IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 751 documents. Displaying 25 entries per page.


Determination of toxic limits of wood preservatives towards wood-destroying Basidiomycetes. Investigation on the effect of the use of two impregnated wood blocks and of one impregnated and an untreated block respectively in Kolle jars on the toxic limits of wood preservatives
1973 - IRG/WP 225
O Wälchli


Collaborative soft rot tests: Proposed amendments to Document No: IRG/WP/208
1973 - IRG/WP 224
J K Carey, J G Savory


Incorporating insect behaviour in standard tests of wood preservatives - A possible way to reduce pesticide loadings
2000 - IRG/WP 00-20190
The application of wood preservatives to protect timber against insect infestation is common practice world wide. The effectiveness of wood protecting insecticides is usually determined in various standard tests. Depending on the target pest species and the test method, larvae of different developmental stages and sizes or adult insects are exposed artificially to the insecticide-treated commodity...
H Hertel, R Plarre


Natural durability of some common Indian timbers and marine plywood against biodeterioration in Kochi waters (India)
1992 - IRG/WP 92-4177
Panels of thirty-eight timber species and marine plywood were tested in Kochi harbour (South-west India) for periods ranging from 3 to 21 months, so as to evaluate their natural resistance against marine borers. Results indicate that all the timber species studied are non-durable, 6 of them having undergone more than 50% internal destruction within 3 months; 14 species in 6 months, 13 species and ...
L N Santhakumaran, M V Rao


Water-borne preservative marine trials in Western Canada
1981 - IRG/WP 470
Red pine boards treated with chromated copper arsenate, ammoniacal copper arsenate, copper zinc arsenic additive, a modified ammoniacal copper arsenate, and zinc arsenic additive, have been installed in a marine field test at West Vancouver, British Columbia. After two and a quarter years exposure, all the test samples are in excellent condition with the exception of those treated with the zinc ar...
J N R Ruddick


Some experiments with hexabutylditin against fungi
1977 - IRG/WP 388
The investigation was carried out in 1972 and 1973 to collect experimental data about the poisonousness of hexabutylditin (HBDT) against the woodrotting fungi Coniophora puteana (Coniophora cerebella), strain 15, and Chaetomium globosum, strain hexabutylditin was being manufactured by the Organisch Chemisch Instituut (O.C.I.) TNO, at Utrecht....
J W P T Van der Drift


Leaching tests - A paper for discussion
1973 - IRG/WP 221
J W W Morgan


Plastic-coated marine piling in Los Angeles Harbour
1984 - IRG/WP 4105
G Horeczko


Laboratory experiments on aerial emissions from wood treated with wood stains
1993 - IRG/WP 93-50001-06
Due to the actual environmental interest in wood preservation, a series of experiments was carried out on the emission of biocides from treated wood. The research focussed on the volatilization of 5 biocides from boards treated with wood preservative finishes containing dichlofluanide (DCF) azaconazole (AZA), pentachlorphenol (PCP), iodopropynylbuthylcarbamate (IPCB) and tributhyltinoxide (TBTO). ...
G M F Van Eetvelde, M Stevens


Correlation between a laboratory bioassay and field trial conducted to determine the termiticidal effectiveness of bifenthrin
2002 - IRG/WP 02-20248
Details are given of a laboratory bioassay and field trial undertaken to determine the termiticidal effectiveness of the synthetic pyrethroid bifenthrin, when impregnated into Pinus radiata D. Don sapwood specimens. Results show a strong correlation between the laboratory and field methods of evaluation. Protection threshold limits obtained were the same for the two test species of termite employe...
J W Creffield, K Watson


A new laboratory technique devised with the intention of determining whether, related to practical conditions, there should be a relationship between growth rate and decay capacity (of different strains) of Serpula lacrymans
1989 - IRG/WP 1384
Most laboratory techniques for the determination of growth rate not only use a medium (agar) unrelated to practice, but also yield values that are often far less than those found in practice. Also, most laboratory techniques for the determination of decay capacity ensure that the whole of a small test block becomes fully surface-colonised within the first few days; whereas in Australian practice S...
J D Thornton


Sub-group on Basidiomycete tests: Responses to proposals for programme of work
1980 - IRG/WP 2137
A F Bravery


Standardisation of tests of toxicity of preservatives to soft rot fungi
1978 - IRG/WP 2119
J G Savory


Performance of CCA treated Eucalyptus round ties
1985 - IRG/WP 3342
After 5.5 years of field exposure in the south of Brazil round Eucalyptus ties treated with CCA type A Oxide (OSMOSE K-33-A) preservative with retentions from 12 to 14 kg/m³ (0.75 to 0.873 PCF) (active ingredient basis) are performing very well. No decay or insect attack was observed in the 100 ties in test in real conditions of use; 10% of ties show incipient checking (what is a natural trend of...
V J Carlos, F R Niederauer, J P P Wehr


Antagonistic effect of Trichoderma spp. against Serpula lacrymans in the soil treatment test
1991 - IRG/WP 1473
Soil treatment tests for preventing growth of Serpula lacrymans were conducted using Trichoderma spp. as antagonists. Soil specimens tested were Kanuma-soil without organic matter and the horticultural soil which was collected from the test site of the stake test. Perfect efficacy of treatment with Trichoderma spp. was shown when the horticultural soil without sterilization was used as a soil spec...
S Doi, A Yamada


Evaluation of termiticides in field trials
1990 - IRG/WP 3633
Termiticide-treated posts and stakes have been tested at the field test site in Kagoshima, Southern Kyushu, Japan. Various commercial and alternative termiticides have been evaluated annually as TAI (termite attack index), calculated by the equation: TAI = R x P, where R is the mean of attack rating of 0 (sound), 10 (sign of tasting), 30 (slight attack), 50 (moderate attack), 100 (severe attack), ...
M Takahashi, Y Imamura, K Tsunoda, A Adachi, K Nishimoto


Laboratory simulation of leaching from creosote treated wood in aquatic exposures
2000 - IRG/WP 00-50157
Creosote has a long history of use as a preservative particularly in industrial wood products, but its use has come under increasing scrutiny as a result of concerns about its potential effects on aquatic and terrestrial non-target organisms. Despite its long use, there is relatively little data on the rates of creosote loss in many exposures. In this report, we describe small scale leaching tank ...
Ying Xiao, J Simonsen, J J Morrell


The variability of preservative distribution in test blocks
1973 - IRG/WP 220
The techniques for the assessment of likely effectiveness of preservative systems have long been the subject of much discussion. The whole field has recently been reviewed by Hilditch and Hamblyn (1971) who described in detail many of the laboratory test procedures used, but who also indicated the deficiencies in many of these techniques. It has long been the view of many associated with the wood ...
F W Brooks, M R Gayles, R W Watson


A laboratory method for assessing the effectiveness of remedial treatments in preventing post-treatment emergence of Anobium punctatum
1982 - IRG/WP 2175
R W Berry


36 years of wood preservative tests in Tanzania
1992 - IRG/WP 92-3731
The performanee of major wood presevatives which are used widely commereially are given. These include creosote, CCA's and 5% Pentachlorophenol dissolved in heavy industrial diesel. Tests are conducted at three ecologically different using pine stakes. Results show that the striking performance of creosote and CCA's is noticeable at above 128 kg/m³ and 16 kg/m³ respectively....
K K Murira, P F Nangawe


A method of predicting the average life of field tests on preservative-treated stakes
1977 - IRG/WP 297
The paper presents an analysis of the results of completed field stake tests on untreated and preserved timber, and develops a method of predicting the average life of incomplete stake tests on wood preservatives from the failures that have occurred so far....
D F Purslow


A case for adopting a standardised protocol of field and laboratory bioassays to evaluate a potential soil termiticide
2003 - IRG/WP 03-20275
The rationale for adopting a new approach to the field testing of potential soil termiticides is advocated on the grounds that current testing methods are limited to termite bioassays and do not address quantitatively the persistence and bioavailability of soil termiticides to foraging subterranean termites over time and in different soil types. Furthermore, the present testing regimes assume fiel...
J R J French, B M Ahmed


The efficacy of polyurethane coatings on wood samples exposed in the marine environment. Final Report -10 Year Assessment
1996 - IRG/WP 96-10170
The results of an IRG collaborative marine trial to investigate the long-term permanence and efficacy of polyurethane coatings against marine borers are reported. PU-coated wood samples were exposed at a range of sites from tropical to cold temperate locations. The marine borer species present at the sites included teredinids, pholads, limnoriids and sphaeromatids so that each site offered its own...
R A Eaton


Water-borne wood preservatives against marine borers. Results from NWPC marine trials started in 1972 and 1976
1990 - IRG/WP 4162
The paper presents the results from NWPC (Nordic Wood Preservation Council) marine trials started in 1972 and 1976. The trials are carried out according to the NWPC Standard No. 1.4.2.2./73 "Marine test - a test against marine wood boring organisms in sea water". The test site is Kristineberg Marine Biology Station on the west coast of Sweden. The wood blocks used in the trials were made from sapw...
Ö Bergman, C Lundberg


Results of field tests on the natural durability of timber (1932-1975)
1976 - IRG/WP 3105
This paper describes a continuing field stake trial to determine the natural resistance of different species of timber to decay. Data are presented for about 180 timbers, covering over 6000 stakes, and the results are discussed in terms of a natural durability classification....
D W Purslow


Previous Page | Next Page