IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 186 documents. Displaying 25 entries per page.


Screening techniques for potential wood preservative chemicals. Proceedings of a special seminar held in association with the 10th Annual Meeting of the IRG, Peebles 1978. Report No 136, 1979
1980 - IRG/WP 2138
This paper continues following issues: I. SCREENING INSECTICIDES 1) R W Berry (BRE/PRL, UK): Screen testing of insecticides for use in remedial wood preservatives. 2) D J Cross (FRI, New Zealand): Rapid screening of contact insecticides for use on forest products. 3) C R Coggins; A Forsyth; A E Glaser (Rentokil, UK): Experience in the use of indicative screening techniques for termiticides. ...
Anonymous


Comparison between two laboratory test methods for determining the effectiveness on wood preservatives against blue stain in fresh wood
1987 - IRG/WP 2289
Most of the work done on determination of the effectiveness of new formulae for treating fresh wood against blue stain have been focussed on their use in the manufacture of saw timber. This work explains two laboratory methods, one which simulates the working and climatological conditions of factories making packages for fruit and vegetables in the Spanish Levante, showing that contamination of wo...
A M Navarrete, M T De Troya


The registration of wood preservatives in Canada
1977 - IRG/WP 394
The Pest Control Products Act in Canada is a part of Federal Agricultural legislation affecting chemicals for wood protection. Other parts of Federal legislation include Canadian Fisheries Act, Fed. Food and Drug act, Environmental Contaminants Act, Clear Air Act, Navigable Waters Protection Act and the Criminal Code Section 165. Some of the main excerpts from the Pest Control Products Act are as ...
J Rak, J K Shields


Surface retentions of PCP, TCMTB and MTC obtained during a field trial of antisapstain formulations
1993 - IRG/WP 93-20002
Formulations containing NaPCP or TCMTB and MTC were included as reference products in a recent field trial of antisapstain formulations in Queensland. Retentions of these actives on the surface of treated sawn Pinus elliottii were monitored by ultrasonic solvent extraction of excised samples and analytical determination by high performance liquid chromatography. Distribution of actives with depth ...
D E Ferlazzo, M D Needham, M J Kennedy


Effectiveness of some microbiocides against the development of molds and sapstain in Pinus elliottii
1981 - IRG/WP 3169
Eleven commercial biocidal formulations were tested in the field to determine their effectiveness in protecting logs and lumber of Pinus elliottii sapwood from sap stain and molds. Among these formulations 2-(thiocyanomethylthio) benzothiazole showed the best performance in controlling both types of fungi. Potassium N-hydroxymethyl-N-methyl dithiocarbamate and the mixture potassium N-methyl dithio...
S Milano


A field trial of water repellents as anti-sapstain treatment additives
1987 - IRG/WP 3417
The assessment of water repellents as anti-sapstain treatment additives has been included in a recent FRI research programme investigating improved surface protection of New Zealand Pinus radiata. Laboratory work has shown variation in water repellent effectiveness with chemical type and subsequently a field trial was established to examine the performance of selected water repellent/anti-sapstain...
J A Drysdale, D V Plackett


Some studies on fungal deterioration of rubber wood (Hevea brasiliensis)
1980 - IRG/WP 2140
For the sreening of anti-stain chemicals trials with selected agricultural fungicides and new chemicals were carried out. Botryodiplodia theobromae, Aspergillus sp. and Penicillium sp. were used at test organisms. For testing the durability of rubber wood (Hevea brasiliensis) suitable local rotting fungi (Basidiomycetes), based on high degrading power, which may later be employed in standard tests...
A Sujan, A G Tan, M Stevens


Recent development in North American industrial wood preservation plants
1988 - IRG/WP 3467
After remaining static for many years there have been a number of changes in plant design and treating cycles in recent years. This has been particularly true in the USA where few restrictions are placed on plant treating cycles by specifications; since only results type specifications are used. It is also important to realize that the AWPA Specifications for Southern Yellow Pine only call for tre...
J F Bridges


A field test with anti-stain chemicals on sawn pine timber in Brazil
1989 - IRG/WP 3513
Field tests were carried out in São Paulo State - Brazil, to evaluate pre-treatment formulations of O-Phenyl-Phenol (OPP) based products. The Sodium Pentachlorophenate solution was used as a reference formulation. The treated test blocks were stacked in a covered shed, and in an uncovered place for air drying. The evaluation was done by measuring the percentage of stained surface on each test blo...
M B B Monteiro, S Brazolin


Artificial weathering as an aid to assessing the effectiveness of chemicals for preventing blue stain in service - a co-operative study
1984 - IRG/WP 2215
The paper reports co-operative studies carried out within Working Group II of the International Research Group on Wood Preservation to assess the effects of different artificial weathering systems on the performance of fungicides to control blue-stain in service. It has been shown that Atlas, Xenotest and Marr equipments operated according to particular standard schedules can give essentially the ...
A F Bravery, D J Dickinson


Microemulsion formulations for wood protection chemicals
1993 - IRG/WP 93-30030
A microemulsion is a thermodynamically stable oil-water dispersion system. As a formulation it provides many unique features such as water compatibility for water-insoluble chemicals, formulation stability, good bioavailability and environmental acceptance. This paper discusses the major criteria for the formulations of water-insoluble wood biocides and the comparison in properties between convent...
Bing Yu, L E Leightley


Distribution of fire retardant chemicals in kempas (Koompassia malaccensis)
1994 - IRG/WP 94-40037
Samples of Kempas (Koompassia malaccensis) heartwood were treated by vacuumpressure impregnation with solutions of monammonium phosphate, diammonium phosphate, ammonium sulphate or a borax-boric acid mixture. A commercial saltbased fire retardant formulation was also used. After slow air drying, the treated wood samples were sub-divided and zonal analysis carried out in order to determine the grad...
A R A Malek, R J Murphy


Evaluation of the effectiveness of defence anti-stain in the control of sapstain in laboratory and field tests
1990 - IRG/WP 3593
The anti-sapstain product Defence Anti-stain (DAS) has been evaluated internationally in laboratory and field tests during the years 1988 and 1989. Results of tests carried out by institutes and by own companies in countries like Indonesia, Ivory Coast, Japan, Portugal, Belgium, The Netherlands and Spain will be presented. In the several tests Defence Anti-stain showed a high fungicidal activity t...
G Rustenburg, C J Klaver


Preliminary tests on the effect of naturally occurring chemicals on termites
1983 - IRG/WP 1181
Twenty-eight naturally occurring chemicals consisting of monoterpenes, quinones and wood·extractives were tested against seven species of termite. Small pieces of filter pad and agathis wood chips measuring 5 mm by 10 mm were treated with the chemicals and exposed to the termites in polystyrene weighing bottles. Results of the tests revealed that the chemicals inhibited the feeding behaviour of t...
Nana Supriana


Special seminar on screening techniques for potential wood preservative chemicals
1978 - IRG/WP 2113
This paper continues following issues: I. SCREENING INSECTICIDES 1) R W Berry (BRE/PRL, UK): Screen testing of insecticides for use in remedial wood preservatives. 2) D J Cross (FRI, New Zealand): Rapid screening of contact insecticides for use on forest products. 3) C R Coggins; A Forsyth; A E Glaser (Rentokil, UK): Experience in the use of indicative screening techniques for termiticides. ...
Anonymous


Mobility and bioavailability of wood preservation chemicals in soil - actual field measurements
1998 - IRG/WP 98-50101-11
Wood material intended for outdoor use is often impregnated with chemicals to withstand attack from fungi and bacteria. Both inorganic and organic substances are used to protect the wood, and they are used in a toxic and bioavailable form. At wood preservation facilities severe soil contamination can be encountered due to spills and deposition of sludge, especially at old sites. Two sites, one whe...
S Andersen, G Rasmussen


Comparison of two laboratory methods for screening potential anti-sapstain chemicals
1993 - IRG/WP 93-10036
Two methods were used to screen a number of potential anti-sapstain chemicals in the laboratory. In one method miniature boards of freshly felled Scots pine sapwood were dip treated with the candidate chemical, sprayed with a suspension of stainers or moulds and incubated for five weeks. In the other method antibiotic assay discs were treated with precise quantities of chemical, plated out on malt...
S M Gray, D J Dickinson


Commercial antisapstain chemicals in New Zealand
1980 - IRG/WP 3142
Almost all sawn timber of exotic softwoods (principally Pinus radiata) and a large proportion of indigenous sawn timber receives an antisapstain chemical treatment to prevent fungal degrade during subsequent seasoning, storage, or transportation (if exported). Antisapstain chemicals are also widely used to protect freshly peeled round produce during drying. A further, specialised, use is as the fu...
J A Butcher


Industrial fixation systems: key factors, limitations and optimisation through the use of computer simulation modelling. Discussion paper
1994 - IRG/WP 94-40026
This paper briefly describes four fixation operative in the Netherlands, namely: circulating and non-circulating steam fixation cylinders, steam fixation chambers and controlled climate rooms. The general limitations of industrial practice are reviewed against the background of established fixation theory. The controlling variables, both material and process-related, for fixation processing are sp...
A J Pendlebury, M Riepen, M J Boonstra, W Gard


Bending properties of wood after its decay with Coniophora puteana and subsequent modification with selected chemicals
1999 - IRG/WP 99-40146
Mechanical properties of wood are often decreased due to decay processes caused by biotic and/or abiotic factors. Damaged wooden elements (e.g. historical structures) can be reinforced by more methods, including their modification with convenient chemicals. This paper presents influences of selected chemicals on basic bending properties (modulus of elasticity - MOE, modulus of rupture - MOR) of so...
L Reinprecht, S Varinska


Economical schedule for boron treatment of rubber wood: Pilot plant investigations
1993 - IRG/WP 93-40002
An economical treatment schedule (15 minutes initial vacuum of 85 kPa; 15 minutes pressure of 1000 kPa; 5 minutes final vacuum of 85 kPa) was arrived at for treating air-dried rubber wood (Hevea brasiliensis) in a pilot plant cylinder. Treating with 3% BAE (boric acid equivalent) solution resulted in a dry salt retention of 13.1 kg/m³. Also, the study showed that green rubber wood can be treated ...
R Gnanaharan, T K Dhamodaran


Industrial fixation of chromium based wood preservatives
1990 - IRG/WP 3630
Fixation is an abstract and non-defined process. Nevertheless it is a specified requirement in most impregnation standards. The impregnation industry is facing increased pressure to deliver fixed products and to increase the safety of the handling of impregnated products. Industrial fixation of impregnated wood can be obtained by using different methods. The purpose of the process is to transform ...
T Christensen


Review of current wood preservation in Turkey
2003 - IRG/WP 03-30315
The aim of this study was to find out the current potential of the Turkish wood preservation industry, and to make some suggestions for its further proceeding, because the forest products potential and the geographical location combined may give to the wood preservation industry in Turkey a great advantage for exportation treated wood materials to the Middle East Countries. In this study, therefo...
I Usta


Evaluation of the efficiency of industrial kiln type CCA fixation chambers
1996 - IRG/WP 96-40063
Six commercial CCA treating plants in Canada were assessed for the fixation efficiency of their hot air fixation chambers. The wood temperature was measured with thermocouples over the fixation period at different locations in the chamber and at the end of the fixation cycle, the degree of chromium fixation was determined by a boring leaching procedure. There was a great variation in the effective...
A Taylor, P A Cooper


Environmental aspects of wood preservation
1987 - IRG/WP 3406
The preservation industry employs a wide range of chemicals and processes to provide timber commodities capable of resisting biodeterioration and degradation. The public often perceives the chemicals as health hazards and treatment plants as potential threats to the environment. This paper attempts to place in proper perspective the value of wood preservation. It discusses aspects of health and sa...
H Greaves


Previous Page | Next Page