Your search resulted in 6688 documents. Displaying 25 entries per page.
Above-Ground Durability Estimation in Australia. Results after 16 years exposure
2005 - IRG/WP 05-20314
A program of research was established in 1987 to examine the above-ground durability of a selection of timbers that are commercially significant in Australia. Test samples were assembled in an L-Joint design and placed on exposure racks in a format to replicate joinery that is exposed to the weather above ground. Both painted and unpainted material has been exposed.
Test samples have been evaluat...
L P Francis, J Norton
Tolerance of Wood Decay Fungi to Commercial Copper Based Wood Preservatives
2002 - IRG/WP 02-30291
Due to the use of copper based preservatives like CCB or CCA for more than a century, copper tolerant fungi have appeared in some European countries in recent times. It is therefore important to find out whether this phenomenon is specific for only classical copper ingredients, or generally for all copper based formulation. Thus, we tested the tolerance of three commercial copper based
pres...
F Pohleven, M Humar, S A Amartey, J Benedik
Timber deterioration and its prevention in marine environment
2005 - IRG/WP 05-10559
Wood-borer activity is an established fact in Mumbai harbour that leads to severe deterioration of timber. In order to prevent the deterioration caused by wood borers three resin preservatives containing Zinc borate, Organo-copper polymer (4 wt% Cu) and Organo-Tin polymer Copoly(TBTM-MMA) were used for timber treatment. Test panels were treated using standard method and the...
B S Swami, M Udhayakumar, P Kumar, A B Samui
Decay resistance of Platanus acerifolia wood against White Rot Fungi (Coriolus versicolor)
2002 - IRG/WP 02-10431
Degradation of the lignocellulose complex in wood varies on the microorganism causing decay and chemical composition of wood. The weight loss of Platanus acerifolia wood after decay by white rot fungus (Coriolus versicolor) for period 16 weeks were evaluated according to European standard EN 113 and beech wood as a control. The samples were collected in October 2000 from Nantes, France. The aim of...
M Irmouli, O Duchelier, N Ayadi, B Charrier
On the laboratory use of X-rays in timber decay evaluations
1981 - IRG/WP 2144
The paper reports the results of laboratory experiments on the X-raying of some Pinus radiata sapwood blocks infected with Serpula lacrymans to determine the effect of density and moisture content on the absorption of X-rays by wood. It is concluded that with increasing moisture content there is a very marked increase in time required to pass a constant quantity of X-rays through a test block and ...
J D Thornton, J W Creffield, O Collett
Marine trials with water-borne salts and organotin compound
1986 - IRG/WP 4128
Pinus sylvestris blocks treated with water-borne salts (CCA, CCB, CCF) and organotin compounds (TBTO, TBTCl) were submerged in the sea at Follonica station. The results obtained after 12 years of immersion are presented. The samples treated with CCA, CCB and CCF at the lowest concentration (2%) were destroyed after 7-9 years and the samples treated with CCB and CCF at the highest concentrations (4...
A Gambetta, E Orlandi
Water-storage for improving the permeability of sugi (Cryptomeria japonica D. Don)wood
1999 - IRG/WP 99-40129
The viable bacterial counts in sapwood and intermediate wood of sugi bolts increased immediately after floated in a fresh water pond. Bacterial invasion into the heartwood was not detected apparently during water-storage for 36 weeks, although a few bacterial species have inhabited in freshly-cut heartwood samples. The bacterial species isolated from the water-stored bolts were almost Gramnegative...
S Ohta, S Doi
Effect of vapour boron treatment on mechanical properties of wood based board materials
1992 - IRG/WP 92-3727
The mechanical properties of Medium density fibre board, Chipboard and Oriented strand board were investigated after treatment to two retention levels of boric acid applied as a vapour phase system. A range of mechanical properties were investigated. The vapour boron treatment does not have any significant effect on most of the mechanical properties of the boards. The exception is a reduction in i...
R Hashim, D J Dickinson, R J Murphy, J Dinwoodie
Variation of natural durability of sugi (Cryptomeria japonica) wood in 15 clones examined by decay test (Preliminary report)
2004 - IRG/WP 04-10526
Natural durability of wood in 27 trees from 15 clones of sugi (Cryptomeria japonica)  was investigated by an accelerated decay test. Thirty years old trees were collected from a clonal trial in Ibaraki prefecture, Japan. Natural durability is usually evaluated in heartwood. Mass losses of heartwood caused by a brown rot decay fungus, Fomitopsis palustris and a white rot decay fungus, Py...
K Yamamoto, A Tamura, R Nakada
Black Stain of Western red-cedar by Aureobasidium pullulans and its Relationship with Tropolone Depletion
2005 - IRG/WP 05-10564
Western red-cedar is valued for its natural durability conferred by fungicidal tropolone chemicals. However, weathered surfaces of WRC products are still susceptible to ‘black stain’ caused by fungi such as Aureobasidium pullulans. The effect of weathering on the tropolone content of heartwood was characterized and correlated with the ability of this fungal species to colonize the same weather...
R Chedgy, R Daniels, P I Morris, C Breuil
Anti-feedant activity of stilbenic components from bark of Picea glehnii against a subterranean termite, Reticulitermes speratus
2002 - IRG/WP 02-10447
Stilbenic components, one of polyphenolic groups, widely distributed in plant bodies have been known as anti-microbial agents, but not known whether to have anti-termite activities. A stilbene glucoside, isorhapontin, from the bark of Picea glehnii was examined on the anti-feedant activity against a subterranean Reticulitermes speratus. Isorhapontigenin, the aglycone of isorhapontin, induced from ...
S Shibutani, M Samejima, S Doi
The wood-attacking insects in wooden houses of an old open air museum in southern Finland
1989 - IRG/WP 1409
Harmful insects of wood in a open-air museum were investigated in 1985-1988 by order of the National Board of Antiquities and Historical Monuments of Finland in nine old log houses. Many thousands of insects and altogether 1073 anobiids (Coleoptera, Anobidae) were obtained by window and light traps. The most common Anobiidae-species were Hadrobregmus confusus (Kraatz) 60.3%, Hadrobregmus pertinax ...
H Viitanen, M Pulkkinen
On the occurrence of Phialophora species in preservative treated wood in ground contact
1977 - IRG/WP 163
Phialophora is a fairly large genus comprising about thirty described species. They are widespread in very diverse environments, such as soil, sea water, wood and wood pulps. Some species are known as parasites on plants and animals, including man. Phialophora species were early known for their ability to produce blue stain in timber. Later it was discovered that several species were able to produ...
T Nilsson, B Henningsson
The long road to understanding brown-rot decay. A view from the ditch
1995 - IRG/WP 95-10101
Interest in understanding how brown-rot fungi decay wood has received increasing interest in recent years because of a need to identify novel targets that can be inhibited for the next generation of antifungal wood preservatives. Brown-rot fungi are unique in that they can degrade holocellulose (cellulose and hemicellulose) in wood without first removing the lignin. Furthermore, they degrade holoc...
F Green III, T L Highley
A comparison of the migration behaviour in soil of different waterborne wood preservatives and their leachates
1997 - IRG/WP 97-50091
Lysimeter tests were carried out on water-soluble wood preservatives and on wood preservative components leached out of impregnated wood. The purpose of these tests was to determine the extent to which the migration behaviour of environmentally relevant ions in the soil is influenced under comparable conditions. The results clearly show that the groundwater is especially at risk when wood preserva...
E Melcher, R-D Peek
Acceleration of boric acid uptake into the subterranean termite, Coptotermes formosanus Shiraki using steamed larch wood
2000 - IRG/WP 00-10353
Laboratory tests were done to measure the efficacy of addition of steamed larch (Larix leptolepis (Sieb. et Zucc.) Gord.) heartwood extracts for the uptake of boric acid against the termite, Coptotermes formosanus Shiraki. Paper discs were treated with the water-soluble fraction obtained from hot-water extracts of steamed larch wood (S-Water) with or without 0.01-2.0% boric acid, followed by expos...
W Ohmura, S Doi, S Ohara
Laboratory tests on the residual effects of pyrethroids against termites after one year
1983 - IRG/WP 1216
Due to recent restrictions of ecological nature which most of pesticides are been submitted, it is necessary in wood preservation to test new products and formulation with low mamalian toxicity for substitution of the traditional products. The efficiency of five synthetic pyrethroids in comparison to the traditional organo-chlorinated pesticide chlordane was evaluated. Wood blocks impregnated with...
A M F Oliveira
Assessment of the Inhibition of wood decay fungi by volatile organic compounds identified from Trichoderma spp.
1999 - IRG/WP 99-10302
Previous research identified five volatile organic compounds produced by Trichoderma spp. that may be inhibitory to wood decay fungi. The effects of four of these volatile organic compounds, 2-propanone, 2-methyl-1-butanol, heptanal and octanal were tested over a range of concentrations against four selected wood decay fungi. The fungi were incubated in malt extract broth under appropriate conditi...
S N Humphris, R E Wheatley, A Bruce, C Payne
Evaluation of a new anti-sapstain formulation
1994 - IRG/WP 94-30035
A new anti-sapstain mixture, which consists of 2% IPBC (3-iodo-2-propynylbutyl carbamate) and 1.5% DCOI (4,5-dichloro-2-n-octylisothiazolin-3-one), was evaluated by three methods in the laboratory. A standardized test (JWPA standard 2) demonstrated that the new anti-sapstain formulation was highly effective in controlling growth of monocultures of five test fungi on wood substrate. When exposed to...
K Tsunoda, H Kumagai, M Sakurai
A laboratory study on effect of coating materials on leaching of copper from CCA treated wood
2001 - IRG/WP 01-50176
Components of CCA preservatives can leach into surrounding soil and water and have some effect on germination and growth of some plants. In this report, the effect of coating materials in reducing chemical concentration in the leachate were evaluated. Rubber wood blocks (Hevea brasiliensis) treated with CCA were fixed at room temperature at high humidity. After air dried, they were painted with co...
A Veenin, T Veenin
A review of incising as a means of improving treatment of sawnwood
1994 - IRG/WP 94-40019
The use of incising, perforation of the wood surface, is increased because of the need to treat refractory wood species. This paper reviews the development of incising and shows how the required incising patterns can be determined and specified. Most of the development has been in the area of toothed-roller incisors because of their rapid throughput. Needle, Laser, drill and water jet incisors hav...
P I Morris, J J Morrell, J N R Ruddick
Rapid loss of lignin at wood surfaces during natural weathering
1992 - IRG/WP 92-2390
Thin veneers of radiata pine (Pinus radiata D. Don) were exposed to natural weathering over a period of 30 days. Incident UV radiation was monitored at the test site. FTIR internal reflectance spectroscopy was used to study the chemical changes taking place at the veneer surface during weathering. Spectra obtained show that after only 3 days exposure there was substantial delignification at veneer...
P D Evans, K J Schmalzl, A J Michell
Is laboratory testing of decay resistance questionable as a single criterion for natural durability?
1996 - IRG/WP 96-20096
In a laboratory test set up over 20 hardwood species were evaluated according to the European Standard EN 350-1 including Basidiomycete and soft rot testing. Half of the species used were of a known natural durability. The Basidiomycete testing was carried out using Coriolus versicolor, Gloeophyllum trabeum and Coniophora puteana in a malt agar test similar to EN 113. From this test it was not pos...
J Van Acker, M Stevens, T Van Cauwenberghe, T Seynaeve
Moisture content development in lap-joints of different wood species in outside exposure trials
1998 - IRG/WP 98-20143
Lap-joint trails (following European Standard EN 12037) were set up with 11 different softwood and hardwood species. Half of the number of the lap-joint specimens were coated with an alkyd coating. The moisture development has been followed during a 19 months period. In this paper, the out comes of different moisture contents evaluations are presented. The results show, that the moisture content o...
H Militz, M Broertjes, C J Bloom
A shower test protocol for measuring antisapstain wash-off from small individual log billets
1996 - IRG/WP 96-50069
According to New Zealand Timber Industry Federation statistics New Zealand exported 4,835,000 m³ of logs in 1994 and it is estimated that c. 20% were anti-sapstain treated. Loss of preservative from logs as a result of rain impact after application is of considerable concern both with respect to potential loss of efficacy and environmental contamination. Whilst Environment Canada have a proposed ...
A J Pendlebury, H Pearson