IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 239 documents. Displaying 25 entries per page.


Termite Resistance of Different Wood Panels Treated with Bifex® under Laboratory and Field Trials
2011 - IRG/WP 11-10745
The effects of Biflex® on termite resistance of laminated chip Board, MDF (Medium Density Fiber), Ply Wood and Veen Board at 50 ppm were evaluated. Laboratory and field trials resistance tests showed that all woods treated with Biflex were resistant to termites as compared to untreated ones. It was concluded that as chemical loadings increased, termite mortalities increased, and at the same time...
F Manzoor, S A Malik, B M Ahmed Shiday, A Liaquat, N Naz


Investigating extraction of bifenthrin from composite wood products
2011 - IRG/WP 11-20467
Bifenthrin is added to resin prior to lay-up of plywood and laminated veneer lumber to provide termite protection. Analysis of this chemical in resins can be challenging. The potential for using ground wood in place of sawn material to recover bifenthrin was investigated using laminated veneer lumber composed of Douglas-fir veneers analyzed by three laboratories. Although the results differed amo...
J J Morrell, L Bell, J Norton, C Shaw


Effects Of Wood Preservative On Mechanical Properties Of Glulam Manufactured From Lower Density Malaysian Tropical Timber
2012 - IRG/WP 12-40590
This study is to investigate the effect of wood preservative on the mechanical properties of glulam timbers made from low density Malaysian hardwood timbers. Utilization of lower density Malaysian tropical timber for structural applications have not exploited extensively due to their inferior strength. By converting into treated glued laminated (glulam) timbers it could offer the possibility of th...
L Francis, Z Ahmad


Classifying white rot decay resistance of some hardwoods from Sarawak and Peninsular Malaysia and correlations with their tropical in-ground durability
2012 - IRG/WP 12-10788
White rot wood decay under Malaysian (humid tropical) terrestrial conditions pose more serious threats to the in-ground service life of hardwoods than other common fungal decay types. A study is made on decay resistance variation for a total combined list of 30 Peninsular Malaysian and Sarawak timber species (plus 6 exotic reference temperate commercial woods for comparison) using the laboratory s...
A H H Wong, J M E Jem, Lai Jiew Kok


Cost effective extension of service life of bridge tie (sleepers) - Effectively applying borate during Boulton conditioning and treatment with copper naphthenate
2014 - IRG/WP 14-30637
Current longevity of creosote treated wooden bridge ties in the South Eastern US is about 15 to 25 years, which is well below of the average service life of 33-50 years of railroad ties. Such short service life increases costs associated with maintenance of railroads including bridge down time for tie replacement as well as the cost for the new ties themselves. Because of this, many railroads are...
J D Lloyd, T Chambers, J-W Kim


Copper naphthenate treatment for wood crossties and timbers
2014 - IRG/WP 14-30647
Copper naphthenate (CuN) has a long history in wood preservation and is recently finding increased usage as a treatment for wooden crossties and timbers. One of the principal reasons that CuN has gained market acceptance, in addition to its efficacy against decay fungi and wood-destroying insects, is its low mammalian toxicity and environmental impact. CuN is a well proven non-restricted use pres...
J Brient


Comparison of untreated plywood and untreated LVL in a field trial against Coptotermes acinaciformis and in laboratory trials against Tyromyces palustris and Coniophora puteana
2014 - IRG/WP 14-40671
In Australasia, efficacy data obtained on plywood is generally acceptable for laminated veneer lumber (LVL) and vice versa. This is particularly the case with glueline treatment approvals. The rationale is that the two wood products have predominately the same basic structure with the key difference being orientation of the veneer. LVL typically has all veneers in parallel while plywood typical...
A Siraa, K Day, S Millward, P Lobb


Commercial Timbers of Kenya
2016 - IRG/WP 16-10876
The global timber trade has for years been too familiar with an assortment of available African timbers, reputed for their appearance in terms of colour, grain, pattern and durability. African forests are fast disappearing through over-exploitation as a result of demand for agricultural land. Kenya, the home of some of these valuable hardwoods, has been similarly affected, with its forest land cov...
R Venkatasamy


The durability of manufactured structural building materials
2016 - IRG/WP 16-40718
The projected market potential for Engineered Wood Products such as CLT (cross laminated timber) is very positive however, potential prolonged rain leakage or moisture exposure during construction and in-service could pose considerable concern for its durability and reputation. This research was conducted to assess the decay resistance of CLT and OSB (oriented strand board) in an accelerated trial...
T Singh, D Page


Bacterial adhesion to selected wood finishes
2017 - IRG/WP 17-40793
A new generation of furniture, including antibacterial surfaces, should adjust to the changing needs of an ageing population. Respectively, determination of bacterial adhesion on wooden surfaces, finished with various wood finishes or coating is an important topic. The main aims of our work were of a preliminary character. We wanted to state if the existing methods for testing of bacterial adhesio...
M Petrič, D Kekec, J Žigon, K Godič Torkar, K Bohinc


Borate and Copper Naphthenate Dual Treatment of Bridge Timbers-Borate movement over time
2017 - IRG/WP 17-40795
Preservative treated wooden bridge ties in the South Eastern USA have a service life of about 15 to 20 years, which falls well below the average service life of 40 years of railroad cross ties (sleepers). It has been shown that cross tie life is significantly extended using borate dual treatment and this is now commercialized in bridge timbers using borate inserts. In previous research, it was dem...
J-W Kim, J D Lloyd


Dual Borate and Copper Naphthenate Treatment of Bridge Timbers:- Potential Performance Enhancements and Cost Savings
2017 - IRG/WP 17-40797
Dual treatment technology combining diffusible preservatives with oil borne preservatives, widely used for crossties in the USA, has now also been commercialized with bridge ties/timbers. In order to understand the implications of these changes, the historic service life of creosote treated bridge timbers in northern and southeastern USA were considered as well as field test data for both creosote...
J Lloyd, C Brischke, R Bennett, A Taylor


A summary of history and use of timber bridges in New Zealand
2017 - IRG/WP 17-40801
Wooden bridges have been an important part of road and rail networks in New Zealand. While wooden structures have largely been replaced by concrete and steel on major arteries they still have a place where lightweight, easily assembled structures are needed. These timber bridges may also be a cheaper alternative to other materials in roads which carry relatively low traffic loads. In the last ten ...
D Page, T Singh


Durability of energy efficient wooden buildings: a building physical point of view
2017 - IRG/WP 17-40812
The drive for more energy efficient and sustainable buildings resulted in an increased popularity of wooden buildings, even in countries with a masonry tradition. Often guidelines and prescriptions then are copied from other countries. Different climatic boundary conditions and tradition of finishing, though, do require different moisture tolerance criteria. This is clearly the case for water vapo...
S Roels, J Langmans


Self-Extinguishment Phenomena of Mass Timber in Medium-Scale Compartment Fires
2018 - IRG/WP 18-30729
This paper presents a review of the fire safety risks that mass timber construction may introduce in buildings, with special consideration to medium- and high-rise buildings. These main risks are represented by an effect to the classical fire safety strategy for buildings: (1) Compartmentalisation, to ensure that the fire will not spread farther than the compartment of origin, (2) Preventing verti...
C Gorska, J P Hidalgo


Performance of untreated timbers in above ground decking tests: Preliminary results from an international collaborative trial
2019 - IRG/WP 19-10940
The ability to accurately predict wood decay risks under varying environmental conditions has long been of interest to timber users. Accurate predictions are difficult owing to the myriad of variables associated with the decay process including wood species, wood inhabiting organisms, timber building element design and environmental conditions. Despite these difficulties, decay predictions have be...
L P Francis, J Norton, E Melcher, A H H Wong, J Kok Lai, M Klamer, M J Konkler, J J. Morrell


Visual assessment of longitudinal wheel timbers and assessing the feasibility of extending wheel timber service life in the UK railway network
2019 - IRG/WP 19-20651
Timber has been a versatile building material for centuries and during the start of the Railway Age in the nineteenth century it was in considerable demand for use in the railway network, particularly bridge building. Timber is still in service and widely used throughout the UK railway network. The resilience and favourable strength to weight ratio and its relative ease of fabrication make it an...
J R Williams


Protecting Sustainable Wood Infrastructure ̶ Improving the Performance of Poles, Piles, Ties & Timbers with Dual Treatments
2019 - IRG/WP 19-30735
Wood is by far the best structural material in terms of environmental impact, as shown by a number of LCA studies. This environmental impact superiority can be improved if the longevity of the commodity is extended. The main durability concern in large cross-section treated materials is the susceptibility of the heartwood to decay, as it is not typically treatable using traditional methods. This ...
J Lloyd, A Taylor, C Brischke, N Irby, M Manning


Treatability of native and exotic alternative timber species
2019 - IRG/WP 19-40864
The service life of moderately durable species can be extended significantly if the challenge of effective treatment of refractory wood species can be overcome. Along with preservative effectiveness, the performance of preservative in treated wood depends on factors such as retention and penetration in treated wood, the wood anatomy, the uniformity of penetration and micro-distribution within the ...
D Page, T Singh


Durability testing of mass timber building elements: a call for a collaborative trial
2019 - IRG/WP 19-40875
Mass timber buildings have captured the imagination of architects and engineers seeking more environmentally friendly building materials. The mass timber movement has tremendous potential to markedly increase timber use in mid-rise to high rise buildings. With great promise, however, comes great risk. Most mass timber structures that have been built or are being planned use no protective treatm...
J J Morrell


Preservative Treatment of CLT: An Example at Shimojishima Airport
2019 - IRG/WP 19-30748
Cross laminated timber (CLT) is a relatively new construction method that allows multi-storey construction using solid wood instead of concrete or steel. It is a method favoured by progressive architects and recognized for its much lower environmental footprint. Wood is an excellent construction material and is a long-term carbon sink that also performs well in the event of earthquakes and fire....
J Lloyd, N Yamashita, A Taylor


Experimental study on compressive strength performance of cross laminated timber with biodeterioration damage
2019 - IRG/WP 19-40883
The mass timber construction has attracted attention around the world. The reasons are due to the environmental impacts and the potential of the strength performance and quantity of the wood. Nowadays, CLT is one of the most important materials for the timber constructions. If we use CLT as a building material, we should consider the biodegradation risk for long time use. From an estimation of fut...
T Mori, Y Otsubo, R Inoue, M Ikeda, K Kambara, W Ohmura


Longterm Performance of Treated Timbers in Marine Exposures
2020 - IRG/WP 20-10969
The performance of preservative-treated or modified woods in marine exposures was evaluated at test sites in Newport, Oregon, USA and Brisbane, Queensland, Australia. All samples have exhibited excellent performance at the Newport, Oregon site, while attack was more aggressive at the sub-tropical Brisbane site. Acetylated wood as well as samples treated with 7.3% chromated copper arsenate (CCA-T...
M Konkler, A R Zahora, J Norton, J J Morrell


Sterilization of Large Timbers during Preservative Treatment: How Quickly We Forget
2020 - IRG/WP 20-40902
Air seasoning is a common method of moisture management in utility poles and is done de facto during pole storage prior to treatment. However, extended air drying prior to treatment encourages fungal attack and can facilitate establishment of decay fungi in poles before a protective preservative barrier is applied. This problem can be mitigated by proper air-seasoning methods coupled with heat ste...
G Presley, J Cappellazzi, M Konkler, K Maguire, R Nelson, J J Morrell


Performance of resin-treated solid wood and laminated veneer lumber (LVL) under marine conditions
2021 - IRG/WP 21-10973
Wood is a traditional building material in the marine environment, where it is exposed to extremely harsh conditions. Most of the indigenous softwood and hardwood species in Europe are not durable against attack by marine organisms. Recently, wood modification has been considered as an alternative to protect non-durable wood species under use class (UC) 5 (EN 335, 2013) conditions. The present stu...
L Emmerich, C Brischke, S Bicke, H Militz


Previous Page | Next Page