Decay initiation in plywood, OSB and solid wood under marginal moisture conditions
2011 - IRG/WP 11-20469
Hygrothermal models are increasingly used as research tools by building scientists and and design tools by designers to simulate heat, air, vapour, and water movements within and through building envelope and even to predict the consequences in terms of mould/decay growth and metal corrosion. This work was designed to generate data on decay initiation under marginal moisture conditions to support...
Jieying Wang, P Morris


Biological and mechanical performances of particleboard panels made from maritime pine (Pinus pinaster) and glued with cornstarch-mimosa tannin-urea formaldehyde adhesive
2011 - IRG/WP 11-40542
The objective of this work was to demonstrate the utility of cornstarch-mimosa tannin-based resins designed for application as an adhesive in the particleboard production. Bond qualities of cornstarch-mimosa tannin- urea formaldehyde (UF) (10:4:86, weight ratios) resins and commercial UF resin were assessed by using an automatic bonding evaluation system, prior to production of particleboard panel...
A Moubarik, F Charrier, A Pizzi, A Allal, B Charrier


Moisture protection and performance during 5 years exposure of 19 wood coating systems on a cladding in Vienna
2011 - IRG/WP 11-40561
A cladding with vertical boards of Norway spruce (Picea abies) comprising different coating systems had been exposed to natural weathering oriented south west in Vienna for 5 years. Weathering behaviour of the boards was assessed in intervals and wood moisture content was measured over the first 22 months of exposure. The moisture protective properties of the coating systems were assessed using la...
G Grüll, I Spitaler, M Truskaller


Long term durability of the heartwood of seven common softwood species in above ground conditions
2012 - IRG/WP 12-10771
The natural durability for wood in above ground use has been evaluated based on results after 11 years of exposure in a test site situated at the Danish Technological Institute in Taastrup, Denmark. Selected results for seven common softwood species exposed horizontally are reported. The test results cover samples with direct rain exposure (use class 3 of the European standard EN335-1:2006) and sa...
E Tang Engelund, M Klamer, T Mark Venås, B Lindegaard


Influence of soil moisture, Sarawak soil types and decay types on decay susceptibility of rubberwood and kelempayan
2012 - IRG/WP 12-10780
Wood and soils are important natural resources of the land, the former widely used as structural supports in contact with the latter. Many low durability wood species exposed to soil contact has reportedly high incidence of decay failures in poorly treated and untreated materials depending on soil types, properties and soil microbial virulence. This paper probes the relationship of the main soil t...
A H.H. Wong, P K.F. Chong, J Sabang


Plywood under the scanner: linking moisture dynamics and 3D structure
2012 - IRG/WP 12-20491
Plywood is highly esteemed as a construction material. Yet, the influence of moisture on both strength and durability are important factors. Especially the dynamics of moisture desorption and absorption should be taken into account when assessing the quality of a panel, which is a fact for all panel materials. This paper therefore focuses on the monitoring of the moisture dynamics of plywood subje...
J Van den Bulcke, I De Windt, N Defoirdt, J Van Acker


Comparative studies on the moisture performance and durability of wooden facades
2012 - IRG/WP 12-20492
Wooden claddings are traditionally used in many parts of the world. Also modern structures are frequently made from timber and timber engineering panel products. However, wood has to compete with other cladding materials and its durability needs to assure sufficient functional and aesthetic service life. Besides many other factors the durability of a wooden facade is dominated by its moisture perf...
T Bornemann, C Brischke, J-M Lück


Accessibility of Wood Cell Walls to Well-defined Platinum Nanoparticles
2012 - IRG/WP 12-20494
Copper nanoparticles are found in the walls of parenchyma cells in southern pine sapwood treated with a micronised wood preservative, but they are absent from tracheid walls. Hence, we hypothesized that small nanoparticles can penetrate the walls of unlignified parenchyma cells, but are excluded from lignified tracheid walls. This paper tests this hypothesis by treating pine sapwood with an aqueou...
H Matsunaga, Y Kataoka, M Kiguchi, P D Evans


Moisture performance based wood durability testing
2012 - IRG/WP 12-20495
In the frame of a scientific cooperation within the Swedish research program ‘WoodBuild’ comparative field and laboratory durability studies have been carried out by the Technical Research Institute of Sweden SP and Leibniz University Hannover. One objective was to improve test methods as well as evaluation systems in order to facilitate the use of (field) testing for service life prediction. ...
L Meyer, C Brischke, A Pilgård


Performance of wood treated with linseed and tung oil against wood decay fungi and wetting
2012 - IRG/WP 12-30598
Most of the European wood species does not have durable wood. In order to use it in outdoor conditions nondurable material has to be protected. Nowadays, non-biocidal solutions for wood protection are attracting a lot of attention, particularly in use class 2 and 3 applications. One of the non-biocidal techniques is treatment of wood with water repellents like wax emulsions and oils. Linseed oil a...
M Humar, B Lesar


Effects of Nano-Zycosil on Liquid and Gas Permeability of MDF
2012 - IRG/WP 12-40578
Effects were studied of zycosil nanoparticles, with size range from 30 to 90 nm, on liquid and gas permeability of medium density fiberboard. 100 g of nanozycosil was added to each kg of dry fibers. Density was kept constant at 0.67 g/cm3. The obtained results indicated that addition of zycosil to the mat resulted in a significant increase in gas permeability due to the lower fiber-content in the ...
H Reza Taghiyari, K Heidarhaee, P Noori, A Karimi


The effect of press time on springback and water absorption of acetylated particleboard
2012 - IRG/WP 12-40579
In this study the effect of press time on springback, thickness swelling and water absorption was investigated. After 24 hours soaking in acetic anhydride, in order to achieving WPG 17%, acetylated particles were heated in an oven at 120 0C for 360 minutes. Acetylated and nonacetylated (control) particleboards were produced with 10% melamine urea formaldehyde (based on the oven-dry weight of part...
F Bavaneghi, M Ghorbani, A Kargarfard


Influence of heat treatment intensity on the structural integrity of 14 timber species
2012 - IRG/WP 12-40586
Thermally modified timber (TMT) is characterized by improved durability and dimensionally stability, but strength properties, especially the dynamic ones, are compromised at the same time. Because dynamic standard tests require high efforts and time, the high-energy multiple impact (HEMI) –test was developed for the fast and reliable characterisation of the structural integrity of TMT, showing a...
C R Welzbacher, C Brischke, G Maier


Relationships between heat treatment intensity and some conferred properties of different European softwood and hardwood species
2012 - IRG/WP 12-40593
Effect of treatment intensity on conferred properties like elemental composition, durability, anti swelling efficiency (ASE) and equilibrium moisture content (EMC) of different European softwood and hardwood species subjected to mild pyrolysis at 230°C under nitrogen for different durations has been investigated. Independently of the wood species studied, elemental composition is strongly correl...
M Chaouch, S Dumarçay, A Pétrissans, M Pétrissans, P Gérardin


Field-testing of Norway Spruce Claddings with Monitoring of Moisture Content, Material Temperature and Microclimate
2012 - IRG/WP 12-20502
The physical function of a cladding is to protect the interior construction. Under normal circumstances the performance requirements can be met for a very long time, meaning that the technical service life of a wooden cladding can be very long. Since the cladding is a major part of the facade, it also has visual requirements that may define the aesthetic service life, and often it is much shorter ...
G I Vestøl, L Ross Gobakken


The effect on moisture content of water trapped in wood joints
2012 - IRG/WP 12-40613
To predict the service life of a structure, a model where the exposure of a structure is compared to its resistance can be used. Which exposure and resistance parameters that are relevant depend on which materials the structure consist of. This approach, with an exposure and a resistance parameter, is similar to the one used in structural engineering where a load (exposure) is compared to the bear...
M Fredriksson, L Wadsö, P Johansson


High-throughput sequencing highlighted contrasted pioneer fungal communities associated to coniferous and deciduous wood preservation assays
2013 - IRG/WP 13-10800
Studying the fungal communities in the wood, in particular during the first events of the colonization, and the factors that underlie the dynamics of fungal species assemblages remain a challenge in ecology, because of the absence of fructification during the pioneer steps of wood degradation. The use of Next-generation DNA sequencing methods, which produce massive volumes of data, provided new pe...
Y Mathieu, A Dassé, I Le Bayon, M Kutnik, L Harvengt, E Gelhaye, M Buée


The influence of microclimate on the moisture conditions in a Norway spruce (Picea abies (L.) Karst.) joint exposed to artificial rain
2013 - IRG/WP 13-20505
Wood structures outdoors are susceptible to decay if they are exposed to high moisture contents during long periods of time. Structures with joints that act as water traps are especially exposed since high moisture contents are reached in such positions. This paper presents a part of a laboratory study that concerns the relationship between the microclimate and the material climate, i.e. the moist...
M Fredriksson, L Wadsö, P Johansson


Testing the performance of timber using 27 different field test methods
2013 - IRG/WP 13-20517
Numerous test methods to determine the durability of timber and timber products have been described in relevant literature. However, only some of these methods have been standardized and thus only very few are regularly used for resistance tests in the field. Since results from extensive comparative field studies have shown differences in moisture performance between different test methods, the ai...
L Meyer, C Brischke, J Rieken


Climatic impacts on the moisture performance of wooden decking and facades
2013 - IRG/WP 13-20518
In outdoor usage wood is exposed to a variety of influences, which reduce its durability against biological deterioration and wetting. Besides many other factors the service life of wooden facades and cladding is dominated by occurring moisture loads on the one hand and their capability to withstand moisture on the other hand. Hence, climatic factors have a direct impact on the material climate an...
T Bornemann, C Brischke, G Alfredsen


Predicting the Rate of Decay, and the Potential for Misinterpretation of Proper Scientific Method
2013 - IRG/WP 13-20525
Predicting the rate of fungal attack in wood-based materials and its effect on properties remains the holy grail of wood products pathologists; however, achieving this goal is difficult because of the many variables associated with the process. This paper reviews some of the more important aspects of the decay process in relation to test methodology and then discusses how data are sometimes used b...
B S Goodell, J J Morrell


Method for determining the critical moisture level for mould growth on building materials
2013 - IRG/WP 13-20530
The natural conditions of relative humidity (RH) and temperature (T) in different parts of a building is rarely constant over time. Instead, RH and T often vary cyclically and may pose a risk of mould growth as these conditions are the two key environmental parameters that controls mould growth. Consideration to both humidity and temperature conditions and the susceptibility to mould in a material...
A Ekstrand-Tobin, P Johansson, G Bok


Moisture distribution in glulam beams with natural cracks observed with CT Scanning before and after rain
2013 - IRG/WP 13-20534
The way cracks in outdoor wooden constructions affect durability is an interesting topic, since a certain amount of cracks can always be found naturally in wood and glued laminated wood. The question in this was, can cracks lead water into the wood and thereby increase the risk for decay and reduce strength and service life. Moisture balance, i.e., water absorption and water distribution were stud...
K Sandberg


System treatments of Pinus sylvestris - influence on moisture, decay and discoloration
2013 - IRG/WP 13-30612
Biological activity can cause challenges for the use of wood in outdoor exposure. Decay and discolouring fungi influence the service life of wooden constructions, and the moisture content of the wood is often an important factor. The aim of this study was to evaluate the performance of different combinations of preservative/modified wood protection treatments and surface treatments for wooden deck...
A Schabacker, G Alfredsen, L Ross Gobakken, H Militz, P O Flæte


The resistance of high performance acetylated wood to attack by wood-destroying fungi and termites
2013 - IRG/WP 13-40621
The resistance of high acetyl solid timber (Accoya) and medium density fibreboard (Tricoya) to attack by wood-destroying fungi and termites was investigated under both laboratory and field conditions. Laboratory studies were conducted in Japan, New Zealand and USA. Field studies were conducted in Australia, Japan, New Zealand, Thailand and UK. The results of the laboratory and field studies agains...