IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 347 documents. Displaying 25 entries per page.


Climatic impacts on the moisture performance of wooden decking and facades
2013 - IRG/WP 13-20518
In outdoor usage wood is exposed to a variety of influences, which reduce its durability against biological deterioration and wetting. Besides many other factors the service life of wooden facades and cladding is dominated by occurring moisture loads on the one hand and their capability to withstand moisture on the other hand. Hence, climatic factors have a direct impact on the material climate an...
T Bornemann, C Brischke, G Alfredsen


Moisture distribution in glulam beams with natural cracks observed with CT Scanning before and after rain
2013 - IRG/WP 13-20534
The way cracks in outdoor wooden constructions affect durability is an interesting topic, since a certain amount of cracks can always be found naturally in wood and glued laminated wood. The question in this was, can cracks lead water into the wood and thereby increase the risk for decay and reduce strength and service life. Moisture balance, i.e., water absorption and water distribution were stud...
K Sandberg


The Effect of Water Repellent on Semi-Field Leaching of Active Substances from Metal Free Wood Preservative Formulation
2013 - IRG/WP 13-30615
The risk assessments for the use of wood preservatives proposed by the OECD and used under the Biocidal Products Directive (BPD) (98/8/EC) require the derivation of leaching rates for active substances. These rates are to be used as input data in to agreed exposure scenarios. A comparison of the leaching of active substances from wood treated with a metal free preservative formulation with and wit...
D G Cantrell


Application of a model for the prediction of fungal degradation of thermally modified beech timber by Trametes versicolor
2013 - IRG/WP 13-40622
Colour measurement technology is found to be feasible for characterization of the property changes of thermally modified timber (TMT). In opposite to time-consuming and expensive laboratory tests a non-destructive test represents an improvement for the manufacturer of TMT. Therefore the aim of this study was to develop a method which allows sorting the different treatment intensities after the man...
Clauder, L., Richter S., Unger, W., Pfriem, A


Modelling the risk for mould growth on timber stored outdoors protected from rain
2013 - IRG/WP 13-20529
A mould resistance design (MRD) model was used to calculate the maximum duration of storage of timber outdoors under cover (protected from rain) before the onset of mould growth on the surface of wood. The prediction model is based on laboratory tests performed in constant and cyclic climates and were also confirmed against exposure tests in attics and crawl spaces. The prediction model presented ...
E Frühwald Hansson, S Bardage, S Thelandersson


Estimation of service life of treated wood in ground contact based on early indicators
2013 - IRG/WP 13-20536
A well-known problem with field testing is that it takes a long time before meaningful and reliable results are achieved. Only when a trial has come to an end the so called average life for the samples in a group can be calculated and compared with other samples. The aim of the present study was to investigate if it is possible to get a reasonable and good estimation of the average life long befor...
M Hansson, J Jermer, P Larsson Brelid, N Terziev


Performance standards for wood in construction – delivering customer service life requirements
2013 - IRG/WP 13-20537
There is increasing need for consideration of performance classification for wood products in construction, as evidenced by the CPR, warranty providers and end user demands for information. This means we need to radically consider how the tests we conduct on wood for durability (especially biological durability) can inform on service life and how they might if possible be translated into a perform...
E Suttie, C Brischke, F Englund, E Heisel, J Jermer, D Lorenzo, M Polášek, S Thelandersson, J Van Acker


Performance of recent and old Sweet chestnut (Castanea sativa) wood
2014 - IRG/WP 14-10816
Sweet chestnut (Castanea sativa) hardwood is one of the most durable European wood species. In the present research, various aspects that could potentially influence the durability were elucidated, namely: presence of extractives, ring width, and weathering. Simultaneously, properties of wood, which was in outdoor use for 35 years, were elucidated as well. The results indicate that ring width and ...
M Humar, M Žlahtič, N Thaler


Assessment of Scots pine sapwood susceptibility to moulds by determination of fungi growth and ergosterol content in infested wood
2014 - IRG/WP 14-20540
The susceptibility of wood to filamentous fungi (mould) attack is determine mainly by laboratory methods with descriptive grading of fungal growth on the surface of the wood specimens. It is a lot of different grading scale of fungi growth, but determination of the size of fungi growth is many times not easy, not clear and often difficult. Although the filamentous fungi are not included to microor...
A Fojutowski, A Koziróg, A Kropacz


Performance classification of wood in construction – drafting a user friendly European standard
2014 - IRG/WP 14-20545
The performance classification for wood products in construction is an extremely important topic in Europe and beyond – warranty providers and end users demand service life and performance information in the face of competition with other materials. The European project PerformWOOD has formalised and drawn together the on-going research to focus on generation of a material resistance factor for ...
E Suttie, C Brischke, L Meyer, J Van Acker, M Kutnik, E Heisel, F Englund, J Jermer, S Thelandersson, M Polášek, D Lorenzo


In-ground durability of wood-based products – Comparative assessment of graveyard field tests and terrestrial microcosms
2014 - IRG/WP 14-20538
Traditionally wood durability and the effectiveness of wood preservatives are determined in so-called graveyard tests (according to EN 252 or AWPA E7). For laboratory testing, terrestrial microcosms (TMC) can serve as an alternative. Both tests have been applied for different types of wood-based materials, preservative treated, modified and unmodified wood. However, the usability of laboratory res...
A Soetbeer, L Meyer, C Brischke, P Larsson-Brelid, J Jermer


Changes in mechanical and chemical properties of wood exposed outdoors
2014 - IRG/WP 14-20550
The aim of this study was to investigate differences in certain mechanical and chemical properties of three different wood species (common beach (Fagus sylvatica), Norway spruce (Picea abies), and copper-ethanolamine (CuE) impregnated Norway spruce (Picea abies)) that were exposed in use class 3 (CEN, 2006) for periods between 4 and 30 months. The results show, that changes in the investigated me...
N Thaler, C Brischke, D Žlindra, V Vek, M Humar


Critical parameters on moisture dynamics in relation to time of wetness as factor in service life prediction
2014 - IRG/WP 14-20555
The concept of natural durability or enhanced durability based on the presence of active ingredients having an impact on both fungi and insects is not the only parameter steering the material resistance. Complementary resistance to getting wet (wetting ability) and consequently the ease of drying afterwards will lead to a parameter related to the time a piece of wood will remain under such wet con...
J Van Acker, I De Windt, W Li, J Van den Bulcke


Cost effective extension of service life of bridge tie (sleepers) - Effectively applying borate during Boulton conditioning and treatment with copper naphthenate
2014 - IRG/WP 14-30637
Current longevity of creosote treated wooden bridge ties in the South Eastern US is about 15 to 25 years, which is well below of the average service life of 33-50 years of railroad ties. Such short service life increases costs associated with maintenance of railroads including bridge down time for tie replacement as well as the cost for the new ties themselves. Because of this, many railroads are...
J D Lloyd, T Chambers, J-W Kim


Encapsulation Systems Combined with DOT Borate Treatments – The Future of Treated Crossties
2014 - IRG/WP 14-40670
Borates have been utilized in wood protection systems for many decades but only recently have been used in North America to treat crossties. This colorless, ordorless and very effective wood protection chemical has the ability to arrest and prevent the colonization of wood by both basidiomycete decay fungi and insects such as beetles and termites while ties are air seasoning or in service. Since ...
S C Kitchens, T L Amburgey


Acceptance levels of surface disfigurement - tolerance to defects of coated wood
2015 - IRG/WP 15-20564
Service life planning (PSL) has become an important issue in performance based building and substantial progress has been made in recent years. The role of predicting the aesthetical service life of wooden building components has been underestimated for quite long time but is recently attracting more and more notice. It is influenced by numerous factors such as discoloration, fading, flaking, crac...
C Brischke, P Kaudewitz


The combined effect of wetting ability and durability on field performance – verification of a new prediction approach
2015 - IRG/WP 15-20565
Comprehensive approaches to predict performance of wood products are requested by international standards and the first attempts have been made in the frame of European research projects. However, there is still an immanent need for a methodology to implement the durability and moisture performance of wood in a performance classification system. The aim of this study was therefore to establish an ...
C Brischke, G Alfredsen, P-O Flæte, M Humar, T Isaksson, L Meyer


Non-destructive monitoring of structure and moisture dynamics of plywood exposed outdoors to improve service life prediction and fit-for-purpose design
2015 - IRG/WP 15-20570
Plywood is an important construction material yet prone to water uptake, which can decrease strength and increase decay risk. To predict service life and improve fit-for-purpose design, it is crucial to understand the moisture behavior and structural changes of plywood. In this research, several plywood specimens were exposed outdoors for approximately one year. During this period, the moisture di...
W Li, J Van den Bulcke, I De Windt, M Dierick, J Van Acker


Performance of bio-based building materials – viewpoints from the first year of COST Action FP1303
2015 - IRG/WP 15-20572
Maintaining and expanding the market potential for bio-based building products in indoor and outdoor construction uses remains a key activity for industries in the forestry and biotechnological sector, particularly in Europe. Whilst there are ongoing activities within IRG for collecting and populating a database on performance on wood, the performance data for many other (i.e. non-wood) "environme...
D Jones


Indentation and pendulum hardness tests: two convenient assessment methods of the performance of exterior wood coatings
2015 - IRG/WP 15-40689
Developing formulations of exterior wood coatings with long service life is a big challenge. For many years in Europe the performances have been mainly evaluated through weathering tests (within the EN 927 series) followed by visual assessment (blistering, flaking, mould growth, chalking and cracking), colour and gloss measurements, and adhesion tests. Very recently the importance of the mechanica...
L Malassenet, L Podgorski, M Truskaller, G Grüll


A review of the analytical methods used in determining the decay resistance of heat treated wood
2015 - IRG/WP 15-40690
Heat treatment as a wood process is increasingly used because of its non-biocide behaviour and its low environmental impact. This sort of treatment is based on biopolymer chemical degradation by heat transfer. This process improves mainly the dimensional stability and the decay resistance of wood. Wood becomes darker after this type of treatment and thus gives it an aesthetic appearance. These i...
K Candelier, M-F Thévenon, A Pétrissans, S Dumarçay, P Gérardin, M Pétrissans


How to Increase the Lifespan of Exterior Wood Coatings
2015 - IRG/WP 15-40700
In addition to aesthetic appeal, coatings are designed to protect the wood from weathering degradation in outdoor conditions. This paper gives an overview of the effects of main components of coating, coating properties, and wood treatments on coating performance. Understanding how different type of resins (alkyd, acrylic or polyurethane), amount of pigments, type of solvents (organic or water), a...
M Nejad


Environmental Fate of Micronized Copper
2015 - IRG/WP 15-50310
The environmental fate of wood preservatives is an important aspect to estimate the health and environmental impact. Although biocides from treated wood may be released into the soil, water or air, the latter pathway is frequently neglected in favour of leaching studies. Nonetheless, wood dust is well known to cause a variety of adverse health effects, in particular diseases to the respiratory tra...
C Civardi, L Schlagenhauf, J Benz, C Hirsch, J Van den Bulcke, M Schubert, J Van Acker, P Wick,


Foundation piles: analysis of beech wood decay in service life conditions
2016 - IRG/WP 16-10858
Wood piles foundation system was largely used over decades. Thus, numerous buildings over the world are based on this constructive system. In the context of reduction of CO2 emissions in the building field of constructions, substitution of concrete by wood as material for foundation piles seems to be a promising alternative. However, fluctuation of the water table level in soil may promote fungal ...
Q Kleindienst, A Besserer, M-L Antoine, C Perrin, J-F Bocquet, L Bléron


Identification of the key factors influencing development of the blue stain fungi
2016 - IRG/WP 16-10872
Service life of wood is more and more frequently affected by aesthetic requirements than functional ones. In order to elucidate various aspects of service life, model house with façade elements made of 22 materials was built on the field test site at Department of Wood Science and Technology in Ljubljana. Colour and fungal disfigurement is among other parameters monitored on this house. In parall...
D Kržišnik, B Lesar, N Thaler, M Humar


Previous Page | Next Page