IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 6688 documents. Displaying 25 entries per page.


Termite response to Agricultural Fiber Composites: Bagasse
2005 - IRG/WP 05-10549
Bagasse, or sugarcane rind, is a fibrous by-product of sugar extraction from sugarcane, Saccharum officinarum L. Bagasse fiber performs similarly to hardwood fiber in composite board products. In laboratory studies, Formosan subterranean termites survived as well on a diet of Bagasse as on Douglas-fir wood. Field tests with a compressed Bagasse panel (produced by heat extrusion) indicated that ter...
J K Grace


Annual Report 2022
2023 - IRG/WP 23-60516
IRG Secretariat


Plenary 2023 Agenda
2023 - IRG/WP 23-60517
IRG Secretariat


Revised Budget 2023 (forecast May 2023)
2023 - IRG/WP 23-60519
IRG Secretariat


Budget 2024
2023 - IRG/WP 23-60520
IRG Secretariat


IRG documents 2023
2023 - IRG/WP 23-60530
IRG Secretariat


Programme. The IRG54 Scientific Conference on Wood Protection
2023 - IRG/WP 23-60518
IRG Secretariat


In service performance of wood sound abatement barriers
2024 - IRG/WP 24-41006
Sound abatement barriers made form treated hem-fir in service near Vancouver, Canada were inspected after about 10-12 years in service. The barriers appeared in good condition and no boards were to the point of needing replacement. The sound abatement decibel readings at all locations indicate they perform as well as concrete barriers and exceed the 5 dBA regulatory requirement for noise reduction...
S Kus, D Wong, R Stirling


Effect of mobile fungicides on fungal pre-infection in radiata pine billets.
1999 - IRG/WP 99-30191
In New Zealand, fungal infection of logs begins directly after felling and whilst severe degrade can be prevented if antisapstain-treated within 24 hours, such short turn-around times of logs are not always practicable. However, conventional antisapstain formulations in use only provide an envelope of protection on the log surface but are unable to control pre-infections below the surface. The obj...
D R Eden, T Singh, B Kreber


A new technique for testing decay resistance of framing lumber
2002 - IRG/WP 02-20247
Model house frame units (two studs, top and bottom plates and a central “dwang”) were constructed using short (500-600 mm) lengths of framing timber. Constructed frames were impregnated with water using a mild pressure schedule to raise the initial moisture content to 35-40 % mc. The back face of each unit was then covered with black polyethylene. Two locations at the stud/dwang and stud/botto...
M E Hedley, D Page, B E Patterson


Efficacy of deltamethrin associated with TCMTB and MBT for the temporary protection of timbers immediately following their sawing, in tropical countries
1987 - IRG/WP 1321
K-Othrine bois 2.5 "sciage"Ò containing 2.5 g/l of deltamethrin, 50 g/l of TCMTB and 50 g/l of MBT used at a 6% dilution controls effectively during the drying process of the freshly sawn wood, the insects attacking wet wood, the staining fungi and the rots. The protection lasts 4 months. The efficacy trials carried in 1985 and 1986 in the CTFT ("Centre Technique Forestier Tropical") of Abidjan, ...
J S Duguet, V Dartigues


Moisture requirements and wood degradation of pine and spruce wood by some Basidiomycetes-fungi
1989 - IRG/WP 1406
The minimum moisture requirements for the growth of the brown rot fungi, Coniophora puteana, Gloeophyllum trabeum and Serpula lacrymans were near or above the fibre saturation point of pine and spruce, sap and heartwood, during 160 days incubation according to the standard method EN 113. The moisture of wood for the optimum growth of Coniophora puteana and Serpula lacrymans was about 35-80% and fo...
H Viitanen, A-C Ritschkoff


The past, present and future of hardwoods in North America
2024 - IRG/WP 24-50400
Abstract will be added later...
D Brooks


Annual Report 2023
2024 - IRG/WP 24-60532
IRG Secretariat


IRG documents 2023
2024 - IRG/WP 24-60546
IRG Secretariat


Programme. The IRG55 Scientific Conference on Wood Protection
2024 - IRG/WP 24-60534
IRG Secretariat


Treatability problems - Relationships between anatomy, chemical composition and treatability
2001 - IRG/WP 01-40213
This report documents the results of phase 1 and 2 of a 3-phase research program. In phase 1, two hundred and fifty-six (256) Southern pine (pinus spp.) nominal 2 x 6's (38 mm x 140 mm) from a single mill in Georgia (southeastern US) were evaluated for treatability with CCA preservative. After treatment, 128 pieces representing a broad range of treatment characteristics were selected and ...
J E Winandy, F Green III, D Keefe


Wood preservation in Kenya
2000 - IRG/WP 00-40190
Focussing an Wood Preservation in Kenya, the Report discusses and elaborates on Education and Training, Research, Wood deteriorating organisms, Treatment Plants and Processes, Preserving Chemicals, Specifications, Markets, Health and Safety and Environmental issues. Education and Research is limited to one Institution only, other Institutions involved with the properties and utilization of wood ha...
R Venkatasamy


Durability of Wood Plastic Composites Relative to Natural Weathering and Preservative Treatment With Zinc Borate
2005 - IRG/WP 05-40316
Wood-Plastic Composites (WPCs) used for decking have experienced dramatic increases in North America, averaging 25% growth per annum since 1998. A key factor contributing to this growth has been the successfully communicated message that they are "virtually maintenance free". The common perception being that the wood fiber is completely encapsulated by the thermoplastic resin, minimizing the pot...
M E Mankowski, F M Ascherl, M J Manning


Formation of soft rot cavities in relation to concentric layers in wood fibre walls
1983 - IRG/WP 1185
A large number of timber species attacked by soft rot have been examined using light microscopy. The S2 layers in a large number of the timbers exhibited special structural features in the form of thin concentric layers. Several observations indicate that these layers may be characterised as "weak" zones by being more easily degradable than the surrounding wall layers. The chemical structure of th...
T Nilsson, G F Daniel


Microbial breakdown mechanisms. Mini-Symposium at the 18th IRG meeting, Honey Harbour, Ontario, Canada
1987 - IRG/WP 1327
An understanding of how micro-organisms cause chemical alternation to wood is essential for effective wood preservation. Investigation of the Microbial Breakdown of wood is a very dynamic research field and is increasing in importance as several biocides are being examined as alternativesw to classic wood preservatives. These biocides often do not possess broad spectrum activity. It is esential th...
L E Leightley


Correlation between changes in colour and chemical composition during photo-degradation of wood surfaces
2005 - IRG/WP 05-40301
Changes in colour of wood (yellowing) during photo degradation or weathering reflect chemical changes in wood. Therefore, the relationship between changes in chemical composition and CIELAB colour parameters is very important to characterize photodegradation of lignocellulosic surfaces. In this study, the changes in chemical composition and yellowing due to photo-degradation was studied by expos...
K K Pandey


Some observations on the damage to timbers and wooden articles in cultural properties by insects in Italy
1981 - IRG/WP 1135
The damage to cultural properties by insects, especially of wooden material, is a serious problem in Italy. We have carried out a preliminary investigation concerning the most widely distributed and dangerous insects damaging timbers and wooden articles in cultural properties. Up to now the investigation has been carried out in Toscana, Lazio and Emilia Romagna and has concerned some collections o...
A Gambetta


Evaluating the natural durability of native and tropical wood species against Reticulitermes flavip
2004 - IRG/WP 04-10539
Environmental pressures to eliminate arsenate from wood preservatives has resulted in voluntary removal of CCA for residential applications in the United States. A new generation of copper organic preservatives has been formulated to replace CCA for decking and in-ground applications but there is no guarantee that these preservatives represent a permanent solution to all related problems. There...
R A Arango, F Green III, K Hintz, R B Miller


Lifetime of impels in poles maintenance cycles for utility poles
2001 - IRG/WP 01-30258
In 1992-98 15.000-20.000 utility poles in Denmark received remedial treatment against decay with fused Boron-rods (IMPEL®). Economically simple, the Impel-rods are placed with the PillarTreat Method as concentrated depots in the ground-line. From there it is distributed by diffusion through the natural moisture in the wood, which ensures that it reaches moist wood in that parts of the pole where ...
A Peylo, C G Bechgaard


Previous Page | Next Page