IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 251 documents. Displaying 25 entries per page.


Über Hausbock Hylotrupes bajulus (L.), (Col., Cerambycidae), in Laubholz: Versuche mit Laubholzarten, Prüfung der Wirkung von Ligninstoffen und von Ginkgo biloba, Beobachtungen an Hesperophanes. [On House-longhorn Beetle Hylotrupes bajulus (L.), (Col., Cerambycidae) in hardwood: Investigations with several hardwood-species, tests on activity of lignin components and Ginkgo biloba, observations on Hesperophanes]
1982 - IRG/WP 1144
Hylotrupes bajulus-larvae feed and develop in softwoods, hardwood acts as a feeding poison. The reason for this is still little known. According to literature some observations contradict this established opinion and the question was raised, whether the colour-strain scutifer (= lividus) is able to live in hardwood. Testing ten European and tropical hardwood-species (following the DIN-EN test proc...
S Cymorek


Development of a model system to assess the efficacy and environmental impact of a chromated fluoride remedial treatment for creosoted distribution poles
1992 - IRG/WP 92-2395
A closed model system was designed to facilitate a controlled study of the leachability and environmental fate of a remedial preservative under laboratory conditions. The elements of the model include a precipitation apparatus above a treated pole section which is positioned in a representative soil profile supporting a sward of perennial ryegrass. The model will allow detailed examination of the ...
D C R Sinclair, G M Smith, A Bruce, B King


Durability of heat-treated wood
1999 - IRG/WP 99-40145
Heat-treated wood from the French process were laboratory tested against decay using agar block test and a modified soil block test. Water absorption, bending strength, lignin content and acid number were also determined to evaluate the effect of heat treatment. Heat treated samples exhibit a higher lignin content and a lower acid number compared to untreated control indicating the degradation of ...
D P Kamdem, A Pizzi, R Guyonnet, A Jermannaud


The effect of preservative distribution in small blocks of Pinus sylvestris on the toxicity of tributyltin oxide to Reticulitermes santonensis Feytaud
1971 - IRG/WP 206
Small blocks of Pinus sylvestris (50x25x15 mm³) were treated by a full-cell method with various concentrations of tributyltin oxide in benzene. Replicate blocks were then freeze dried, rapidly air dried or slowly air dried and exposed to surface attack by the subterranean moistwood termite Reticulitermes santonensis Feytaud. At all concentrations it was found that the freeze-dried blocks were mor...
M P Levi, D N R Smith


Untersuchungen über das Vorkommen und den Schaden der Rossameisen (Camponotus herculeanus und Camponotus ligniperda) in Gebäuden in Schweden
1976 - IRG/WP 147
Die wichtigsten Ergebnisse der vorliegenden Untersuchung der von Rossameisen befallenen Häuser in Schweden können wie folgt zusammengefasst werden. Rossameisenschaden kommt in ganz Schweden vor, jedoch hauptsächlich in Küstengebieten und in der Nähe von grossen Seen. Beide Rossameisenarten schaden in gleicher Weise. Camponotus herculeanus ist im ganzen Lande zu finden, Camponotus ligniperda d...
V Butovitsch


Fundamentals on steam fixation of chromated wood preservatives
1988 - IRG/WP 3483
Weathering of treated wood directly after impregnation leaches up to 2% of copper-chromate-containing wood preservatives. Almost total fixation of Cr+6 is achieved by steaming the treated wood at 100°C to 120°C, preferably 110°C. To initiate such spontaneous fixation 85°C to 90°C inside the wood are essential, which requires heating times ranging from 20 to 80 min, depending on timber species...
R-D Peek, H Willeitner


An appraisal of the vertical distribution of attack of untreated and treated wood by warm water sphaeromatids at some tropical sites - A discussion paper
1986 - IRG/WP 4124
Examples of the vertical distribution of burrows of warm water sphaeromatids relative to tide levels and mud line from sites in India, Papua New Guinea and tropical Australia are discussed in detail. These data show clearly that these animals concentrate their attack of resistant natural wood or resistant treated wood in the tidal zone, particularly around Mean Sea Level. Supportive evidence from ...
J E Barnacle, L J Cookson, C N McEvoy


Relationship between degradation of wood, cellulose or lignin-related compounds and production of hydroxyl radical or accumulation of oxalic acid in cultures of brown-rot fungi
1994 - IRG/WP 94-10062
The degradation activities of brown rot fungi against wood, cellulose, and lignin-related compounds were measured in cultures containing glucose or wood as a carbon source. Also the activities of one-electron oxidation and hydroxyl radical production and the amount of oxalic acid present in the cultures were measured. The degradation activities of the fungi against wood, crystalline cellulose and ...
S Itakura, T Hirano, H Tanaka, A Enoki


Cell wall microdistribution of chloropicrin and methylisothiocyanate in treated spruce
1989 - IRG/WP 3548
Chloropicrin and methylisothiocyanate (MIT) residues were observed using SEM/EDXA and TEM/EDXA in treated spruce wafers that had been exposed to the vapors of the two fumigant preservatives. Chlorinated residues from chloropicrin were found throughout the wood cell wall, even in acetone extracted material. The residues were most heavily concentrated in extractive materials in the rays, but unlike ...
G F Daniel, B Goodell


Old and new facts on the dry rot fungus Serpula lacrymans
1991 - IRG/WP 1470
The article collates some of the recent literature on the biology of the dry rot fungus Serpula lacrymans. The fungus can grow at 28°C, and maximum wood moisture is above 55%. Serpula Iacrymans degrades crystalline cellulose. The intensive production of extracellular oxalic acid is neutralized by calcium and iron. There is considerable variation among the strains with regard to factors such as gr...
O Schmidt, U Moreth-Kebernik


Introducing bamboos for their importance and conservation
2005 - IRG/WP 05-10546
Bamboo is a socio-economically, industrially and environmentally important forest and rural crop in Asia. It is an essential task for the people in this region to conserve the bamboos and preserve the bamboo products for their sustainable continuity. An earnest need for this task is to introduce a variety of important information on bamboos. In this research paper the botanical position, distribut...
A K Lahiry


Tunnelling bacteria
1983 - IRG/WP 1186
The micromorphology of decay in wood caused by a certain group of single-cell bacteria, called tunnelling bacteria (TB), is described. TB are characterised by their tunnelling ability within the secondary cell walls of wood fibres. Pure cultures of TB have not yet been obtained although the typical decay patterns can be reproduced using mixed bacterial cultures. Some indications of lignin degradin...
T Nilsson, G F Daniel


Occurrence of wood-boring pholads in Kochi harbour waters (south-west coast of India)
1992 - IRG/WP 92-4175
The paper reports the occurrence of four species of wood-boring pholads (Pholadidae: Martesiinae), namely Martesia (Martesia) striata (Linnaeus), Martesia (Martesia) fragilis Verrill and Bush. Martesia (Particoma) nairi Turner and Santhakumaran and Lignopholas fluminalis (Blanford), in the Kochi back-waters, south-west coast of India. Of these Martesia nairi and Lignopholas fluminalis are now reco...
L N Santhakumaran, M V Rao


Movement of water through quaternary ammonium treated wood
1987 - IRG/WP 3440
Radiata pine sapwood stakes were treated with didodecyl methyl 1, 3 dichloropropenyl ammonium chloride and distearyl dimethyl ammonium chloride. Various ratios of these two chemicals were, tested to determine the extent of water movement through the treated wood. Measurements were taken of the amount of water moved through the wood, degree of wetting of various sectors of the stakes, and the distr...
P J Hayward, J Duff


Accelerated diffusion treatment of sawn Sitka spruce grown in the UK
1986 - IRG/WP 3395
The treatment of 'green' sapwood and heartwood of Sitka spruce by diffusion methods was investigated. Steam/dip treatment processes gave increased solution uptakes and depths of penetration of copper in comparison with a simple dip treatment. Further investigation is required to reduce diffusion gradients with copper based formulations and to improve the penetration of '...
R J Murphy, D J Dickinson


The influence of drying and chemical stress on the lignin degradation in aspen by Phanerochaete chrysosporium
1992 - IRG/WP 92-1573
Wood wafers of Populus tremuloides sapwood were incubated on common media with the white rot fungus Phanaerochaete chrysosporium (wild isolate) and subjected to cyclic drying or chemical agents (low levels of borate or trifluoperazine [a calmodulin antagonist]). After a mass loss of approximately 5.5%, wafers were dried and analyzed for acid-insoluble lignin. Those wafers containing chemical agent...
E L Schmidt, Y-L Lin


Dimensional stabilization and decay resistance of wood treated with brown-rotted lignin and copper sulfate
1990 - IRG/WP 3608
The objective of this study was to evaluate the potential usefulness of brown-rotted lignin (BRL) as a dimensional stabilization and copper complexing agent for wood treatment. For dimensional stabilization, aqueous solutions of the lignin extract were combined with either copper sulfate, glyoxal or other additives. Anti-shrink efficiency (ASE) values as high as 42% were obtained with wood treated...
L Jin, D D Nicholas, T Schultz


Mechanistic aspects of the reactions of copper complexes with lignin in the presence of hydrogen peroxide and lipid hydroperoxide model compounds as proposed for white rot fungi
2001 - IRG/WP 01-10399
The structural principles and the oxidative reactions of the catalytic system consisting of copper, hydroperoxides, and copper coordination compounds that contain aromatic nitrogen atoms are similar to those of catalytic centers of oxidative enzymes involved in delignification reactions of white rot fungi. The system is capable of selectively degrading lignin and its low molecular weight would all...
K Fackler, P Lamaipis, E Srebotnik, M Humar, C Tavzes, F Pohleven, M Sentjurc, T Watanabe, K Messner


The nature of osmiophilic particles and their distribution during different stages of brown and white rot decay
1983 - IRG/WP 1213
The distribution of osmiophilic particles during the course of brown and white rot decay was investigated by applying transmission electron microscopic (TEM) methods. It was found that it correlates with the brown and white rot pattern.The osmiophilic particles are produced by the fungus and are supposed to be wood rotting enzymes....
K Messner, H Stachelberger


Influence of variable lignin content amongst hardwoods on soft-rot susceptibility and performance of CCA preservative
1982 - IRG/WP 1151
This paper presents the outline of an argument, based on both new and established data, which relates varying lignin content to variation of soft-rot susceptibility between hardwood species and of performance of CCA preservatives in controlling soft-rot. Although more data need to be generated to prove this relationship, sufficient evidence exists for the hypothesis to be given close attention, pa...
J A Butcher, T Nilsson


Distribution of fire retardant chemicals in kempas (Koompassia malaccensis)
1994 - IRG/WP 94-40037
Samples of Kempas (Koompassia malaccensis) heartwood were treated by vacuumpressure impregnation with solutions of monammonium phosphate, diammonium phosphate, ammonium sulphate or a borax-boric acid mixture. A commercial saltbased fire retardant formulation was also used. After slow air drying, the treated wood samples were sub-divided and zonal analysis carried out in order to determine the grad...
A R A Malek, R J Murphy


Utilization of coconut timber from north Sulawesi, Indonesia. Part 2: Treatability
1994 - IRG/WP 94-40025
Under tropical conditions coconut wood is quickly degraded by mold and blue stain fungi. Low density wood in ground contact is commonly decomposed by wood destroying fungi within a period of only a few months, higher density wood from the outer stem regions within 24 to 30 months (MOSTEIRO, CASIN, SERIBAN 1976; McQUIRE 1975). Moreover, according to McQUIRE (1975) green wood of lower density is hig...
R-D Peek


Weathering of copper-amine treated wood
2000 - IRG/WP 00-40155
Copper ethanolamine (Cu-EA) treated southern pine (SP) were artificially weathered with a QUV Weathering Tester. The weathering regime was composed of a continuous UV-light irradiation for 2 hours followed by a water spray for 18 minutes for a total time of 1200 hours. The changes on the surface of the weathered samples were characterized by Fourier transform infrared spectroscopy (FTIR) analysis,...
J Zhang, D P Kamdem


Dura-Treet II, a water dispersible pentachlorophenol
1980 - IRG/WP 3165
During the past several decades, penta petroleum wood treating has become increasingly popular. Penta is an effective chemical compound against wood organisms causing decay and rot, is safe to handle, also clean and easy to use. In terms of preservative cost, it has been and remains by far the least expensive of the three major preservatives. However, when the cost of petroleum carrier is added, t...
D B Hatcher


Diffusion and interaction of components of water-borne preservatives in the wood cell wall
1988 - IRG/WP 3474
This study investigates the rates of diffusion and ultimate distributions of copper and arsenate components of wood preservatives in wood cell walls following vacuum treatment. Adsorption studies of copper on red pine (Pinus resinosa) and trembling aspen (Populus tremuloides) wood confirm the importance of cation exchange reactions on the ultimate distribution of copper in the wood substance and i...
P A Cooper


Previous Page | Next Page