Bundle tests - Simple alternatives to standard above ground field test methods
2016 - IRG/WP 16-20581
Within this study we applied different new above ground test set ups to untreated Norway spruce (Picea abies Karst.) and Scots pine sapwood (Pinus sylvestris L.) which are frequently used as reference or control species in wood durability field tests. The overall aim of this study was to find a simple alternative method to the few standardized above ground field test methods, such as the L-joint a...
C Brischke, L Meyer-Veltrup


Modelling the performance of bio-based building materials
2016 - IRG/WP 16-20582
The ‘bio-based economy’ represents a growing area of development globally and covers a wide range of building materials including wood and wood-based products. A ‘bio-based’ material is intentionally made from substances derived from living (or once-living) organisms. In this context it means that the materials and products are made from renewable resources, with the criteria that a renewa...
C Brischke


Evaluation of field test data
2016 - IRG/WP 16-20594
The resistance against fungal decay and insect attack of wood can be highly variable, between boards and even within boards. The variability in durability is not always an issue, but for high demanding applications information about its reliability is required. This comprises the variability of outdoor performance. Durability testing in laboratory and outdoor exposures can provide a good basis to ...
F Bongers, C Brischke, J Van den Bulcke, W Gard, I De Windt, H Militz


Laboratory and Field evaluation on Resistance of Thiacloprid-treated Pine Species to Termites in Mexico
2016 - IRG/WP 16-30687
The usage of Neonicotinoids for wood preservatives is common practice in several countries. Especially the active ingredient Imidacloprid is well established for this application due to its high efficacy against termites. (2Z)-3-(6-chloro-3-pyridylmethyl)-1,3-thiazolidin-2-ylidene-cyanamide, also known as Thiacloprid showed a good efficacy against Reticulitermes santonensis De Feytaud in efficacy ...
P Meckler, T Jaetsch, I Rodriguez


Encapsulation of poles to prevent moisture uptake – a laboratory test
2016 - IRG/WP 16-40753
Premature failure of utility poles due to decay in soil contact is the main reason for early removal of utility poles, a measure that implies extra costs for utilities. Remedial treatments and barriers are common methods to prolong the service life of utility poles. The first part of this paper gives an overview of mode of action and commercial application of barrier systems as described in the li...
K-C Mahnert, U Hundhausen


Estimation of wood degradation determined by visual inspection, mechanical testing and DNA characterisation – report after 3 years of exposure
2016 - IRG/WP 16-30700
The influence of two separate treatments, thermal modification and alkaline copper quaternary (ACQ, Silvanolin©) treatment, on fungal decay, visual disfigurement, deterioration in mechanical properties and fungal community structure was assessed on Norway spruce (Picea abies) and compared with the performance of two naturally more resistant tree species native to North America: Douglas fir (Pseud...
N Thaler, T Martinović, M Bajc, D Finžgar, H Kraigher, A Sinha, J J Morrell, M Humar


Evaluation of the effects of different concentrations of Fipronil against Reticulitermes grassei (Blattodea: Rhinotermitidae)
2016 - IRG/WP 16-30702
A laboratory evaluation of the effect of different concentrations of Termidor (fipronil at 9.09%) has been carried out. Six concentrations (10,000; 1,000; 100; 50; 10 and 5 ppm) have been tested in two different colony models imitating an open environment. After five days treatment, mortality data were collected. The three higher concentrations showed nearly 100% mortality. At 50 ppm the mortalit...
J R Carbonero-Pacheco, R Molero, M E Alcaide, J Diz, M Gaju


10 year Report on COST E37 Round Robin Tests – Comparison of results from laboratory and field tests
2017 - IRG/WP 17-30718
A round robin involving 15 European participants was set up in 2006. The round robin consisted of both a field test according to the double layer test method and a laboratory test with two different preconditioning methods. The laboratory test results were reported in an earlier IRG paper (IRG/WP13-20535) but are included also in this paper in order to facilitate the comparison with the field test...
M Westin, E Conti, J Creemers, P-O Flæte, A Gellerich, I Irbe, M Klamer, E Melcher, R Moeller, L Nunes, S Palanti, L Reinprecht, E Suttie, H Viitanen


Durability Testing of a Cattail (Typha spp.) based Insulation Material against Termite Attack
2017 - IRG/WP 17-10879
The use of insulating materials is particularly important in the construction industries, especially with regard to the use of wood and naturally occurring substances. The use and durability of natural materials as insulating materials is of keen interest to many construction experts, and continues to be a topic of intense investigation. It is generally agreed that the use of natural substances ...
M Dass, W Unger, T L Woods


Monitoring of wood biodeterioration by infrared spectroscopy
2017 - IRG/WP 17-20607
The susceptibility of wood to deterioration by rotting fungi is intrinsically related to its chemical composition and the environmental conditions at its place of use, and if not detected in time, can cause enormous financial losses. The process of wood biodeterioration by decay fungi can be evaluated through laboratory accelerated test, in specific field tests, or through non-destructive techniqu...
E Meneses Oliveira, A Florian da Costa, J W Batista Braga


Bio-deterioration of Southern Pine Stakes at Geographically Different Testing Sites
2017 - IRG/WP 17-20609
Southern pine (SP) sapwood is commonly used in preparing the standardized stakes for performance testing as referenced in the American Wood Protection Association (AWPA) Book of Standards. For example, the standardized above ground test methods E16/E18 and the standardized ground contact test method E7 all use sapwood of SP as the preferred wood species for preservative performance test. In this...
Jun Zhang, J Horton


Redwood Durability in NZ – Can pure culture laboratory tests predict outdoor service life
2017 - IRG/WP 17-20610
Coast Redwood (Sequoia sempervirens) is an alternative species in New Zealand to the large scale Pinus radiata plantations. Redwood is classified as moderately durable but its durability is extremely variable. In order to reduce this variability in future stock, understanding growth conditions, clone, and tree age effects are important however this involves many samples and is not suitable for ass...
D O’Callahan, C Chittenden, J van der Waals, D Meason, T Singh


Moisture performance of wood determined in laboratory and field trials
2017 - IRG/WP 17-20621
It is widely accepted that wood moisture content (MC) is the key factor when it comes to durability of wooden structures exposed to weathering. The moisture performance of wood and wood-based products has been recognized as key element in wood durability and wood protection. Actually, it should be considered as major component of the material-intrinsic resistance of wood, but never found its way i...
D Kržišnik, N Thaler, B Lesar, M Humar


Testing of the resistance of acetylated wood against marine borers at three Italian sites
2017 - IRG/WP 17-30719
The aim of this research is the determination of resistance of acetylated wood against marine biodeterioration in use class 5 (EN 335) in temperate sea waters. The resistance of acetylated Pinus radiata (radiate pine) in solid and MDF form is compared with that of the untreated radiata pine and other untreated wood of European species such as Fagus sylvatica (European beech) Castanea sativa (chest...
S Palanti, M Faimali, D Tagliapietra, M Andrenacci, M Anichini, M Sigovini


Termite resistance of wood-plastic composites made with acetylated wood flour, coupling agent or zinc borate
2018 - IRG/WP 18-10917
There is little published scientific literature on the laboratory or field testing of wood-plastic composites (WPC) against termite attack. Therefore, the objective of this research was to investigate termite resistance (both laboratory and field) of 5 different extruded WPC blends of 50% western pine wood flour (WF) and high-density polyethylene (HDPE), and untreated pine solid wood. The study in...
R E Ibach, Y S Hadi, C M Clemons, S Yusuf


Impact of sapwood portions on the durability of adjacent heartwood of Pinus sylvestris, Pseudotsuga menziesii and Quercus robur. Part 1: Laboratory studies
2018 - IRG/WP 18-10922
Sapwood is generally considered as non-durable and assigned to durability class DC 5 according to European standards independent from the wood species. It is commonly agreed that sapwood decays faster than adjacent heartwood, but it is controversially discussed whether sapwood serves as feeder material and thus accelerates onset and progress of decay in more durable heartwood or decays independent...
C Brischke, P Homann, A Gellerich


Natural resistance of Bambusa vulgaris to termite and powder-post beetle attack in laboratory and graveyard tests
2018 - IRG/WP 18-10925
Deterioration is the major setback to the utilisation of bamboo products. To enhance bamboo utilization, an understanding of the level of resistance to degradation is important. In this study, level at which Bambusa vulgaris will naturally resistant attack by subterranean termites and powder-post beetles were evaluated. B. vulgaris aged 2, 3 and 4 years were subjected to attack by subterranean ter...
N A Sadiku, S O Bada


Testing the durability of timber products above ground using the block-test method – A critical review
2018 - IRG/WP 18-20637
The block-test method for testing the durability of wood and wood products above ground is reviewed critically with respect to practical aspects, moisture loads, corresponding decay development, and the possibilities of assessing test specimens by determining the dynamic modulus of elasticity (MOEdyn) of wood. In total, 36 blocks representing different modifications of the original set-up and a wi...
C Brischke, A Gellerich, H Militz


Above-ground testing methods – review of Rotorua, New Zealand test site results after ten years
2018 - RG/WP 18-20642
A series of seven different types of above ground durability tests were initially conducted over four years to determine which type of tests would give the fastest, most consistent results. Five types of test; ground proximity, two types of decking, flat panels and double layer, were reassessed after ten years. Exposure conditions varied between tests with ground proximity producing close to groun...
D Page, T Singh


Glueline fungicides in veneer based engineered wood products – updated results from laboratory work for the H1.2 hazard class in New Zealand
2018 - IRG/WP 18-30726
Results from New Zealand H1.2 ‘bin’ trials containing plywood glueline treated with triadimefon and cyproconazole were reported in 2012 (IRG/WP 12-30593). One of these trials has continued to the present day (2108) and updated results of this trial are reported. The triadimefon and cyproconazole glueline treatment continues to compare with, or outperform, the reference preservative used, bei...
A Siraa, K Day, B Kibby


Selection of heat flux value for wood fire retardants testing using MLC
2018 - IRG/WP 18-40846
One of more crucial elements of investigating treated wood combustion properties with the use of a cone calorimeter is a proper selection of heat flux (HF). The HF level is directly reflected in time to ignition and a thermal degradation degree. The ignition of raw wood or of wood ineffectively protected against fire occurs at a low HF level, i.e. 10-20 kW/m2. By contrast, the ignition of wood whi...
B Mazela, W Perdoch, W Grześkowiak, A Batista


Green Coloration of Wood in the Forest and Laboratory by Chlorociboria spp. – Applications for Furniture
2019 - IRG/WP 19-10947
Discoloration of wood caused by living saprophytic fungi is commonly found on lumber. These fungi do not destroy the integrity of wood, but the discolorations they cause are often considered undesirable. In Tunbrigde Wells (Great Britain), seldomly found green colored wood, usually considered commercially irrelevant, was valued for use in restoration of wood inlay artwork. The aim of this researc...
S Krause, W Unger, P Heydeck


Improvement of analytical methods of wood preservatives and its validation with collaborative testing
2019 - IRG/WP 19-20655
This discussion paper presents on-going collaborative test of analytical methods of wood preservatives according to the standardization process of Japan Agricultural Standard (JAS) by the Ministry of Agriculture, Forestry and Fisheries (MAFF). Food and Agricultural Materials Inspection Center (FAMIC) in close cooperated organization with the MAFF, has wide range of tasks about inspections and anal...
T Miyauchi, K Yamamoto, N Shota, Y Akabori, M Ikeda, J Eisawa, K Kambara, T Osawa, C Igarashi, Y Baba, W Ohmura, M Shimizu, M Samejima


Exploring the use of X-ray micro CT as a tool for the monitoring of moisture production and mass loss during lab-based fungal degradation testing
2019 - IRG/WP 19-20654
Bio-based building materials, such as wood and wood-engineered products, are susceptible to degradation by decay fungi. In-depth knowledge on the intricate material-fungus relationship as well as performance data for many bio-based building materials are still lacking, and especially knowledge on how a material’s structure and moisture properties affect the degradation process is missing. Althou...
L De Ligne, J Van den Bulcke, A De Muynck, J M Baetens, B De Baets, L Van Hoorebeke, J Van Acker


Performance of field cut preservatives above-ground and in ground contact exposures
2019 - IRG/WP 19-30742
Field cut preservatives are needed to protect cut ends and drill holes that expose the untreated interior of preserved wood. A series of field cut preservatives were assessed in ground contact and above-ground exposures. After 10 years in ground contact exposure, all of the untreated controls had failed or exhibited very advanced decay. In contrast, the copper naphthenate (2% Cu in mineral spirits...
R Stirling, D Wong


Previous Page | Next Page