An attempt to grow dry rot fungus Serpula lacrymans on mortar substrate in non-sterile conditions
1989 - IRG/WP 1385
According to many experts, Serpula lacrymans is probably the most dangerous wood destroying fungus in houses. Investigations of KOCH, A.P. (2) showed that incidence of this fungus in percent was around 20% when the frequency of some other standard fungi was far below (Coriolus versicolor: 0.2% for example). The work presented here is a part of a program carried out at CTFT for assessing the resist...
L N Trong


European standardization for wood preservation
1991 - IRG/WP 2365
Since the last IRG 21 conference in New-Zealand, there one meeting of the plenary committee and several meetings of working groups. The interprative documents prepared by CCE for expliciting the essential requirements of the CCE Directive on the construction products and specially: mechanical resistance and stability / hygiene, health and environment / safety in use are waited to valid the progra...
Anonymous


Synergistic combination of an antioxidant and wood preservative: a preliminary study
1998 - IRG/WP 98-30172
We previously proposed that extractives in highly durable angiosperm heartwood may protect wood against white-rot fungal colonization and subsequent degradation by a dual mechanism: extractives have some fungicidal activity and are also free radical scavengers (antioxidants) and thus interfere with the fungal free radical degradative mechanisms. We tested this hypothesis using the commercial bioci...
T Schultz, D D Nicholas, J Minn, K D McMurtrey, T H Fisher


The high decay resistance in the sapwood of the naturally durable Malaysian hardwood Belian (Eusideroxylon zwageri)
2001 - IRG/WP 01-10410
It has long been assumed that the observed natural durability of the heartwood in certain timbers is perhaps associated with a relatively lower decay susceptibility also of the sapwood of these species. While the heartwood of Belian is reputedly highly decay resistant among the tropical hardwoods of Southeast Asia, laboratory decay tests reported in this paper have also confirmed the high decay re...
A A H Wong, A P Singh


Microscopic analysis of southern pine utility pole core segments
1992 - IRG/WP 92-1542
Fifteen macroscopic core descriptive categories were evaluated by microscopic analysis for accuracy in detecting decay and judging decay severity. Five categories were good indicators of decay as decay was detected in 28 of 48 samples. Five categories were possible indicators of early decay as decay was detected in 6 of 40 core segments and an additional 18 contained hyphae. The remaining five cat...
S E Anagnost, C J K Wang, M Wright


Performance of Tuff Brite C™ and other formulations against blue-stain, mold and brown-stain in freshly-sawn rubberwood (Hevea brasiliensis) in the humid tropics of Peninsular Malaysia
1997 - IRG/WP 97-30163
The relative anti-sapstain and anti-mold efficacies, including brown-stain development in freshly-sawn rubberwood (Hevea brasiliensis) in the Malaysian tropics, between selected water-based product concentrations of formulations Tuff Brite CTM without/with added Borax (at 1.5/0, 1/1.5, 1.5/1.5 and 2%/1.5%), PQ8TM without/with added Borax (at 2.5/0, 1.5/1.5, 2/1.5 and 2.5%/1.5%) and NeXgenTM/NeX-Br...
A H H Wong, T L Woods


Suitability of cotton strip testing as a screening method for the development of wood preservative formulations
2003 - IRG/WP 03-20270
This paper outlines a simple and rapid test method for screening the efficacy of wood preservative formulations against microbiological attack using cotton strips. The method was evaluated against soft rot and was found to provide reliable information on the protection of lignocellulosic material against microbiological attack. The assessment is based on visual interpretation of decay and on a sim...
H Leithoff, I Stephan, H Härtner


Dimensional stabilization and decay resistance of wood treated with brown-rotted lignin and copper sulfate
1990 - IRG/WP 3608
The objective of this study was to evaluate the potential usefulness of brown-rotted lignin (BRL) as a dimensional stabilization and copper complexing agent for wood treatment. For dimensional stabilization, aqueous solutions of the lignin extract were combined with either copper sulfate, glyoxal or other additives. Anti-shrink efficiency (ASE) values as high as 42% were obtained with wood treated...
L Jin, D D Nicholas, T Schultz


Reduction of kiln brown stain in radiata pine lumber after log fumigation with methyl bromide
1997 - IRG/WP 97-30129
Methyl bromide fumigation of freshly felled radiata pine log sections effectively killed living cells in parenchyma to at least 75mm into sapwood. Lumber cut from logs (fumigated and control) stored 1 month outdoors (dry) showed slightly reduced brown stain when kiln dried at conventional temperatures. A more dramatic reduction and elimination of brown stain was noted in lumber cut from fumigated ...
E Schmidt, M E Hedley, D R Page, D Cross


Mechanistic aspects of the reactions of copper complexes with lignin in the presence of hydrogen peroxide and lipid hydroperoxide model compounds as proposed for white rot fungi
2001 - IRG/WP 01-10399
The structural principles and the oxidative reactions of the catalytic system consisting of copper, hydroperoxides, and copper coordination compounds that contain aromatic nitrogen atoms are similar to those of catalytic centers of oxidative enzymes involved in delignification reactions of white rot fungi. The system is capable of selectively degrading lignin and its low molecular weight would all...
K Fackler, P Lamaipis, E Srebotnik, M Humar, C Tavzes, F Pohleven, M Sentjurc, T Watanabe, K Messner


Developments in unsterile soil soft rot testing
1984 - IRG/WP 2210
Two unsterile soil test methods, the soil burial technique and a method using vermiculite burial with soil inoculation, were compared using different soils to determine their effectiveness in evaluation of wood preservatives against soft rot. Isolation of fungi and microscopy of decayed wood indicated that both methods produced accelerated soft rot attack in treated and untreated birch. Vermiculit...
P A McKaig


Collaborative soft rot tests: Tests conducted at Princes Risborough and Delft on soil samples from collaborating laboratories
1972 - IRG/WP 210
The laboratories which took part in the original collaborative soft rot test (Savory and Bravery, Holz u Org 5 (1) 58-90, 1970) sent samples of the soil used in the original test to Princes Risborough. Portions of this material were sent to Dr Hof for soil analyses at TNO and the remainder was employed at Princes Risborough for the conduct of comparative tests of soil virulence when used as a comb...
J G Savory


Fruitbody formation and basidiosporogenesis by the white rot fungus Pycnoporus cinnabarinus
1988 - IRG/WP 1348
Conditions for fruitbody formation by the white rot fungus Pycnoporus cinnabarinus in vitro were outlined. A marked difference in substrate requirements in comparison to previously tested brown rot fungi was revealed. Agar media containing Walseth cellulose and NH4 tartrate at 1 g/l permit profound production of basidiospores particularly at 15°C but only under light treatment. Higher NH4 tartrat...
J Bjurman


Which substrate to use in a laboratory test with soft rot micro-fungi: vermiculite or unsterile soil?
1991 - IRG/WP 2372
A draft European Standard is being proposed by CEN TC 38 in which a vermiculite-burial and a soil-burial test to be carried out in succession are required. Various experiments with both procedures were set up with CCA, CC and propiconazole-formulations. The results show that vermiculite and unsterile soil yield comparable threshold values against soft rot. This poses the question of whether a two-...
A R Valcke


Influence of variable lignin content amongst hardwoods on soft-rot susceptibility and performance of CCA preservative
1982 - IRG/WP 1151
This paper presents the outline of an argument, based on both new and established data, which relates varying lignin content to variation of soft-rot susceptibility between hardwood species and of performance of CCA preservatives in controlling soft-rot. Although more data need to be generated to prove this relationship, sufficient evidence exists for the hypothesis to be given close attention, pa...
J A Butcher, T Nilsson


Effect of moisture and cellulosic substrate on decay of hardwoods by soft-rot fungi
1982 - IRG/WP 2173
The development by Forintek Canada Corp. of standard test procedures for laboratory preservative evaluations using soft-rot fungi was requested by the American Wood Preservers' Association. In Europe, through cooperative studies in the International Research Group on Wood Preservation, several attempts have been made to produce a standard procedure, but variability in results obtained bet...
A Byrne, R S Smith


Collaborative soft rot tests: Statistical treatment of results of soil analyses
1971 - IRG/WP 29
Institutes taking part in the collaborative experiments already reported forwarded samples of the soils employed in the tests to the Forest Products Research Laboratory, England. The soils were then autoclaved sterilised under uniform conditions and sent to the Department of Forest Soils, the Royal College of Forestry, Stockholm, Sweden. The results of the soil analyses are given in Table 1, toget...
A F Bravery


Soft-rot in Tabebuia sp. wood used in water cooling tower: identification and degradation capacity of the fungi
1998 - IRG/WP 98-10253
Tabebuia sp. (ipe), a native Brazilian wood, is considered of high natural resistance to decaying fungi, and has been used in harsh environments, as cooling towers. Fifty-one fungi, belonging to mitosporic fungi group (Fungi Imperfecti), were isolated from deteriorated Tabebuia sp. wood samples, collected from the mist eliminator and packing of a cooling tower in operation for about 23 years. The ...
S Brazolin, M Tomazello, I H Schoenlein-Crusius


Design of a laboratory method for evaluating the effectiveness of soft rot preservatives
1988 - IRG/WP 2312
This purpose of this work was to design a method which makes it possible to evaluate the effectiveness of products which present protect wood against soft rot, using new products·of a different nature, on wood of·Pinus sylvestris L. and Fagus sylvatica L., and which, suitably applied, avoid big economic losses deriving from lack of knowledge of the active principles suitable to present protect w...
M T De Troya, A M Navarrete


Practical experiments with Boracol 10 Rh used as a fungicide in the repair process after attack by the dry rot fungus (Serpula lacrymans)
1987 - IRG/WP 3458
The test is carried out in an old house in Nyhavn, Copenhagen. The roof and the walls close to were heavily attacked by dry rot fungus (Serpula lacrymans) because damage to the zinc covering the frontspice were letting in water to the wood and wall construction. An attack by the dry rot fungus is more complicated to repair compared with other wood destroying fungi because beside the damage on wood...
J Bech-Andersen


Soft rot fungi found in copper/chrome/arsenic treated hardwood power transmission poles in Queensland
1978 - IRG/WP 185
In Queensland the effective service life of copper/chrome/arsenic (CCA) treated hardwood telegraph and power transmission poles is being dramatically shortened due to attack by soft rot decay fungi. The Australian Wood Preservation and Pole Industries are funding research into this serious soft rot problem involving C.S.I.R.O. and the University of Queensland. The C.S.I.R.O. is actively engaged wi...
L E Leightley


The evaluation of a survey of dry rot damages in Japan
1983 - IRG/WP 1179
The damage of wooden houses from Serpula lacrymans has increased in Japan, particularly in the northern area, Hokkaido Prefecture (See Figure 1). The weather conditions in Asahikawa have been recorded. The data obtained from the survey carried out over the five years from 1975 to 1980 were previously reported to the 5th International Biodeterioration Symposium which was held in Aberdeen, Scotland ...
S Doi


Assessing the bioresistance conferred to solid wood by chemical modification
1997 - IRG/WP 97-40099
The chemical modification of wood using straight chain alkyl anhydrides can considerably enhance its durability. This paper presents an assessment of the effectiveness of these modifiers in improving the biological resistance of a susceptible softwood when exposed to four different basidiomycete fungi, soft rots and the larvae of the house longhorn beetle (Hylotrupes bajulus). It was clear that so...
E D Suttie, C A S Hill, D Jones, R J Orsler


Soft rot decay in CCA treated eucalypts in Queensland - A comment
1986 - IRG/WP 1301
A survey has been completed concerned with the distribution and severity of groundline soft rot decay in the CCA treated sapwood of eucalypt poles in Queensland. The survey encountered some 1000 poles of which 55% were slightly, 28% moderately and 17% severely decayed. Soft rot decay was more severe in urban than rural locations. Embedment of poles in concrete resulted in severe soft rot. No signi...
L E Leightley


Mould growth at lumber surfaces of pine after kiln and air drying
1994 - IRG/WP 94-40033
Distribution of water soluble substances in green wood and later redistribution during drying is of importance for the colonisation of wood by microorganisms. According to literature the availability of nitrogenous materials is probably a major limiting factor to the microbial colonisation of wood. King et al. (1974) and Oxley et al. (1976) have shown correlation between surface nutrient concentra...