Monitoring of wood biodeterioration by infrared spectroscopy
2017 - IRG/WP 17-20607
The susceptibility of wood to deterioration by rotting fungi is intrinsically related to its chemical composition and the environmental conditions at its place of use, and if not detected in time, can cause enormous financial losses. The process of wood biodeterioration by decay fungi can be evaluated through laboratory accelerated test, in specific field tests, or through non-destructive techniqu...
E Meneses Oliveira, A Florian da Costa, J W Batista Braga


COST FP 1303 Cooperative Performance Test – Results after two years outdoor exposure
2017 - IRG/WP 17-20620
COST Action FP 1303 ‘Performance of Bio-Based Building Materials’ started in October 2013 and an ambitious program was set up for four years. Among this a collaborative field test was planned. The idea of the cooperative performance test was to distribute a fairly simple test set up to as many places in Europe as possible in order to collect performance data reflecting the full range of climat...
B Lesar, M Humar, C Brischke, L Meyer-Veltrup, D Jones, N Thaler, J M Abascal, G Alfredsen, B Brunnhuber, E Grodås, M Irle, J Kers, M Klamer, K-C Mahnert, E Melcher, S Palanti, M Noël, E Suttie, N Pfabigan, M Touza


Possibility of using lichen (Usnea filipendula) and mistletoe (Viscum album L.) extracts as potential natural wood preservative
2017 - IRG/WP 17-30712
Increasing environmental pressures on toxic chemical wood preservatives lead to the development of natural and environmentally friendly wood preservatives. In this study, using possibilities of lichen (Usnea filipendula) and leaves of mistletoe (Viscum album L.) as potential natural wood preservative were researched. Treatment solutions have been prepared with two different solvents, water and met...
Ü C Yildiz, C Kiliç, A Gürgen, S Yildiz


Agar block durability test of plywood made of neem (Azadiracta indica) leaves treated veneer using two white rot fungi
2017 - IRG/WP 17-40782
This study has been undertaken to investigate the durability of plywood made from non-durable wood (simul, Bombax ceiba) veneer treated by neem (Azadiracta indica, A. Juss.) leaves. The veneers were treated with cold and hot water solution of neem leaves of different concentrations (10%, 5%, 2.5%) and treatment durations (1, 2, 3 days) for cold water and 20, 40 and 60 minutes for hot water. The pl...
K Akhter, M A Hashem, S Akhter


A summary of history and use of timber bridges in New Zealand
2017 - IRG/WP 17-40801
Wooden bridges have been an important part of road and rail networks in New Zealand. While wooden structures have largely been replaced by concrete and steel on major arteries they still have a place where lightweight, easily assembled structures are needed. These timber bridges may also be a cheaper alternative to other materials in roads which carry relatively low traffic loads. In the last ten ...
D Page, T Singh


Evaluation of coating applied in treated wood: experiences in Brazil
2017 - IRG/WP 17-40814
Weathering assays study the coating degradation caused by its exposure to the action of ultraviolet radiation, winds, heat and humidity. The use of test specimens in different arrangements and exposure angles is intended to reproduce various conditions in which a product can be used. The purpose of this paper is to present the efficacy of an oil-borne varnish applied on treated wood exposed to wea...
M F Natale, J M Vidal


Preliminary Investigation into the Natural Decay Resistance of Nigerian Grown Hevea brasiliensis and Mitragyna ciliata wood to Phanerochaete chrysosporium White-Rot Fungus
2018 - IRG/WP 18-10919
Wood is an important and versatile structural building material that finds applications in numerous uses. However, wood is also a biological material vulnerable to degradation by microbial activities; this is especially true in the tropics. Following the scarcity of highly durable species from our natural forests and the introduction of so many lesser used/durable wood species into the booming tim...
J M Owoyemi, U O Emmanuel


Long-time efficacy of some soil termiticides tested according to “Modified Ground Board Test”
2018 - IRG/WP 18-10935
Field trials of efficacy of soil termiticides available in Thailand were started back in the 1980s at four different locations representing different unique weather types of the country. The method used in the trials (Modified Ground Board Test) is the compulsory test for every soil termiticides aiming to be registered for termite control in Thailand. The ongoing record reveals that some particula...
C Vongkaluang, K Charoenkrung, N Same Rain


Testing the durability of timber products above ground using the block-test method – A critical review
2018 - IRG/WP 18-20637
The block-test method for testing the durability of wood and wood products above ground is reviewed critically with respect to practical aspects, moisture loads, corresponding decay development, and the possibilities of assessing test specimens by determining the dynamic modulus of elasticity (MOEdyn) of wood. In total, 36 blocks representing different modifications of the original set-up and a wi...
C Brischke, A Gellerich, H Militz


Towards durability classification of preservative treated wood – first attempts using different European standards
2018 - RG/WP 18-20638
EN 350 (2016) gives guidance on methods for determining and classifying the durability of wood and wood-based material against biological wood destroying agents. “Wood-based materials are those derived from trees and include amongst others: untreated wood, heat treated wood, chemically modified wood, glue laminated wood, wood-based panels, wood polymer composites and wood treated with wood prese...
S Bollmus, A Gellerich, C Brischke, H Militz


Can CCA be substituted as reference preservative?
2018 - IRG/WP 18-20641
While field testing of wood protective formulations remains probably the best method to find out the effective preservative concentration, the use of chrome-copper arsenate (CCA) as reference becomes debatable due to environmental and legislative reasons. This emerges from the European standardization bodies who have discussed reference alternatives that can omit the use of CCA. The present debate...
N Terziev, M Jebrane, P Larsson Brelid, N Morsing, P-O Flaete, P Torniainen, J S Kim, G Daniel


Above-ground testing methods – review of Rotorua, New Zealand test site results after ten years
2018 - RG/WP 18-20642
A series of seven different types of above ground durability tests were initially conducted over four years to determine which type of tests would give the fastest, most consistent results. Five types of test; ground proximity, two types of decking, flat panels and double layer, were reassessed after ten years. Exposure conditions varied between tests with ground proximity producing close to groun...
D Page, T Singh


Rapid Screening test of potential antimicrobial agents for wood coatings
2018 - RG/WP 18-20644
A two-part screening test has been developed to evaluate additives for wood coatings. First, an additive is tested in the microbial laboratory and evaluated based on its inhibitory properties against selected test organisms, directly on agar plates. A microbial growth analysis is prepared and evaluated. If the additive is considered effective, it will be tested in a standard top coating (acrylic o...
J Stenbæk, E Morsing, T Østergaard Jensen


Determining the natural durability on xylarium samples: mini-block test, wood powder and chemical profiling
2019 - IRG/WP 19-10944
Xylaria, or wood collections, can be considered sleeping beauties in terms of wood technological and biological output. In this study we focus on determining the natural durability of xylarium specimens from the Federal Xylarium in the Royal Museum for Central Africa. The Federal Xylarium contains over 80,000 specimens, covering more than 13,000 species, mainly from Central Africa. These specimens...
V Deklerck, L De Ligne, J Van den Bulcke, E Espinoza, H Beeckman, J Van Acker


Improvement of analytical methods of wood preservatives and its validation with collaborative testing
2019 - IRG/WP 19-20655
This discussion paper presents on-going collaborative test of analytical methods of wood preservatives according to the standardization process of Japan Agricultural Standard (JAS) by the Ministry of Agriculture, Forestry and Fisheries (MAFF). Food and Agricultural Materials Inspection Center (FAMIC) in close cooperated organization with the MAFF, has wide range of tasks about inspections and anal...
T Miyauchi, K Yamamoto, N Shota, Y Akabori, M Ikeda, J Eisawa, K Kambara, T Osawa, C Igarashi, Y Baba, W Ohmura, M Shimizu, M Samejima


Durability classification of preservative treated and modified wood
2019 - IRG/WP 19-20659
EN 350 (2016) allows formally to determine durability classes (DC) for wood products and wood-based materials, which was previously only possible for untreated wood in the form of natural durability. In a first study, the University of Goettingen carried out the durability classification of chemically modified (modified with 1,3-dimethylol-4,5-dihydroxyethyleneurea, DMDHEU) and preservative-treate...
S Bollmus, L Bachle, C Brischke, H Militz


Impact of water holding capacity and moisture content of soil substrates on the moisture content of wood in terrestrial microcosms
2019 - IRG/WP 19-20662
Terrestrial microcosms (TMC) are frequently used for testing the durability of wood and wood-based materials as well as the protective effectiveness of wood preservatives. In contrary to experiments in soil ecology sciences, the experimental set-up is usually rather simple. However, for service life prediction of wood exposed in ground, it is of immanent interest to better understand the different...
C Brischke, F L Wegener


Development of accelerated decay test for CLT using a fungus grown on agar medium
2019 - IRG/WP 19-20664
CLT is a large-scale wooden board which consists of several layers of sawn lumber stacked in altering directions. Therefore, a lot of large cross sections appear on all narrow faces of CLT. As water penetrates easily into timber from cross section, wooden material whose cross section is exposed to water in in a usage environment is susceptible to deterioration by organisms. Wood deterioration orga...
T Miyauchi, K Kambara, W Ohmura, T Mori, H Matsunaga, N Hattori


Color change of timber exposed outdoors - Influence of season exposure test starts
2019 - IRG/WP 19-40865
For the client the material and color of the exterior wall are important, because they affect the impression of the building [1]. However, discoloration of the exterior wall begins as soon as the building is completed, by various factors such as rainfall. We tried to quantitatively evaluate the changes of the exterior wood, and to organize the influences of climate conditions, in order to use the ...
K Usami, H Ishiyama


Knowledge exchange and transfer from academia to industry in the field of wood protection research – Activities of the IRG-WP Communications Committee
2019 - IRG/WP 19-50354
The International Research Group on Wood Protection (IRG) was founded in 1969 as a structured group of like-minded scientists and technologists focused on generating knowledge of the science of wood deterioration, and novel solutions to provide sustainably and environmentally responsible products for the protection of wood-based materials. The primary function of the IRG is to provide opportunitie...
F Latorre, B Abbott, C Brischke, M Humar, D Jones, E Larnoy, L Nunes, A Preston, T Singh


Performance of bio-based building materials – durability and moisture dynamics
2020 - IRG/WP 20-20666
When exposed to conditions favourable for decay, bio-based building materials can be susceptible to degradation. Their ability to withstand deterioration over time (performance) depends on the intrinsic or enhanced durability of the material as well as its wetting and drying behaviour. The effect of fungicidal components in wood is known since long. Other material characteristics, such as the mate...
L De Ligne, J Caes, S Omar, J Van den Bulcke, J M Baetens, B De Baets, J Van Acker


Impact of fungal decay on the bending properties of wood
2020 - IRG/WP 20-20671
Wood used outdoors is generally prone to fungal degradation, and its impact on the structural integrity of wood is an immanent factor for service life planning with timber. Wood decayed to very small mass losses can suffer from a significant reduction in mechanical strength and elastic properties. Hence, the latter are preferred indicators to detect decay in wood durability studies. Numerous previ...
S Bollmus, P B van Niekerk, C Brischke


Future development of durability assessment of wood, according to typical usage of preservative-treated wood and naturally durable wood in Japan
2020 - IRG/WP 20-20675
A market of preserved wood products in Japan has two unique histories. First is the market shift to residential ground sills from utility poles and sleepers; the other is the stop of CCA treatment caused by the new effluent standard. In 2018, around 85% of preserved wood products used for residential ground sills were treated with non-CCA such as Cu-based agents. Since the market of treated wood h...
T Osawa, W Ohmura, H Kurisaki


Sterilization of Large Timbers during Preservative Treatment: How Quickly We Forget
2020 - IRG/WP 20-40902
Air seasoning is a common method of moisture management in utility poles and is done de facto during pole storage prior to treatment. However, extended air drying prior to treatment encourages fungal attack and can facilitate establishment of decay fungi in poles before a protective preservative barrier is applied. This problem can be mitigated by proper air-seasoning methods coupled with heat ste...
G Presley, J Cappellazzi, M Konkler, K Maguire, R Nelson, J J Morrell


Performance of resin-treated solid wood and laminated veneer lumber (LVL) under marine conditions
2021 - IRG/WP 21-10973
Wood is a traditional building material in the marine environment, where it is exposed to extremely harsh conditions. Most of the indigenous softwood and hardwood species in Europe are not durable against attack by marine organisms. Recently, wood modification has been considered as an alternative to protect non-durable wood species under use class (UC) 5 (EN 335, 2013) conditions. The present stu...
L Emmerich, C Brischke, S Bicke, H Militz