A light and electron microscopic study of decayed CCA-treated radiata pine (Pinus radiata) wood from a cooling tower
1994 - IRG/WP 94-10056
An inspection of an industrial cooling tower in New Zealand showed surface decay of 12 year old Pinus radiata wood panels treated with CCA preservative to a retention of around 15 kg/m³ of salt. Wood decay micromorphology typical of that caused by soft rot fungi, white rot fungi, 'stripy' and 'v-shaped' erosion bacteria and cavitation bacteria were all commonly...
A P Singh, R N Wakeling, D R Page


Resistance of painted wood to mould fungi. Part 3. The effect of weathering, wood substrate and fungicides on mould growth
1998 - IRG/WP 98-10284
The effect of 6 month outdoor weathering on the resistance of acrylate paint systems on different types of pine and spruce sapwood to mould fungi was studied. Dipping into the preservative prior to painting, a primer with and without a fungicide (propiconazole + IPBC 0.50 + 0.2%) and a topcoat with and without a fungicide (propiconazole + IPBC 0.25 + 0.12%) were combinations of the treatments stud...
H Viitanen, P Ahola


Microscopic characteristics of microbial attacks of CCA-treated radiata pine wood
1993 - IRG/WP 93-10011
Light and electron microscopic observations were made of CCA-treated radiata timbers, which had been placed in service in a vineyard soil as supporting poles and as part of a house pile, to determine the cause of their deterioration. The house pile had failed in service after between 9 and 13 years and was of particular interest because decay was more severe in deeper regions than at the surface a...
A P Singh, R N Wakeling


Use of wood-decay fungi for disposal of PCP-treated wood
1995 - IRG/WP 95-50040-33
Although PCP has been classified as a priority pollutant, PCP-treated wood products are currently allowed to be disposed of as ordinary solid (non-hazardous) wastes in the US. Non-regulated disposal of these materials is allowed because PCP concentrations in extracts from PCP-treated products such as utility poles and crossarms, determined by the Toxicity Characteristic Leaching Procedure (TCLP) h...
R T Lamar


On the effectiveness of fumigants against wood-destroying insects and fungi in wooden cultural property
1993 - IRG/WP 93-10030
Based on a survey of the history of the use of fumigants the actual agents are mentioned in relation to their biogenic effect on wood-destroying insects and fungi as well as their corrosive behavior on cultural property. Furthermore the conditions for the use of reactive fumigants in buildings are discussed. Trials to control wood-destroying insects and fungi by nitrogen and bromomethane are the m...
W Unger, A Unger


Unsuitability of the limiting dose as a criterion for assessing the toxicity of preservatives to wood-destroying fungi
1974 - IRG/WP 243
In the majority of methods for investigating preservatives for wood-destroying fungi their toxicity is assessed by determining what is called the "limiting dose". This normally denotes a range of preservative solution concentrations or retentions of dry preservative in the timber, the lower value serving to indicate the amount of preservative at which is observed the expected effect, e.g. the grow...
D A Belenkov


The probable mechanism of action of boric acid and borates as wood preservatives
1990 - IRG/WP 1450
The tetrahydroxyborate ion [B(OH)4-] acts by complexation with poly-ols and probably attacks decay fungi through extracellular substrate sequestration; intracellular substrate sequestration; enzyme inhibition; and change in membrane function. Work was carried out to investigate this further and to try to explain certain phenomena observed in the area of boron preservation. The effect of Na borate ...
J D Lloyd, D J Dickinson, R J Murphy


Poplar wood and its damages in Iran
1987 - IRG/WP 1332
In Iran poplar planting has been used for many centuries ago specially in regions without forests. It had rural uses in ancient time, but recently many fast growing poplar species have been planted and many hybrids also have been planted; the following species had been cultivated widely in Iran: Populus nigra L. var. italica, Populus alba L., Populus caspica Bornm, Populus deltoides L., Populus X....
D Parsapajouh, P Niloufari


Lethal temperature for some wood-destroying fungi with respect to eradication by heat treatment
1984 - IRG/WP 1229
The lethal heat dosis as a function of temperature and time of exposure has been tested for mycelium and for wood infested by three strains of Serpula lacrymans and by Coniophora puteana, Poria monticola, Paxillus panuoides, Gloeophyllum trabeum and Gloeophyllum sepiarium. Even for Serpula lacrymans, which is well known for its sensivity to heat treatment, 30 min at 55°C were necessary to kill th...
M Miric, H Willeitner


Analysis of D-glucose metabolism of wood decay fungi using 13C-NMR and 13C-labeled substrates
2003 - IRG/WP 03-10475
D-Glucose metabolism is thought to be important during wood decay by fungi, not only for anabolic and catabolic purposes of central metabolism, but also as a potential source of peroxide required by extracellular peroxidases. There has been some confusion in the literature as to whether this peroxide-generating activity is of the glucose 1-oxidase or pyranose 2-oxidase (glucose 2-oxidase) type wi...
T H de Koker, M D Mozuch, P J Kersten


Biodegradation of wood in wet environments: A review
1997 - IRG/WP 97-10217
Wood in wet environments is attacked and degraded by soft rot fungi and erosion and tunnelling bacteria, which are more tolerant to high moisture and reduced oxygen conditions than basidiomycetes, such as white and brown rot fungi. Since basidiomycetes are normally more aggressive and can degrade wood faster than soft rot fungi and bacteria wood in wet environments can survive longer. In fact, arc...
A P Singh, Yoon Soo Kim


A technique for assessing the preventive efficacy against decay fungi of preservative treatments applied to wood
1988 - IRG/WP 2309
A method is described in which test blocks with envelope preservative treatments can be challenged by selected test fungi previously established on an untreated feeder block. The progress of the test fungus through the treated zone is monitored using novel baits or sensors inserted in holes drilled into blocks to within predetermined distances of the face being challenged. Preliminary results show...
J K Carey, A F Bravery


Statistical evaluation of 'micro-bending' samples for classification of wood attacking fungi
1992 - IRG/WP 92-1544
Micro-specimens from both hardwood and softwood were exposed to selected species of field isolated fungi. The strength reduction and weight loss caused by these fungi were determined. A statistical procedure was then developed to classify the fungi into brown-, white-rot, or non-decay fungal categories based on these data. The procedure reveals the extent of hazard a fungus poses to wood members. ...
B Goodell, Jing Liu, A Homola, J Jellison, J Shottafer


Wood colonizing fungi as a human pathogen
1992 - IRG/WP 92-1523
Today we recognize some 174 "pathogens" among the approximately 100000 species of fungi, which cause different diseases on man. 24 fungi which are well known as wood colonizing fungi have been identified as opportunistic human pathogen. Some of them have been found on the surface of the human body, causing superficial mycoses, or cutaneous infection, like dermatophytosis or dermatomycosis. Other c...
R Benko


Isolation of soil borne bacteria and fungi from treated timber
2001 - IRG/WP 01-50174
Most research in the last few decades has focused on the development of new strategies to control biological attack and the means to quantify this. Comparatively little work has been done to examine the effect that treated timber might have on its surrounding environment. This presentation will describe a methodology that attempts to detect any changes which might occur in the soil microflora foll...
I Stephan, A Stegemann, G Heidrich


A study of the colonization of wood blocks in a laboratory unsterile soil test
1988 - IRG/WP 2318
CCA treated and untreated beech blocks were exposed to a defined horticultural loam using the method proposed for the collaborative soft rot test in the soft rot sub-group of Working Group Two. At intervals during the incubation wood samples were removed and fungal isolations were made using selective media. Fungi were identified and tested for their cellulolytic ability and their decay capacity i...
M T De Troya, S M Gray, D J Dickinson


Contribution to the knowledge of wood-rotting fungi in Brazil. Part 1: Occurrence and distribution of fungi on different substrates from the Manaus region, Amazonas State
1995 - IRG/WP 95-10096
A total of 945 spezimens of fungi were studied with regard to their distribution on ditterent substrates, abundances and economic importance. The samples came from the collection ot the Wood Pathology Laboratory of CPPF/INPA in Manaus, Brazil. Altogether, 163 spezies and 87 genera were identified. The following genera Trametes, Auricularia, Panus, Rigidoporus and Hymenochaete were represently by m...
M Aparecida de Jesus


Preservative-efficacy of boric acid-triethanol amine solution against wood-decay fungi
1994 - IRG/WP 94-30050
Laboratory preservative-efficacy tests were conducted using boric acid-triethanol amine (BTEA) solution in accordance with the JIS A 9201 (1991) test method excluding the standard weathering process. Sapwood specimens of Picea jezoensis or Fagus crenata to achieve nominal retentions of 0.40-41.2 kg/m³ of boric acid were exposed to Tyromyces palustris, Coriolus versicolor, Serpula lacrymans or Cha...
S Doi, M Mori, Y Mineki


Antifungal properties of metabolites produced by Trichoderma isolates from sawdust media of edible fungi against wood decay fungi
1994 - IRG/WP 94-10051
Trichoderma isolated from a sawdust medium of Pholiota nameko produced filtrates which had antifungal activities to four wood decay fungi tested on the agar plates. Filtrates produced from another isolate, from a sawdust medium of Lentinus edodes, had antifungal activities only to the white rot fungi, Coriolus versicolor and Pycnoporus coccineus. These results did not agree with those from earlier...
S Doi, M Mori


Studies on the resistance of DMDHEU treated wood against white-rot and brown-rot fungi
2005 - IRG/WP 05-10566
Beech wood (Fagus sylvatica) modified with the textile finishing agent 1,3 dimethylol-4,5-dihydroxyethylen urea (DMDHEU) has shown to improve durability against the white-rot fungus Trametes versicolor. In a mini-block test, the weight loss over eight weeks of incubation decreased with increasing weight percent gain (WPG) of DMDHEU. At 25% WPG, no significant weight loss was observed, while untrea...
P Verma, C Mai, A Krause, H Militz


Destaining wood sapstains caused by Ceratocystis coerulescens
1996 - IRG/WP 96-10159
Fungal sapstain does not reduce the strength of wood, but it does discolor the wood, detracting from its appearance and decreasing the value of wood and wood products. The purpose of this investigation was to assess whether wood sapstain caused by Ceratocystis coerulescens could be destained and existing growth eradicated. The hydroxyl radicals generation under optimized conditions destained the s...
S C Croan


Evaluation of chlorpyrifos and fungicides alone and in combination for control of insects and fungi in wood and wood composites
1998 - IRG/WP 98-30187
Wood composites are rapidly being adapted for use in exterior applications. The incorporation of a preservative system to prevent fungus and insect attack is necessary with most exterior composites. Research studies were reviewed pertaining to organic preservative systems based on Lentrek* insecticide wood treatment which contains the active ingredient chlorpyrifos alone and in combination with te...
M P Tolley, P E Laks, R Fears


Protection of southern pine using N,N-Napthaloylhydroxylamine: Field tests, soft-rot cellars and aquatic bioassay leach testing
1999 - IRG/WP 99-30204
Recent environmental restrictions are limiting the use of broad-spectrum biocides for wood preservation. There is an urgent need for new, sharply targeted, environmentally benign wood preservatives. N'N-Napthaloylhydroxylamine (NHA), a water-soluble calcium-precipitating agent, has been shown to inhibit decay by brown-rot and white-rot fungi in soil-block tests and prevent damage by Easte...
D M Crawford, F Green III


Fungi causing sap stain in wood
1980 - IRG/WP 199
The present paper is a revised edition of former Document No: IRG/WP/125. It contains some additions and an explanation of terminology, as was suggested at a previous meeting of the Group. The paper is a compilation based mainly on available literature. Some of my own unpublished results have been added together with other unpublished data which have been received from the Bundesanstalt für Mater...
A Käärik


Resistance of wood inorganic material composites against decay fungi and subterranean termites
1996 - IRG/WP 96-40062
Double diffusion process was applied to the treatment of small sound sapwood specimens [20(T) x 20(R) x 10(L) mm³] of Cryptomeria japonica D. Don. The specimens were consecutively dipped in the two kinds of acqueous solutions to form water insoluble deposits within the wood after an expected reaction between the solutes. Following the comparison of deposits formed and treating conditions (tempera...
K Tsunoda, T Yoshimura, M Takahashi, S Hirao, H Usui