Degradation of the normal fibre walls of rubberwood (Hevea brasiliensis) by the tropical blue-stain fungus Botryodiplodia theobromae
1998 - IRG/WP 98-10286
Rubberwood was examined by light microscopy and transmission electron microscopy (TEM) after exposure to the common tropical sapstain fungus Botryodiplodia theobromae for four weeks to study hyphal colonisation of wood cells and to determine if this fungus also degraded lignified normal fibre cell walls in addition to the walls of non-lignified elements. Light microscopy revealed relatively large ...
A A H Wong, A P Singh


TBTO absorption and penetration in pine joinery treated by various processes
1989 - IRG/WP 3523
Matched sections of several White pine (Pinus strobus) and Ponderosa pine (Pinus ponderosa) mouldings were treated with TBTO by Double vacuum, modified empty-cell, 15 second dip and several preheating treatments followed by a 15 s dip treatments. As expected the double vacuum and empty-cell (batch) treatments resulted in much greater retentions and penetrations than the dip treatments. The absorpt...
P A Cooper, Y T Ung


The isolation of actinomycetes from wood in ground contact and the sea
1980 - IRG/WP 1110
M S Cavalcante, R A Eaton


Detection of incipient brown rot decay in wood by fourier transform infrared spectrometry
1987 - IRG/WP 2275
Fourier transform infrared spectrometry was evaluated as a possible method for detecting different levels of brown-rot decay in pine sapwood. By using first derivative spectra and regression analysis, an equation based on 4 absorption peaks, normalized with an internal standard peak, was developed. The correlation between weight loss and absorption was highly significant indicating that this is a ...
D D Nicholas, T Schultz


Agenda WG Ib
1988 - IRG/WP 1372
IRG Secretariat


Agenda WG II
1972 - IRG/WP 207
IRG Secretariat


Collaborative soft rot test: Amended test method
1972 - IRG/WP 208
The initial draft of a standard test method (Document IRG/WP/201) was discussed at the meeting in Brussels in 1971. It was agreed that a revised draft should be prepared and that the Princes Risborough Laboratory (formerly FPRL) should conduct a trial test using the method as a preliminary to the main collaborative test....
J G Savory


Some relationship between physical characteristics and treatability of Bolivian woods
1987 - IRG/WP 3434
Using the available data on physical characteristics of 25 Bolivian woods, some relationships between porosity, specific gravity and treatability (hot and cold open tank process with 5% pentachlorophenol) were analysed. The aim of this report is to give information on technical characteristics of Bolivian hardwoods which have been studied in this country by Centro de Desarrollo Forestal and in Per...
A S Viscarra


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. 3rd Interim Report
1983 - IRG/WP 4101
This paper updates the results of microbiological examination and marine borer assessment of untreated wood samples (15 x 2 x 2 cm³) and samples treated with 3, 6 and 10% CCA and CCB preservatives. Three reference species - Alstonia scholaris, Fagus sylvatica, Pinus sylvestris were used at all the test sites in addition to local species chosen by participants in the test....
R A Eaton


Fungi associated with groundline soft rot decay in copper/chrome/arsenic treated heartwood utility poles of Malaysian hardwoods
1992 - IRG/WP 92-1567
Copper-chrome-arsenic treated heartwood from Malaysian hardwood utility poles in service for 8-23 y at two localities in the wet tropical Peninsula Malaysia were surveyed for soft rot in the ground-contact region. Soft rot decay was detected in all the poles. Isolation studies indicated the ability of a variety of microfungi and basidiomycetes to colonize treated heartwood. Most isolates exhibited...
A H H Wong, R B Pearce, S C Watkinson


A collaborative test to determine the efficacy of poyurethane coatings on wood samples exposed in the marine environment. 1st Interim Report
1988 - IRG/WP 4145
Wood samples coated with elastomeric polyurethane (ca. 50 mils thick) were exposed for up to 2 years in 12 tropical and temperate marine test sites with known teredinid, pholad and/or crustacean infestations. All uncoated control samples were destroyed or partially destroyed. Polyurethane-coated samples were not attacked, the surfaces of the coating were sound and the polyurethane adhered well to ...
R A Eaton


Natural durability of some common Indian timbers and marine plywood against biodeterioration in Kochi waters (India)
1992 - IRG/WP 92-4177
Panels of thirty-eight timber species and marine plywood were tested in Kochi harbour (South-west India) for periods ranging from 3 to 21 months, so as to evaluate their natural resistance against marine borers. Results indicate that all the timber species studied are non-durable, 6 of them having undergone more than 50% internal destruction within 3 months; 14 species in 6 months, 13 species and ...
L N Santhakumaran, M V Rao


Minutes of the meetings of WG I
1983 - IRG/WP 1218
IRG Secretariat


Agenda WG II
1985 - IRG/WP 2245
IRG Secretariat


Minutes of the meetings of WG Ia
1985 - IRG/WP 1275
IRG Secretariat


Minutes of the meetings of WG II
1978 - IRG/WP 2122
IRG Secretariat


An investigation to assess the feasibility of developing an accelerated laboratory test to determine the abrasion resistance of lesser-used timber species for use in marine constructio
2005 - IRG/WP 05-20317
The paper describes the evaluation of a laboratory-accelerated test to compare the shingle abrasion resistance of current and potential timbers for use in marine construction. Useful results were achieved in 47.5 hours, but identified a number of issues to be resolved for the test to be refined and the subsequent results to be interpreted correctly....
G S Sawyer, J R Williams


1970 Official Photo
1970 -
IRG Secretariat


Observations on the penetration of preservatives into green timber
1985 - IRG/WP 3335
Differences in the rate and extent of diffusion of MBT and NaPCP-based preservatives following a short dip treatment were observed. The importance of preservative distribution as well as toxicity to the target organisms in governing the ultimate performance of any anti-sapstain compound is discussed....
G R Williams, R A Eaton, D A Lewis


Sap displacement treatment of utility poles in Papua New Guinea
1977 - IRG/WP 3102
Rapid growth of rural electrification in P.N.G. has created a considerable demand for treated poles. In the past power lines have been run on steel poles but the Government of P.N.G. is now seeking to make maximum use of the country's own resources rather than continue to rely upon imported materials such as steel poles. To some extent, this demand is being met by expansion of existing va...
C R Levy


Antifungal properties of new quaternary ammonium and imidazolium salts against wood decay, staining and mould fungi
2004 - IRG/WP 04-30347
The biological activity of twenty-four potential wood preservatives – imidazolium and quaternary ammonium salts with a modified anion structure was determined employing screening agar-plate and agar-block methods. Experiments were carried out on Scots pine (Pinus sylvestris L.) wood. The aim of the performed studies was to investigate the effect of structure modification of IC and QAC with organ...
J Zabielska-Matejuk, W Wieczorek


Environmental behaviour of treated wood in (semi-)permanent contact with fresh or seawater
1998 - IRG/WP 98-50101-20
This study presents a strategy for the environmental toxicity evaluation of treated wood towards the aquatic compartment, using non target water organisms toxicity tests. A lixiviation process is applied on wood (Pinus sylvestris) treated with several wood preservatives formulations. The lixiviation process is carried out in the laboratory with ultrapure water or synthetic seawater. After chemica...
P Marchal, C Martin


An experimental method to simulate incipient decay of wood by basidiomycete fungi
2000 - IRG/WP 00-20200
At very early stages of decay of wood by basidiomycete fungi, strength loss can be measured from wood before any measurable weight loss. Therefore, strength loss is a more efficient measure of incipient decay than weight loss. However, common standard decay tests (e.g. EN 113 or ASTM D2017) use weight loss as the measure of decay. A method was developed that allowed progressive removal of samples ...
S F Curling, J E Winandy, C A Clausen


Budget for 2003, forecast May 2003
2003 - IRG/WP 03-60172
IRG Secretariat


WG I Sub-group 4 Termite problems: Documents before the meeting
1983 - IRG/WP 1215
IRG Secretariat