Aesthetic service life of coated and uncoated wooden cladding - influencing factors and modelling
2011 - IRG/WP 11-20470
Mould growth on exterior coated cladding façades is an undesirable element and will often shorten the aesthetical service life. Mould growth on painted surfaces is influenced by type and concentration of film fungicides, the paint formulation and the wood substrate itself, and wooden cladding may experience exponential fungal deterioration caused by variation in the climatic factors, often within...
L Ross Gobakken, O A Høibø


Termite resistance of timber envelope treated with imidacloprid then modified by typical building site operations
2011 - IRG/WP 11-30570
Imidacloprid is a new envelope insecticide approved by Australian regulatory authorities for framing timber. It is a non repellent insecticide. Results are reported for timber envelope treated with imidacloprid and altered post treatment with typical building site operations to expose untreated surfaces. These modifications included, cutting, notching and drilling. Pinus radiata timber samples w...
K Day, A Siraa, P Lobb


Effectiveness of Water Based Bentonite-Borate Slurry for In-situ Remedial Protection of Historic Wooden Piles: The Eurobor Protocol, Part 2
2011 - IRG/WP 11-30574
The study of the biocide product Eurobor®, water mixture of boric acid, borax and sodium bentonite, aimed to verify previous findings regarding borates penetration from a clay-water mixture of foundation timber. The product was applied on samples from 100 year old timber foundation from the city of Göteborg. Although in ground for this long the timber was in acceptable god condition due to groun...
M. Theorin, K. Fimmerstad, K-M. Bandh


The Effectiveness of Machined Profiles at Reducing the Checking of Wooden Decking
2011 - IRG/WP 11-40541
This study tests the hypothesis that ‘the ability of surface profiling to reduce checking of deck boards exposed to weathering will vary with wood species and profile type’. Southern pine (Pinus sp.) and Pacific silver fir (Abies amabilis) deck boards were machined to produce three different types of surface profiles: flat (control), ribbed (V-shaped grooves), and rippled (U-shaped grooves). B...
P Evans, I Cullis, P Morris


A Critical Review and Survey of the US Wooden Pallet Industry: Focusing on Market Segmentation & N. American Trends
2011 - IRG/WP 11-40545
This paper reviews the history and current and predicted future use values in N. America. Included in this work is historical data on rationality and wood species used to manufacture wooden pallets in the USA and an ongoing current market survey sent to the 1000 largest manufacturers and re-manufacturers in the USA based on SIC Code 2448(Standard Industrial Code Classification). Although CHEP, the...
M H Freeman


The overview of ISPM 15 implementation in Croatian wood-working companies
2011 - IRG/WP 11-30576
Croatia is a small European county, but in the same time a great country according to it’s tradition in the forestry and wood working industry. However, around 48% of it’s territory is afforested. As the export is one of the main directions in the Croatian development conception, the production and distribution of wood package intended for the international trade, is one of the most important ...
R Despot, V Jambrekovic, M Hasan


In-situ experimental treatment and consolidation of degraded timber elements from a XIX century building
2012 - IRG/WP 12-10767
This paper presents the in situ experimental conservation work performed on three timber structural elements from a XIX century building: two floor beams and one roof beam. The palace was built in 1877 in the centre of Lisbon initially with residential purposes. It has four floors, with timber structural horizontal elements, stairs and roof beams (generally of Pinus sylvestris L.). The exterior wa...
D F Henriques, J de Brito, L Nunes


The Significance of Natural Durability of Croatian Mediterranean Wood Species for their Traditional and Present Protection Methods and Use
2012 - IRG/WP 12-10770
The aim of this article is to contribute to the better cognition of the protection and use of some most important Croatian autochthonous Mediterranean wood species. Their traditional use and protection are observed by two aspects. The first one is the presence of these species in the Croatian Mediterranean regions for many centuries, and the long tradition of their use, regardless of their natural...
R Despot, M Hasan


Effects of microclimate, wood temperature and surface colour on fungal disfigurement on wooden claddings
2012 - IRG/WP 12-20490
Wooden claddings are common in façades in Norway, and Norway spruce (Picea abies) is the most frequently used species. The cladding is a major part of the facade, and it has visual requirements that may define the aesthetic service life. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more of...
L Ross Gobakken, G I Vestøl


Comparative studies on the moisture performance and durability of wooden facades
2012 - IRG/WP 12-20492
Wooden claddings are traditionally used in many parts of the world. Also modern structures are frequently made from timber and timber engineering panel products. However, wood has to compete with other cladding materials and its durability needs to assure sufficient functional and aesthetic service life. Besides many other factors the durability of a wooden facade is dominated by its moisture perf...
T Bornemann, C Brischke, J-M Lück


Performance superiority of CCA-C treated wooden jetty poles and piles used for 30 years in Bangladesh against marine borers
2012 - IRG/WP 12-30582
Observational study along with previous investigation and records revealed that chromated copper arsenate type C (CCA-C) impregnated southern pine poles and piles of jetty constructed in most vulnerable brackish water in Bangladesh are stable and resistant to attack of all types of marine borers after 30 years of use. It is evident from the service records of other construction materials that CCA-...
A K Lahiry


Recommendations for handling of mold infestation of wooden artifacts
2012 - IRG/WP 12-10790
The presentation gives an overview of the handling of wooden artifacts with mold infestation. The causes of mold deterioration are demonstrated by investigations in a church, a historic library and a monastery in Germany. Investigated infested wooden artifacts were altars, sculptures, picture frames and sarcophagi. Important investigation methods including indoor climate measurement, material an...
K Plaschkies, B Weiss, W Scheiding


Wood Aging. Characteristics of aged Hinoki wood from Japanese historical buildings
2012 - IRG/WP 12-40610
Wood has always played a major role in Japanese traditional culture. More than 90% of buildings listed as a National property or a nationally important cultural property of Japan are constructed with wood. In the ancient capitals Kyoto and Nara, many traditional wooden buildings were inscribed as World Cultural Heritage of the UNESCO. The most famous and the world’s oldest wooden construction st...
M Yokohama, S Kawai


Wood-leather panels – A biological, fire retardant building material
2012 - IRG/WP 12-40615
The poor flame retardant properties of wood-based products are among the severest obstacles, hindering its use in the commercial building sector. Recently, some attempts to improve the fire properties, relying on inflammable salts or reactive halogen compounds, have been presented, although they either cause problems with machining or embody harmful compounds (halogen derivates). In this paper, ...
S Wieland, U Stöckl, T Grünewald, S Ostrowski, A Petutschnigg


Communities of mold fungi on flooded building materials
2013 - IRG/WP 13-10799
A small building built to residential code was flooded using farmland pond water to a depth of two feet at Tuskegee University. The building was drained and left enclosed for an additional three weeks. A total of 168 material samples were removed either immediately after opening (wet) or seven months after flooding (dry). Wall materials sampled included fiberglass batt insulation, gypsum wallboard...
F Skrobot III, H Aglan, S V Diehl


Climatic impacts on the moisture performance of wooden decking and facades
2013 - IRG/WP 13-20518
In outdoor usage wood is exposed to a variety of influences, which reduce its durability against biological deterioration and wetting. Besides many other factors the service life of wooden facades and cladding is dominated by occurring moisture loads on the one hand and their capability to withstand moisture on the other hand. Hence, climatic factors have a direct impact on the material climate an...
T Bornemann, C Brischke, G Alfredsen


Method for determining the critical moisture level for mould growth on building materials
2013 - IRG/WP 13-20530
The natural conditions of relative humidity (RH) and temperature (T) in different parts of a building is rarely constant over time. Instead, RH and T often vary cyclically and may pose a risk of mould growth as these conditions are the two key environmental parameters that controls mould growth. Consideration to both humidity and temperature conditions and the susceptibility to mould in a material...
A Ekstrand-Tobin, P Johansson, G Bok


The effects of impregnation with secondary metabolite extracted from Ipe on durability of Japanese cedar and beech wood
2013 - IRG/WP 13-30618
Ipe wood is known for its high durability; it has been widely used in exterior structures that are exposed to the weather. In this paper, to increase the durability of less durable wood, Japanese cedar and beech specimens were impregnated with a secondary metabolite from Ipe. In a previous study, secondary metabolites extracted by a Soxhlet extraction method showed antifungal properties. Therefore...
T Iida, R Konuma, K Kawarada


Protective effectiveness of antifouling coatings for wooden boats in the Northern Adriatic Sea
2013 - IRG/WP 13-40634
There are various conventional biocide containing antifouling coatings and some more environmentally friendly paints for boats on the market. However, the question of their performance in accordance with the manufacturers’ statements or guaranties arises. The aim of our preliminary investigation was to state which type of antifouling coating exhibits better effectiveness against fouling organism...
M Petrič, M Humar, J Adamek, B Kričej


Communities of mold fungi in moisture damaged building materials
2014 - IRG/WP 14-20542
The critical conditions needed for the development of mould and decay fungi have been modelled for different building materials. However, current knowledge of indoor microbes growing on building materials relies on culture-based methods and more advanced molecular biological techniques should be employed to study the complex microbial communities in building materials. In this paper molecular biol...
E Sohlberg, H Viitanen


The development of accelerated test systems to evaluate the durability of framing timber
2014 - IRG /WP 14-20547
Various accelerated decay resistance trials including small simulated wall units, samples exposed in enclosed tanks and ‘I’ samples in stacks have been explored and used to test the durability of treated and untreated radiata pine framing at Scion since 2001. These testing methods have been established to determine the effectiveness of commercial formulations in preventing decay in framing sub...
T Singh, D Page, J van der Waals


On-site remediation treatments for framing timber in leaky buildings
2014 - IRG/WP 14-20549
Weathertightness failures in New Zealand buildings due to the combined effects of cladding choices, design and construction faults and the use of untreated framing timber has led to the so called ‘leaky building syndrome’. The latest estimated cost of the leaky building crisis in New Zealand is about NZ$11 billion. This research was conducted to provide a better understanding of the option...
T Singh, D Page, A Bennett


Study on Biological Distribution to Conserve the Tripitaka Koreana woodblocks in Haeinsa Temple
2015 - IRG/WP 15-10844
Tripitaka Koreana is the Wood-carved Buddhist scriptures which were made in 13th century. And Janggyeong Panjeon that is depository for the Tripitaka Koreana was built in 15th century. In recent days, biological damage becomes a serious problem to wooden cultural heritage including historical wooden buildings with global warming. In this study, termite monitoring on whole Haein-sa temple area and ...
Si Hyun Kim, Hyun Ju Lee, Yong Jae Chung


Applicability of wood durability testing methods to bio-based building materials
2015 - IRG/WP 15-20561
It is well known that organic materials may be susceptible to attack from a range of fungal organisms and any bio-based material used in locations where there is the possibility of microbiological activity must be expected to be able to withstand or prevent such attack. There are a wide range of test methods and standards in place to test susceptibility although most of these test individual compo...
S F Curling, B K Stefanowski, E Mansour, G A Ormondroyd


Performance of bio-based building materials – viewpoints from the first year of COST Action FP1303
2015 - IRG/WP 15-20572
Maintaining and expanding the market potential for bio-based building products in indoor and outdoor construction uses remains a key activity for industries in the forestry and biotechnological sector, particularly in Europe. Whilst there are ongoing activities within IRG for collecting and populating a database on performance on wood, the performance data for many other (i.e. non-wood) "environme...