IRG Documents Database and Compendium


Search and Download IRG Documents:



Between and , sort by


Displaying your search results

Your search resulted in 181 documents. Displaying 25 entries per page.


Influence of wood swelling agents on penetration and copper leaching of copper-ethanolamine based wood preservatives
2011 - IRG/WP 11-30556
Copper ethanolamine based preservatives are currently the most important solutions for impregnation of wood in ground contact in Europe. One of the issues related to those and similar water based solutions is insufficient penetration to refractory wood species like Norway spruce. In order to elucidate this issue, commercial copper ethanolamine based solution was supplemented with five different wo...
M Humar, N Thaler, B Lesar


The potential of silicone-based formulations to enhance wood properties through industrial treatment for outdoor use
2011 - IRG/WP 11-30578
High hygroscopicity is one of the main weaknesses of wood as far as its susceptibility to biodegradation, and specifically to fungal decay. New wood preservation technologies are constantly entering the wood protection market, competing with traditional, biocide-based preservation. Silicones are commercially used as hydrophobic agents on stones and concrete. They belong to the restricted number of...
F Simon, F Marchal, F Pochon, M Kutnik, I Le Bayon


Effects of nano-silver on brittleness of heat-treated solid woods
2011 - IRG/WP 11-40572
The present study is aimed at the effect of heat-treatment of normal as well as nano-silver-impregnated Populus nigra, Populus deltoides, and Fagus orientalis on brittleness. Specimens were impregnated with 200 ppm water-based solution of nano-silver particles under 3 bars in a pressure vessel using empty-cell process. For heat treatment, both nano-silver-impregnated and normal specimens were kept...
H Reza Taghiyari, B Moradi Malek, A Karimi


Supercritical impregnation of wood with siloxane
2012 - IRG/WP 12-30595
This paper describes the effect of supercritical impregnation with siloxane on the water repellency of Scots pine (Pinus sylvestris) sapwood samples. Samples were impregnated with a low amount of siloxane dissolved in supercritical carbon dioxide using isopropanol as a co-solvent. Siloxane retention (i.e. weight percent gain (WPG)) of the treated samples was 1.3 % (w/w) as found by mass balance. T...
A Kjellow, F Imsgard, J Fernandes, O Henriksen, E Klaassen, R Wagner, J Delis


Effects of nano-wollastonite impregnation on fire resistance and dimensional stability of Poplar wood
2012 - IRG/WP 12-40595
The fire-retardant properties of Nano-Wollastonite (NW) in poplar wood (Populus nigra) were determined in this study. Some physical properties such as water absorption, volumetric swelling and Anti-Swelling Efficiency (ASE) were also measured. Specimens were prepared according to the ISO 11925 standard for the fire-retarding properties, and ASTM D4446-2002 standard for the physical properties. Imp...
A Karimi, A Haghighi Poshtir, H Reza Taghiyari, Y Hamzeh, A Akbar Enayati


The Effects of Industrial-Scale Heat Treatment and Impregnation with Boron Compounds on Water Uptake and Tangential Swelling of Some Wood Species
2012 - IRG/WP 12-40599
This study evaluated the effects of boron impregnation and heat treatment on water uptake and tangential swelling of spruce (Picea orientalis), pine (Pinus nigra), beech (Fagus orientalis) and poplar (Populus deltoides) wood species. The samples (10 x 5 x 40 - tangential x radial x longitudinal cm) were impregnated with 4 % boric acid and 4 % borax according to the ASTM D-1413 standard method. Aft...
A Can, S Yildiz, Ü C Yildiz


Effect of preservative treatment on mechanical performance of round and square poles made of small diameter Scots pine
2012 - IRG/WP 12-40612
A growing proportion of harvested Scots pine (Pinus sylvestris L.) timber originates from the first or second commercial thinning stands. There is a need to find economically viable and high quality wood products that can be manufactured from this raw material. Small log volume means not only demands of increased efficiency for material handling in logistics and manufacturing processes, but also c...
V Möttönen, R Stöd, K Heikkilä, H Heräjärvi


Water absorption and desorption of non treated, pressure impregnated, and pine oil treated glulam made of small diameter Scots pine and Norway spruce
2012 - IRG/WP 12-40616
A growing proportion of harvested timber originates from the first or second commercial thinning stands in Finland, which means smaller average log volumes in comparison to final felling stands. Smaller log volume means challenging wood properties such as higher proportion of juvenile wood and sapwood. Due to these facts, products made of small diameter logs are prone to twist and check, and have ...
H Heräjärvi, V Möttönen, R Stöd


The effects of impregnation with secondary metabolite extracted from Ipe on durability of Japanese cedar and beech wood
2013 - IRG/WP 13-30618
Ipe wood is known for its high durability; it has been widely used in exterior structures that are exposed to the weather. In this paper, to increase the durability of less durable wood, Japanese cedar and beech specimens were impregnated with a secondary metabolite from Ipe. In a previous study, secondary metabolites extracted by a Soxhlet extraction method showed antifungal properties. Therefore...
T Iida, R Konuma, K Kawarada


Hygroscopicity of wood after polyethylene glycol (PEG) impregnation and/or heat treatment
2013 - IRG/WP 13-40623
The hygroscopicity of wood after polyethylene glycol (PEG) impregnation and/or heat treatment was investigated by testing the water uptake, equilibrium moisture content (EMC) at various relative humidity levels, and contact angle of the poplar wood surface. The results showed that: (1) At the first moment, the heat treatment at temperatures lower than 160 ℃ did not reduce the water uptake be...
Weiyue Xu Yuan Zhu, Jinzhen Cao


Field performance of wood impregnated with siloxanes using supercritical carbon dioxide
2013 - IRG/WP 13-40632
This paper presents preliminary results from a 13-month field test containing pine sapwood samples (Pinus sylvestris) impregnated with a mixture of siloxane and organic biocides using supercritical carbon dioxide as carrier. Samples were exposed above ground at a Danish field test site using matched non-treated sapwood controls for every treated sample. All samples were painted before exposure. Pi...
A Kjellow, F Imsgard, J Fernandes, R Wagner, J Delis


Combined effects of thermal modification and ACQ-D impregnation on properties of southern yellow pine wood
2013 - IRG/WP 13-40637
In this study, samples of southern yellow pine sapwood were first thermally modified and then treated by the alkaline copper quat-type D (ACQ-D) wood preservative. Two heating temperature (180℃ and 220℃) and two concentrations of ACQ-D solution (0.9% and 1.35%) were used in the experiments. The combined effects of thermal modification and ACQ-D on leaching performance, mechanical prope...
Wang Wang, Yuan Zhu, Jinzhen Cao


Effect of bio-resin from cashew nut shell liquid (CNSL) on decay resistance properties of wood
2013 - IRG/WP 13-40649
This study assesses the decay resistance properties of bio-resin modified wood against decay fungi of the Basidiomycota according to the EN 113 protocol. A bio-resin system was developed by ozonolysis process from cashew nut shell liquid (CNSL), a naturally occurring mixture of phenolics. Small wood blocks from sapwood of Scots pine (Pinus sylvestris), Obeche (Triplochiton scleroxylon) and Gmelina...
M Ashaduzzaman, M D Hale, V Tverezovskiy, G A Ormondroyd


Resistance to Decay Fungi of Scots Pine Impregnated with Natural and Chemical Preservatives
2014 - IRG/WP 14-30650
In this study, heart-wood and sap-wood specimens of the Scots pine which is naturally grown in Turkey were treated with natural (valex) and some chemical preservatives such as CCA - C (Copper / Chrome / Arsenic), CBA - A (Copper / Boron / Azole). The wood protective efficacies of these preservatives were investigated by means of fungi decay test (EN 113). As a result of the study it was found t...
S Yildiz, U B Şimşek


Visualization of gold/silver nanostars in wood by surface enhanced Raman spectroscopy
2014 - IRG/WP 14-30653
Nanotechnology is a fast growing up-to-date technology and ventures expeditiously in the wood preservative market. However, there is still a huge lack of understanding about the interaction and incorporation of nanoparticles (NSs) in wood. Surface-enhanced Raman scattering (SERS) offers unique advantages as an analytical tool with a high selectivity and sensitivity without matrix interference. Her...
C Geers, L Rodríguez-Lorenzo, M Placencia Peña, P Brodard, T Volkmer, B Rothen-Rutishauser, A Petri-Fink


Full-scale impregnation of wood with siloxane using supercritical carbon dioxide
2014 - IRG/WP 14-40659
Full-scale impregnation of wood with siloxane was carried out using supercritical carbon dioxide as solvent. A batch of 3530 kg of Scots pine sapwood was impregnated to a retention of approximately 1.3% siloxane. The treatment also consisted of a simultaneous impregnation with organic biocides. The performance of the wood was evaluated in terms of capillary water uptake according to a modified EN ...
A Kjellow, F Imsgard, J Fernandes, R Wagner, J Delis


Improving dimensional stability of thermally treated wood by secondary modification – potential and limitations
2014 - IRG/WP 14-40664
The potential of treating thermally modified wood with melamine resin to improve the dimensional stabilization is tested in this research. Two different boards of poplar (Populus ssp.) were cut into two halves. One half of each board was thermally modified (T1 and T2) in a commercial process, the other half was used as untreated reference material. The material was thermally modified using the vac...
G Behr, K-C Mahnert, S Bollmus, H Militz


Development of new wood treatments combining boron impregnation and thermo modification - Effect on decay and termites durability
2014 - IRG/WP 14-40666
Environmental pressures appeared in most European countries during the last decade has lead to the development of more environmentally acceptable preservation methods. In this context, wood heat treatment has been one of the most investigated alternative methods during the last years. Treated at temperatures ranging between 180 and 220°C, wood components undergo more or less important chemical mo...
S Salman, A Pétrissans, M-F Thévenon, S Dumarçay, B Pollier, P Gérardin


Functional silicones used as a potential tool for the development of non-biocidal wood treatments
2015 - IRG/WP 15-30665
The increase of wood resistance against biological agents for outdoor use is conventionally performed by deep impregnation with preservatives. However, some of the traditional wood preservatives, used for decades for wood protection and regarded as the most effective, are currently subjected to severe restrictions because of their toxicity. In fact, new preservation technologies are constantly ent...
F Lhumeau, C Delaite, F Marchal, F Pochon, M Kutnik


Characterization of biofilm formation on wood treated with vegetable oils by color-based image interpretation method
2015 - IRG/WP 15-40697
The protection of wood in order to extend its service life is an important issue nowadays. As an alternative to traditional wood coatings biofilms can be used. It is a living protective coating for the wood surface against UV and bio-degradation that has the ability to recover from local damage, such as cracks. This paper presents preliminary results of biofilm formation from an 8-month’s fie...
K Filippovych, H Huinink, L van der Ven, O C G Adan


Accelerated Weathering Performance of Impregnated Wood Samples Coated with Zinc by Means of Plasma-Assisted Particle Deposition
2016 - IRG/WP 16-30682
Many different methods are currently applied for wood protection against outdoor conditions. The most important of these is the process of impregnation with liquid substances. However, this kind of wood preservatives cannot provide a long-term protection of wooden surfaces. Weathering-resistant surfaces can be obtained by applying UV absorbing agents. In this study, the influence of zinc particles...
A Can, H Sivrikaya


The termite resistance of wood impregnated with nano-zinc oxide and nano-zinc borate dispersions
2016 - IRG/WP 16-30691
In this work, the effects of the impregnation with nano-ZnO and nano-ZnB dispersions on the termite resistance of European beech wood were investigated. Three different concentrations (namely 0.5%, 1% and 2%) of the above two materials were tested. Water leaching effect was also investigated. It was concluded that a severe effect in terms of termite workers mortality is induced by the use of both ...
C Lykidis, T de Troya, M Conde, J Galván, G Mantanis


Modifying wood with paraffin wax emulsion impregnation and thermal modification: hydrophobization effect and mechanism of the combined treatment
2016 - IRG/WP 16-40726
The aim of this study was to enhance the water repellency of wood by a combined treatment of paraffin wax emulsion (PWE) impregnation and thermal modification. Two different treating procedures were used to modify the southern pine (pinus spp.). One is first PWE impregnation and then thermal modification, another is first thermal modification and then PWE impregnation. The treated samples were imm...
Wang Wang, Jinzhen Cao, Cong Chen


Impregnation of railway sleepers - Pressure gradient and transversal penetration
2016 - IRG/WP 16-40731
Based on the possible ban of creosote in the future, the need for oil based alternative products has gained in importance. Due to possible differences in impregnation properties compared to creosote the need for re-implementing former technology is given, to determine if momentarily used impregnation processes have to be modified. The here reported tests measure the pressure gradient during the im...
M Starck, A Gellerich, H Militz


Dynamic mechanical analysis of viscoelastic properties of heat treated glycerol-impregnation poplar wood
2016 - IRG/WP 16-40732
The viscoelastic properties of glycerol-impregnated poplar wood after heat treatments at various temperatures were examined by dynamic-mechanical analysis. The spectra of storage modulus (E’) and loss tangent (tgδ) in the frequency at 10 Hz were measured at the temperature range from -100 to 300℃. Compared to no peak in E’ spectra and two relaxation processes in tanδ spectra of...
Li Yan


Previous Page | Next Page