Preliminary indications of the natural durability of Spruce bark board
1999 - IRG/WP 99-10312
A board material made from pressed bark, with no added adhesive, has been developed by Forintek's composites group and tested for durability by Forintek's treated-wood group and the University of Hawaii. This material was also manufactured with veneers in a one-step process. Since one role of bark on the tree is protection against pests and diseases, barkboard was expected to hav...
P I Morris, J K Grace, G E Troughton


The effects of accelerated drying of green Pinus radiata on its attractiveness to Anobium punctatum as an egg-laying site
1984 - IRG/WP 1199
The methods and results are given for a series of experiments in drying Pinus radiata sapwood under a variety of conditions, then exposing the material to Anobium punctatum egg-laying. The results showed very clearly that the attractiveness of the wood to gravid females was drastically reduced when dried from green at temperatures much above 35°C. Both simple oven drying and steam kilning produce...
D J Cross


Conforming to European standards on preservative treatment
1998 - IRG/WP 98-20150
New European standards require that specifications for the preservative treatment of timber are written in terms of the penetration and retention of preservative within the treated commodity that result from the treatment process. In order to check compliance with this type of specification, suitable methods of quantitative analysis must be available. This paper presents the results of a study by ...
E D Suttie, R J Orsler


Upgrading the fungal resistance of OSB
1999 - IRG/WP 99-40138
There is a perception that oriented strand board (OSB) is less resistant to fungl than plywood under conditions of moderate exposure to moisture. Douglas fir-faced plywood (DFP) has been suggested as a benchmark for acceptable durability under such conditions. This project was initiated to determine the minimum level of low-toxicity chemical treatment needed to upgrade the fungal resistance of OSB...
P I Morris, J E Clark, D Minchin, R Wellwood


Programme d'études sur le pentachlorophénol
1993 - IRG/WP 93-50001-09
In 1989, Hydro-Québec began a study program on pentachlorophenol (PCP), with a view to ensuring safe management of the product at all stages of its utilization. The topics under study include storage of treated poles, behavior of PCP in the environment, soil decontamination, water treatment, characterization and disposal of treated wood waste, and assessment of substitutes. This paper summarizes ...
G Beaulieu, A Bériault, R Chénier, L Houde


Decay rates and strength and stiffness loss in foundation beams
1992 - IRG/WP 92-1563
The TNO Centre for Timber Research has executed an extensive research programme into the rate of decay in foundation beams, as a result of lowering of ground water tables. The aim of the research was to develop a method, predicting the decrease in strength and stiffness in beams, due to wood decay during drytime of foundation beams. With the calculated extremes in decay, the damage caused by local...
P Esser, H S Buitenkamp


Mould growth and permeability in relation to wet-storage
1989 - IRG/WP 1414
The positive influences of wet-storage of roundwood to avoid attack by blue stain fungi and insects and to avoid cracking of wood during storage are well documented. Comparatively little information is, however, available on the effects on microbial susceptibility of the material after the storage period. The permeability of the wet-stored and the non-wet-stored material was determined. Wood block...
J Bjurman, E L Holappa


Influence of fungal exposure on the redistribution of copper in treated spruce wood
2002 - IRG/WP 02-10450
The redistribution of copper in treated wood after exposure to basidiomycete decay fungi is described. The micro-distribution of copper in copper(II) sulphate or copper(II) octanoate/ethanolamine treated Norway spruce wood before and after exposure to 3 different wood decay fungi was studied using transmission electron microscopy with X-ray microanalysis. The copper content of the mycelium and the...
M Humar, F Pohleven, R J Murphy, D J Dickinson, I Moris, M Zupancic, P Kalan, M Petric


What is OECD doing to promote harmonization of biocide regulations
1999 - IRG/WP 99-20182
OECD began work on biocides in 1997 to help Member countries co-operate in the assessment and registration of these products. The work is a part of OECD's Pesticide Programme, and is co-ordinated by the Biocides Steering Group. The goal is to harmonize regulatory approaches to allow countries to conduct evaluations of biocides more efficiently. More efficient evaluations can advance the p...
M Paneli, N Grandy


Effects of the sulfuric acid modification of CCA treating solution
1987 - IRG/WP 3415
Sulfuric acid modification of CCA treating solution is often used to control the formation of sludges and undesirable deposits on the surface of treated wood. The consequences of sulfuric acid addition are examined in this work and negative effects are shown to far outweigh any benefits. Major risks include the loss of copper due to leaching from treated wood and the accelerated corrosion of treat...
R F Fox, H J Fry, E A Pasek, A S Ross


Evaluation of hydroxamates as wood preservatives
2004 - IRG/WP 04-30330
Fungicidal activity of different hydroxamates was investigated by laboratory malt-agar block tests to evaluate their potential as wood preservatives. Results obtained indicate that benzohydroxamic acids substituted or not on the aromatic nuclei were unable to protect wood blocks against the white rot fungus Coriolus versicolor while 2-hydroxypyridine-N-oxide (2-HPNO) possesses an interesting activ...
P Gérardin, S Dumarçay, E Gelhaye, A Mbamba, V Mussavu


Information on a project about the conditions of admissibility of wood-protecting agents in connection with environmental protection in Poland
1974 - IRG/WP 57
Wood-protecting agents are compounds acting toxically on fungi and insects. If handled improperly or carelessly, they may exert an action harmful to health and safety of men. This action is concerning: a) workers employed at the production of wood-protecting agents; b) workers employed at the impregnation, or at the transport and handling of impregnated wood; c) inhabitants of buildings with impre...
J Wazny


Laboratory evaluation of anti-sapstain formulations
1989 - IRG/WP 3510
Four formulations were tested for their efficacy in controlling molds and sapstaining fungi on wood according to the Standard-II of Japan Wood Preserving Association (JWPA). Relative efficacy was compared on the basis of visual rating of the fungal growth on the treated and untreated wood surfaces when the wood specimens were exposed to each monoculture of 5 test fungi at 26±2°C and 70-80% for 4...
K Tsunoda


Resistance of board materials against fungal decay: A comparative experiment on Kolle flask tests method and direct test method
1985 - IRG/WP 2243
Two sets of plywood (Aucoumea klaineana Pierre) 7 and 11 ply, treated by two preservatives, and untreated, were tested by two methods: 1. Kolle flask test method on malt-agar substrate according to the French standard NF B 51.295; 2. A direct test method in non sterile conditions according to DocNo: IRG/WP/2214. The exposure time far both methods was 12 weeks. After exposure, the degree of attack ...
G R Y Déon, L N Trong


The potential of high pressure pulsation processes to treat white spruce lumber with water-borne preservatives
1988 - IRG/WP 3471
Laboratory work using end sealed 4x8x46 cm³ white spruce samples has been done to explore the suitability of three variants of a 2.1 MPa pulsation process for the impregnation of white spruce with CCA. The results showed that the process improved significantly the penetration of the preservatives and reduced significantly cell collapse, when compared with the results of treatment using a 2.1 MPa ...
J P Hösli, J N R Ruddick


The UK termite eradication programme: Justification and implementation
2000 - IRG/WP 00-10373
In May 1998, an established infestation of subterranean termites (Reticulitermes lucifugus subsp. grassei) was found in a semi-rural, coastal setting in Saunton, North Devon. Surveys and monitoring revealed a discrete, highly localised infestation extending over some 2400 square metres. There is some evidence that the termites were imported accidentally possibly more than 30 years previously. With...
R H J Verkerk, A F Bravery


IRG/COIPM INTERNATIONAL MARINE TEST - to determine the effect of timber substrate on the effectiveness of water-borne salt preservatives in sea-water. Progress Report 17: Report of fifth inspection (4 years) in Italy
1983 - IRG/WP 4103
The wood samples of Alstonia scholaris, Fagus sylvatica, Pinus sylvestris were submerged in the sea at Follonica, Italy, in April 1977. Follonica, latitude 42°55' North and longitude 10°45' East, is situated on the Tyrrhenian coast. The recorded temperature varies from 13°C to 25°C, salinity 37-38% and pH about 8. The inspections were carried out after 6 months (10/1977), 12 ...
A Gambetta, E Orlandi


Soft rot in heartwood of preservative-treated pole stubs of Eucalyptus cypellocarpa L. Johnson
1983 - IRG/WP 1204
Pole stubs of Eucalyptus cypellocarpa L. Johnson, treated in the sapwood with certain waterborne preservatives and exposed for 21 to 23 years in a dry tropical region were severely soft-rotted in the heartwood, as well as the sapwood. They broke with a brash fracture when stress tested (loaded as a cantilever) in the field. The severe soft rot in the heartwood was not detected by the knife test or...
J E Barnacle, G C Johnson, M A Tighe


The effect of stack height on the performance of preservatives used for the prevention of sapstain on seasoning wood
1997 - IRG/WP 97-10192
The performance of three anti-sapstain preservatives was investigated under field conditions in south east England. The preservatives under test were: copper-8-quinolinolate (Mitrol PQ8) trimethylalkylammoniumchloride and sodium hexanoate (Sinesto B) and chlorothalonil (Tuff Brite). The preservatives were tested on Corsican Pine grown in south east England. The field trial was set up to investigat...
J R Williams, D J Dickinson, J F Webber


Amenability of radial permeability of Sitka spruce (Picea sitchensis (Bong.) Carr.) as affected by aspects of cell ends in uniseriate ray parenchyma tissue
2003 - IRG/WP 03-40252
The principal objective of this article was to recognise and understand the amenability of ray parenchyma cell ends (end platform) in uniseriate ray tissue to influence the radial permeability of Sitka spruce (Picea sitchensis (Bong.) Carr.) by examination of most (Queen Charlotte Islands in Rhondda, South Wales) and the least (South Oregon in Dalby, North-East England) seed origins that grown in ...
I Usta, M D C Hale


A novel technique for comparative toxicity studies of potential insecticidal wood preservatives
1983 - IRG/WP 2198
For some years now a device has been under development at the New Zealand Forest Research Institute, the purpose of which is to study the effects of sub-lethal amounts of stomach poisons (but also of fumigants and contact active materials) on the co-ordinative abilities of a cerambycid larva. This insect is Prionoplus reticularis - indigenous to New Zealand its larvae feed in decaying logs and are...
D J Cross


Preservation of basidiomycete hyphae in ancient waterlogged wood materials
1992 - IRG/WP 92-1536
Studies on waterlogged archaeological wood show that basidiomycete hyphae may persist as long as 800 years. In two pine wood samples with Phellinus pini heartrot, one from the foremast of the ship Vasa and the other from a bulwark constructed in the first part of the 12th century, numerous resin covered hyphae were observed. Hyphae with clamp connections that were associated with brown and white r...
T Nilsson, G F Daniel


Evaluation of fungi isolated from the galleries of the striped ambrosia beetle Xyloterus lineatus (Ol.) (Col., Scolytidae)
1995 - IRG/WP 95-10092
Fungi from the galleries of the striped ambrosia beetle Xyloterus lineatus (Trypodendron lineatum) (Ol.) found in spruce logs were studied. The following fungi were isolated and identified: Trichoderma harzianum Rifai, the yeast Pichia anomale Hansen (Kurzman), the blue-stain fungus Ceratocystis piceae (graphium) (Münch) Bakshi and a fungus closely similar to Ceratocystis araucariae (anamorph). T...
G Babuder,F Pohleven


Questionnaire relating to the occurrence, prevention and repair of Dry Rot attacks in buildings
1989 - IRG/WP 1418
Dry Rot attack in buildings has become an increasing problem in Denmark. The reason is that old multi-storey houses from about 1890-1920 are being renovated and modernised and connected to this well-hidden Dry Rot attacks are detected. The traditional methods for repair used in Denmark are very expensive but with a high degree of confidence when done carefully. There is a big need for development ...
A P Koch


Alternative methodology for the environmental impact assessment of treated wood: the wood emissions ecotoxicology
2000 - IRG/WP 00-50161
Preservative products and technologies are important for optimising the use of wood and wood products in our society. The regulations of their use under the european Biocidal Products Directive 98/8/EC will require an evaluation of the environmental impact of treated wood. The methodology currently used for this determination is the PEC/PNEC ratio. It consists of calculating PEC values (Predictive...
P Marchal, H W Wegen, J Van Acker, E Melcher, R-D Peek, W J Homan, D Aston, D Rudolph, E F Baines