Evaluation of the effectiveness of Tuff Brite C in the control of sapstain in laboratory and field tests
1992 - IRG/WP 92-3718
Since 1990, the anti-sapstain product Tuff Brite C (ASC 66898) has been evaluated internationally in laboratory and field tests, and has been commercially introduced in New Zealand. The product is an aqueous flowable formulation of chlorothalonil and carbendazim. Efficacy tests which have been carried out in New Zealand, Australia, USA, South Africa and Europe are described and summarized. Tuff Br...
T L Woods, C J Klaver


Performance of proprietary formulations of anti-sapstain preservatives on Hevea brasiliensis timbers in laboratory tests
1989 - IRG/WP 3532
A total of 10 proprietary and two experimental formulations were assessed for their effectiveness against sap-stain caused by Botryodiplodia theobromae on Rubberwood (Hevea brasiliensis). Sterilized wood samples 5x20x40 mm³ were dipped in the test chemicals for 60 seconds and then inoculated with 0.5 ml of culture filtrate of Botryodiplodia theobromae for incubation in sterile, damp petri dishes....
L T Hong


Exposure of preservative treated wood to terrestrial microcosms, pure cultures of fungi and in the field
1997 - IRG/WP 97-20114
Small stakes (5x10x100 mm3) of treated and untreated Pinus sylvestris sapwood were exposed in terrestrial microcosms with different soils, two taken from test fields in Sweden, one soil from a conifer forest and one garden compost soil. Stakes of the same size were also exposed to pure cultures of the brown and white rot fungi, Postia placenta and Phanerochaete chrysosporium. After exposure, weigh...
M-L Edlund


Evaluation of a laboratory soft rot test on basis of weight loss and residual strength
1989 - IRG/WP 2336
Based on the principles of different previously reported experimental procedures dealing with laboratory soft rot testing, a study was conducted on treated poplar and beech. Preservatives used were CCA, CCF, AAC, Azaconazole and TCMTB. Treated samples were exposed for three months in a vermiculite substrate to Chaetomium globosum. Evaluation was based on absolute mass loss, percentage weight loss ...
W Verbeke, J Van Acker, M Stevens


Preservation of coppice wood for the fabrication of glued beams or panels
1987 - IRG/WP 3427
In this survey we will examine the specific problems concerning the conservation and the preservation of timber (issued from trunks of small diameter corresponding to products of clearings or coppices) destined for the fabrication of solid reconstituted elements. Thus for six metropolitan species of wood, we first characterized the biological deteriorations which occur after felling and their kine...
G R Y Déon, R Schwartz


The movement of iron into field test stakes
1987 - IRG/WP 2284
Failed and sacrificial stakes recovered from the Westham Island field test site were examined for their iron content. Varying amounts were recorded, which were greatest in the failed stakes. The possible role of the iron taken up by the below ground portion of the stakes, in accelerating the decay process and/or the preservative leaching is under investigation. The reaction of the iron with the ch...
J N R Ruddick, P I Morris


Studies in an accelerated soil bed facility on the decay susceptibility of U.K. grown spruce and pine poles treated with copper/chrome/arsenic (CCA) by pressurised sap-displacement. Part 1: Setting up of soil beds and initial soft rot results
1990 - IRG/WP 2344
The paper describes the methodology used in the construction and early operation of an accelerated soil bed facility used to examine the decay susceptibility of U.K. grown Scots and Corsican pine and Sitka and Norway spruce treated with C.C.A. by high pressure sap-displacememt. The design and control of the facility as well as the preparation, soil exposure and soft rot decay analysis of quarter p...
A Bruce, S D Hainey, G M Smith, B King, P D Evans


A 53-year old field trial to evaluate the performance of a range of chemical treatments on eucalypt poles
1989 - IRG/WP 3526
Hardwood pole stubs of Eucalyptus maculata, Eucalyptus pilularis, Eucalyptus saligna and Eucalyptus paniculata were examined for termite attack and fungal decay after 53 years in ground contact. The trial compared eight different chemical treatments with untreated pole stubs of the four species investigated. Untreated Eucalyptus paniculata, a Class I durability species, performed particularly well...
R S Johnstone, R A Eaton


Depletion of preservatives from treated wood: Results from laboratory, fungus cellar and field test
1993 - IRG/WP 93-50001-07
This paper compares results of preservative component losses using a range of test procedures with several different water-borne preservatives. The data shows that laboratory leaching tests are in some cases comparable to, but in other cases significantly underestimate preservative component losses when compared with field or fungus cellar depletion tests. The results also suggest that preservativ...
L Jin, A F Preston


Laboratory evaluation of AC 217,300 as a termiticidal dust
1983 - IRG/WP 3247
Laboratory bioassays are described with the amidinohydrazone, AC217,300, a candidate termiticide to replace arsenic trioxide in termite control. When used as a dust and topically applied, AC217,300 was toxic to Coptotermes acinaciformis and Mastotermes darwiniensis. Although arsenic trioxide dust causes faster mortality in Coptotermes acinaciformis than AC217,300 dust, the latter has lower mammali...
J R J French, P J Robinson


Moisture content and other tested values in. Double layer tests of different size in Lithuania and Germany
2004 - IRG/WP 04-20299
The paper presents measurement results of moisture content and the analysis of durability trial of double layer wood in variants of varying size, conducted in Girionys, Kaunas distr., Lithuania and in Hamburg, Germany. In this trial 3 sample sets of varying size, containing 25, 50 and 100 specimens, are used. The aim of this trial is to ascertain an optimal number of test specimens. The dynamics o...
J Saladis, A O Rapp


Collaborative soft rot tests: Specific gravity loss resulting from soft rot
1973 - IRG/WP 227
It was proposed at the 5th meeting of Working Group II of the IRG in June 1973 in Lahti, Finland, that the specific gravity (swollen volume basis) of test blocks used in the IRG Collaborative Soft Rot Tests should be determined on all the blocks at the completion of the exposure period. Specific gravity determined on the basis of the oven dry weight and water swollen volume was selected because (1...
C R Levy


Bethoguard; A new wood protecting fungicide for use in metal free ground contact wood preservatives
2002 - IRG/WP 02-30301
Research has identified the limitations in both the spectrum of activity and permanence of organic biocides placed in wood in high hazard environments, particularly in the absence of heavy metals such as copper. More specifically, the control of soft rot decay in wood in soil contact has proven to be most problematic. The new organic biocide, Bethoguard; an oxathiazine, has demonstrated excellen...
S C Forster, G R Williams, M Van Der Flaas, M Bacon, J Gors


Soft rot - Soil burial - Tests. Influence of the addition of nitrogen compounds to the soil on wood decay by soft rot
1972 - IRG/WP 213
The decay of wood specimens buried in soil is influenced by various factors. Decisive are the water content, the content of organic substances, the pH-value, the content of mineral nutritive salts, nitrogen content, etc. of the soil. These tests were carried out in order to investigate if the decay of wood in the soil will be influenced by additions of various nitrogen-compounds in different conce...
O Wälchli


Leaching tests on CCA-treated wood using inorganic salt solutions
1984 - IRG/WP 3310
Pinus radiata sapwood treated to approximately 10 kg/m³ with Tanalith NCA or Tanalith C-type CCA preservatives was ground to a fine powder and samples were then leached with solutions of calcium chloride, calcium nitrate, magnesium nitrate, or a mixture of potassium di-hydrogen orthophosphate and di-potassium hydrogen orthophosphate, at 0.03M-1.00M solution concentrations. Leached wood samples we...
D V Plackett


Suitability of different termite species for laboratory testing
1982 - IRG/WP 1159
Different termite species were tested in the laboratory to evaluate the effectiveness of insecticides and wood preservatives in wood against termite attack. Determined were the optimum group size and composition, the matrix (vermiculite) volume and its moisture content. Choice feeding tests with fully impregnated wood blocks which are carried out according to a modified EN 117 procedure for Reticu...
U Kny, H Kühne


Methods of testing anti-stain chemicals for protecting sawn timber during storage and transport
1976 - IRG/WP 273
No international standard method for testing anti-stain chemicals for protecting fresh sawn timber exists. The methods used can be divided into three types: a) Rapid screening tests for finding chemicals effective against blue-stain and mould fungi. The chemicals are tested in agar medium, in pieces of filter paper or on small pieces of wood using pure cultures. b) Laboratory tests for evaluating ...
T Vihavainen


Decay rates and strength and stiffness loss in foundation beams
1992 - IRG/WP 92-1563
The TNO Centre for Timber Research has executed an extensive research programme into the rate of decay in foundation beams, as a result of lowering of ground water tables. The aim of the research was to develop a method, predicting the decrease in strength and stiffness in beams, due to wood decay during drytime of foundation beams. With the calculated extremes in decay, the damage caused by local...
P Esser, H S Buitenkamp


Resistance of board materials against fungal decay: A comparative experiment on Kolle flask tests method and direct test method
1985 - IRG/WP 2243
Two sets of plywood (Aucoumea klaineana Pierre) 7 and 11 ply, treated by two preservatives, and untreated, were tested by two methods: 1. Kolle flask test method on malt-agar substrate according to the French standard NF B 51.295; 2. A direct test method in non sterile conditions according to DocNo: IRG/WP/2214. The exposure time far both methods was 12 weeks. After exposure, the degree of attack ...
G R Y Déon, L N Trong


Laboratory tests on the residual effects of pyrethroids against termites thirteen years after application
1994 - IRG/WP 94-30056
This paper is in continuation to a series of articles published on the work being developed in Brazil regarding the feasibility of using photostabl synthetic pyrethroids against termites. Tests were carried out to compare the efficacy of five synthetic pyrethroids with the traditional organo-chlorinated pesticide, chlordane. Wooden blocks were impregnated with alcohol-based solutions of the above-...
A M F Oliveira


Performance of above ground decay test units treated with a substituted isothiazolone
1989 - IRG/WP 3503
RH 287, a substituted isothiazolone, was evaluated for efficacy against decay fungi in an above ground test in Mississippi. After 45 months of exposure, all test units that were pressure treated with this biocide at levels of 0.026 pcf and higher have no deterioration. In addition, the test units that were dip-treated with a solution concentration of 0.5% also have no deterioration. Compared to pe...
D D Nicholas, J A Wilson, D E Greenley


Acoustic technique for assessing decay in preservative treated wood
1998 - IRG/WP 98-20138
This study investigated the suitability of vibration techniques to assess the performance of wood preservatives in ground contact. Small stakes (10 x 5 x 100 mm3) of treated and untreated Scots pine sapwood were exposed to decay in lab-scale terrestrial ecosystems. Tests were conducted using three different soils including a garden compost soil, and soils obtained from a test field and a conifer f...
L Machek, M-L Edlund, R Sierra-Alvarez, H Millitz


Laboratory evaluation of disodium octaborate tetrahydrate (TIM-BORÒ ) as a wood preservative or a bait-toxicant against the Formosan and eastern subterranean termites (Isoptera: Rhinotermitidae)
1991 - IRG/WP 1513
A no-choice bioassay indicated that termite feeding was significantly reduced when wood was treated with TIM-BORÒ at retentions of >3600 ppm and >900 ppm (w/w) for Coptotermes formosanus and Reticulitermes flavipes, respectively, and thus these wood preservative retention rates may be considered for these termite species. Results of a choice bioassay suggested retention rates of 450-1800 pp...
N-Y Su, R H Scheffrahn


New Observations and Interpretation for Tunnelling Bacteria Decay
2006 - IRG/WP 06-10579
Decay micromorphology was studied systematically for diversely preservative treated Pinus radiata and Fagus sylvatica 20 x 20 x 500 mm stakes across 13 in-ground field test sites, during a 6.5 year exposure. Sites were selected to maximise occurrence of a diverse range of decay types. Micromorphology that suggested orientation of tunnelling bacteria with the cellulose microfibrils of the S2 and S1...
R Wakeling


Common Decay Micromorphology “Anomalies” Challenge Current Decay Classification
2006 - IRG/WP 06-10578
Decay micromorphology was studied systematically for diversely preservative treated Pinus radiata and Fagus sylvatica 20 x 20 x 500 mm stakes across 13 in-ground field test sites, during a 6.5 year exposure. New insight into the micromorphology of the early stages of decay enabled new and more detailed interpretation of the mechanism of their formation and suggested that current decay classificati...
R Wakeling