A novel device for detecting internal defects in wooden poles
1989 - IRG/WP 2329
The diagnosis of internal defects caused by termites and decay in hardwood transmission poles has been investigated using a novel Automatic Feed Drill (AFD) pole testing device. Internal defects were recognised by changes in drill feed-rate as the automatic air-driven drill traversed its 100 mm working stroke. The instrument is portable, simple to operate and recognises defects instantaneously. Te...
R A Eaton, R S Johnstone


Chemical evaluation of borate treated pine sapwood attacked by the subterranean termite Coptotermes acinaciformis
1993 - IRG/WP 93-20003
Sapwood of hoop (Araucaria cunninghamii Ait. ex D. Don) and slash (Pinus elliottii Englem.) pines were treated by Vacuum Pressure Impregnation (VPI) to provide test specimens. The concentration of boron was defined by chemical analyses of the timber, in the zone of primary attack by the termite being bioassayed. A common method of definition of preservative retention, weight uptake of preservative...
A R Moffat, B C Peters


An investigation of the effects of pre-steaming on the treatment of sawn spruce timber with Celcure A, a copper/chrome/arsenic preservative
1981 - IRG/WP 3180
Difficulties in the treatment of spruce using standard vacuum/pressure techniques with both water-borne and organic solvent preservatives are well known. The growth characteristics of spruces (Picea spp) make them attractive candidates for forestry schemes. In 1975 the UK Forestry Commission had about 400 000 hectares, about 20% of total UK forest area, planted with Sitka spruce (Picea sitchensis)...
C R Coggins


The use of the Shigometer® and Pilodyn® as non-destructive test methods for detecting decay in CCA treated eucalypt poles
1981 - IRG/WP 2153
The groundline condition of sixty C.C.A. treated eucalypt poles comprising six different species was examined using the Pilodyn® and Shigometer®. Although sensitive to the presence of soft-rot decay, the Shigometer® would seem to offer little practical advantage in the eucalypt soft-rot decay situation, since a comparable visual examination could reveal the presence and extent of decay. Initial...
L E Leightley


Evaluation of the pulsed-current resistance meter (Shigometer®) for determination of the internal condition of utility poles
1979 - IRG/WP 2128
A number of Telecom poles, which had been removed from service to be replaced by a radio link, were inspected using an electrical resistance meter (Shigometer®). These poles were creosoted, non-durable Victorian species in service in New South Wales. Six of these poles, chosen to represent various internal conditions typical of the range of the population tested, are discussed here. Data, from tr...
J D Thornton, W G Seaman, M McKiterick


A method for the preliminary assessment of timbers for their treatability with preservatives under pressure
1977 - IRG/WP 3100
President Maurice Fougerousse has provided the following references to a IUFRO report, published in English, French and German, which may be of interest to IRG members: 'A method for the preliminary assessment of timbers for their treatability with preservatives under pressure', PANS Vol 23, No 2, 153 158, June 1977. 'Une methode d'evaluation preliminaire de l...
M Fougerousse


Possibilities of improving the oscillating pressure method
1991 - IRG/WP 3668
Studies on the dynamics of pressure changes in wood during impregnation revealed no significant effect of fast pressure changes for green spruce as used by OPM (IRG/WP/3615). The following experiments were carried out on several hundreds of spruce palisades to examine the modification of single procedure parameters of common use OPM and to record the effects on the impregnation result with the aim...
S Goetsch, R-D Peek


Treatability of waterstored poles of Norway spruce by sap-displacement and pressure treatment with Boliden K33 and creosote
1973 - IRG/WP 328
Poles of windthrown Norway spruce were stored in bark under water sprinklers for 11-20 months or fully submerged in a lake for 3 years (tab. 1 and 2). Water content after storage is shown in fig. 1 and 8. Treatment with Boliden K33 by sap-displacement (open tank suction) gave a poor result. The Danish requirements of delivery claim a penetration of 20 mm and a net retention of 12 kg/m³ in outer 2...
P Moltesen, E Borsholt, B Bang


Boron treatment methods for lyctid susceptible hardwoods growing in Tasmania
1998 - IRG/WP 98-30168
A survey of existing boron plants that treat to protect hardwoods from attack by lyctids in Australia showed that hot and cold bath, and vacuum pressure impregnation (vpi), were the two most common methods employed. In experimental work, two of the treatment methods, vpi and dip diffusion, were used to treat seasoned and green messmate (Eucalyptus obliqua) and blackwood (Acacia melanoxylon). The t...
L J Cookson, D Scown, K McCarthy


Preservative treatment and field test monitoring of spruce pole stock: Pressure and diffusible chemical treatments
1990 - IRG/WP 3605
One hundred and forty four spruce (test species) and southern yellow pine (reference species) poles were variously treated by center boring, incising, or kerfing, followed by pressure treatment with CCA and/or diffusible preservatives. The diffusible preservatives included NaF/creosote, borax and ammonium bifluoride. The poles were set at a test site and evaluated for preservative distribution and...
B Goodell, A J Pendlebury


Discoloration of pressure impregnated wood caused by Amorphotheca resinae
1990 - IRG/WP 1438
Amorphotheca resinae Parbery with the anamorph Cladosporium resinae (Lindau) von Arx & de Vries is a cosmopolitan fungus known from aviation kerosene, hydrocarbon contaminated soil and creosoted timbers. In Denmark it causes heavy discoloration on wood treated with waterborne chromate-containing preservatives e.g. CCA-oxide type. The teleomorph produces small spherical fruitbodies widespread o...
F Rune, A P Koch


The suitability of high pressure sap-displacement for the retention of UK grown spruce and pine
1990 - IRG/WP 3595
The concentration and radial distribution of copper, chrome, arsenic (CCA), and the moisture content and depth of radial checking in UK grown, field exposed spruce and pine poles treated by high pressure sap-displacement are examined. The concentration of CCA elements in samples obtained from increment cores is similar in Norway spruce, Scots pine and Corsican pine but is significantly lower in Si...
P D Evans, S D Hainey, A Bruce, G M Smith, B King


Multiple-Phase Pressure (MPP) Process: Pilot plant trials for disposal of kickback using reverse osmosis membrane filtration
2001 - IRG/WP 01-40202
The MPP Process (a one-stage CCA treatment and accelerated fixation process) generates ~ 250 litres of kickback per cubic metre of timber treated. Composition of kickback is mainly wood sugars and traces of copper, chromium and arsenic. In pilot plant scale trials, MPP process kickback was filtered through a Reverse Osmosis (RO) membrane of a type found from earlier small-scale trials to be the mo...
H Pearson, G Durbin, M E Hedley


A study on the pressure impregnation of Eucalyptus globulus fence-posts with CCA preservatives. Part 2
1989 - IRG/WP 3514
This paper describes the second part of a study on pressure impregnation of Eucalyptus globulus fence-posts with CCA preservatives presented at the IRG 19th Meeting. Fence-posts of three diameter classes, were treated, considering only one treatment schedule. The results show possibility of vacuum-pressure impregnation of blue gum fence-posts, with diameter less than 9 cm, though mainly by longitu...
L Nunes, D De Sousa Castro Reimão


Metal Leaching from Pressure Treated Wood in Sanitary Landfill Leachate
2004 - IRG/WP 04-50220
Pressure treated wood products contain heavy metals to prevent biological decay. Scrap treated wood from construction activities and demolished structures containing treated wood are typically disposed in landfills. To examine the potential mobility of metals from pressure-treated wood disposed in landfills, wood samples were leached using leachate from lined landfills and the concentrations of ar...
B Dubey, T G Townsend, H M Solo-Gabriele


A novel solvent penetration assessment technique for wood preservativation treatments using waterborne systems
1990 - IRG/WP 2346
Solvent and hence solute (a.i.) penetration during any wood preservation treatment cycle and the flow pathways taken by the solvent in the wood are crucial elements in determining the adequacy of any treatment. Inadequate solvent penetration into specimens or an inappropriate tissue throughflow pattern during impregnation will markedly affect the distribution pattern achieved by many non-diffusibl...
A J Pendlebury, J Coetzee, E Sorfa, A Botha


Effect of kerfing on performance of Douglas-fir utility poles in the Pacific Northwest
1990 - IRG/WP 3604
Preservative treatment produces an external layer of protection in Douglas-fir poles, but the development of deep checks as the wood dries after treatment can permit entry by fungi and insects. A variety of remedial treatments can arrest this decay; however, it is far more efficient to prevent checking. Kerfing represents one potential method for limiting the development of deep checks. In previou...
J J Morrell


Penetration and distribution of styrene in pressure treated hardwoods
1997 - IRG/WP 97-40094
A styrene impregnation method was used to compare liquid distribution in several species as affected by flow direction, sapwood/heartwood, and method of impregnation. Twenty-five mm ( 1") cubes were cut from the sapwood and heartwood of red maple (Acer rubrum), white birch (Betula papyrifera), yellow poplar (Liriodendron tulipifera), trembling aspen (Populus tremuloides), red oak (Quercus rubra), ...
P A Cooper, T S Janezic, U Srinivasan, A Omidvar


The relationship between the electrical resistance and fixation of water-borne CCA salts and pressure-treated wood
1991 - IRG/WP 3657
Two investigations at 22°C and 30°C have been carried out. The electrical resistance in the treated wood and chemical analyses of the remaining amount of unfixed copper, chromium and arsenic were investigated. Samples impregnated with water were used as references. To hold the samples moist during the investigation, each sample was wrapped in a polyethylene plastic foil immediately after impregn...
F G Evans, B Nossen


Notes on a wood preservation industry in Medan, North Sumatera, Indonesia
1987 - IRG/WP 3405
This paper deals with a descriptive account on the development of a wood preservation industry in Medan, North Sumatera (Indonesia). The industry was established in 1974 when the State Owned Electicity Corporation decided to use wooden power poles for their distribution network in North Sumatera province. However, the use of wooden power poles was discontinued in 1981, so as the preservation indus...
N Supriana, A Murad


The effect of pretreatments on the impregnation of air-dried sawn Belgian spruce
1988 - IRG/WP 3490
In general the impregnation of airdried spruce results in a variable treatment and limited penetration. This is the result of pit aspiration that occurs during drying of the spruce sapwood and heartwood. Spruce timber is becoming of greater importance in Belgium and hence research for better treatment of this vulnerable wood species is needed. Squared airdried timber of different dimensions were e...
J Van Acker, M Stevens


Laboratory evaluation of copper naphthenate pressure treatments against the Formosan subterranean termite
1993 - IRG/WP 93-10005
Southern pine wafers and Douglas-fir cubes pressure treated with copper naphthenate in AWPA P9 Type A oil or in toluene were evaluated for resistance to attack by the Formosan subterranean termite, Coptotermes formosanus Shiraki (Isoptera: Rhinotermitidae). Wood samples were pressure treated to target copper retentions of 0.040, 0.075, 0.095, or 0.150 pcf, conditioned to simulate field exposure, a...
J K Grace, R T Yamamoto, P E Laks


Ability of an acoustic inspection device to detect internal voids in untreated pole sections
2002 - IRG/WP 02-20246
Detecting deterioration before substantial losses in material properties occur poses a major challenge to most wood users. While physical inspection techniques such as drilling or coring are useful, these methods can miss small pockets of damage and they lack the ability to detect early or incipient decay. The development of sonic test methodologies has created the potential for detecting change...
J J Morrell, R G Rhatigan


The difficult choice of the preservation industry when changing to more environmentally acceptable products
2000 - IRG/WP 00-50156
Until recent years the preservation industry in Norway had no problems with the environmental authorities. However, during the last three years the pressure has increased, and the authorities' solution to restrict hazardous chemicals is to introduce green (environmental) taxes for the products containing these chemicals, and also for the pressure-treated wood. The preservation industry ac...
F G Evans


Temperature and pressure inside wood during creosote impregnation
1991 - IRG/WP 3649
Creosote gives the best protection against decay for sleepers and poles. However, it has a major drawback - bleeding. Modified impregnation processes to reduce bleeding have been tried. For developing such processes it is important to know the actual temperature and pressure inside the wood. This paper describes measurement of temperature and pressure inside wood during creosote impregnation. The ...