Ability of heartwood extractives to inhibit the growth of a bacterial symbiont of Teredo navalis
2000 - IRG/WP 00-10369
Shipworms are important destroyers of wood in the marine environment, and wood users have long sought methods for preventing or limiting their attack. While heavy -duty wood preservatives are highly effective against these organisms, there is increasing concern about risks to non-target organisms. This has resulted in a gradual shift away from broadly toxic materials to either alternative material...
C S Love, A R Sipe, S C Cary, J J Morrell


A study of methanogenesis and sulphate-reduction: A possible source of explosive gas mixtures in a gold mine
1989 - IRG/WP 1399
Previous work isolated anaerobic bacteria from timbers and drainage water in a gold mine. The present work identifies the predominant methanogen in the mine ecosystem as Methanobacterium bryantii and sulphate-reducing isolates as Desulphovibrio desulphuricans and Desulphotomaculum antarcticum. Laboratory studies using model systems evaluate the activity of methanogenic and sulphate-reducing bacter...
L D Abraham, J F Putterill, A A W Baecker


Why don't more people work with Serpula lacrymans nowadays? A discussion of some of the different approaches to experimenting with this unique fungus
1989 - IRG/WP 1383
Remarkably few laboratories are currently investigating this well-known fungus. Not only has it failed to gain acceptance as a standard test organism (for wood preservative evaluation) in many countries, but is also sometimes excluded from pure research studies when it ought to be an obvious first choice as a representative basidiomycete. This paper discusses some different approaches that have be...
J D Thornton


Soft rot - Soil burial - Tests. Influence of the addition of nitrogen compounds to the soil on wood decay by soft rot
1972 - IRG/WP 213
The decay of wood specimens buried in soil is influenced by various factors. Decisive are the water content, the content of organic substances, the pH-value, the content of mineral nutritive salts, nitrogen content, etc. of the soil. These tests were carried out in order to investigate if the decay of wood in the soil will be influenced by additions of various nitrogen-compounds in different conce...
O Wälchli


Antagonism of Gliocladium virens against wood decay fungi
1995 - IRG/WP 95-10102
Antagonistic abilities of a commercial biofungicide, Gliocladium virens (GL-21, Grace) were evaluated against three white-rot fungi, Trametes versicolor, Phlebia brevispora, Irpex lacteus, and three brown-rot fungi, Postia placenta, Neolentinus lepideus, Gloeophyllum trabeum. In dual culture of Gliocladium virens and wood decay fungi, Gliocladium virens rapidly overgrow the decay fungi and killed ...
T L Highley, L Ferge


Diagnostics methods and routes proposalsto define selective sorting of demolition wood wastes
2001 - IRG/WP 01-50177
Wood wastes are more and more often used in different wood waste valorisation industries (panels, wood energy, cement factories, ...). These industries are in progress to include in their processes, wood wastes coming from demolition wood. A state of the art and an analysis have been made to propose : (1) diagnostics methods to carry out a classification of wood wastes on demolition sites and in t...
G Labat, E Bucket, C Fréret, G Deroubaix


Changes of copper and chromium content after leaching in wood impregnated with the CCB and CB preservatives
2000 - IRG/WP 00-50147
The objective of the study was impregnated with CCB and CB preservatives pine wood of moisture content varying from 12% to 55% subjected to leaching. Losses of copper and chromium were determined for individual layers of wood up to 3 cm from the girth. The results were compared to the total amount of metals determined in water extracts. The degree of leaching of metal ions from wood of 55% moistur...
B Mazela


Long-Term Release of Arsenic, Chromium, and Copper from CCA-Treated Wood and Ash
2005 - IRG/WP 05-50227
In this study, laboratory long-term leaching studies were conducted to characterize the leaching behavior of arsenic, chromium, and copper from CCA-treated wood samples (block, chip, and sawdust) and CCA-wood ash and to determine the rate of release of the metals from the CCA wood products. The leaching solutions were periodically collected and analyzed for the concentrations of arsenic, chromium,...
Hyunmyung Yoon, Heeseok Kang, Yong-Chul Jang


Biocidal property of the phenolic fraction of ethanol extractives of Hopea parviflora heartwood
1993 - IRG/WP 93-30003
Natural resistance of some species of timber to fungal decay and insect damage (particularly termite) is ascribed toxic nature and quantity of certain chemical substances present in the cell wall of heartwood. These chemical substances generally known to be Phenolic and Polyphenolic compounds (Rao 1982). Earlier investigations on extractives were mainly in relation to resistance of timber to decay...
R V Krishnan, K S Theagarajan, H S Ananthapadmanabha, M Nagaraja Sharma, V V Prabhu, H C Nagaveni


Wood preservation in Croatia
2004 - IRG/WP 04-30360
Croatia, as all the other countries in transition, however also because of its specific and well-known reasons, is on a path to gradual drawing nearer to the European standards. Only the scientists working at the Faculty of Forestry in Zagreb are engaged in scientific work relating to wood preservation. The construction and wood industry, which should enhance the chemical industry, also have subs...
R Despot, M Hasan


Leaching tests on CCA-treated wood using inorganic salt solutions
1984 - IRG/WP 3310
Pinus radiata sapwood treated to approximately 10 kg/m³ with Tanalith NCA or Tanalith C-type CCA preservatives was ground to a fine powder and samples were then leached with solutions of calcium chloride, calcium nitrate, magnesium nitrate, or a mixture of potassium di-hydrogen orthophosphate and di-potassium hydrogen orthophosphate, at 0.03M-1.00M solution concentrations. Leached wood samples we...
D V Plackett


Borate diffusion from fused borate rods in douglas-fir transmission poles
1994 - IRG/WP 94-30042
Pressure-treated utility poles have given many years of excellent service, but their lifetime is often shortened by internal decay of the untreated heartwood center, particularly in refractory species, such as Douglas-fir. This paper reports the distribution of boron from fused borate rods installed in CCA-treated Douglas-fir transmission poles. The boric acid equivalent was roughly monitored by t...
T L Highley, W Finney, F Green III


Suitability of different termite species for laboratory testing
1982 - IRG/WP 1159
Different termite species were tested in the laboratory to evaluate the effectiveness of insecticides and wood preservatives in wood against termite attack. Determined were the optimum group size and composition, the matrix (vermiculite) volume and its moisture content. Choice feeding tests with fully impregnated wood blocks which are carried out according to a modified EN 117 procedure for Reticu...
U Kny, H Kühne


Characterization and differentiation of wood rotting fungi by protein and enzyme patterns
1999 - IRG/WP 99-20177
Standardized tests for wood preservatives are performed with defined fungal strains to ensure comparability between laboratories. However, changes of virulence and variation of results are well known events. Suitable and reliable measures to control the stability of the test organisms are necessary.Comparison of protein patterns produced by SDS-electrophoresis was already described by several auth...
U Schoknecht


Wood preservation in Canada - Regulation and Registration
2001 - IRG/WP 01-50166-02
The Canadian wood preservation industry is at a critical juncture now as a number of initiatives converge on the industry over the next few years. Issues facing the industry include: Re-evaluation of the conventional wood preservative chemicals - inorganic arsenicals, creosote and pentachlorophenol targeted for July 2001. Delayed registration of new actives as a result of re-evaluation activity an...
P A Cooper


Redistribution of boric acid in radiata pine during drying after preservative treatment
1993 - IRG/WP 93-40010
Samples of 100 x 50 mm² radiata pine were processed with a variety of options to produce dry, boron-treated wood. Concentrations of boric acid in the central one-ninth and in the whole of the wood cross-sections were determined by chemical analysis and compared. Diffusion treated material was dried by air, conventional kiln (70/60°C), or high temperature kiln (120/70°C). Four different predryin...
A J Bergervoet, D R Page, J A Drysdale


Examination of power poles by computerized tomography
1980 - IRG/WP 2142
The technique known as computed axial tomography (CAT or CT) has become widely known because of the success it has achieved in medical imaging and diagnostics. It has now been used to give non-destructive crosssectional pictures of a variety of industrial objects, including wooden power poles, with a spatial resolution of about 1 mm (0.04 in.). It is obvious the benefits that would be derived from...
J A Taylor, I L Morgan, H Ellinger


Antagonistic effects of Dacrymyces stillatus against growth of other fungi
1991 - IRG/WP 2363
The antagonistic effects in dual cultures on malt extract agar of 5 wood decay fungi and the antagonistic effects of Dacrymyces stillatus against 1 mould fungus and 1 blue stain fungus were determined. Dacrymyces stillatus was the only fungus which exhibited clear antagonistic effects. The effects of Dacrymyces stillatus against the different test fungi varied however to a great extent. Dacrymyces...
J Bjurman


Risk of extension of Hylotrupes bajulus attack in glued laminated timber
1977 - IRG/WP 278
Although efficient work-methods and maintenance procedures, which prevent the wood from becoming damp and are therefore successful in considerably reducing and even in excluding the risks of decay, such methods are ineffective in eliminating the risks of infestation and destruction of timber by the House Longhorn Beetle, Hylotrupes bajulus, the chief enemy of softwood timber structures. The possib...
M-M Serment


A determination of the toxic level of ACQ2100 wood preservative for the powder post borer Lyctus brunneus (Stephens)
1994 - IRG/WP 94-20029
The sapwood of two Lyctus susceptible Australian hardwoods, messmate (Eucalyptus obliqua L'Herit.) and black bean (Castanospermum australe A. Cunn. et Fraser ex Hook) were pressure impregnated with ACQ2100, a wood preservative, to produce replicates of a range of retentions. Preservative retentions were determined by solution weight uptake at treatment and chemical analyses of selected sa...
A R Moffat


Exclusion of anions from the wood cell wall
1991 - IRG/WP 3661
Anionic components of wood preservatives and fire retardants such, as arsenates and phosphates, equilibrate at much lower concentrations in the cell wall bound water than in the free solution in the cell lumens. A degree of anion exclusion is expected in wood, due to the Donnan membrane effect. Fixed anions in the wood cell wall, produced by pH-dependent dissociation of the weak acid groups in woo...
P A Cooper


Analysis of the boron content of preservative treated oak and pitch pine heartwood before and after leaching
1992 - IRG/WP 92-3697
Studies to determine the effects, if any, of a variety of boron formulations on heartwood of English oak and American Pitch pine have been previously reported (King et al (1991)). Small wood blocks were treated, at 10°C or 45°C, with borax, polybor or Boracol 20 for periods of 1 month or 4 months then analysed or continuously leached with tap water for a period of 1 month. Reported results showe...
S McCutcheon, G M Smith, J W Palfreyman, B King


Safe handling of solvents in relation to classification and labelling
1990 - IRG/WP 3569
The classification and labelling of chemical products, safety data sheets and personal protective equipment are topics which at present are given a very high priority in Denmark. The area is very large and may seem extremely difficult to comprehend. The frequent publication of acts and announcements from the authorities does not make the work any easier. In the following I will try explain how we ...
J Haugaard


Relating CCA fixation to leaching of CCA components from treated products
1995 - IRG/WP 95-50045
The relationship between chromium fixation in CCA-C treated wood, as determined by CrVI analysis of solution expressed from treated wood and the leaching of Cu, Cr, As and CrVI in a simulated rain test are evaluated for dimension lumber (2"x6") and pole sections. Leachate concentrations after 2 hour exposure to a misting spray (about 300 mm cumulative rainfall) decrease rapidly with increased degr...
P A Cooper, R MacVicar, Y T Ung


Methods of testing anti-stain chemicals for protecting sawn timber during storage and transport
1976 - IRG/WP 273
No international standard method for testing anti-stain chemicals for protecting fresh sawn timber exists. The methods used can be divided into three types: a) Rapid screening tests for finding chemicals effective against blue-stain and mould fungi. The chemicals are tested in agar medium, in pieces of filter paper or on small pieces of wood using pure cultures. b) Laboratory tests for evaluating ...
T Vihavainen