Tropical In-Ground Durability of Structural Sarawak Hardwoods Impregnated to High Retention with CCA-salts, CCA-oxide and FCAP after 20 Years Exposure
2005 - IRG/WP 05-30384
Statistical analysis (ANOVA) was conducted on durability (termite and decay combined) rating data collected over 20 years exposure period of over 140 species of Sarawak timbers with altogether 30,000 stake specimens, at the Forest Department’s Sibu “graveyard” stake test sites from 1977. About 20 replicated stakes were pressure-treated to refusal with 10% g/ml concentration of up to 3 CCA-sa...
Wang Choon Ling, A H H Wong


Cleistanthus collinus (Roxb.) Benth. ex Hook. f. and Wrightia tinctoria (Roxb.) R. Br. -- two timbers with promising durability under marine conditions
2005 - IRG/WP 05-10552
During the course of natural durability studies on indigenous timber at Visakhapatnam harbour, two species, namely, Cleistanthus collinus (Karada) and Wrightia tinctoria (Dudhi) were found to resist marine borer attack for reasonably longer periods. The panels of C. collinus completely resisted borer attack for 9 months but became susceptible to teredinid attack thereafter. The teredinids gradua...
M V Rao, M Balaji, V Kuppusamy, K S Rao


Accidental mold/termite testing of high density fiberboard (HDF) treated with borates and N’N-naphthaloylhydroxylamine (NHA)
2003 - IRG/WP 03-10462
High density fibreboard (HDF) was made from beech and pine furnish (50:50) and treated with boric acid (0.1-3%), borax (0.1-3%) or N'-N-(1,8-naphthalyl) hydroxylamine (NHA) (0.1-1%) prior to gluing with urea formaldehyde (UF) resin in order to determine resistance to Eastern subterranean termites (Reticulitermes flavipes Kollar), the most economically important termite species in North Am...
S N Kartal, H H Burdsall Jr, F Green III


Accelerated anti-termite laboratory tests, simulation of field conditions and assessment of results for service life
1994 - IRG/WP 94-20034
Termites are one of the most serious biodegrading agents in the tropics. Though some species of termites occur in the warmer temperate regions, only a few species can withstand the rigours of colder regions. Testing of termite resistance of material is done either by field tests or by accelerated laboratory tests. Field tests, though realistic to assess service life, are elaborate, take a long tim...
P K Sen-Sarma


Termite durability of sugi (Cryptomeria japonica) heartwood kiln-dried under high-temperature process in relation to wood extractives
2005 - IRG/WP 05-10547
Termite durability of sugi heartwood samples kiln-dried under a high-temperature process were evaluated by using Reticulitermes speratus (Kolbe) as a test termite sp. The n-hexane extractives of these samples were analysed by a GC technique. The less termite durability was shown on the wood samples dried under the high-temperature process, in comparison with that of the air-dried samples. No GC-p...
S Shibutani, E Obataya, K Hanata, S Doi


Biological resistance of wood-based composites under protected, aboveground conditions
2005 - IRG/WP 05-20312
Five kinds of wood-based composites (density fiberboard=MDF, hardwood plywood=HP, softwood plywood =SP, particleboard=PB and aspen oriented strand board=OSB) were tested for their resistance against subterranean termites and decay under protected aboveground conditions. The exposure method was previously developed for evaluating performance of sill plates (dodai) in Japanese homes. Ten replicates ...
K Tsunoda


Deltamethrin effectiveness against subterranean termite attack on wood under natural conditions
1989 - IRG/WP 1407
On fighting subterranean termites on wood, out of ground contact, the synthetic pyrethroid Deltamethrin shows positive aspects such as its efficiency and low mammalian toxicity. To evaluate its performance in conditions very similar to those in service use, specimens of Pinus sp were treated with solutions of Deltamethrin diluted in "white spirits" at 0.005% (w/w) and 0.01% (w/w) and exposed in a ...
P A Zanotto


Changes in some important mechanical and physical properties of untreated and treated mining timber after exposure to the conditions of a colliery
1996 - IRG/WP 96-20082
Each of salt treated and untreated mining timber (wedge) pairs with 5x15 cm² cross-section and 155 cm length prepared from Scots pine, Bornmüller's fir and oriental beech was cut in the small standard test specimens to determine changes in some important mechanical and physical properties, 13 month after exposure to the conditions of Kozlu Hard Coal Mines in the depth of 52 m. Thus, the...
A Bobat


Gaseous preservative treatment of wood
1990 - IRG/WP 3631
A recent development in processing wood with a gaseous preservative means that dry, treated wood can be produced in under 30 hours with the benefits of product diversification, faster stock turnover and the ability to respond to short term demand. About 400,000 m³ of wood are treated each year in New Zealand with boron salts to protect from borer infestation. Traditionally this treatment is effec...
R Burton, A J Bergervoet, K Nasheri, P Vinden, D R Page


Durability of Sugi (Cryptomeria japonica D.DoN ) wood treated in high temperature liquid paraffin
2002 - IRG/WP 02-40221
Sugi(Cryptomeria japonica D.DoN )wood was subject to a heat treatment in high-temperature liquid paraffin for the purpose of improving the resistance against fungi and termites without chemicals. The bath of paraffin liquid, which can provide a uniform heat transfer (±2?), was used at temperatures of 90?,120?and 150?.?ecay resistance according to JIS K 15711) was evaluated using a brown rot fungu...
Y Matsuoka, W Ohmura, S Fujiwara, Y Kanagawa


Permeability measurements on surface layers for detecting wood with abnormally high permeability
1988 - IRG/WP 2298
Wet storage of timber during the warm period of the year may lead to an increased permeability of the wood, an undesirable phenomenon for several wood industries and also for many end-uses. Neither before nor after drying, such wood with "wet storage damage" can be visually distinguished from wood with a normal permeability. A non-destructive method for inspecting the permeability of surface layer...
J B Boutelje, G Hägglund


Experimental variations in the distribution of CCA preservative in lignin and holocellulose as a function of treating conditions (temperature, concentration, pH, species, and time)
1984 - IRG/WP 3277
The exact distributions between lignin and holocellulose and retentions on wood of copper, chromium and arsenic as a function of various sets of conditions in a 3x3x4x2 factorial experiment in which combinations of three temperatures of treatment, three CCA solution concentrations, four pH's of the initial CCA solution and two timber species, namely Pinus radiata and Eucalyptus grandis, a...
A Pizzi, E Orovan, M Singmin, A Jansen, M C Vogel


Information on a project about the conditions of admissibility of wood-protecting agents in connection with environmental protection in Poland
1974 - IRG/WP 57
Wood-protecting agents are compounds acting toxically on fungi and insects. If handled improperly or carelessly, they may exert an action harmful to health and safety of men. This action is concerning: a) workers employed at the production of wood-protecting agents; b) workers employed at the impregnation, or at the transport and handling of impregnated wood; c) inhabitants of buildings with impre...
J Wazny


The potential of high pressure pulsation processes to treat white spruce lumber with water-borne preservatives
1988 - IRG/WP 3471
Laboratory work using end sealed 4x8x46 cm³ white spruce samples has been done to explore the suitability of three variants of a 2.1 MPa pulsation process for the impregnation of white spruce with CCA. The results showed that the process improved significantly the penetration of the preservatives and reduced significantly cell collapse, when compared with the results of treatment using a 2.1 MPa ...
J P Hösli, J N R Ruddick


Effects of CCA treatment on settlement and growth of barnacles under field conditions
1998 - IRG/WP 98-50116
As part of a field experiment at seven European marine sites evaluating the effects of CCA treatments on non-target marine organisms, panels treated to nominal loadings of 12, 24 and 48 kg/m3 CCA were exposed at marine sites around the coast of Europe. Within two weeks of exposure, a heavy settlement of barnacles took place on the panels exposed intertidally in France. The intensity of settlement ...
S M Cragg, C Brown, R M Albuquerque, R A Eaton, P Goulletquer


Comparative study on the leaching of wood preservatives between natural exposure and accelerating laboratory conditions
1999 - IRG/WP 99-50134
Impregnated specimens with CCA, ACQ, and BAAC were subjected to leaching tests. Specimens of 2x2x1 cm3 in size were used for the laboratory leaching test for 10 days according to JIS K 1571. Specimens of 25x1 x1 cm3 were used for outdoor leaching test for 6 months. Total leaching amounts of boron per cm3 of specimens treated with BAAC were 325 µg in the laboratory test and 206 µg in the outdoor ...
K Yamamoto, S Motegi, A Inai


Research activities on marine wood biodeterioration in Indian waters
1992 - IRG/WP 92-4182
India has a sea coast of about 8,000 km - taking into account all islands in Arabian sea and Bay of Bengal. Considerable quantity of wood is used for jetties, piles, catamarans, coastal and fishing vessels etc. and expenditure made on all these strutures including losses involved due to damage by marine borers is considerable. Continous and rapid depletion of timber from our forests particulary at...
V V Srinivasan


Social and economocal impact of an extension of service life resulting of an adequate preventive treatment. Application to wooden components used in urban areas with a high density of population
1993 - IRG/WP 93-50001-15
Le document évalue les problèmes rencontrés en zone urbaine pour le sauvetage des constructions: coordination de la lutte, délimination des chantieres et des périmètres d'investigation, nuisances causées par les interventions, risques pour la santé, risques pour l'environnement. Coûts. Comparaison socio-économique du traitement préventif et des interventions à posteri...
A T De Lelis, G A C Lopez


The effect of high and low boron soils on foraging termite behaviour and their metabolic systems
2007 - IRG/WP 07-10602
The highest concentrations of boron are found in ground water and soils of some of the driest climate areas (arid and semi arid regions) in the world. This present study examined the various concentrations of boron levels on filter papers against the subterranean termite species Coptotermes from different provenances and different boron soil levels. The termites were presented with no-choice bioas...
B M Ahmed, J R J French, P Vinden


Comparative studies of natural durability of Japanese cedar (Cryptomeria japonica D. Don) among the geographic cultivates
2006 - IRG/WP 06-10592
Variation of natural durability of Japanese cedar (Cryptomeria japonica D. Don) (also known as Sugi) was investigated by accelerated tests for decay (Fomitopsis palustris (Berk. et Curt.) Murr.) and termite (Reticulitermes speratus Kolbe) attacks on 13 clones of Sugi trees from Kyushu-Okinawa Region (Fukuka, Ooita, Saga, Miyazaki, Kagoshima). For this purpose, 57 twenty-five years old Sugi trees o...
I Usta, K Takata, S Doi


Identification of fungi colonising coated and modified wood exposed outdoors using sequencing and T-RFLP profiling
2006 - IRG/WP 06-20326
Wood decay and staining fungi are known to colonize coated and modified wood. Rapid and reliable ways of identifying fungi on coated and modified wood may improve diagnostics and product development. In this work nine fungi growing in painted wood panels exposed outdoors at a test field in Uppsala, Sweden, were identified using sequencing and T-RFLP (Terminal Restriction Fragment Length Polymorphi...
U Råberg, J Bijelovic, C J Land, S Bardage, N Terziev


High-energy multiple impact (HEMI)-test – Part 2: A mechanical test for the detection of fungal decay
2006 - IRG/WP 06-20339
The suitability of the high-energy multiple impact (HEMI)-test for detection of early fungal decay was examined. The HEMI – test characterizes the treatment quality of thermally modified wood by stressing the treated material by thousands of impacts of pounding steel balls. This method differentiates between heat treatment intensities, which are expressed by structural changes of the wood. Simil...
C R Welzbacher, C Brischke, A O Rapp


L-joint based testing for service life prediction of exterior plywood in out of ground contact conditions
2006 - IRG/WP 06-20342
Good biological performance of several plywood types in exterior conditions is most probably related to altered wood moisture behaviour compared to solid wood. Therefore a test set up was developed, using EN 330 L-joint testing methodology, to facilitate differentiation of plywood for exterior applications. The proposed test set up is an adaptation of an accelerated L-joint method introduced by V...
J De Smet, I De Windt, J Van Acker


High-energy multiple impact (HEMI)-test – Part 1: A new tool for quality control of thermally modified timber
2006 - IRG/WP 06-20346
Thermal modification processes improve durability and dimensional stability of wood, but the strength properties, especially the dynamic ones, are compromised and need to be considered with respect to industrial quality control. Results from standard dynamic strength testing, such as impact bending tests, suffer from high variability, and therefore require a high number of replicates. To overcome ...
C Brischke, A O Rapp, C R Welzbacher


Leaching of CCA from Paraserianthus falcataria panels exposed to field conditions at Krishnapatnam harbour, Andhra Pradesh
2006 - IRG/WP 06-50241
This study assessed the leaching of copper, chrome and arsenic (CCA) from Paraserianthus falcataria (=Albizia falcataria) panels exposed to marine condition at Krishnapatnam harbour on the east coast of India. Metal loss was assessed in test panels after 6, 12, 24 and 36 months of exposure using Atomic Absorption spectrophotometer (AAS). The metal loss was found slightly higher in panels treated ...