An aquaria test of the natural resistance against marine borers of some commercial timbers available in Australia
1996 - IRG/WP 96-10145
The natural resistance of the heartwood of 22 different timbers grown or commercially available in Australia was examined. Radiata pine sapwood both untreated, and treated with 5.4 kg/m³ CCA salt, was included for comparison. Small timber blocks were exposed for one year in tanks containing either Limnoria tripunctata or Lyrodus pedicellatus. Four softwood species tested were heavily attacked and...
L J Cookson


Restrictions on the use of chlorosilanes as potential wood preservatives
1985 - IRG/WP 3345
The biological protection of wood by chemical modification with different types of chlorosilanes has been investigated. The impregnation of wood has been carried out by means of liquid phase and vapor phase treatments using pure silane and silane-solvent systems. The biological efficacy against wood rotting fungi, molds and staining fungi was determined in a number of screening trials, subsequentl...
M Stevens


Glass splinters as physical termite barriers: Optimized material properties in use with and without insecticidal pretreatment minimizes environmental contaminations
1991 - IRG/WP 1476
The major advantage of physically acting barriers against termites using sand or cinder is to be impenetrable for a number of termite species by showing environmental compatibility in a high degree. The major disadvantage of these barriers is the ability of termites to build galleries over them. Glass or glass-like materials are showing optimum material properties: crushed to a particle size from ...
M Pallaske, A Igarashi


Evaluation of impact of CCA-treated wood on the marine environment
1995 - IRG/WP 95-50040-15
This paper reviews the literature relating to the potential of CCA-treated wood to affect the marine environment and outlines the compounds required for a model which could be used to predict the environemental impact of maritime construction using such timber. Marine pilings require high loadings of CCA to provide protection from marine borers. Though loadings of 32-48 kg/m³ provide long-term pr...
R M Albuquerque, S M Cragg


Resistance of acrylic paints on wood against growth of the rot fungus Dacrymyces stillatus
1990 - IRG/WP 2345
In the last few years the presence of the rot fungus Dacrymyces stillatus has been repeatedly confirmed in external wood panels, particularly from wood painted with water based paints. A laboratory method for testing of the fungal resistance of paint films on wood has been developed.This method has been used to test the efficacy of the fungicides Parmetol DF 18 and Parmetol HF 25 against attack by...
J Bjurman


International comparison of three field methods for assessing the in-ground resistance of preservative-treated and untreated wood to termites and fungal decay – Summary of observations after five years
2003 - IRG/WP 03-20261
Results are presented from a five-year study conducted in five locations in Australia, Thailand and the USA. Three methods of exposure were assessed (below-ground, graveyard and ground contact) for evaluating the in-ground termite and decay resistance of Pinus radiata D. Don sapwood stakes that had been vacuum pressure impregnated with CCA (Type C) and ACQ (Type D) each at two nominal retentions (...
M Lenz, J W Creffield, T A Evans, B M Kard, C Vongkaluang, Y Sornnuwat, A F Preston


A comparison of the leaching resistance of copper 2-ethanolamine and copper ethylenediamine treated Scots pine
2000 - IRG/WP 00-30233
The depletion of copper from copper 2-ethanolamine and copper ethylenediamine treated Scots pine blocks was investigated. A greater leaching resistance was found for copper 2-ethanolamine, which retained ca. 86% and ca. 50% copper after water and buffer leaching, respectively. Leached amine treated blocks also contained significant residual amine. This was consistent with other observations linked...
Xiao Jiang, J N R Ruddick


Biological resistance of electrolessly plated wood (1). Preliminary report
1994 - IRG/WP 94-40024
Surface metal coating is considered to improve biological resistance of wood as some metal ions are fungitoxic. Six wood species (three softwoods: Cryptomeria japonica, Tsuga heterophylla and Larix spp; three hardwoods: Fagus crenata, Acer mono and Betula platyphylla) were electrolessly plated with nickel or copper, and those were served for laboratory evaluation of their resistance against decay ...
M Hasegawa, K Tsunoda, T Yoshimura


Biological resistances of wood-metaborate composites using the borax solution system
2001 - IRG/WP 01-30259
Combinations of wood and metaborate composite were prepared from sapwood specimens of Japanese cedar (Cryptomeria japonica) and the borax and metallic salts system using the diffusion-penetrated process. Wood-metaborate composites were produced as follows: water-saturated specimens were first impregnated by a saturated borax solution and then diffuse-penetrated with Zn2+, Ca2+, or Pb2+ solution. B...
Liang Lin, T Furuno


Fungal decay resistance of Rubber wood treated with heartwood extract of Rosewood
2005 - IRG/WP 05-30367
Alcoholic extract of Dalbergia latifolia heartwood was studied for its toxicity towards wood decaying fungi. Rubber wood blocks were treated with this extract to three different retention levels (0.1%, 0.2% & 0.5%) and the treated wood blocks were assessed for their resistance towards two white rot and two brown rot fungi. Treated blocks showed improved resistance over the control blocks. At 0...
A K Sethy, H C Nagaveni, S Mohan, K T Chandrashekar


A real scale evaluation method and results on termite resistance of housing wall systems and floor framings
1999 - IRG/WP 99-10314
For evaluating the termite resistance of real scale houses especially housing wall systems and floor framings, a experimental building was prepared. After initial feeding of termite, this house was constructed. In this experimental building, several parts which were built by different wall systems and floor framing. The room temperature of these parts were controlled. Water can be provided in the ...
K Suzuki, K Okada, K Hagio, Y Tanaka


In situ testing the influence of melamine resins on the enzymatic activity of basidiomycetes
1999 - IRG/WP 99-30194
Waterbased methanol etherificated melamine formaldehyde resins have the potential to increase the resistance of impregnated wood against wood destroying fungi. The mechanism of the increased wood durability is not clear yet. In the present paper the possible interference of melamine resins with wood degrading enzymes of Coniophora puteana and Trametes versicolor was investigated as a possible cont...
D Lukowsky, F Büschelberger, O Schmidt


Biological degradation resistance of wood acetylated with thioacetic acid
1983 - IRG/WP 3223
Chemically, modification of wood is being considered as an alternative to conventional preservation by toxic chemicals. Acetylated wood has been reported to be quite resistant to most biodegrading organisms at weight percent gains (WPG) around 15-19. The conventional acetylation techniques with acethic anhyrdride result in generation of acetic acid. However, acetylation with thioacetic acid overco...
S Kumar, S C Agarwal


Three years of field tests with "Lignomer" stakes in ground contact
1981 - IRG/WP 3166
The "Lignomer" (Wood Polymer Composite) is a material obtained during the polymerisation of various monomers or its mixtures in wood. As laboratory tests have shown, this material is characterized by a high resistance against biological deteriorating agents. The laboratory investigations on the durability of various materials against biological deterioration are in many instances extended by field...
K Lutomski


Future insecticidal treatments for wood products
1980 - IRG/WP 3140
Protective measures involving chemical treatment of wood use only a narrow range of toxic materials which are divisible into two groups, (i) those that are water-soluble, (ii) those that are soluble only in organic solvents. It is generally true to say that, as far as protection against insects is concerned, the former are stomach poisons while the latter are largely (though not exclusively) conta...
D J Cross


Biological resistance of wood-based composites under protected, aboveground conditions
2005 - IRG/WP 05-20312
Five kinds of wood-based composites (density fiberboard=MDF, hardwood plywood=HP, softwood plywood =SP, particleboard=PB and aspen oriented strand board=OSB) were tested for their resistance against subterranean termites and decay under protected aboveground conditions. The exposure method was previously developed for evaluating performance of sill plates (dodai) in Japanese homes. Ten replicates ...
K Tsunoda


Biological resistance of furfuryl alcohol-treated wood
1992 - IRG/WP 92-3703
Biological resistance of FFA (furfuryl alcohol)-treated wood was investigated in relation to the rise of ASE (anti-swelling efficiency) resulting from the treatment. Sapwood blocks of Japanese red pine, cedar and beech were vacuum-impregnated with various concentrations of aqueous FFA solutions to get the target levels of% (w/w) RL (resin loading). Air-dried blocks were kept in an oven at 120°C f...
J Y Ryu, Y Imamura, M Takahashi


Termite resistance of treated wood in an above-ground field test
1985 - IRG/WP 2241
A field test method has been developed for evaluating the susceptibility of wood products to termites in protected situations above ground. In this method fungal attack on the wood products is minimal, though decay has been observed in conjunction with termite attack in some specimens. Preliminary results from exposure of replicate wood samples treated with preservatives in Florida to Reticuliterm...
A F Preston, P A McKaig, P J Walcheski


Durability of Sugi (Cryptomeria japonica D.DoN ) wood treated in high temperature liquid paraffin
2002 - IRG/WP 02-40221
Sugi(Cryptomeria japonica D.DoN )wood was subject to a heat treatment in high-temperature liquid paraffin for the purpose of improving the resistance against fungi and termites without chemicals. The bath of paraffin liquid, which can provide a uniform heat transfer (±2?), was used at temperatures of 90?,120?and 150?.?ecay resistance according to JIS K 15711) was evaluated using a brown rot fungu...
Y Matsuoka, W Ohmura, S Fujiwara, Y Kanagawa


The resistance of timbers to impregnation with wood preservatives
1979 - IRG/WP 3137
It is anatomical structure which determines liquid flow rate within different timber species. This cannot be deduced from properties such as density or rate of growth, and can only be found by experiment. A standard test has been in use at the Princes Risborough Laboratory for many years, employing a pressure-impregnation treatment, and a large number of timbers have been studied. The test consist...
Anonymous


Comparative study of blue stain resistance of various types of wood stains after artificial and natural weathering
1992 - IRG/WP 92-2411
For the determination of the protective effectiveness of a preservative treatment against blue stain in service, artificial weathering has been proposed as an alternative for the natural weathering period of 6 months in the European standard EN 152. Research on a range of products and on complete finishing systems for external joinery was conducted during 1986-1990. It revealed that the decisions ...
J Van Acker, M Stevens, M Nys


Termite resistance of treated wood in an above-ground field test
1986 - IRG/WP 1300
This paper provides an update on the results from an above ground field test evaluating the effectiveness of wood preservatives against subterranean termites. Results for the one and two year inspections of treated southern pine sapwood exposed in Hawaii to Coptotermes formosanus are presented. Chromated copper arsenate is providing excellent protection as is the pyrethroid deltamethrin. Borate an...
A F Preston, P A McKaig, P J Walcheski


Algal growth resistance of paints for coating of wood; a laboratory study
1997 - IRG/WP 97-10213
Twelve paints were tested for resistance against algae. In addition, one algicidal compound commercially used for remedial treatments of algal growth on paints was tested for its effectiveness for prevention of algal growth. An agar diffusion bioassay was employed in which paint films on filter paper discs were placed on mineral salt medium and sprayed with an algal suspension containing a mixture...
J Bjurman


The effect of moisture content on the electrical resistance of timber as detected by a pulsed current reistance meter (Shigometer)
1984 - IRG/WP 2212
The literature concerning the use of the Shigometer® for detecting decay in standing trees and wood poles is reviewed and the differences of opinion over the effect of timber moisture content on electrical resistance are highlighted. A simple experiment designed to test this effect is described and the implications of the results for testing poles in service are discussed. There was a large diffe...
P I Morris, D J Dickinson


Influence of the content of organic matter of soil on the degradation of wood by soft rot fungi
1970 - IRG/WP 27
The degradation of wood specimen burried in the soil by soft rot fungi is influenced by a number of factors. These are in particular the water holding capacity, water content, content of organic matter, pH, content of mineral nutritive substances etc. The results of the interlaboratory tests, carried out within the IRG/WP let presume that the intensity of wood degradation occurs proportionally inv...
O Wälchli