Diazenes and some organic complexes of boron as potential fungicides for preservation of wood
1999 - IRG/WP 99-30197
Screening for fungicidal activity represents the first step in searching for new active components with enhanced environmental profile in comparison with traditional wood preservatives. Diazenes, their salts, and the salts of the corresponding semicarbazides, as well as several complexes of boron, were screened for fungicidal activity against wood decay fungi Trametes versicolor, Coniophora putean...
M Petric, B Paradiz, J Stern, F Pohleven, S Polanc, B Stefane, R Lenarsic


Wood preservation sites polluted by CCA. Is potassium diphosphate incubation a catalyst for the electrodialytic remediation of these soils?
1998 - IRG/WP 98-50106
As part of an evaluation of a newly developed electrodialytic soil remediation technique, we investigated the incubation of a contaminated soil (from a Portuguese wood preservation site polluted with CCA) with potassium diphosphate as a possible catalyst for the removal of heavy metals and metalloids. A chemical sequential extraction scheme (SE) applied to the soil has shown that the potassium dip...
A B Ribeiro, G Bech-Nielsen, A Villumsen, A Réfega, J Vieira e Silva


Moisture correction for ultrasonic MOE measurements above fibre saturation point in Scots pine sapwood
2006 - IRG/WP 06-20333
There is a high correlation between methods for dynamic modulus of elasticity (MOEdyn) and static modulus of elasticity (MOEstat). MOEdyn methods have been found sensitive to detect early stages of decay and may be seen as an option for non-destructive wood durability testing. As the MOEstat measurements do not change after reaching the fibre saturation point, the uncorrected MOEdyn data from ultr...
E Larnøy, G Alfredsen, H Militz


Investigation of new wood preservation formulations based on synergies between antioxidant, 2-HPNO and Propiconazole
2006 - IRG/WP 06-30401
Wood degradation by fungi is a complex phenomenon taking place in part through oxidative reactions involving many oxidizing agents like free radicals and hydroperoxide. In order to develop novel and more environmentally benign preservative systems, mixtures of Propiconazole and antioxidants with different stabilization mechanisms were investigated to detect possible synergies allowing to reduce th...
B Bakhsous, S Dumarçay, E Gelhaye, P Gérardin


Addition of boron compounds and octanoic acid for improvement of biocidal properties and copper fixation at copper-ethanolamine based wood preservatives
2006 - IRG/WP 06-30408
Copper-ethanolamine based wood preservatives became important active substance (formulation) for wood protection, novelty. As copper itself can not ensure sufficient protection against wood destroying organisms and fixation in wood we combine it with other biocides like ethanolamine, boron and octanoic acid. This investigates were performance on spruce wood impregnated with different combination o...
F Pohleven, M Humar


Criteria for environmentally and socially sound and sustainable wood preservation industry
2006 - IRG/WP 06-50237
This paper is dealing with critical criteria for environmentally and socially sound and sustainable wood preservation industry. A research study supported by past experience, knowledge and training on relevant topics and consultation of relevant appraisal manual, training module and technical guideline revealed concise widespread checklists for sustainable establishment of wood preservation indust...
A K Lahiry, M Hasan, M A J H Chowdhury


Nanotechnology: Implications for the Wood Preservation Industry
2007 - IRG/WP 07-30415
Nanotechnology has the potential to greatly impact the wood protection industry through the creation of nanomaterials with unique properties. Nanobiocides may find applications as co-biocides, or may alter treatability properties such as penetration and biocide distribution. Nanocarrier delivery systems may increase the applications for organic biocides through controlled release of biocide, treat...
C A Clausen


Marine Borer Resistance of Modified Wood - Results from Seven Years in Field
2007 - IRG/WP 07-40375
Wood modified by several methods has been tested for seven years in a marine field with high marine borer activity. Several wood modification methods were included, e.g. thermal modification (with different processes), acetylation, maleoylation, succinylation, furfurylation, treatment with methylated melamine resin and modification with reactive linseed oil derivative. Furthermore, some combinatio...
M Westin, A O Rapp, T Nilsson


Effects of caffeine on growth of wood-decaying fungi
2007 - IRG/WP 07-30427
The wide-used triazoles alter the biosynthesis of ergosterol leading to a disruption of fungal membrane functions. The aim of this study was to investigate the effects of another cell wall perturbing agent, caffeine, in combination with propiconazole on the growth of wood-decaying fungi. 10 mM caffeine inhibits totally the growth of five fungal species. The obtained results showed that caffeine ha...
S Lekounougou, J P Ondo, J P Jacquot, G Nevers, P Gérardin, E Gelhaye


Synthesis of boric acid ammonium oleate salt for wood preservation: Leachability and termite resistance test
2007 - IRG/WP 07-30435
A new chemical compound coupling boric acid and oleic acid through a joint of ammonium salt has been produced and its synthesis followed and validated by Fourier Transformed Infra Red (FTIR). This compound named ammonium borate oleate (BAO) combining biocidal properties of boron and water repellence of fatty acids has then been studied as a wood preservative. Synthesis of BAO involved different...
F Lyon, A Pizzi, Y Imamura, M F Thevenon, S N Kartal, J Gril


Comparative study between full cell and passive impregnation method of wood preservation for laser incised Douglas-fir lumber
2007 - IRG/WP 07-40359
Many wood species are highly resistant to conventional pressure treatment. To improve the chemical impregnation into Douglas-fir (Pseudotsuga menziesii Franco) lumber, the passive impregnation method had been developed. In this study, ability of the passive impregnation for lumber was compared with a conventional full cell method. Square Douglas-fir lumber with the incising density of 10,000 holes...
Md N Islam, K Ando, H Yamauchi, Y Kobayashi, N Hattori


Evaluatiang the potency of cinnamaldehyde as a natural wood preservatives
2007 - IRG/WP 07-30444
Since cinnamaldehyde, the major constituent of leaf essential oil from Cinnamomum osmophloeum, has significant antifungal and antitermitic activities, it is worthy of understanding whether cinnamaldehyde has potential to be used as a natural preservative for improving the durability of wood. In this study, the fungi and termite resistance of cinnamaldehyde-treated wood (CTW) were evaluated accordi...
Chun-Ya Lin, Chi-Lin Wu, Shang-Tzen Chang


Development of boron/linseed oil combined treatment as a low-toxic wood protection. Evaluation of boron fixation and resistance to termites according to Japanese and European standards
2007 - IRG/WP 07-30448
Combinations of boric acid as a first step of treatment and linseed oil as a second step have been performed in order to enhance boron retention to leaching and wood resistance to termites. Classic leaching and termites resistance standards are inappropriate to evaluate this combination which can be considered as both a wood core preservation treatment and a coating. Japanese Industrial Standard...
F Lyon, M-F Thevenon, Y Imamura, J Gril, A Pizzi


Wood boring species present in the Tagus Estuary and the severity of their attack on wooden piles exposed in the area: a case study
2008 - IRG/WP 08-10664
Wood exposed in the marine environment is subject to degradation by wood boring organisms. This is probably one of the reasons why wood has been substituted by concrete and steel in maritime structures in many European coastal areas. Wooden piles obtained from a wharf exposed in the Tagus Estuary, Porto Brandão (Almada, Portugal) provided an opportunity to understand the main agents of biodeter...
L M S Borges, L Nunes, A A Valente, P Palma


Antifungal activity of different molecular weights of a biopolymer chitosan against wood decay fungi
2008 - IRG/WP 08-30456
In recent years chitosan has been investigated as a natural polymer for wood preservation against fungal decay. From an environmental point of view, chitosan seems to possess a potential approaches as wood protecting agent. In this study, three different molecular weights of chitosan compounds (with approximately the same degree of deacetylation 83 ± 2 %) were evaluated as in vitro and in vivo as...
A S O Mohareb, M E I Badawy


Influence of Polyvinyl acetate emulsion (PVA) on boron leaching and fungicidal properties
2008 - IRG/WP 08-30451
Boron compounds are very effective fungicides, but unfortunately they leach from wood. In order to improve boron fixation, boric acid, borax were combined with polyvinyl acetate emulsion (PVA). For comparison copper salts were included into this research as well. Selected preservative solutions were chosen for impregnation of Norway spruce wood specimens (Picea abies). Wood blocks were exposed to ...
M Humar, B Lesar, P Kralj


Wood preservation by a mixed anhydride treatment: Using simple models of polymeric wood compounds
2008 - IRG/WP 08-30457
Treatment of wood by a mixed aceto/oleic (or other fatty acid residue) anhydride promoted as a safe and environment friendly wood preservation system has been examined quantitatively by liquid phase 13C NMR and solid phase MAS-DEC (proton decoupling) 13C NMR through all its different stages to determine which reactions occur with simple model compounds of the polymeric constituents of wood. The p...
F Lyon, M-F Thevenon, A Pizzi, G Tondi, A Despres, J Gril, S Rigolet


Primary Study on Compressed Preservative-treated Wood (CPW) for Outdoor Applications
2008 - IRG/WP 08-40412
In this study, the compressed wood samples pre-treated with hot water bath or water spraying were immersed in the ammoniacal copper quat –type D (ACQ-D) preservative solution to get compressed preservative-treated wood (CPW). The liquid absorption and the recovery rate of compression deformation of the compressed wood was determined, as well as the surface hardness, the distribution of density a...
Jinzhen Cao, Jia Mao


Investigation into the antifungal properties of herbal remedies for potential use in the wood preservation industry
2008 - IRG/WP 08-30462
The efficacy of herbal remedies as potential antifungal agents was evaluated against two sapstain and three decay fungi. Sapstain fungi included Sphaeropsis sapinea, and Leptographium procerum, and decay fungi were Oligoporus placenta, Coniophora puteana, and Schizophyllum commune. Out of six herbal remedies tested, three showed moderate to high antifungal activity. Caprylic acid had high antif...
D O’Callahan


Effects of Moisture Content and Species on Penetration of Liquid in Laser Incised Lumber by the Passive Impregnation Method
2008 - IRG/WP 08-40408
Penetration of liquid by passive impregnation method for Douglas-fir (Pseudotsuga menziesii Franco), sugi (Cryptomeria japonica D. Don) and Japanese larch (Larix leptolepis Gordon) were studied. Effects of initial moisture content of sugi (16, 43 and 70% moisture content) on liquid penetration by the method were also studied. Dried Douglas-fir and sugi, and green Japanese larch and sugi were treat...
N Hattori, M Nazrul Islam, K Ando, H Yamauchi


Comparison of permeability at different levels of moisture content in Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) impregnated under vacuum/pressure through full-cell method by using CCA and CCB of different concentrations
2007 - IRG/WP 07-40366
In this study, a comparison has been made in terms of the combined, longitudinal, tangential, and radial permeability of the species of Bornmullerian fir (Abies bornmulleriana Mattf.) and Eastern spruce (Picea orientalis L.) with moisture contents of 50 % and 15 %, which were impregnated under vacuum/pressure through full-cell method by using water-borne wood preservatives (impregnation materials)...
I Usta


Preservación de madera en Uruguay
2008 - IRG/WP 08-30492
Uruguay has a temperate climate and predominantly gently undulating landscape which is naturally suitable for farming activities. Therefore, its economy has always been based upon them and the related industries. In the sixties, the government decided it was necessary to increase forested areas in the country. Based on different consultancies, the legal frame was built in order to promote a sustai...
S Böthig


The Present Situation and Future Development in Quality Assurance for Wood Protection in China
2009 - IRG/WP 09-20418
This paper provides a comprehensive review of the quality assurance program for wood protection industry in China in term of guiding policies, standardization and implementation activities. The potential deficiencies with the existing practices regarding to the quality of wood protection products and suggestions for the further research and development directions to improve the system are also dis...
Kang Hua Cheng


A theoretical-industrial correlation and perspective on copper-based wood preservatives - a review of thermodynamic and kinetic aspects on copper-wood fixation mechanism
2009 - IRG/WP 09-30499
Copper was and it will continue to remain one of the key active component in wood protection industry. Over the past decades, a significant effort from R&D teams in industry, academia and research institutes was directed toward understanding the copper-wood fixation mechanism, optimising the copper retentions in the wood and reduce leaching in order to maximized performance, prolong the lifetime o...
R Craciun, M Maier, J Habicht


Effects of new fixative additives on leachability of boron wood preservatives
2009 - IRG/WP 09-30507
Borates are well known with their protective capacity against both fungi and insects with low mammalian toxicity and environmental acceptable. However, boron itself does not ensure the appropriate protection for wood in the exterior applications because of their easily depletion from the treated wood under wet conditions. In this study, the potential use of monoglyceride and polyvinyl alcohol prod...
A Mohareb, J Henry, E Wozniak, P Gérardin


Previous Page | Next Page