IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 482 documents. Displaying 25 entries per page.


Moisture performance testing of wood – Practical experiences
2014 - IRG/WP 14-20546
Different methods are used to characterize the moisture performance of wood and to quantify the effect of moisture loads on the resulting service life. These methods can be divided into direct and indirect methods. Furthermore they can be distinguished by characteristics like continuous or periodical measurements and measuring local or global moisture content (MC). Furthermore each measuring metho...
L Meyer, C Brischke, M Kasselmann, C Rösmann


Statistical analysis of 40 years of preservative in-ground stake testing in Australia
2014 - IRG/WP 14-20552
Wood is widely recognized as a valuable material, yet the natural durability of some wood species limits its use for certain outdoor purposes. For decades, a wide range of methods and chemicals have been developed to increase the resistance of wood against degrading microorganisms and termites. Preservative treatment has a long and widespread tradition in wood protection. Proper testing of the eff...
J Van den Bulcke, L J Cookson, I De Windt, W Li, J Van Acker


Ammoniacal Copper Zinc Arsenate Preservative Treated Wood Ties Their Performance in Testing and Track
2014 - IRG/WP 14-30636
While not a new preservative system, Ammoniacal Copper Zinc Arsenate (ACZA), had not previously been used to protect crossties. Its performance in treating difficult or refractory species of wood has been documented through its wide range of uses approved in AWPA. The establishment of appropriate testing for railroad material use was put in place and includes laboratory, field as well as commercia...
T Carey


Study of in-situ gel polymerization established by Si-O-Si framework within wood micropores
2014 - IRG/WP 14-40672
Sodium silicate was used to form Si–O–Si framework by gel process and optimize the effect of the methylolurea impregnation on poplar wood. The modifier cured within the wood micropores by in-situ gel polymerization during the kiln drying. The results showed that treated wood acquired higher mechanical strength, but lower hygroscopicity. New positions of the XRD peaks appeared which caused by s...
Zeng Bi, Qian Lang, Heyu Chen, Junwen Pu


Biocidal Products Regulation – Structure and Impact for Product Authorization and Testing in EU
2014 - IRG/WP 14-50308
Since September 2013 the Biocidal Products Regulations (BPR) has been in force in Europe. BPR replaces the Biocidal Products Directive (EC/98/8) and in some respect marks a turning point in the European legislation concerning registration of all types of biocides. BPR introduces some changes both for suppliers of active substances and for companies that produce and place biocide containing wood p...
M Klamer


Applicability of wood durability testing methods to bio-based building materials
2015 - IRG/WP 15-20561
It is well known that organic materials may be susceptible to attack from a range of fungal organisms and any bio-based material used in locations where there is the possibility of microbiological activity must be expected to be able to withstand or prevent such attack. There are a wide range of test methods and standards in place to test susceptibility although most of these test individual compo...
S F Curling, B K Stefanowski, E Mansour, G A Ormondroyd


Above ground field testing: results of experiments in Brazil after one year
2015 - IRG/WP 15-30660
After the development of new products they need to be field-tested to assess their efficacy under diverse conditions of climate, comparing them with a preservative with proven efficacy. In some testing sites, decay occurs very slowly. The solution would be to bring these tests to locations that are conducive to biodeterioration, like tropical climates. Tropical sites provide higher temperature and...
M F Natale, J M Vidal


Mould growth on spruce claddings and the effect of selected influencing factors after 4 years of outdoor testing
2015 - IRG/WP 15-30671
Norway spruce (Picea abies) is the most frequently chosen wood species as claddings in façades in Norway, and is used both coated and uncoated. The visual changes that occur during weathering can be colour changes, abrasion or wear, blistering, flaking, and even cracks in the wood or coating, but more often growth of mould and blue stain fungi is the main challenge. A field test with synchronous monitoring of relative humidity, air temperature, material temperature and wood moisture content in Norway spruce claddings has been performed in southern Norway as part of the ClimateLife project. Visual evaluation of blue stain and mould growth according to EN 927-3 was performed, and evaluation data after 46 months exposure is presented. The objectives were to study the effect of 1) environment, 2) cardinal direction and 3) colour of the coated surface on growth of blue stain and mould fungi and to study the variation in relative humidity, air temperature, wood moisture content and material temperature. After 46 months exposure, the red coating system had generally the lowest mould ratings and the uncoated claddings had the highest. Of the white coloured claddings the ones facing south had lower mould ratings than those facing north, but the opposite were found for red coloured claddings. The relative humidity was higher in front of claddings exposed northwards and in a shaded environment compared to an open environment against south. In an open environment red coloured claddings had the lowest wood moisture content and highest material temperature, and red coloured claddings against south had the highest maximum material temperature.
L Ross Gobakken, G I Vestøl


Some comments on durability testing of WPC according to EN 15534-1
2015 - IRG/WP 15-40695
The standard EN 15534-1 (2014) gives advice for broad characterization of WPC materials and products. It contains instructions for test procedures concerning different properties e.g. mechanical properties, thermal properties, as well as durability. In this paper some WPC materials from the market were tested for their resistance against brown rot. Furthermore, the water uptake and bending prope...
S Bollmus, A Gellerich, H Militz


How does the test methodology influence the outcome of durability testing of thermally modified wood
2015 - IRG/WP 15-40699
Thermally modified wood is commercially available on the European market since many years. Today, many production units with various production capacities and different modification processes exist. Industrial scale wood heat treatment processes, under the trade name of ThermoWood were developed in Finland. ThermoWood has two standard treatment classes with different target properties, namely Ther...
A Gellerich, S Bollmus, H Militz


Polyamidoamines (PAA) functionalized with siloxane fragments as potential wood preservatives
2015 - IRG/WP 15-40708
Polyamidoamines (PAAs) utilized in this research were obtained by the reaction between N,N-methyl-bis-acrylamide (MBA) and Ethanolalmine (EtA) and/or aminopropytriethoxysilane (APTES). Different combinations between them were tested as wood preservatives against fungal decay. First, in situ impregnations of PAAs, with the reagents above described in different ratio, were performed and the effectiv...
S Palanti, G Predieri, E Feci, L Bergamonti


Global survey on durability variation – on the effect of the reference species
2016 - IRG/WP 16-20573
Climate change due to anthropogenic emissions is the largest environmental challenge of our time. Forest-based value chains play an important role in reducing the accumulation of CO2 in the atmosphere. Maximizing the use of wood to tackle climate change requires improved understanding of the service life of timber products. This information can best be obtained from field testing and while there i...
R Stirling, G Alfredsen, C Brischke, I De Windt, L P Francis, E Frühwald Hansson, M Humar, J Jermer, M Klamer, M Kutnik, P Laks, I Le Bayon, S Metsä-Kortelainen, L Meyer-Veltrup, P I Morris, J Norton, T Singh, J Van Acker, J Van den Bulcke, T M Venås, H Viitanen, A H H Wong


Moisture induced risk and fungal development in various field test set-ups in and above ground
2016 - IRG/WP 16-20577
A high number of studies on the decay performance of wood in outdoor exposure have been conducted in the past. However, no testing methodology for wooden components exposed above ground reflecting the variety of different loads has been established so far. Many test protocols were modified in different ways throughout the years and results were often published in an encoded or incomplete way. This...
L Meyer-Veltrup, C Brischke


Bundle tests - Simple alternatives to standard above ground field test methods
2016 - IRG/WP 16-20581
Within this study we applied different new above ground test set ups to untreated Norway spruce (Picea abies Karst.) and Scots pine sapwood (Pinus sylvestris L.) which are frequently used as reference or control species in wood durability field tests. The overall aim of this study was to find a simple alternative method to the few standardized above ground field test methods, such as the L-joint a...
C Brischke, L Meyer-Veltrup


Modelling the performance of bio-based building materials
2016 - IRG/WP 16-20582
The ‘bio-based economy’ represents a growing area of development globally and covers a wide range of building materials including wood and wood-based products. A ‘bio-based’ material is intentionally made from substances derived from living (or once-living) organisms. In this context it means that the materials and products are made from renewable resources, with the criteria that a renewa...
C Brischke


Evaluation of field test data
2016 - IRG/WP 16-20594
The resistance against fungal decay and insect attack of wood can be highly variable, between boards and even within boards. The variability in durability is not always an issue, but for high demanding applications information about its reliability is required. This comprises the variability of outdoor performance. Durability testing in laboratory and outdoor exposures can provide a good basis to ...
F Bongers, C Brischke, J Van den Bulcke, W Gard, I De Windt, H Militz


Bacterial Degradation of Pentachlorophenol Indicated in Groundwater Undergoing Long Term In-Situ Remediation
2016 - IRG/WP 16-50318
Pentachlorophenol (PCP, Penta) is a worldwide soil and water contaminant. The pervasive use of PCP as a fungicide, herbicide, pesticide, and as preservative for wood products has led to its global distribution. It is a highly effective preventative measure for most invasive insects, bacteria, fungi, and molds, as well as an excellent wood protection treatment. This study examined a known PCP conta...
C E Stokes, H Borazjani, L Prewitt


Estimation of wood degradation determined by visual inspection, mechanical testing and DNA characterisation – report after 3 years of exposure
2016 - IRG/WP 16-30700
The influence of two separate treatments, thermal modification and alkaline copper quaternary (ACQ, Silvanolin©) treatment, on fungal decay, visual disfigurement, deterioration in mechanical properties and fungal community structure was assessed on Norway spruce (Picea abies) and compared with the performance of two naturally more resistant tree species native to North America: Douglas fir (Pseud...
N Thaler, T Martinović, M Bajc, D Finžgar, H Kraigher, A Sinha, J J Morrell, M Humar


Durability Testing of a Cattail (Typha spp.) based Insulation Material against Termite Attack
2017 - IRG/WP 17-10879
The use of insulating materials is particularly important in the construction industries, especially with regard to the use of wood and naturally occurring substances. The use and durability of natural materials as insulating materials is of keen interest to many construction experts, and continues to be a topic of intense investigation. It is generally agreed that the use of natural substances ...
M Dass, W Unger, T L Woods


Comparative studies on the durability of English oak (Quercus robur L.) under in-service, field and laboratory conditions
2017 - IRG/WP 17-10881
The durability of many wood species varies due to differences in extractive content, anatomical features, growth conditions, and not at least in dependence of the respective exposure conditions either under test or in real life applications. And so does the durability of English oak (Quercus robur L.), which has recently been considered in the revised European standard EN 350 (2016) and is now cla...
C Brischke, L Meyer-Veltrup, A Soetbeer, M Höpken, E Melcher, J Trautner


Laboratory test to determine the effect on durability of combining biobased building materials with timber in construction
2017 - IRG/WP 17-20604
The use of Structural Insulated panels is a construction approach that is seeing more abundant use and is becoming a widely available method. Preformed units are usually a composite structure which often include a range of bio-based materials such as timber, wool or straw. Traditional laboratory based wood decay tests do not take into account this combination of biobased materials and it may be po...
S F Curling, G A Ormondroyd


Bio-deterioration of Southern Pine Stakes at Geographically Different Testing Sites
2017 - IRG/WP 17-20609
Southern pine (SP) sapwood is commonly used in preparing the standardized stakes for performance testing as referenced in the American Wood Protection Association (AWPA) Book of Standards. For example, the standardized above ground test methods E16/E18 and the standardized ground contact test method E7 all use sapwood of SP as the preferred wood species for preservative performance test. In this...
Jun Zhang, J Horton


Testing of the resistance of acetylated wood against marine borers at three Italian sites
2017 - IRG/WP 17-30719
The aim of this research is the determination of resistance of acetylated wood against marine biodeterioration in use class 5 (EN 335) in temperate sea waters. The resistance of acetylated Pinus radiata (radiate pine) in solid and MDF form is compared with that of the untreated radiata pine and other untreated wood of European species such as Fagus sylvatica (European beech) Castanea sativa (chest...
S Palanti, M Faimali, D Tagliapietra, M Andrenacci, M Anichini, M Sigovini


Testing the durability of timber products above ground using the block-test method – A critical review
2018 - IRG/WP 18-20637
The block-test method for testing the durability of wood and wood products above ground is reviewed critically with respect to practical aspects, moisture loads, corresponding decay development, and the possibilities of assessing test specimens by determining the dynamic modulus of elasticity (MOEdyn) of wood. In total, 36 blocks representing different modifications of the original set-up and a wi...
C Brischke, A Gellerich, H Militz


Above-ground testing methods – review of Rotorua, New Zealand test site results after ten years
2018 - RG/WP 18-20642
A series of seven different types of above ground durability tests were initially conducted over four years to determine which type of tests would give the fastest, most consistent results. Five types of test; ground proximity, two types of decking, flat panels and double layer, were reassessed after ten years. Exposure conditions varied between tests with ground proximity producing close to groun...
D Page, T Singh


Previous Page | Next Page