is not sufficient to estimate the service life of them in the climate of Japan. Highly durable species such as Jarrh, Teak, Ipe, Ekki, Selangan batu, Red wood, Western red cedar showed no significant percent mass losses by accelerate...
K Yamamoto, I Momohara


Biological control of decay in standing creosote-treated poles
1976 - IRG/WP 156
Internal decay caused by basidiomycetes in standing creosoted poles can be controlled biologically, it seems, by artificial inoculation near the ground line. For such inoculation IC-type facultative mycoparasites, Scytalidium sp FY strain or Trichoderma spp for example, may be used. Apparent residual action can be explained by the release of non water soluble chemically stable antibiotics from the...
J Ricard


An insight into brown rot decay of timber as revealed by 13C CP/MAS NMR
1985 - IRG/WP 1259
L E Leightley


Monographic card: Coniophora puteana (Schum. ex Fr.) Karst. (Second draft)
1978 - IRG/WP 171
A Käärik


Comparison of decay rates of preservative-treated stakes in field and fungus cellar tests
1980 - IRG/WP 2135
With the exception of acid-copper-chromate, zinc-chrome-arsenate, and sodium pentachlorophenoxide, the relative performance of preservatives in the fungus cellar was similar to that in the field....
M E Hedley


A new approach to the maintenance of wooden railway sleepers. (Second report)
1988 - IRG/WP 3492
The microenvironment and micro-ecology of wooden railway sleepers was investigated to assess their condition to determine the necessary treatment, repair and replacement criteria. In this report the efficacy of the secondary preservative treatment with solid boron rods is discussed and the development of an in-situ, nondestructive test method based on the creation and assessment of structural dyna...
W Beauford, P I Morris, A M Brown, D J Dickinson


Studies on the preservation of structrual plywood - Part 1: Decay resistance of structural plywood
1974 - IRG/WP 238
The weight loss and the decreases in the compression strength and in the modulus of elasticity were measured to determine the decay resistance of structural plywood (lauan). Test pieces (50x25xA mm³) were exposed to the wood destroying fungi (Coriolus versicolor and Coriolellus palustris) for 2-3 or 2-4 months. After exposure, the measurement of the compression strength was carried out on the pie...
K Minami, Y Kenjo, S Sugiyama


Previous Page | Next Page