IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 235 documents. Displaying 25 entries per page.


Theoretic discussion on the way and driving forces of moisture migration in wood during vacuum drying
2011 - IRG/WP 10-40538
Most of parameters in conventional drying cannot explain a lot of phenomena appeared in vacuum condition, so it is necessary to further explore the moisture migration way and driving forces in wood under vacuum condition. For the water movement channel in wood is very narrow, the characteristic of heat and mass transfer in wood is similar to that in microscale. This article applies theory of liqui...
Zhengbin He, Xueli Yao, Liqiong Chen, Songlin Yi


The study of fungicidal values und sorption processes of ionic liquids- potential wood preservatives on soils
2011 - IRG/WP 11-30572
In the paper, the fungicidal activity of new ionic liquids structures, N,N-dimethylalkylamines derivatives, containing a spacer built of 7 or 10 methylene groups with nitrate(V) and tetrafluoroborate anions, didecyldimethylammonium and benzalkonium nitrate(V) were presented. The research was also conducted on the sorption of cations of ammonium ionic liquids on five types of podzolic, humic alluvi...
W Przybylska, J Zabielska-Matejuk, A Stangierska, A Skrzypczak


Use of Variable Pressure Scanning Electron Microscopy for in situ Observation of Degradation of Wood Surfaces during Artificial Weathering
2012 - IRG/WP 12-20489
Variable pressure scanning electron microscopy (VPSEM) is capable of observing electrically non-conductive materials like wood without the need to render the surface conductive by applying a coating of gold, platinum or carbon. Hence, there is the possibility that VPSEM could be used to non-destructively follow the structural changes occurring at wood surfaces during weathering, because specimens ...
F Hatae, Y Kataoka, M Kiguchi, H Matsunaga, J Matsumura


Smart hydrogels from low molecular weight amphiphilic compounds: toward a solution to decrease leachability and increase efficacy of boron preservatives?
2012 - IRG/WP 12-30589
A new catanionic system associating amphiphilic carnosine (AlaHisC8) and lauric acid forms supramolecular hydrogel at very low concentration. This gel was investigated and we have checked the validity of the concept of hydrogels utilization to reduce boron leachability and to develop new wood protection treatments. Impregnation with 5% aqueous borax solution (w/w) and 0.3% gelator agent (...
F Obounou Akong, P Gérardin, C Gérardin-Charbonnier


Hydrogels: a solution to reduce boron leachability without reduction of its biodisponibility to wood decaying fungi?
2012 - IRG/WP 12-30602
Products used today for wood protection must fulfill to more and more environmental constraints, such as being of low toxicity in answer to the Biocidal Product Directory, but also to involve waterborne treatments to limit rejection of volatile organic compounds in the atmosphere. Boron preservatives have been described as valuable alternatives for wood protection for non-ground contact applicatio...
F Obounou Akong, P Gérardin, M-F Thévenon, S Parant, C Gérardin-Charbonnier


Effect of preservative treatment on mechanical performance of round and square poles made of small diameter Scots pine
2012 - IRG/WP 12-40612
A growing proportion of harvested Scots pine (Pinus sylvestris L.) timber originates from the first or second commercial thinning stands. There is a need to find economically viable and high quality wood products that can be manufactured from this raw material. Small log volume means not only demands of increased efficiency for material handling in logistics and manufacturing processes, but also c...
V Möttönen, R Stöd, K Heikkilä, H Heräjärvi


Water absorption and desorption of non treated, pressure impregnated, and pine oil treated glulam made of small diameter Scots pine and Norway spruce
2012 - IRG/WP 12-40616
A growing proportion of harvested timber originates from the first or second commercial thinning stands in Finland, which means smaller average log volumes in comparison to final felling stands. Smaller log volume means challenging wood properties such as higher proportion of juvenile wood and sapwood. Due to these facts, products made of small diameter logs are prone to twist and check, and have ...
H Heräjärvi, V Möttönen, R Stöd


Activities of moulds on wood as a function of relative humidity during desorption and absorption processes
2013 - IRG/WP 13-10794
Three different types of indoor moulds: Penicillium brevicompactum, primary colonizer; Alternaria tenuissima, secondary colonizer and Trichoderma harzianum, tertiary colonizer, grown on wood were measured for their activities under different relative humidity levels. The activities were measured by isothermal calorimetry. The activities of the moulds changed with the change of the relative humidit...
Yujing Li, L Wadsö


State of progress of utilisation of supramolecular gels for formulations of water-soluble wood preservation salts
2013 - IRG/WP 13-30630
This article is a compilation of the work done so far concerning the utilization of supramolecular hydrogels, built on low-molecular-weight amphiphilic molecules and containing boron salts conferring fungicidal properties. Mixing boron with thermoreversible hydrogels allows the formation of a supra molecular network incorporating boron and important amount of water upon gelification of the solutio...
F Obounou Akong, P Gérardin, M-F Thévenon, C Gérardin-Charbonnier


Natural durability of plantation-grown coast redwood (Sequoia sempervirens) in New Zealand
2014 - IRG/WP 14-10817
There is wide variation in the wood properties of plantation-grown coast redwood in New Zealand. Contributing factors are the seed source, silviculture, growth and age of the trees in the plantation forests. Little is known about how these factors affect the variation of wood properties among and within the trees of New Zealand’s coast redwood forests. Heartwood of plantation-grown coast redwood...
D O’Callahan, T Jones, C Low, C Chittenden


Bamboo: A poor man’s timber
2015 - IRG/WP 15-10852
Bamboo, known as poor man’s timber in the past gained some importance in the last decade when TIFAC under Department of Science & Technology and Ministry of Agriculture awoke to find a better future for this unique gift of nature. Until then it was considered a good for nothing grass suitable only for making paper and building effigies of Ravan, Kumbhkaran and Meghnath year after year at Dussehr...
S Kumar


The effect of preservative treatment on mechanical strength and structural integrity of wood
2015 - IRG/WP 15-30667
The use of wood for demanding construction applications is increasing in Europe. Wooden constructions are frequently designed of susceptible conifer wood, which is endangered by wood decay fungi in wet applications. Therefore in many cases treating wood with preservatives is unavoidable to ensure the desired service life. However, chemical treatment of wood can result in changes of its mechanical ...
M Humar, D Kržišnik, C Brischke


Measurement of Cell Wall Moisture in Acetylated Radiata Pine Using Low-Field Nuclear Magnetic Resonance
2016 - IRG/WP 16-20583
Understanding the interaction of water with acetylated wood is necessary to explain how the protective mechanism of acetylation functions. Low-field nuclear magnetic resonance is one technique for assessing water in wood. Pinus radiata earlywood sapwood samples were acetylated to various weight percentage gains and then analysed with this method. Increased levels of acetylation showed significantl...
H G Beck, C A S Hill


Release of Copper from Pressure Treated Wood
2016 - IRG/WP 16-20584
Micronized copper based wood preservatives including micronized copper quat (MCQ) and micronized copper azole (MCA) have been introduced commercially to the North American market since 2006 as alternatives to alkaline copper quat (ACQ) or soluble copper azole (CA) preservatives. Unlike ACQ or CA, MCQ and MCA use dispersed particulate copper particles rather than soluble ionic copper to make treat...
Jun Zhang, J Horton


Resistance of heat treated Ash wood under steam pressure: rot fungi, soil micro-organisms and termites
2016 - IRG/WP 16-40724
Thermal modification processes have been developed to increase the biological durability and dimensional stability of wood. The aim of this paper was to study the influence of ThermoWood® treatment intensity on wood decay resistance improvement against soil-inhabiting micro-organisms, brown/white rots and termite’s exposures. All of the tests were carried out in the laboratory with two differen...
K Candelier, S Hannouz, M-F Thévenon, D Guibal, P Gérardin, M Pétrissans, R Collet


Impregnation of railway sleepers - Pressure gradient and transversal penetration
2016 - IRG/WP 16-40731
Based on the possible ban of creosote in the future, the need for oil based alternative products has gained in importance. Due to possible differences in impregnation properties compared to creosote the need for re-implementing former technology is given, to determine if momentarily used impregnation processes have to be modified. The here reported tests measure the pressure gradient during the im...
M Starck, A Gellerich, H Militz


Influence of pressure phase impregnation time on the uptake and distribution of wood preservatives in Scots pine material of diverse treatability
2016 - IRG/WP 16-40752
In spite of the general opinion that Scots pine sapwood is easy to impregnate considerable variations in treatability are reported. In order to study impregnation results of diverse Scots pine sapwood treated with increasing process times, Scots pine sapwood from two different predefined treatability groups was impregnated. A copper solution was used as impregnation agent in ten different vacuum p...
K Zimmer, B Kerfriden


Treatability of beechwood railway sleepers with potential creosote substitutes
2017 - IRG/WP 17-40790
Maintenance of an efficient railway infrastructure still requires the use of wooden railway sleepers, particularly because wooden sleepers have more favourable properties for intensified vibrations than concrete or steel sleepers. Creosote, used for decades for the impregnation of railway sleepers, will possibly no longer be available for this application due to European legislation. This reveals ...
N Pfabigan, E Habla, R Gründlinger


Recent findings clarifying the mechanism of brown-rot decay protection in acetylated wood
2018 - IRG/WP 18-40827
This paper summarizes the findings obtained during my PhD research over the past three years. The results provide insights which help to understand the enhanced brown-rot decay resistance of acetylated wood with particular emphasis on the role of water. The protection acetylation provides is derived from moisture exclusion within the acetylated cell wall, but the exact mechanism by which water is ...
G Beck


In-line quality control of the film thickness in industrial coating processes for exterior cladding
2018 - IRG/WP 18-40835
The production of industrially coated wood cladding has been strongly increasing in Scandinavia during the last years. In the beginning of this development, industrial coating processes included solely the application of pigmented primers; these however provide only a short protection of the wood surface and the application of a top coat is required during the first 6 to 12 months after mounting t...
U Hundhausen, M Slabohm


Promoting Commercially Available Epoxy Resins for Non-biocidal Wood Preservation
2019 - IRG/WP 19-40877
Commercially available epoxy and polyamine resins were evaluated with the aim of developing new non-biocidal wood preservation treatments. A simple method allowing the impregnation of wood by vacuum double impregnation followed by a curing process was developed for two reference species, beech Fagus sylvatica and Scots pine Pinus sylvestris. The tested products were evaluated for their ability to ...
P Poveda, M Mubarok, S Dumarcay, M Montibus, I Le Bayon, M Kutnik, P Gerardin, F Simon


Water interactions in wood polyesterified with sorbitol and citric acid
2020 - IRG/WP 20-40888
Polyesterifcation of wood with sorbitol and citric acid seems to be a promising chemical wood modification technique that is both low-cost and produced from bio-based chemicals. An interesting aspect of the modification is the interaction of water with the polyesterified wood since the relationship with moisture appears to be unique compared to other wood modification systems. This communication p...
G Beck, A Treu, E Larnøy


Studying amount, location and state of water in modified wood at moisture levels relevant for fungal degradation
2020 - IRG/WP 20-40889
Water is an essential parameter for fungal degradation of wood, but degradation primarily occurs at high moisture levels at water potential in the range of -4 to -0.1 MPa, which corresponds to 97-99.9% relative humidity. At these moisture levels, water is present in the wood structure both in and outside of cell walls. The majority of previous studies on the interaction between wood and water for ...
M Fredriksson, E Engelund Thybring, Ramunas Digaitis


Enhancing the durability of low durability Eucalyptus plantation species: a review of strategies
2020 - IRG/WP 20-40910
Eucalyptus species native to Australia have shown excellent growth rates, good physical properties and resistance to diseases. As a result, they are widely planted globally for a variety of uses. One negative aspect of many of these faster growing species is that they have a high percentage of low durability heartwood that resists preservative treatment. In Australia, large plantations of these sp...
K C Wood, J J Morrell, W Leggate


Preliminary investigation for preservation method of CLT using non-pressure treatment
2021 - IRG/WP 21-40919
Cross-laminated Timber (CLT) is increasingly being used in residential and non-residential construction around the world, and some of these areas are at high risk of biodeterioration. Addition to moisture management of construction, preservative treatment of CLT may be needed to prevent decay and termite attack in the area. Pressure treatment being most reliable, is not feasible due to the large d...
T Miyauchi, Y Ohashi, J Miyazaki, R Takanashi, H Shibui, S Isaji, T Shigeyama, Y Sugai, A Yamamoto, T Hramiishi, T Mori, H Matsunaga


Previous Page | Next Page