Soft rot test of copper/chrome/arsenic treated heartwood of three Malaysian timbers by the vermiculite-burial method. (+ correction document of 25 July 1990)
1990 - IRG/WP 2354
Heartwood of copper-chrome-arsenic (CCA) treated kempas (Koompassia malaccensis), tualang (Koompassia excelsa) and keruing (Dipterocarpus spec.) was found to be susceptible to soft rot in recent pole surveys. Standardized heartwood blocks were impregnated with 0 to 6.3% (w/v) CCA and challenged to decay for twelve weeks by a mixed inocula of Chaetomium globosum, Glenospora graphii, Humicula grisea...
R-D Peek, A H H Wong


Distribution of boron from fused borate rods in Douglas-fir transmission poles
1996 - IRG/WP 96-30112
The diffusion of boron from fused borate rods (disodium octaborate tetrachydrate) was monitored over 42 months in CCA-treated Douglas-fir transmission poles. The boric acid equivalent was estimated by the curcumin/salicylic acid color test on increment cores removed from the poles. Moisture content of the poles was quite variable but was always above 20 percent. The percent of increment core lengt...
T L Highley, F Green III, W F Finney


The effect of Tween 80 on the growth, morphology, and enzyme secretion of Postia placenta
1990 - IRG/WP 1456
The nonionic surfactant Tween 80 (polyethylene oxide sorbitan mono-oleate) has been reported to increase enzyme production and/or secretion in bacteria and fungi. Such a procedure could greatly facilitate research into the physiology of wood-decay fungi since quantities of available enzyme are often limiting. The brown-rot fungus Postia placenta was grown in a synthetic medium supplemented with 0,...
J A Micales


Multiple-Phase Pressure (MPP) Process: One-stage CCA treatment and accelerated fixation process. 4. MPP compared with other processes for achieving acceptable treatment of radiata pine heartwood
1998 - IRG/WP 98-40115
Although radiata pine sapwood is very amenable to preservative treatment, it is often difficult to achieve the required standard for heartwood treatment. A preliminary investigation showed that to achieve the NZ Timber Preservation Council minimum penetration requirements for radiata pine heartwood using the Multiple-Phase Pressure (MPP) Process, a hydraulic pressure of at least 1250 kPa for 20 m...
K Nasheri, J A Drysdale, G Durbin, M E Hedley


Exposure of preservative treated wood to terrestrial microcosms, pure cultures of fungi and in the field
1997 - IRG/WP 97-20114
Small stakes (5x10x100 mm3) of treated and untreated Pinus sylvestris sapwood were exposed in terrestrial microcosms with different soils, two taken from test fields in Sweden, one soil from a conifer forest and one garden compost soil. Stakes of the same size were also exposed to pure cultures of the brown and white rot fungi, Postia placenta and Phanerochaete chrysosporium. After exposure, weigh...
M-L Edlund


The influence of fungal species and the level of decay on the mortality and feeding activity of adult Euophryum confine (Broun)
2002 - IRG/WP 02-10448
The mortality and feeding activity of adult Euophryum confine (Broun) (Coleoptera: Curculionidae) are used to establish the substrate conditions most suitable for their rearing. Weevils were allowed to feed on Pinus nigra (Arnold) sapwood blocks, either undecayed or decayed to 10% weight loss ±5% by two brown rots Coniophora puteana (Schum.:Fr.) Karst. and Serpula lacrymans (Wulf.:Fr.) Schroeter...
M Green, A J Pitman


Treatment groups and remedies for CCA treated hardwood and softwood poles
1999 - IRG/WP 99-40142
Different hardwood and softwood species from Bangladesh and Bhutan was investigated regarding density, green fiber stress, natural durability of heartwood and CCA treated sapwood, CCA treatability grades, sapwood thickness, and kiln-drying properties for long term use as electric poles. These properties along with the past service records for nineteen years, separated ten heardwood and five softwo...
A K Lahiry


The development of soft rot decay in bamboo fibres
1992 - IRG/WP 92-1572
The development of decay by soft rot fungus Chaetomium globosum was investigated in young and mature culms of bamboo Phyllostachys virideglaucescens. Soft rot decay was influenced both quantitatively and qualitatively by the differing levels of lignification in the material. Weight loss was significantly greater in the younger culm compared with the older, more heavily lignified culm. The distribu...
O Sulaiman, R J Murphy


Potential toxicants for controlling soft rot in preservative treated hardwoods. Part 2: Laboratory screening tests using sawdust
1977 - IRG/WP 2101
A technique is described for the rapid screening of toxicants against microorganisms, represented by the brown rot, Gloeophyllum trabeum, and a natural inoculum from soft rotted wood. Sawdust, in this case from sapwood of Eucalyptus maculata, is pretreated with the candidate formulation and moistened before inoculation. Visual scoring of growth can be used to discriminate suitable candidates as ea...
J D Thornton


Screening of fungal strains for wood extractive degradation
1998 - IRG/WP 98-10254
Fungal strains were screened for their ability to degrade apolar extractives in wood from scots pine. The degradation of total wood extractives by 91 different strains was monitored in stationary batch assays incubated for 6 weeks. The results obtained show that the ability of wood-inhabiting fungi to utilize wood extractives varied greatly, even for different isolates of the same species. Fungal ...
J Dorado, M J Martinez-Inigo, T A van Beek, F W Claassen, J B P A Wijnberg, R Sierra-Alvarez


Differential retention and leaching of CCA (C) in sapwood and heartwood of Kenyan-grown blue gum (Eucalyptus saligna) and black wattle (Acacia mearnsii)
2005 - IRG/WP 05-30371
Retention and leaching of CCA(C) in small samples of sapwood and heartwood of Kenyan-grown blue gum (Eucalyptus saligna) and black wattle (Acacia mearnsii) were tested under laboratory conditions. Clear samples (100mm x 30mm x 40mm) were removed from the sapwood and heartwood of sampled defect-free and sound plantation trees of the two species. These were separately air-dried to 15% MC, end-seal...
R Venkatasamy


The effect of stilbenes on decay fungi of birch and aspen
2000 - IRG/WP 00-10364
Fourteen species of decay fungi, mainly species growing on birch and aspen, one leaf spot fungus of birch and the pine canker fungus Gremmeniella abietina were used to investigate how the stilbenes resveratrol and pinosylvin influence their relative growth on malt agar. With some species the ability to decay with stilbenes impregnated wood was also studied. The concentration of pinosylvin needed t...
L Syrjälä, K Von Weissenberg, A Pappinen, L Paajanen


Dominant genera of fungi isolated from the surfaces of Sugi (Cryptomeria japonica D. Don) heartwood lumbers exposed at six test sites from northern to southern regions of Japanese islands
1999 - IRG/WP 99-10304
The surfaces of wood materials are disintegrated not only by sunlight and rainwater but also by microbes when exposed above ground condition. This paper deals with the investigation of fungi isolated from the surfaces of Sugi heartwood lumbers (W100 by T10 by L300 mm) exposed at an angle of 45° without ground contact for 16 months at the six test sites from northern to southern regions of Japan. ...
S Doi, M Mori, M Kiguchi, Y Imamura, M Hasegawa, S Morita, S Nakamra, Y Kadegaru


Preservation of coppice wood for the fabrication of glued beams or panels
1987 - IRG/WP 3427
In this survey we will examine the specific problems concerning the conservation and the preservation of timber (issued from trunks of small diameter corresponding to products of clearings or coppices) destined for the fabrication of solid reconstituted elements. Thus for six metropolitan species of wood, we first characterized the biological deteriorations which occur after felling and their kine...
G R Y Déon, R Schwartz


The movement of iron into field test stakes
1987 - IRG/WP 2284
Failed and sacrificial stakes recovered from the Westham Island field test site were examined for their iron content. Varying amounts were recorded, which were greatest in the failed stakes. The possible role of the iron taken up by the below ground portion of the stakes, in accelerating the decay process and/or the preservative leaching is under investigation. The reaction of the iron with the ch...
J N R Ruddick, P I Morris


Preliminary investigation on the natural durability of Guayule (Parthenium argentatum)-based wood products
2000 - IRG/WP 00-40154
Conventional preservatives used to protect wood from insect and microbial damages are presently of major concern to human health and the environment. Finding alternative and economical preservatives has not been successful. Previous studies have shown that the resinous material extracted from the guayule plant (Parthenium argentatum, Gray) has both insect- and microbial-resistant properties. Unfor...
F S Nakayama, P Chow, D S Bajwa, J A Youngquist, J H Muehl, A M Krzysik


Preliminary evaluation of new quaternary ammonia compound, didecyl dimethyl ammonium tetrafluoroborate for preventing fungal decay and termite attack
2005 - IRG/WP 05-30375
This study evaluates the decay and termite resistance of wood treated with didecyl dimethyl ammonium tetrafluoroborate (DBF), a recently developed quaternary ammonia compound containing boron. DBF contains boric tetrafluoride as a counter ion in its chemical structure. Laboratory decay resistance tests were performed using brown-rot fungus, Fomitopsis palustris and white-rot fungus, Trametes versi...
S N Kartal, W J Hwang, Y Imamura


Micromorphological and chemical changes of archaeological woods from wrecked ship's timbers
1987 - IRG/WP 4136
Micromorphological and chemical alterations of sea-waterlogged woods obtained from the ship-wrecked materials which had been submerged in Yellow Sea for over 700 years were investigated. The woods were deteriorated in varying degrees by marine organisms depending on species and parts of the woods. Under the light and scanning electron microscope the morphological characteristics of deteriorated wo...
Y S Kim


Studies in an accelerated soil bed facility on the decay susceptibility of U.K. grown spruce and pine poles treated with copper/chrome/arsenic (CCA) by pressurised sap-displacement. Part 1: Setting up of soil beds and initial soft rot results
1990 - IRG/WP 2344
The paper describes the methodology used in the construction and early operation of an accelerated soil bed facility used to examine the decay susceptibility of U.K. grown Scots and Corsican pine and Sitka and Norway spruce treated with C.C.A. by high pressure sap-displacememt. The design and control of the facility as well as the preparation, soil exposure and soft rot decay analysis of quarter p...
A Bruce, S D Hainey, G M Smith, B King, P D Evans


The ground proximity decay test method
2000 - IRG/WP 00-20205
A decay field test method, which has been recently proposed for the standardization by the AWPA, is described for evaluating the relative performance of wood samples in a severe above ground situation exposed to the weather. Data is presented on the relative performance of untreated control samples and standard preservative systems exposed at the same site at different time periods, or at differen...
A F Preston, P J Walcheski, K J Archer, A R Zahora, L Jin


A technique for determining the efficacy of water diffusible preservative plugs for implanting in joinery in service
1987 - IRG/WP 2291
A technique is described for determining the efficacy of soluble, diffusible preservative plugs for eradicating decay in joinery. It uses blocks of Scots pine sapwood or heartwood adjusted to known moisture contents prior to the establishment of the test fungus Coniophora puteana, from a single longitudinal dowel and the subsequent introduction of the preservative plugs. Prevention of decay, eradi...
J K Carey, A F Bravery


Durability of Sugi (Cryptomeria japonica D.DoN ) wood treated in high temperature liquid paraffin
2002 - IRG/WP 02-40221
Sugi(Cryptomeria japonica D.DoN )wood was subject to a heat treatment in high-temperature liquid paraffin for the purpose of improving the resistance against fungi and termites without chemicals. The bath of paraffin liquid, which can provide a uniform heat transfer (±2?), was used at temperatures of 90?,120?and 150?.?ecay resistance according to JIS K 15711) was evaluated using a brown rot fungu...
Y Matsuoka, W Ohmura, S Fujiwara, Y Kanagawa


The resistance of timbers to impregnation with wood preservatives
1979 - IRG/WP 3137
It is anatomical structure which determines liquid flow rate within different timber species. This cannot be deduced from properties such as density or rate of growth, and can only be found by experiment. A standard test has been in use at the Princes Risborough Laboratory for many years, employing a pressure-impregnation treatment, and a large number of timbers have been studied. The test consist...
Anonymous


An analysis of the effects of some factors on the natural durability of pine (Pinus sylvestris L.) and spruce (Picea abies Karst.)
1986 - IRG/WP 1279
The effects of some factors on the natural resistance of pine and spruce sapwood against fungal decay and against attack of house-longhorn beetle larvae have been studied in laboratory tests and the results are evaluated by analysis of variance and regression analysis. Following conclusions were reached: Wood from summer-felled trees did not have a lower inherent natural durability against fungal ...
J B Boutelje, T Nilsson, S Rasmussen


Defining fungal decay types - A proposal for discussion
1985 - IRG/WP 1264
The present definitions of the fungal decay types, white rot, brown rot, and soft rot are somewhat vague. The definitions are based on a mixture of criteria involving morphological and chemical aspects of decay as well as taxonomic affiliation of the responsible fungal species. The present vague definitions have led some fungi being erroneously places in a wrong decay type. Furthermore, some fungi...
T Nilsson


Previous Page | Next Page