Natural durability of some commercial timbers of Sarawak, Malaysia in tropical marine environment
2005 - IRG/WP 05-10561
The abundant supply of timber resources in Sarawak makes timber an ideal choice to be used for marine construction. The natural durability of the main commercial timber species of Sarawak in ground contact is well established but the same is not available for marine environment. This study was conducted to assess the natural durability of 28 commercial timber species in tropical marine environmen...
K Jenang, Wang Choon Ling


Minutes WG IV
1992 - IRG/WP 92-4183
IRG Secretariat


Nomination procedure for the offices of President, Vice-President and members of the Executive Council
1994 - IRG/WP 94-60023
IRG Secretariat


List of Members and Sponsors
1985 - IRG/WP 5217
IRG Secretariat


A new approach to the maintenance of wooden railway sleepers. (Second report)
1988 - IRG/WP 3492
The microenvironment and micro-ecology of wooden railway sleepers was investigated to assess their condition to determine the necessary treatment, repair and replacement criteria. In this report the efficacy of the secondary preservative treatment with solid boron rods is discussed and the development of an in-situ, nondestructive test method based on the creation and assessment of structural dyna...
W Beauford, P I Morris, A M Brown, D J Dickinson


Heat treated timber in Finland
2000 - IRG/WP 00-40158
Heat treatment permanently changes the physical and chemical properties of wood by means of high temperatures (150 - 240°C). Heat treatment darkens the colour of the wood. Heat treatment improves the equilibrium moisture content of the wood and the shrinkage and swelling of the wood is reduced. Very high temperatures improve the resistance to rot and also reduce the susceptibility to fungal decay...
T Syrjänen, E Kangas


The leachability and specificity of the biological protection of timber using Scytalidium sp. and Trichoderma spp
1986 - IRG/WP 1302
The results of field experiments, using biological control against internal decay of creosoted poles, are briefly reviewed and the evidence concerning the leachability of the antibiotics produced by these species is presented. A pure culture miniblock decay test on biological control treated pine sapwood is described and the results compared to previously published data. The protection against Len...
P I Morris, N A Summers, D J Dickinson


Degradation of the normal fibre walls of rubberwood (Hevea brasiliensis) by the tropical blue-stain fungus Botryodiplodia theobromae
1998 - IRG/WP 98-10286
Rubberwood was examined by light microscopy and transmission electron microscopy (TEM) after exposure to the common tropical sapstain fungus Botryodiplodia theobromae for four weeks to study hyphal colonisation of wood cells and to determine if this fungus also degraded lignified normal fibre cell walls in addition to the walls of non-lignified elements. Light microscopy revealed relatively large ...
A A H Wong, A P Singh


TBTO absorption and penetration in pine joinery treated by various processes
1989 - IRG/WP 3523
Matched sections of several White pine (Pinus strobus) and Ponderosa pine (Pinus ponderosa) mouldings were treated with TBTO by Double vacuum, modified empty-cell, 15 second dip and several preheating treatments followed by a 15 s dip treatments. As expected the double vacuum and empty-cell (batch) treatments resulted in much greater retentions and penetrations than the dip treatments. The absorpt...
P A Cooper, Y T Ung


The isolation of actinomycetes from wood in ground contact and the sea
1980 - IRG/WP 1110
M S Cavalcante, R A Eaton


Detection of incipient brown rot decay in wood by fourier transform infrared spectrometry
1987 - IRG/WP 2275
Fourier transform infrared spectrometry was evaluated as a possible method for detecting different levels of brown-rot decay in pine sapwood. By using first derivative spectra and regression analysis, an equation based on 4 absorption peaks, normalized with an internal standard peak, was developed. The correlation between weight loss and absorption was highly significant indicating that this is a ...
D D Nicholas, T Schultz


Agenda WG Ib
1988 - IRG/WP 1372
IRG Secretariat


Agenda WG II
1972 - IRG/WP 207
IRG Secretariat


Collaborative soft rot test: Amended test method
1972 - IRG/WP 208
The initial draft of a standard test method (Document IRG/WP/201) was discussed at the meeting in Brussels in 1971. It was agreed that a revised draft should be prepared and that the Princes Risborough Laboratory (formerly FPRL) should conduct a trial test using the method as a preliminary to the main collaborative test....
J G Savory


Some relationship between physical characteristics and treatability of Bolivian woods
1987 - IRG/WP 3434
Using the available data on physical characteristics of 25 Bolivian woods, some relationships between porosity, specific gravity and treatability (hot and cold open tank process with 5% pentachlorophenol) were analysed. The aim of this report is to give information on technical characteristics of Bolivian hardwoods which have been studied in this country by Centro de Desarrollo Forestal and in Per...
A S Viscarra


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. 3rd Interim Report
1983 - IRG/WP 4101
This paper updates the results of microbiological examination and marine borer assessment of untreated wood samples (15 x 2 x 2 cm³) and samples treated with 3, 6 and 10% CCA and CCB preservatives. Three reference species - Alstonia scholaris, Fagus sylvatica, Pinus sylvestris were used at all the test sites in addition to local species chosen by participants in the test....
R A Eaton


Fungi associated with groundline soft rot decay in copper/chrome/arsenic treated heartwood utility poles of Malaysian hardwoods
1992 - IRG/WP 92-1567
Copper-chrome-arsenic treated heartwood from Malaysian hardwood utility poles in service for 8-23 y at two localities in the wet tropical Peninsula Malaysia were surveyed for soft rot in the ground-contact region. Soft rot decay was detected in all the poles. Isolation studies indicated the ability of a variety of microfungi and basidiomycetes to colonize treated heartwood. Most isolates exhibited...
A H H Wong, R B Pearce, S C Watkinson


A collaborative test to determine the efficacy of poyurethane coatings on wood samples exposed in the marine environment. 1st Interim Report
1988 - IRG/WP 4145
Wood samples coated with elastomeric polyurethane (ca. 50 mils thick) were exposed for up to 2 years in 12 tropical and temperate marine test sites with known teredinid, pholad and/or crustacean infestations. All uncoated control samples were destroyed or partially destroyed. Polyurethane-coated samples were not attacked, the surfaces of the coating were sound and the polyurethane adhered well to ...
R A Eaton


Natural durability of some common Indian timbers and marine plywood against biodeterioration in Kochi waters (India)
1992 - IRG/WP 92-4177
Panels of thirty-eight timber species and marine plywood were tested in Kochi harbour (South-west India) for periods ranging from 3 to 21 months, so as to evaluate their natural resistance against marine borers. Results indicate that all the timber species studied are non-durable, 6 of them having undergone more than 50% internal destruction within 3 months; 14 species in 6 months, 13 species and ...
L N Santhakumaran, M V Rao


Minutes of the meetings of WG I
1983 - IRG/WP 1218
IRG Secretariat


Agenda WG II
1985 - IRG/WP 2245
IRG Secretariat


Minutes of the meetings of WG Ia
1985 - IRG/WP 1275
IRG Secretariat


Minutes of the meetings of WG II
1978 - IRG/WP 2122
IRG Secretariat


An investigation to assess the feasibility of developing an accelerated laboratory test to determine the abrasion resistance of lesser-used timber species for use in marine constructio
2005 - IRG/WP 05-20317
The paper describes the evaluation of a laboratory-accelerated test to compare the shingle abrasion resistance of current and potential timbers for use in marine construction. Useful results were achieved in 47.5 hours, but identified a number of issues to be resolved for the test to be refined and the subsequent results to be interpreted correctly....