Which fungi cause sapstain in Canadian softwoods?
1998 - IRG/WP 98-10285
The Canadian forest products industry suffers considerable losses in revenue due to fungal stains. There is an increased awareness that more complete knowledge about the causal organisms might help solve the problem. A first step was to initiate a thorough survey of bluestain fungi in Canada. Systematic sampling was done at seven selected sawmills in six Canadian provinces. In summer 1997 fresh lo...
A Uzunovic, Dian-Qing Yang, P Gagné, C Breuil, L Bernier, A Byrne
Annual Report 1998
1999 - IRG/WP 99-60115
IRG Secretariat
Errata in Document NO: IRG/WP/472
1981 - IRG/WP 483
L N Santhakumaran, J C Jain
Proposal for further work on accelerated ageing
1988 - IRG/WP 2314
M-L Edlund
Microbiological degradation of wooden piles in building foundations
1988 - IRG/WP 1370
White rot, soft rot and bacterial attack have been detected in softwood piles under buildings. In some cases bacteria were found to be the main degradation organisms in the studied piles. The water content of degraded piles was very high. The compression strength was quite low also in the piles deteriorated by bacteria. The density of wood was very variable, and the degree of degradation could not...
L Paajanen, H Viitanen
Abstracts of some papers and posters promised for IRG 26, Part 2
1995 - IRG/WP 95-60061
IRG Secretariat
Report of Section 5 1995
1995 - IRG/WP 95-50061
IRG Secretariat
Minutes of the WG I meetings 1976
1976 - IRG/WP 146
IRG Secretariat
Progress report on co-operative research project on L-joint testing
1983 - IRG/WP 2192
A F Bravery, D J Dickinson, M Fougerousse
Guidelines for oral presentation
1990 - IRG/WP 5354
IRG Secretariat
Agenda WG IV
1986 - IRG/WP 4126
IRG Secretariat
Agenda WG IV
1973 - IRG/WP 402
IRG Secretariat
Confocal laser scanning microscopy of a novel decay in preservative treated radiata pine in wet acidic soils
1997 - IRG/WP 97-10215
Light microscopy of radiata pine (Pinus radiata D. Don) field test stakes (20x20x500mm3) exposed in wet acidic (pH 3-4) soil for 12 - 24 months showed predominance of an unusual type of decay characte-rised by tunnelling attack of wood cell walls. After two years decay was moderate to severe in wood treated to ground contact CCA specifications and also equivalent retentions of creosote, and a numb...
R N Wakeling, Ying Xiao, A P Singh
Effect of acetylation on decay resistance of wood against brown-rot, white-rot and soft-rot fungi
1989 - IRG/WP 3540
Effect of acetylation on decay resistance of wood was investigated using wood blocks of Cryptomeria japonica, Pinus densiflora, Albizia falcata and Fagus crenata. Blocks were treated with uncatalyzed acetic anhydride for different lengths of time and exposed to Tyromyces palustris, Serpula lacrymans, Coriolus versicolor and unsterilized soil. The action of OH-radical on acetylated wood was also ex...
M Takahashi, Y Imamura, M Tanahashi
Solvent drying and preservation of timber
1977 - IRG/WP 381
Processes which combine drying and preservation are first reviewed. Some preliminary experiments are then described in which blocks of green Sitka spruce sapwood were immersed, in a solution of tributyltin oxide (TBTO) in methanol at 60°C. Satisfactory penetration of the preservative and exchange of methanol and water occurred in a few hours. The methanol was removed rapidly from the wood by evap...
J A Petty
A comparison of soft rot, white rot and brown rot in CCA, CCP, CCF, CCB, TCMTB and benzalkonium chloride treated Pinus radiata IUFRO stakes, after 9-15 years exposure at five test sites in New Zealand
1991 - IRG/WP 1485
The aim of this study was to determine if decay type varies significantly between five field trial test sites of different soil type, aspect and climate in 9-15 year old, replicate CCA, CCF, CCP. CCB, TCMTB and AAC treated IUFRO stakes. A visual on-site assessment of decay type on every test stake was made and observations confirmed by microscopical examination. Regression analyses were used to de...
R N Wakeling
Annual report 1999
2000 - IRG/WP 00-60123
IRG Secretariat
Statutes
1970 - IRG/WP A 1A
IRG Secretariat
Finishes for outdoor timbers
1975 - IRG/WP 378
Anonymous
Minutes of the meetings of WG III
1980 - IRG/WP 3161
IRG Secretariat
Minutes of the meetings of WG II
1983 - IRG/WP 2207
IRG Secretariat
Agenda WG II
1989 - IRG/WP 2337
IRG Secretariat
Field trial with poles of Scots pine treated with six different creosotes
1996 - IRG/WP 96-30115
In the middle of the 50's field trials with creosote-treated poles were started in France, Germany and Sweden. The trials were initiated by WEI (Western-European Institute for Wood Preservation). Six different creosotes were used and 40 poles per creosote were installed at each test field. Results after 39 years of exposure in Simlangsdalen, Sweden are reported. Poles treated with a heavy...
Ö Bergman
Management of the wood and additives wastes in the wood processing industries: Problematics and technical answers review
1996 - IRG/WP 96-50073
Management pathways for pure wood subproducts are well known and used; but as soon as additives like preservatives, glues, varnishes or coatings are present within the wood wastes, their disposal or valorization becomes more tricky. The different kinds of mixed wood wastes of the wood processing industries, from the sawmill to the furniture manufacture, are identified herewith and their diversity ...
S Mouras, G Labat, G Deroubaix
Biological screening assays of wood samples treated with creosote plus chemical additives exposed to Limnoria tripunctata
1980 - IRG/WP 408
Laboratory methods for exposure of treated wood coupons to Limnoria tripunctata are described. Chemical additions to creosote were screened using this method. Three pesticides, Endrin, Kepone, and Malathion proved particularly effective. The addition of varying percentages of naphthalene to creosote using several treatment methods are currently being assayed. Results to date show that the coupons ...
B R Richards, D A Webb