IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water: Final report
1987 - IRG/WP 4133
Three timbers chosen as reference species were treated with 3, 6 and 10% solutions of CCA and CCB preservatives and exposed for up to 93 months at 8 tropical and temperate marine sites. Eleven local species treated in the same way were exposed at 4 of the 8 sites. There was no apparent difference in performance between CCA and CCB treated specimens. The severest test site was Panama Canal but mari...
R A Eaton


Biological control of decay in standing creosote-treated poles
1976 - IRG/WP 156
Internal decay caused by basidiomycetes in standing creosoted poles can be controlled biologically, it seems, by artificial inoculation near the ground line. For such inoculation IC-type facultative mycoparasites, Scytalidium sp FY strain or Trichoderma spp for example, may be used. Apparent residual action can be explained by the release of non water soluble chemically stable antibiotics from the...
J Ricard


An insight into brown rot decay of timber as revealed by 13C CP/MAS NMR
1985 - IRG/WP 1259
L E Leightley


Biological agents of timber degradation in Portugal. Marine borers
1991 - IRG/WP 4171
A brief report of the studies carried out in Portugal on marine borers is presented. The marine borers found in the portuguese coast are refered as well as the wood species where those organisms were identified. Emphasis is given to a study carried out from 1960 to 1975 at the Tagus estuary in Lisbon with the purpose, among others, of establishing the natural durability of different timbers....
J S Machado, L Nunes


Effects of the anaerobic wood decay bacterium Clostridium xylanolyticum on unbleached Pinus and Eucalyptus pulp
1991 - IRG/WP 1506
Clostridium xylanolyticum has been shown to produce extracellular enzymes capable of degrading wood. The present work was conducted to quantify growth on various lignocellulosic substrates and degradation of pulped wood fibre. In the latter tests Clostridium xylanolyticum was incubated at 35°C under anaerobic conditions in a medium containing 0.2% (w/v) peptone and 4% (w/v) unbleached Pinus and E...
G D Shelver, U Matai, W Van Wyk, A A W Baecker


Decay resistance of resin treated wood
1999 - IRG/WP 99-30206
Selected natural resin systems were evaluated for their potential as wood protecting agents according to standard test procedures. As indicated by the European standard EN 599 both a Basidiomycete test according to EN 113 and a ENV 807 soil bed test were carried out. Six resin treatments were tested using 3 concentration or treatment levels. Using the biocidal activity criteria as usually applied ...
J Van Acker, A J Nurmi, S M Gray, H Militz, C Hill, H Kokko, A O Rapp


Treatment of Douglas fir heartwood with disodium octaborate tetrahydrate (Tim-BorÒ ) to prevent attack by the Formosan subterranean termite
1991 - IRG/WP 1487
Toxicity of disodium octaborate tetrahydrate (Tim-BorÒ) to Coptotermes formosanus Shiraki (Isoptera: Rhinotermitidae), and termite feeding on treated Douglas-fir heartwood were evaluated in laboratory and field tests. Feeding on filter papers impregnated with Tim-BorÒ solutions reduced but did not eliminate termite gut protozoan populations. In a forced-feeding laboratory assay, Douglas-fir hear...
M Tamashiro, R T Yamamoto, J K Grace


Study of the natural durability and impregnability of a metropolitan species of tree
1986 - IRG/WP 2261
The current and predictable evolution of construction timber supply conditions is motivating research for a more efficient utilization of native woods. It is now important to determine statistically reliable impregnability values on a national scale, and to evaluate the natural durability of woods recently introduced in France, or economically important native woods....
M E Mathieu


A preliminary report on lignicolous marine fungi in the Java Sea, Indonesia
1982 - IRG/WP 488
This report is part of a study on the natural durability of Indonesian timbers against marine borers conducted in Pari Island waters, Java Sea (Suhirman and Eaton, 1981), and contains preliminary information which has not yet been published....
Suhirman, R A Eaton


Laboratory fumigations to determine the minimum temperature for methyl bromide eradication of the oak wilt fungus in red oak
1983 - IRG/WP 3243
Laboratory chamber fumigations of naturally-infected ret oak log sections exterminatet the oak wilt fungus in sapwood at temperatures down to 0°C. Only low, sporadic fungus survival was observed when log sections were gassed with methyl bromide at -5°C and aired for 4 da. at 0°C. Lower temperature treatments were not effective even if gas levels or exposure times were increased by 50%....
E L Schmidt


Wood decay in Danish buildings
1985 - IRG/WP 1261
At Technological Institute identification of fungi and advisory activity concerning repair of damages has taken place since 1935. Statistical analyses based on material from 1982 and 1983 are compared to earlier investigations worked out by L. Harmsen. The material shows that building traditions influence the diversity and frequency of fungal species. Many fungal damages in the last decade have sh...
A P Koch


Termiticidal effectiveness of synthetic pyrethroids, carbaryl and chlordane in wood-block test
1985 - IRG/WP 3356
The results of some wood-block tests with allethrin, permethrin, fenvalerate, carbaryl and chlordane against Coptotermes formosanus are tabled and compared against some organophosphates, chlorpyrifos, fenitrothion, phoxim, tetrachlorvinphos and acephate. The treatment of the wood blocks was exactly as described in Document No: IRG/WP/3330. Among the pyrethroids tested, permethrin was the most effe...
K Tsunoda


Implications for comparability of laboratory experiments revealed in studies on the variability in survival and wood consumption between colonies of Coptotermes acinaciformis (Froggatt) (Isoptera: Rhinotermitidae
1983 - IRG/WP 1196
(Summary of paper 1193) Groups of Coptotermes acinaciformis, originating from six colonies, three taken from each of two localities, 1500 km apart, in northern Australia (Townsville, Darwin) were kept at population densities of 0.005, 0.01 and 0.02 g termites/mL. Survival and wood consumption of the groups after 8 weeks followed a similar pattern in the colonies from both collection areas. Groups were least vigorous at the lowest population density; their performance reached a maximum at a population density of 0.01 g/mL. The subsequent decline in vigour was less marked as the highest population density was approached. However, the actual values for survival and wood consumption varied widely between colonies, irrespective of their origin. It is recommended that in all laboratory experiments which use survival and wood consumption as indicators of termite vigour, controls of a favourable as well as an unfavourable food type are included which would serve to monitor the vigour of the termites. Results from termite sources whose vigour falls below a certain threshold value would have to be treated with caution and could not be used in definative data, as e.g. in defining critical retentions of wood preservatives.
M Lenz


Seasonal effects of the field evaluation on wood preservatives against mold fungi
1996 - IRG/WP 96-20087
For the purpose of the amelioration of field test methods, commercial preservatives against mold fungi were tested under two different seasons, in winter and in summer. The specimens were bundled and set over the water bath and all these systems were covered with plastic film. At top of the system under film, black films for regeneration of sunlight were put in, and windows for changing air were r...
K Suzuki, Y Sugai, K Ryugo, D Watanabe


Monographic card: Coniophora puteana (Schum. ex Fr.) Karst. (Second draft)
1978 - IRG/WP 171
A Käärik


A selective-choice laboratory bioassay technique with Nasutitermes exitiosus (Hill) (Isoptera: Termitidae)
1983 - IRG/WP 1176
This paper presents a laboratory bioassay technique for simultaneous exposure of a variety of specimens to the same termite biomass. Details of the technique are given in a small scale selective-choice assessment with Nasutitermes exitiosus (Hill) in which timber species susceptibility is compared together with the efficacy of sub-lethal concentrations of protective compounds....
C D Howick, J W Creffield, P R Burridge


Proposals for collaborative work on laboratory soft rot testing
1986 - IRG/WP 2265
Proposals for collaborative experiments based on soil burial are presented. It is intended to study the use of defined horticultural loams with a view to obtaining more reproducability in laboratory soft rot tests....
D J Dickinson, S M Gray


Estimation of service life of durable timber species by accelerated decay test and fungal cellar test
2002 - IRG/WP 02-20249
Many kinds of durable wood species for outdoor uses has been imported from all over the world to Japan. However information on the natural durability of these species is not sufficient to estimate the service life of them in the climate of Japan. Highly durable species such as Jarrh, Teak, Ipe, Ekki, Selangan batu, Red wood, Western red cedar showed no significant percent mass losses by accelerate...
K Yamamoto, I Momohara


In ground contact field trial results of preservative treated incised and unincised spruce
1996 - IRG/WP 96-40076
Field trials of treated spruce stakes have been demonstrated that incising the stake before treatment improves the preservative uptake both for CCA and creosote. This results in a substantially extended service life for the incised stakes over the unincised stakes for preservative concentrations at commercial levels. After 24 years in ground contact the majority of incised spruce samples are sound...
E D Suttie


Studies on the preservation of structrual plywood - Part 1: Decay resistance of structural plywood
1974 - IRG/WP 238
The weight loss and the decreases in the compression strength and in the modulus of elasticity were measured to determine the decay resistance of structural plywood (lauan). Test pieces (50x25xA mm³) were exposed to the wood destroying fungi (Coriolus versicolor and Coriolellus palustris) for 2-3 or 2-4 months. After exposure, the measurement of the compression strength was carried out on the pie...
K Minami, Y Kenjo, S Sugiyama


Lignin-copper, a new wood preservative without arsenic and chromium
1992 - IRG/WP 92-3702
A more environmentally sound treatment for wood with preservatives containing no arsenic or chromium, has been developed and studied on a laboratory scale. The method involves a first step impregnation with an aqueous solution containing modified, water-soluble kraft lignin followed by a second step involving impregnation with a copper salt solution to give fixation of the lignin into a water-inso...
B Ohlsson, R Simonson


A new approach to the maintenance of wooden railway sleepers. (Second report)
1988 - IRG/WP 3492
The microenvironment and micro-ecology of wooden railway sleepers was investigated to assess their condition to determine the necessary treatment, repair and replacement criteria. In this report the efficacy of the secondary preservative treatment with solid boron rods is discussed and the development of an in-situ, nondestructive test method based on the creation and assessment of structural dyna...
W Beauford, P I Morris, A M Brown, D J Dickinson


Detection of incipient brown rot decay in wood by fourier transform infrared spectrometry
1987 - IRG/WP 2275
Fourier transform infrared spectrometry was evaluated as a possible method for detecting different levels of brown-rot decay in pine sapwood. By using first derivative spectra and regression analysis, an equation based on 4 absorption peaks, normalized with an internal standard peak, was developed. The correlation between weight loss and absorption was highly significant indicating that this is a ...
D D Nicholas, T Schultz


Sub-group on Basidiomycete tests: Proposals for Sub-group programme of work
1979 - IRG/WP 2127
During the IRG 10 Meetings in Peebles, Scotland in September 1978, it was resolved to establish within Working Group II a sub-group on testing wood preservatives against basidiomycete fungi. The terms of reference and scope of the sub-group's activities were to be determined by consensus among members who registered an interest. Dr A F Bravery (PRL, UK) was asked to act as co-ordinator. D...
A F Bravery


Protection of Ochroma pyramidale from fungal decay with N,N-napthaloylhyroxylamine
1998 - IRG/WP 98-30182
Fungal decay of wood in service results in billions of dollars (U.S.) in losses annually. Recent environmental restrictions, both U.S. and international, are limiting and eliminating the use of broad-spectrum, heavy metal biocides for wood preservation. Restrictions result primarily from problems with disposal. New wood preservatives need to be developed and tested which specifically target key el...
F Green III, T L Highley