rDNA-ITS sequence of Serpula lacrymans and other important indoor rot fungi and taxon-specific priming PCR for their detection
1999 - IRG/WP 99-10298
Taxon-specific priming polymerase chain reaction (TSPP) is a powerful molecular tool for fungal diagnosis. For its application to indoor rot fungi, the internal transcribed spacer (ITS) of the ribosomal DNA (rDNA) of the main fungal species causing wood rot in European buildings was amplified with the polymerase chain reaction (PCR). The ITS region was sequenced. The complete sequences are present...
O Schmidt, U Moreth


Evaluation of bending strength by non-destructive methods of Ezomatzu with white pocket rot
1991 - IRG/WP 2371
The possibility of application of three non-destructive methods was examined for evaluation of bending strength of ezomatsu (Picea jezoensis CARR.) with white pocket rot. As non-destructive methods, the measurements of ultrasonic wave propagation time, impact-induced stress wave propagation time and penetration depth of pin of "PILODYN Wood Tester" were applied to compare with visual evaluation of...
T Tanaka


Preservation of wood composites with zinc borate
1995 - IRG/WP 95-30074
Inorganic borates such as boric acid, borax, disodium octaborate tetrahydrate, and zinc borate can be incorporated into wood composites such as waferboard to impart decay and insect resistance to the final product. Zinc borate is especially well suited for this application due to its efficacy and leach resistance. The paper summarizes the work performed to date in this area. The effects on strengt...
P E Laks, M J Manning


The influence of causing primary blue-stain fungus Ceratocystis imperfecta on selected properties of Scots pine wood
2002 - IRG/WP 02-10425
The effects of development in wood the fungi causing blue-stain on the wood properties are not univocal. There were been undertaken investigation to clear the influence of such fungi on selected physical and mechanical properties of Scots pine wood. Wet sap wood samples of fresh cut Scots pine wood (Pinus sylvestris L.) were infested with pure culture of Ceratocystis imperfecta Mill. et Grenz and...
A Fojutowski


Mechanical properties of CCA-treated southern pine after post-treatment kiln drying
1989 - IRG/WP 3543
This report reviews current research dealing with the effects of waterborne preservative treatment and redrying on the mechanical properties of wood. In general, waterborne preservative treatments reduce average mechanical properties. This effect is exaggerated when treated wood is kiln-dried after treatment, especially at elevated temperatures. For lumber, recently completed research at the Missi...
H M Barnes, J E Winandy


Comparison of thermally modified wood originating from four industrial scale processes – durability
2002 - IRG/WP 02-40229
This study examined the differences in biological wood properties of heat treated wood originating from four different European industrial heat treatment plants. The manufacturers of heat treated material were: PLATO Hout B.V./Netherlands, Thermo Wood/Finland, New Option Wood/France and Menz Holz/Germany where Oil-Heat treated Wood (OHT) is produced. The results of miniblock tests with basidiomyc...
C R Welzbacher, A O Rapp


Physical and mechanical properties of tea (Thea sinensis L.), kanak chura (Peltophorum pterocarpum (DC.) Baker ex Heyne ) and bottle brush (Callistemon citrinus Stapf. ) - Timbers grown is Bangladesh
1999 - IRG/WP 99-40141
The physical and mechanical properties, especially the strength, density, structure, colour, natural durability, workability, seasonableness and treatability of timbers of tea (Thea sinensis), kanak chura (Peltophorum pterocarpum) and bottle brush (Callistemon citrinus) grown in Bangladesh have been found out for the first time. The tea and bottle brush are completely treatable at dry condition an...
A K Lahiry


The effect of concrete embedment on CCA treated hardwood and softwood timbers
1985 - IRG/WP 3340
Small size stakes of Eucalyptus maculata and Pinus elliottii were treated with CCA to various retentions and embedded in concrete collars containing varying amounts of a fungicide additive. During the 30 month trial period stakes were removed after 12, 18, 24 and 30 months and assessed for residual strength. Stakes which showed significant strength reductions were microscopically examined for the ...
L E Leightley, G A Willoughby


A quantitative weathering study of wood surfaces modified by chromium VI and iron III compounds
1989 - IRG/WP 2330
Thin veneers of Pinus radiata were treated with dilute aqueous solutions of chromium VI and iron III compounds and exposed to natural weathering for 35 days. Zero-span tensile strength and weight losses of treated veneers were compared with losses observed in untreated specimens In a study designed to demonstrate the applicability of strength and weight loss measurements to the rapid quantitative ...
P D Evans, K J Schmalzl


Relationship between the bending strength and the degree of termite attacks on western hemlock by Coptotermes formosanus Shiraki
1990 - IRG/WP 1434
For the examination of the relationship between the bending strength and the degree of termite attacks, Western Hemlock (Tsuga heterophylla Sarg.) was used. Sixty specimens (4.5 x 4.5 x 82 cm³) were attacked by termites at the culture room of Coptotermes formosanus Shiraki. The termites were introduced on the central parts (10 cm) of specimens. In the case of the 2 points loading, the bending mom...
K Suzuki, T Tanaka


Protection of pile tops using combinations of internal treatments and water shedding caps
1993 - IRG/WP 93-30020
Preservative treatment produces an excellent barrier against fungal, insect, and marine borer attack; however, fabricators often disrupt this barrier during construction, creating avenues for entry of decay agents. This problem is particularly acute in marinas along the coastal United States. Standards recommend the application of a water-shedding cap at the time of installation to prevent pile to...
P Schnieder, M A Newbill, J J Morrell


Tool wear for vapor boron-treated composites
2001 - IRG/WP 01-40209
A series of composites, including oriented strandboard and medium density fiberboard, were treated via vapor boron technology. Treated samples were compared to untreated composites using a tool force measuring technique. Tool forces measured with a dynamometer indicated a positive effect of boron addition. Visual and SEM examination indicated a wider wear zone on the rake face of the tool for the ...
W A Jones, H M Barnes, H A Stewart, R J Murphy


Nondestructive assessment of biodegradation in southern pine sapwood exposed to attack by natural populations of decay fungi and subterranean termites
1994 - IRG/WP 94-20042
Field methods for evaluating decay resistance of experimentally treated materials lack a means for quantitative measurement of residual strength. Quantitative relationships between speed of impact-induced waves travelling parallel to the grain and residual compressive strength have been demonstrated in softwood attacked by brown rot-decay fungi, but the effects of termites have not been documented...
R C De Groot, R J Ross, W Nelson


Studies and experiences of occurrence and development of soft rot in salt-treated poles of pine (Pinus sylvestris) installed in Swedish transmission lines in the years 1940-1945
1977 - IRG/WP 277
The present work describes the result of microscopic examinations of some 2,000 borings extracted from 20 to 23-year-old salt-treated poles (Scots pine) from the southern and central parts of Sweden. The purpose was to map out the occurrence of soft rot in Sweden and its influence on the mechanical strength of the poles as well as to contribute to the development of new and more satisfactory metho...
H Friis-Hansen


Biodetioration and strength reductions in preservative treated aspen waferboard
1983 - IRG/WP 2195
Experimental aspen waferboards, bonded with liquid or powdered phenol formaldehyde resins and treated by various methods with a wide selection of preservatives, were tested for fungal resistance in accelerated laboratory trials. Mold growth on the surface as well as weight and strength losses due to the actions of decay fungi were determined. Testing of board strength after decay in high and moder...
E L Schmidt, H J Hall, R O Gertjejansen, R C De Groot


A comparison of the diffusion of boron from two types of solid preservative rods into the heartwood of 3 Eucalypt pole species
2000 - IRG/WP 00-30227
The ability of boron to diffuse from polyborate and boron/fluoride rods through the heartwood of three eucalypt pole species (blackbutt, red ironbark and spotted gum) was examined. The aim was simply to determine the effects of rod type, wood species and time on the longitudinal diffusion of boron in eucalypt heartwood. Rapid diffusion of boron from polyborate or boron/fluoride preservative rods o...
P J Beutel, P D Evans


Three years of field tests with "Lignomer" stakes in ground contact
1981 - IRG/WP 3166
The "Lignomer" (Wood Polymer Composite) is a material obtained during the polymerisation of various monomers or its mixtures in wood. As laboratory tests have shown, this material is characterized by a high resistance against biological deteriorating agents. The laboratory investigations on the durability of various materials against biological deterioration are in many instances extended by field...
K Lutomski


Laser incising of spruce lumber for improved preservative penetration
1991 - IRG/WP 3646
Red spruce heartwood specimens were incised using a range of laser beam power levels and pulse durations. The penetration of CCA through these holes into the wood was monitored after pressure treatment. In addition, green and dried spruce samples were incised using two patterns with incision densities of either 16.1 holes/in² or 21.3 holes/in². Following CCA pressure treatment the samples were t...
B Goodell, F A Kamke, Jing Liu


Internal pressure development in Douglas fir lumber during pressure treatment
1997 - IRG/WP 97-40091
Preservative treatment of Douglas fir lumber to meet current industry standards poses a major challenge and a variety of methods have been developed to overcome these problems. One aspect for treatment improvement that has received less attention is the relative effect of treatment parameters on changes in pressure within the wood. Previous studies of spruce and radiata pine suggest that internal ...
P F Schneider, J J Morrell


Biological control of internal decay in Scots pine poles: A seven year experiment
1992 - IRG/WP 92-1529
The interactions between key fungi were monitored, by non-destructive and destructive sampling methods, during the course of an experiment on the effectiveness of Scytalidium sp. and Trichoderma spp. for eliminating established infections of Lentinus lepideus (Fr. ex Fr.) Fr. in creosoted Pinus sylvestris poles. Although extensively isolated at the beginning and end of the experiment, Trichoderma ...
P I Morris, D J Dickinson, B Calver


Changes in some important mechanical and physical properties of untreated and treated mining timber after exposure to the conditions of a colliery
1996 - IRG/WP 96-20082
Each of salt treated and untreated mining timber (wedge) pairs with 5x15 cm² cross-section and 155 cm length prepared from Scots pine, Bornmüller's fir and oriental beech was cut in the small standard test specimens to determine changes in some important mechanical and physical properties, 13 month after exposure to the conditions of Kozlu Hard Coal Mines in the depth of 52 m. Thus, the...
A Bobat


Bending strength of heat-treated spruce and pine timber
2002 - IRG/WP 02-40242
Heat-treatment of spruce (Picea abies) and pine (Pinus sylvestris) beams (45 x 145 mm) gave a reduction in bending strength of approximately 50%. The bending stiffness (modulus of elasticity) only decreased by 3.5%. Tests were carried out according to EN 408. Another effect of the heat-treatment was increased variation in bending strength. The 5th percentile value of the bending strength, the so c...
C Bengtsson, J Jermer, F Brem


Evaluation of a laboratory soft rot test on basis of weight loss and residual strength
1989 - IRG/WP 2336
Based on the principles of different previously reported experimental procedures dealing with laboratory soft rot testing, a study was conducted on treated poplar and beech. Preservatives used were CCA, CCF, AAC, Azaconazole and TCMTB. Treated samples were exposed for three months in a vermiculite substrate to Chaetomium globosum. Evaluation was based on absolute mass loss, percentage weight loss ...
W Verbeke, J Van Acker, M Stevens


A new factory applied preservative treatment for joinery
2002 - IRG/WP 02-40246
Conventional pre-treatment processes involve the principle of applying preservatives to the external surfaces of wood to achieve the necessary penetration and retention of the chemicals although the heartwood remains difficult to treat. The present development involves the production of internal reservoirs within new joinery components, which are subsequently filled with a specially developed g...
I M Robertson, W Beauford


Amine copper reaction with wood components: acidity versus copper adsorption
1997 - IRG/WP 97-30161
The bonding sites for copper in wood from CCA, as well as ammoniacal/amine based systems, has long been a topic of investigation. Both phenolic and carboxylic functional groups have been discussed as potential bonding sites for copper. However, no consensus on the adsorption mechanism has been realized. Thus, the selective adsorption of copper in southern yellow pine from ethanolamine-copper solut...
S M Thomason, E A Pasek