Field Tests of naturally Durable North American Wood Species
2008 - IRG/WP 08-10675
There has been little field test performance data published on North American naturally durable species in general, and no published data on second growth material in particular. Yellow cedar (Callitropsis nootkatensis), western red cedar (Thuja plicata), eastern white cedar (Thuja occidentalis), and three wood species reputed to be moderately durable were installed in ground-contact (stakes) an...
P E Laks, P I Morris, G M Larkin, J K Ingram


The Effects of Solar Radiation on the Fungal Colonization and Color of Weathered Wood
2008 - IRG/WP 08-10676
Solar radiation rapidly depolymerizes lignin at wood surfaces exposed outdoors producing a suite of low molecular weight aromatic compounds within weathered wood. Fungi colonizing weathered wood are able to metabolize these aromatic compounds, and many of them also contain high levels of melanin to protect themselves from the harmful effects of UV radiation. Both of these adaptations suggest that ...
V Hernandez, C Breuil, P D Evans


Selección de hongos reductores de extraíbles del género Ophiostoma, mediante la prueba de opacidad Tween 80
2009 - IRG/WP 08-10677
Wood extractives cause diverse problems in the industry of the wood, the pulp and the paper; among others, they produce pitch deposition during the pulp manufacturing, generating important economic losses for the sector. Recently, to mitigate these effects, it has been proposed the biological pretreatment of chips and the solid wood with colorless fungi of different species from genus Ophiostoma. ...
P Herrera, J Navarrete, C Breuil, E Werner


Wood Decay Research Using Molecular Procedures, What Can It Tell Us?
2008 - IRG/WP 08-10678
There are many unanswered questions in wood decay and protection research, and no single research technique will ever answer all of these questions. The process of wood decay is a very complex series of biochemical and chemical reactions that are heavily influenced by the hundreds of bacterial and fungal species found on environmental samples of wood. There are a variety of molecular techniques b...
S V Diehl, M. L Prewitt, Young-Min Kang, L Mangum, J D Tang


Termites y otros insectos xiliofagos en bienes arquitectonicos monumentos nacionalos de Colombia
2009 - IRG/WP 08-10679
The incidence of termites and other wood destroying insects was surveyed in ten historical buildings in Colombia. The most common insects were termites (Kalotermes, Cryptotermes, Heterotermes), although numerous decay organisms were also detected, including beetles (Anobium, Lyctus, Cerambycids) and various wood decaying fungi. Structural wood elements were classified according to the degree of a...
M G Ramírez


Aislamiento, identificación y evaluación enzimática de hongos de pudrición de madera de la Región de los Lagos
2008 - IRG/WP 08-10680
So far, systematic investigations have not been developed to determine the fungal diversity associated with wood in Chile. In addition, little is known about the mycoflora capabilities or their enzymatic processes in biotechnology although different research has hinted at the great potential of these microorganisms in various industrial processes. The aim of this work is to isolate, identify and e...
R Ortiz, J Navarrete, C Oviedo, R Blanchette


El Rol de la AWPA en las Normas y Códigos Nacionales e Internacionales
2008 - IRG/WP 08-20389
AWPA Standards for treated wood products are recognized around the World in building codes and architectural specifications. Standardization is important in the global marketplace because it leads to increased safety, reliability, and efficiency. Consumers have a profound awareness of and preference for standardized products, even though businesses sometimes ignore them. Historically, market fa...
C McCown


Measurement of wood decay by dynamic MOE in an accelerated soil contact test
2008 - IRG/WP 08-20390
Current laboratory and field testing of preservatives involves various techniques to determine the extent of fungal attack, including visual inspection, mass loss, and static bending and compression strength measurements. The objective of this study was to compare decay measurement by conventional compression strength versus dynamic MOE, employing small wood stakes in an accelerated laboratory so...
Gan Li, D D Nicholas, T P Schultz


Control biológico de la mancha azul en madera aserrada de Pinus radiata D. Don.
2008 - IRG/WP 08-10681
Radiata pine wood is highly susceptible to the attack of sapstaining fungi promoting a discoloration which results in important economical losses. The use of chemicals, a customary procedure to prevent its occurrence is becoming nowadays, due to environmental concern, a more questionable practice. The biological control of blue stain fungi with albino isolates of the Ophiostoma genera appear to ...
J Navarrete, A Segura, P Martínez, R Vera, C Segovia, P Herrera, L Reyes, D McNew, T C Harrington, R L Farrell, J M Thwaites, B Held, R A Blanchette


Near infrared spectroscopy for the quantification of wood preservatives
2008 - IRG/WP 08-20391
Near infrared (NIR) spectroscopy is a rapid, flexible, inexpensive and non-destructive technology that has many applications, including the evaluation of many wood properties. Initial studies have indicated the potential to apply NIRS for the quantification of wood preservatives. However, further evaluation with borate and azole preservative systems has revealed that NIRS technology is challenged ...
A M Taylor, Seung H Baek, Myong K Jeong, J D Lloyd, J J Morrell


To decay or not to decay: An accelerated field test of the validity of the Scheffer index
2008 - IRG/WP 08-20392
The Scheffer Index was introduced in 1971 to predict the relative decay hazard of untreated wood exposed above-ground. Precipitation and temperature parameters are used in the calculation. A higher Scheffer Index value implies a greater risk of decay. An accelerated 18-month study using seven field sites with Scheffer Indices ranging from 35 to 400 and two wood types (Populus tremuloides and Pi...
G M Larkin, P E Laks


Above Ground Field Testing – Influence of test method and location on the relative performance of various preservative systems
2008 - IRG/WP 08-20393
Standardized above ground tests such as the lap-joint or test deck methods can be very slow in producing useful information on the relative performance of wood preservative systems. It often requires many years for decay to develop in wood treated to sub-optimal concentrations of standardized preservatives, making relative comparisons of performance between new systems and established preservativ...
A Zahora


Field testing in Colombia: Three years of evaluations and experiences
2008 - IRG/WP 08-20394
Two field test sites have been established in Colombia for the evaluation of fungal and termite resistance of treated wood. The combination of elevated temperature, high and stable humidity and high rainfall at the two test sites accelerates microbial and insect activity (Scheffer, 1971; Thornton et al, 1994; Freitag et al, 1995). Tests established include above ground termite tests, ground contac...
Y Cabrera, A Preston


Chemical Analysis in Production Quality Control at Wood Treatment Plants
2008 - IRG/WP 08-20396
Analysis methods for quality control analysis in wood treatment plants have evolved with the changes in treatment preservative chemistries and analytical instrument technology. The basic hydrometer specific gravity measurements used for solution strength and classic wet chemistry methods for wood have given way to instrumental techniques such as X-ray fluorescence, automatic titrator, and HPLC. No...
P Walcheski, L Jin


Control de calidad eficiente de proteccion superficial sobre madera
2008 - IRG/WP 08-20397
Quality control is important to assure efficient protection of wood surfaces. When wood is exposed to the environment, it degrades due to weathering or environmental factors alone. Aging tests are utilized to test coating products. Quality control techniques are performed on exposed products according to standardized methods (NCh, ASTM, ISO, DIN, EN, FTMS, NTF, NBINT, or equivalents). Certified l...
A M Fernández S


Utilidad práctica de mini estacas en ensayos de campo
2009 - IRG/WP 08-20395
For testing chemicals for the wood against degradation agents of biotic, known as preservatives, both testing in the laboratory and in the fields are used. Field trials (Cemetery stakes) are often accepted as more "real" whose frequency of observation is set to more or less a year in temperate climates and six months or less in tropical situations, taking into accounts the aggressiveness of the so...
O Encinas, J V Puentes, N K Sarmiento, N Mora


Australian trials on the efficacy of micronized copper
2008 - IRG/WP 08-30480
Alkaline copper quat (ACQ) is an established wood preservative that is formulated with solubilised copper in amine solvent. This paper describes three separate trials in Australia that investigated whether substituting soluble copper with micronized copper affects performance. ACQ and micronized copper quat (MCQ) gave similar performance in Pinus radiata against four brown-rotting fungi in a soil-...
L J Cookson, J W Creffield, K J McCarthy, D K Scown


Evaluación de oxinato cúprico como alternativa al tribromofenato de sodio, para uso como funguicida antimancha. Ensayo final y conclusiones
2008 - IRG/WP 08-30481
This study evaluated the efficacy of oxine-copper (Cas Nº 10380-28-6. Synonyms: copper oxyquinolate, cupric-8-hydroxyquinolate, copper-8-quinolinolate) for the control of stain fungi in lumber. Three field tests were established and sodium tribromophenate was used as a reference preservative. Boards of Pinus elliotis and P. taeda were treated by dipping for 15, 30 or 60 seconds in two different f...
M Alba Valle


Prolongación de la vida util de la madera de Pino Caribe de plantaciónes con sales CCB
2008 - IRG/WP 08-30482
Three concentrations of CCB were evaluated for their efficacy to protect Caribbean pine against fungal attack. Standardized laboratory tests (EN 113) were used to assess CCB effectiveness against a white-rot fungus (Trametes versicolor), and a brown-rot fungus Gloeophyllum trabeum. After 12 weeks, treated cubes of Caribbean pine exposed to the brown-rot fungus had between 2-8% weight losses while ...
A P Sanabria Sanabria, R Arévalo


Effectiveness of MOQ® OX 50 (CCB-Oxide) wood preservative – Part 2: Field tests
2008 - IRG/WP 08-30483
MOQ® OX 50 is a chromated copper borate preservative known around the world as CCB. In Brazil, this product is the only CCB-oxide type preservative with fungicide and insecticide properties registered at the Brazilian Institute for the Environment and Renewable Resources (IBAMA) that complies with the requirements of the Brazilian and European markets for preserved wood. For over five decades, s...
A Gandolfi Jr, C Salvela, D R Macedo, J M Vidal


Multifactorial Antimicrobial Wood Protectants
2008 - IRG/WP 08-30484
It is unlikely that a single antimicrobial compound, whether synthetic or natural, will provide the ‘magic bullet’ for eliminating multiple biological agents affecting wood products. Development of synergistic combinations of selected compounds, especially those derived from natural sources, is recognized as a promising approach to improved wood protection. Recent adoption of effective fungici...
R D Coleman, C A Clausen


Biological efficacy of micronized copper systems
2008 - IRG/WP 08-30485
Soil block, fungal cellar and field stake test data will be presented for micronized copper systems. The copper portion of the formulations is present as a fine dispersion of "micro" particulates while the co-biocide is present as either a soluble quat or an azole containing emulsion. This testing generally used the amine based counterpart as the control preservative system and the micronized fo...
C R McIntyre, M H Freeman


A Comprehensive Review of Copper as a Biocide, with a Focus on Micronized Copper
2008 - IRG/WP 08-30486
This paper reviews the wood preservative biocide active ingredient copper and delvers into new and previously unpublished data regarding the new micronized formulations which are now in vogue and widespread use in N. America in all residential treated lumber markets. Included in this review is the overall discussion of copper containing formulations used for pressure treated wood used over the las...
M H Freeman, C R McIntyre


Polymeric Betaine as a Wood Preservative
2008 - IRG/WP 08-30487
Didecyl polyoxyethyl ammonium borate (DPAB), also known as Polymeric Betaine, was developed as a co-biocide for chromium-free copper based wood preservatives in Europe in the 1980’s. This paper summarizes the properties of DPAB as a wood preservative. Unique properties related to the betaine nature of DPAB are discussed in terms of the structure-property relationship. Physical properties of D...
H Härtner, S Schmitt, Futong Cui, H M Barnes


Biological Performance of micronized copper wood preservative formulations in field and laboratory tests
2008 - IRG/WP 08-30488
Micronized Copper wood preservative formulations with different co-biocides were exposed to brown rot fungi in an 8-week AWPA E10 soil block decay test and two AWPA E7 ground-contact decay tests in Hawaii. The micronized copper formulations performed well against decay at or above the AWPA UC3 and UC4 retentions stipulated by the ICC-ES. Micronized copper preservatives performed comparably to a ...
G M Larkin, J Zhang, D L Richter, R J Ziobro, P E Laks