Influence of acidification on decay processes of CCB treated wood
2004 - IRG/WP 04-10514
The phenomenon of copper tolerance by brown rot fungal strains has been known for a long period but the complete mechanism of copper tolerance by these fungi is not understood yet. Copper tolerance has previously been linked to oxalic acid excreted by copper tolerant brown rot fungal strains. This acid reacts with copper in the wood to form an insoluble and therefore less toxic copper oxalate. The...
M Humar, S A Amartey, M Šentjurc, F Pohleven


Soil treatment tests with the three products of boric acid for the prevention of the hyphal growth of Serpula lacrymans
1992 - IRG/WP 92-3693
Laboratory soil treatment tests were conducted for the evaluation of fungicidal or fungistatic effect of boric acid products against Serpula lacrymans. Boric acid products tested were the following three: a thickened boric acid solution in triethanolamine, boric acid-silica gel complex granules, and a nonwoven fabric laminated with a polypropylene film and coated with boric acid granules on one si...
S Doi, A Yamada, Y Mineki, M Mori


Attempts to isolate tunnelling bacteria through physical separation from other bacteria by the use of cellophane
1992 - IRG/WP 92-1535
During attempts to isolate tunnelling bacteria in pure culture, physical separation from other bacteria was successfully achieved by the use of cellophane. Cellophane was used in liquid cultures as a substrate for tunnelling bacteria that were present in a mixture with other bacteria. By tunnelling into cellophane, TB were physically removed from contaminating bacteria which could then be removed ...
T Nilsson, G F Daniel


Visualising Bacteria in Wood Using Confocal Laser Scanning Microscopy (CLSM)
1998 - IRG/WP 98-10272
A fluorescent phospholipid probe was used in conjunction with confocal laser scanning microscopy (CLSM), to visualise bacteria which inhabit in radiata pine wood and degrade pit membranes. CLSM has the ability to collect fluorescent images through different emission filters at the same time, so it is possible to distinguish gram-positive and gram-negative bacteria in infected wood by counterstaini...
Ying Xiao, A P Singh, R N Wakeling


Old and new facts on the dry rot fungus Serpula lacrymans
1991 - IRG/WP 1470
The article collates some of the recent literature on the biology of the dry rot fungus Serpula lacrymans. The fungus can grow at 28°C, and maximum wood moisture is above 55%. Serpula Iacrymans degrades crystalline cellulose. The intensive production of extracellular oxalic acid is neutralized by calcium and iron. There is considerable variation among the strains with regard to factors such as gr...
O Schmidt, U Moreth-Kebernik


Detoxification of methylene bisthiocyanate by bacteria isolated from freshly felled, anti-sapstain treated timber
1993 - IRG/WP 93-10017
The microbial defacement of freshly-felled timber treated with organic biocides continues to be a major problem in stored lumber. As part of a study to investigate the depletion in chemical activity of methylene-bis-thiocyanate (MBT) in green timber, bacteria were isolated from freshly-felled boards of Corsican pine (Pinus nigra var. maritima Arnold) previously treated with different biocides. The...
R J Wallace, R A Eaton, G R Williams


Detection of methanogenic bacteria in mining timber
1988 - IRG/WP 1352
Methane explosions in gold mines have been attributed to spontaneous ignition of methane/air mixtures. Biogenesis of methane in the heartwood of diseased trees has been shown, but never in timber in service. Studies were therefore undertaken to establish whether methanogens were present in wooden pit props. Core samples were removed by Pressler increment borer from props in disused areas 2,600 m d...
L D Abraham, K Westlake, R I Mackie, J F Putterill, A A W Baecker.


Tunnelling bacteria
1983 - IRG/WP 1186
The micromorphology of decay in wood caused by a certain group of single-cell bacteria, called tunnelling bacteria (TB), is described. TB are characterised by their tunnelling ability within the secondary cell walls of wood fibres. Pure cultures of TB have not yet been obtained although the typical decay patterns can be reproduced using mixed bacterial cultures. Some indications of lignin degradin...
T Nilsson, G F Daniel


Microbial decay in an extremely durable Malaysian hardwood Belian (Eusideroxylon zwageri) - an overview
1997 - IRG/WP 97-10216
The heartwood of Belian (Eusideroxylon zwageri) is highly regarded among the naturally durable Malaysian hardwoods, and is therefore a choice timber for soilcontact use in the humid tropics such as untreated telecommunication poles, fence posts and railway sleepers. The high microbial resistance of the wood is evidenced by the mere superficial degradation observed in some pole samples after 20 yea...
A H H Wong, A P Singh


Reduction of preservatives leaching from wood by the application of animal proteins
2005 - IRG/WP 05-30387
The investigations consisted in the estimation of the effectiveness of protein borates and protein propionates in wood preservation against Coniophora puteana. The estimation was made on the basis of mass losses caused by the test fungus action against treated wood which was subjected to leaching with water. The investigations were performed for Scots pine wood (Pinus sylvestris L.) treated with p...
B Mazela, I Ratajczak, M Bartkowiak


Ponding of radiata pine (Pinus radiata) - 2. The effect of ponding on coating penetration into wood
1998 - IRG/WP 98-10249
Radiata pine (Pinus radiata) wood panels which had been ponded for periods ranging from 2 to 12 weeks, dried and subsequently coated with a primer and examined by light microscopy after staining sections with Sudan IV to enhance the contrast of the primer material. A correlation between the extent of ponding and the extent of coating penetration into wood was observed. The coating penetration var...
A P Singh, S S Gallagher, U Schmitt, B S Dawson, Yoon Soo Kim


Bacterial degradation of Pinus radiata compression wood
1996 - IRG/WP 96-10153
An inspection of twelve year old, CCA-treated Pinus radiata wood from an industrial cooling tower showed extensive surface decay of wood. Electron microscopic examination of decaying compression wood indicated that compression wood cells were attacked exclusively by bacteria, which were of erosion and tunnelling types. As compared to the normal wood, compression wood appeared to be more resistance...
A P Singh, R N Wakeling


Properties of cellulose degraded by the brown rot fungus, Postia placenta
1988 - IRG/WP 1350
To gain further understanding of the nature of the cellulose depolymerizing agent or agents of brown-rot fungi, brown-rotted cellulose was chemically and physically characterized. Various culture conditions, such as low nitrogen and elevated oxygen levels, did not induce degradation of cellulose by Postia placenta in liquid cultures. Therefore, brown-rotted cellulose for analysis was prepared by a...
T L Highley, R E Ibach, T K Kirk


Remedial treatment of creosoted railway sleepers of redwood by selective application of boric acid
1980 - IRG/WP 3134
An ideal preservative for remedial treatment must primarily be characterized by two requirements. First, it must have an ability to diffuse and distribut evenly into the wood and secondly, it must be fixed properly so that it does not leach out too fast. However, these two characteristics conflict with each other, and the choice of preservative must of necessity be a compromise. Wood preservatives...
C Bechgaard, L Borup, B Henningsson, J Jermer


Preservative treatment of rubber wood (Hevea brasiliensis) to increase its service life
2005 - IRG/WP 05-40320
Rubber wood (Hevea brasiliensis) possess excellent properties for interior designing, wood working and furniture making. But it is very much susceptible to sap stain and mould fungi which decreases the service life. For profitable uses , it is necessary to increase the service life of rubber wood. To protect the rubber wood from wood degrading agents, the sawn timber were treated with Borax – b...
K Akhter


Influence of surface coating on the leachability of boric acid and bifluorides from spruce wood
1995 - IRG/WP 95-50050
In the Netherlands, window joinery made from non-durable timber species (spruce) are widely protected with preservative rods. These rods contain non-fixing wood preservatives (e.g. bifluorides or boric acid). This reseach was performed to show the possible influence of a coating system to hinder the leaching of the active ingredients. The results of the leaching tests show, that bifluorides and ev...
W J Homan, H Militz


Experiments on the degradation of tributyltin oxide: A progress report
1984 - IRG/WP 3287
A variety of experiments designed to assess the chemical and physical factors affecting the degradation of tributyltin oxide in treated timber are described. Simple procedures in which temperature and oxygen availability were increased in the presence of wood and water suggest that the wood itself was of prime importance. Attempts to decrease degradation with antioxidants were unsuccessful but led...
R J Orsler, G E Holland


Effect of thickened boron in preventing conidial germination of sapwood-inhabiting fungi
1994 - IRG/WP 94-30059
We evaluated the efficacy of thickened boron preservative "Diffusolä" in preventing conidia germination of sapwood-inhabiting fungi using plate bioassay, Southern Yellow Pine and sweetgum block tests, and green pine log sections. The test fungi were sapstain fungi Ceratocystis coerulescens, Ceratocystis minor, and Aureobasidum pullulans and mold fungi, Aspergillus niger, Penicillium spp, and Tric...
S C Croan


Practical experiments with Boracol 10 Rh used as a fungicide in the repair process after attack by the dry rot fungus (Serpula lacrymans)
1987 - IRG/WP 3458
The test is carried out in an old house in Nyhavn, Copenhagen. The roof and the walls close to were heavily attacked by dry rot fungus (Serpula lacrymans) because damage to the zinc covering the frontspice were letting in water to the wood and wall construction. An attack by the dry rot fungus is more complicated to repair compared with other wood destroying fungi because beside the damage on wood...
J Bech-Andersen


The effect of of sorbitol on the decay of boric acid treated Scots pine
1991 - IRG/WP 1509
The tetra-hydroxy borate ion is known to undergo complexation with polyols of biological importance and probably protects treated timber by this action. The inhibitory effect of boric acid upon fungal growth and dehydrogenases has been shown to be prevented by the addition of certain polyols. This work was extended, with a study of the effects of a polyol on the performance of boric acid in treate...
J D Lloyd, D J Dickinson, R J Murphy


A possible role of unique TCA cycles in wood-rotting basidiomycetes
2003 - IRG/WP 03-10461
The copper tolerant brown-rot fungus, Fomitopsis palustris, acquires metabolic energy by use of the constitutively-occurring Kornberg’s glyoxylate cycle coordinating with oxalate biosynthesis and glucose oxidation (Erman Munir et al. Proc. Natl. Acad. Sci. USA, (2001) 98, 11126-11130). Furthermore, this fungus does not have the normal TCA cycle, lacking 2-oxoglutarate dehydrogenase which is a ke...
E Munir, T Hattori, M Shimada


The use of selective media for studying the colonization of wood in ground contact by microorganisms
1978 - IRG/WP 186
In October1976 a field trial was set up in order to monitor the progressive colonisation of wood in ground contact using orientated small stakes of Scots pine (Pinus sylvestris) and birch (Betula sp.) (30 x 45 x 250 mm³). Half the number of each species were treated with a 1% solution of CCA by a vacuum impregnation process. All the stakes were coated on three sides with an epoxy-resin sealant to...
C P Clubbe


Ultrastructure of Prumnopitys ferruginea wood from a buried forest in New Zealand
1991 - IRG/WP 1489
The buried wood of Prumnopitys ferruginea, a New Zealand native tree, was examined by scanning and transmission electron microscopy to investigate the extent to which the wood had deteriorated and the cause of its deterioration. Examinations showed that some deterioration of wood had occurred. Microscopy revealed a decay pattern similar to that produced by cavitation bacteria. Lenticular cavities ...
A P Singh, T Nilsson, G F Daniel


Biological resistance of steam-compressed wood pretreated with boric compounds
1999 - IRG/WP 99-30190
Wood compression under heating is aimed to enhance dimensional stability and surface hardness. Preservative treatment with an appropriate chemical is additionally required for the protection of wood against biological agents under hazardous service conditions. Boron pretreatment of compressed wood was targeted to a mutual benefit of increasing biological resistance of compressed wood as boron was ...
M K Yalinkilic, W Dwianto, Y Imamura, K Tsunoda, M Takahashi


16S rRNA Analysis of the Bacteria Associated with Biocide Degradation
2004 - IRG/WP 04-10543
The bacterially mediated degradation of the new anti-fungal biocide, bethoxazin, was studied in vitro, by means of 16S rRNA PCR-amplification and cloning techniques. Woodblocks impregnated with a subtoxic concentration of bethoxazin were incubated in compost, and the micro-organisms associated with the wood after 6 and 12 weeks was studied. It was found that after 6 weeks the wood contained a la...
D F Wallace, D J Dickinson


Previous Page | Next Page